  • In this study, the effect of additions on magnetic properties in the system of [$Ni_{0.32}Zn_{0.68}$] 1-x Mx $Fe_2O_4$ have been investigated. The additions, Co or Mg or Cu, was added in turn in place of M, and its composition was varied from 0.1 mo1% to 0.5 mo1%. The materials were blended by hot petroleum drying method, and sintered with the rate of 30$0^{\circ}C$/h in the air. The sintering temperatures were varied from 110$0^{\circ}C$ to 130$0^{\circ}C$, with the intervals of 5$0^{\circ}C$, and matured for 3hrs. The results are: 1) The permeability decreased when the addition, MgO or CoO, was added, and it increased when CuO was added. 2) Resistivity had the lowest Value when CuO was added.

  • PDF

An LTCC Inductor Embedding NiZn Ferrite and Its Application (NiZn 페라이트를 내장한 LTCC 인덕터 개발 및 응용)

  • Won, Yu-June;Kim, Hee-Jun
    • Proceedings of the KIEE Conference
    • /
    • 2006.07b
    • /
    • pp.939-940
    • /
    • 2006
  • An integrated inductor using the low-temperature co-fired ceramics(LTCC ) technology for low-power electronics was fabricated. In the inductor NiZn ferrite sheet(${\mu}_r=230$), was embedded to increase inductance. The inductor has Ag spiral coil with 14 turns($7turns{\times}2layers$), a dimension of 0.6mm in width, 10um in thickness, and 0.15mm pitch. To evaluate the inductance, including the parasitic resistance, the fabricated inductor was calculated and measured. It was confirmed that calculated values were very close to the measured values. Finally as an application of the LTCC integrated inductor to low power electronic circuits, a LTCC buck DC/DC converter with 1W output power and up to 0.5MHz switching frequency using the inductor fabricated was develop.

  • PDF

Physical Properties of Polycrystalline Zinc-Substituted Lithium Ferrite (ZnO가 Lithium ferrite의 물리적 특성에 미치는 영향에 관한 연구)

  • 고재귀
    • Journal of the Korean Magnetics Society
    • /
    • v.9 no.5
    • /
    • pp.234-238
    • /
    • 1999
  • Lithium ferrites are prominent in the element of microwave frequency communication core and high frequency memory core because of their low coercivity and the high squareness ratio. This paper reports primarily the development of lithium ferrites with the low coercivity and high squareness ratio. The materials with $Li_{0.48-0.5x}Bi_{0.02}Ni_{0.04}Zn_xFe_{2.46-0.5x}O_4$ (x = 0,0.01, 0.02, 0.03) have been prepared to investigate the physical properties. The addition of ZnO gave raised maximum induction $(B_m)$ and decreased coercive force $(H_c)$, but the squareness ratio $(R\;=\;B_m/B_r)$ was decreased. The specimen of squareness ratio R=0.82, coercive force $H_c=\;1.80\;Oe$ was obtained for $Li_{0.48-0.5x}Bi_{0.02}Ni_{0.04}Zn_xFe_{2.46-0.5x}O_4$ (X=0) sintered at 105$0^{\circ}C$. Also the sample of squareness ratio R = 0.75, coercive force $H_c=\;1.70\;Oe$ for $Li_{0.48-0.5x}Bi_{0.02}Ni_{0.04}Zn_xFe_{2.46-0.5x}O_4$ (X = 0) sintered at 110$0^{\circ}C$ was measured. The Tc was obtained 463$^{\circ}C$ and the Br of environmental temperature variation was stable.

  • PDF

A Study on Synthesis and Magnetic Properties of Soft Magnetic Materials Sintered at Low Temperature (저온 소결용 연자성 물질의 합성 및 자기적 특성 연구)

