  • The effects of Cu-addition and die-upset temperature on the texture in the die-upset Nd-lean $Nd_xFe_{93.5-(x+y)}-Cu_yGa_{0.5}B_6$ (x = 9-12, y = 0-2) alloys were investigated. The die-upset Cu-containing Nd-lean $Nd_{12}Fe_{81.5-y}-Cu_yGa_{0.5}B_6$ (y = 1, 2) alloys showed a considerable texture. Texture in the Nd-lean alloys developed through basal plane slip deformation. The Cu-addition reduced the melting point of grain boundary phase facilitating grain gliding during the die-upsetting, and providing a greater chance for the $Nd_2Fe_{14}B$ grains to meet the deformation conditions. Die-upsetting at higher temperature facilitated grain gliding and plastic deformation, thus enhancing texture.

$\alpha$-(Fe, Co)기 Nd-(Fe, Co)-B-Nb-Cu 초미세결정립합금의 자기특성에 미치는 Nd의 영향 (Influence of Nd Content on Magnetic Properties of Nanocrystalline $\alpha$-(Fe, Co)-Based Nd-(Fe, Co)-B-Nb-Cu Alloys)

  • 조덕호;조용수;김택기;송민석;김윤배
    • 한국자기학회지
    • /
    • 제9권3호
    • /
    • pp.154-158
    • /
    • 1999
  • Nd 함유량을 2~6at.%로 변화시킨 $\alpha$-(Fe, Co)-B-Nb-Cu 초미세결정립합금의 미세조직 및 자기특성을 조사하였다. 급속응고된 Ndx(Fe0.9Co0.1)90-xB6Nb3Cu1(2$\leq$x$\leq$6, 1at.% 간격) 합금은 x=3 이상에서 비정질상으로 제조되었다. 제조된 비정질합금은 열처리에 의해 $\alpha$-(Fe, Co) 및 Nd2(Fe, Co)14B1상으로 구성된 초미세결정립합금으로 결정화 되었다. 최적열처리조건에서 잔류자화는 Nd의 증가에 따라 감소하며, x=3에서 1.55T로 최대 값을 나타내었다. 보자력은 Nd함유량 증가에 따라 직선적으로 증가하여 x=6에서 4.6kOe이었으며, 최대에너지적은 10.6MGOe였다.

  • PDF

$Nd_{x}{(Fe_{0.9}Co_{0.1})}_{90-x}B_{6}Nb_{3}Cu_{1}(x=\;3,\;4,\;5)$ 초미세결정립합금의 자기특성 (Magnetic Propertes of $Nd_{x}{(Fe_{0.9}Co_{0.1})}_{90-x}B_{6}Nb_{3}Cu_{1}(x=\;3,\;4,\;5)$ Nanocrystalline Alloys)

  • 조용수;김만중;천정남;김택기;박우식;김윤배
    • 한국자기학회지
    • /
    • 제5권5호
    • /
    • pp.880-894
    • /
    • 1995
  • B의 함유량을 6 at% 고정하고 Nd함유량을 3~5 at%로 변화시킨 $\alpha$-Fe기 Nd-Fe-B 합금의 자기특성이 조사 되었다. 급속응고법으로 제조된 $Nd_{x}{(Fe_{0.9}Co_{0.1})}_{90-x}B_{6}Nb_{3}Cu_{1}(x=\;3,\;4,\;5)$ 비정질합금은 열처리에 의하여 초미세결정립으로 결정화하며, Nd의 함유량에 따라 잔류자화 및 보자력이 변한다. x=3의 경우 최적열처리조건에서 $\alpha$-Fe(Co) 부피분율의 증가로 잔류자 화는 증가하나, 보자력은 감소한다. 그러나 Nd 함유량의 증가는 $Nd_{2}{(Fe,\;Co)}_{14}B$ 부피분율의 증가로 인하여 잔류자화는 감소하나 보자력은 향상된다. $640^{\circ}C$, 10 min 열처리조건에서 $Nd_{5}{(Fe_{0.9}Co_{0.1})}_{85}B_{6}Nb_{3}Cu_{1}$의 결정립크기는 약 20 nm이며, 잔류자화, 보자력 및 최대에너지적 은 각각 1.35 T, 219 kA/m (2.75 kOe) 및 $129\;kJ/m^{3}$ (16.2 MGOe)으로 가장 우수하다.

  • PDF

${\alpha}-Fe$ 기 Nd-Fe-B 급속응고합금의 자기특성 (Magnetic Properties of ${\alpha}-Fe$ Based Nd-Fe-B Melt-Spun Alloys)

  • 조용수;김윤배;박우식;김희태;김창석;김택기
    • 한국자기학회지
    • /
    • 제4권2호
    • /
    • pp.122-125
    • /
    • 1994
  • Nd 함유량을 4 at.%로 고정시킨 Nd-Fe-B 합금의 자기특성이 조사되었다. 급속응고된 $Nd_{4}Fe_{85.5}B_{10.5}$ 합금은 열처리에 의하여 ${\alpha}-Fe$ 연자성기지에 석출되며, $Nd_{4}Fe_{85.5}B_{10.5}$ 합금에 Mo, Nb, V 및 Cu의 첨가는 결정립을 미세화시켜 보자력을 향상시킨다. 그러나 ${\alpha}-Fe$ 결정립에 의한 각형성 열화는 잔류자화를 감소시킨다. $Nd_{4}Fe_{82}B_{10}M_{3}Cu_{1}$(M = Mo, Nb, V) 합금에서 보자력은 M = V < Nb < Mo로 증가하며, M = Mo에서 2.7 kOe이고, 잔류자화는 M = Mo < Nb < V순으로 증가하며 M = V에서 1.35 T이다.

  • PDF

INFLUENCE OF B AND Nd CONTENT ON THE MAGNETIC PROPERTIES OF ${\alpha}-Fe$ BASED NdFeB MAGNETS WITH ULTRAFINE GRAINS

  • Cho, Y.S.;Kim, Y.B.;Park, W.S.;Kim, C.S.;Kim, T.K.
    • 한국자기학회지
    • /
    • 제5권5호
    • /
    • pp.427-431
    • /
    • 1995
  • The influence of Nd and B contents on the magnetic properties and structures of ${\alpha}-Fe$ based Nd-(Fe,Co)-B-Mo-Cu alloys was investigated. $Nd_{4}{(Fe_{0.9}Co_{0.1})}_{92-x}B_{x}Mo_{3}Cu_{1}$ and $Nd_{x}{(Fe_{0.9}Co_{0.1})}_{86-x}B_{10}Mo_{3}Cu_{1}$ amorphous alloys prepared by rapid solidification process were crystallized to form nanocrystalline structure. The increase of B content in $Nd_{4}{(Fe_{0.9}Co_{0.1})}_{92-x}B_{x}Mo_{3}Cu_{1}$ nanocrystalline resulted in the change of stucture of soft phase in the sequence of ${\alpha}-Fe$->${\alpha}-Fe+Fe_{3}B$->$Fe_{3}B$. The coercivitis of the alloys were increased with increasing