  • Koh Jae Gu
    • Resources Recycling
    • /
    • v.12 no.6
    • /
    • pp.13-18
    • /
    • 2003
  • The initial NiCuZn synthetic ferrite were acquired from thermally decomposing the metal nitrates Fe($NO_3$)$_3$$9H_2$O, Zn($NO_3$)$_2$$6H_2$O, Ni($NO_3$3)$_2$$6H_2$O and Cu(NO$_3$)$_2$$3H_2$O at 1$50^{\circ}C$ for 24 hours and was calcined at $500^{\circ}C$. Each of those was pulverized for 3 and 9 hours in a steel ball mill and was sintered between $700^{\circ}C$ and $1,000^{\circ}C$ for 1 hour, and then their microstructures and magnetic properties were examined. We could make the initial specimens chemically bonded in liquid at the temperature as low as $150 ^{\circ}C$, by using the melting points less than $ 200^{\circ}C$ of the metal nitrates instead of the mechanical ball milling, then narrowed a distance between the particles into a molecular level, and thus lowed sintering temperature by at least $200 ^{\circ}C$ to $300^{\circ}C$ Their initial permeability was 50 to 490 and their saturation magnetic induction density and coercive force 2,400G and 0.3 Oe to 1.2 Oe each, which were similar to those of NiCuZn ferrite synthesized in the conventional process.

Properties of Three Kinds of Ferrite/Rubber Composite Microwave Absorbers with Various Composition Ratio (조성비에 따른 3종 페라이트/고무 복합형 전파흡수체의 특성)

  • Ryu, Young-Jun;Jun, Hong-Bae;Kim, Cheol-Han;SaGong, Geon
    • Proceedings of the KIEE Conference
    • /
    • 1999.07d
    • /
    • pp.1680-1682
    • /
    • 1999
  • In this study, three kinds of Mn-Zn ferrite/Ni-Zn ferrite/$Ni_2Y$ ferroxplana prepared by the coprecipitation method were compounded with the silicon rubber, and the ring-shaped specimens with various compositional ratio were made. The material constant of ferrite/rubber composite absorbers was obtained by the 2-port method. The material constants of the ferrite/rubber composite microwave absorber made of three kinds of ferrite with various compositional ratio were utilized in design the matching conditions (frequency and thickness) on the impedance matching map. We were able to predict the matching condition from the matching map. On all three kinds of ferrite/rubber composite microwave absorber with less than compositional ratio 60[wt.%] of ferroxplana, we have found that the reflection losses were over than 20[dB] at the S-Band $(2\sim4[GHz])$ and C-Band$(4\sim8[GHz])$.

  • PDF

Effect of Zine Oxide Size and Oxygen Pressure on the Magnetic Properties of (Ni, Zn) Ferrite Powders Prepared by Self-propagating High Temperature Synthesis (ZnO의 입도와 산소압이 고온연소합성법으로 제조된 Ni-Zn Ferrite 분말의 자기적 특성에 미치는 영향)

  • Choi, Yong;Cho, Nam-Ihn;Hahn, Y.D.
    • Journal of the Korean Magnetics Society
    • /
    • v.9 no.2
    • /
    • pp.78-84
    • /
    • 1999
  • $(Ni, Zn)Fe_2O_4$ powders were prepared through self-propagating high temperature synthesis reaction and the effects of initial zinc oxide powder size and oxygen pressure on the magnetic properties of the final combustion products were studied. The ferrite powders were combustion synthesized with iron, iron oxide, nickel oxide, and zinc oxide powders under various oxygen pressures of 0.5~10 atmosphere after blended in n-hexane solution for 5 minutes with a spex mill, followed by dried at 120 $^{\circ}C$ in vacuum for 24 hours. The maximum combustion temperature and propagating rate were about 1250 $^{\circ}C$ and 9.8 mm/sec under the tap density, which were decreased with decreasing ZnO size and oxygen pressure. The final product had porous microstructure with spinel peaks in X-ray spectra. As the ZnO particle size in the reactant powders and oxygen pressure during the combustion reaction increase, coercive force, maximum magnetization, residual magnetization, squareness ratio were changed from 1324 Oe, 43.88 emu/g, 1.27 emu/g, 0.00034 emu/gOe, 37.8$^{\circ}C$ to 11.83 Oe, 68.87 emu/g, 1.23 emu/g, 0.00280 emu/gOe, 43.9 $^{\circ}C$ and 7.99 Oe, 75.84 emu/g, 0.791 emu/g, 0.001937 emu/gOe, 53.8 $^{\circ}C$ respectively. Considering the apparent activation energy changes with oxygen pressure, the combustion reaction significantly depended on initial oxygen pressure and ZnO particle size.

  • PDF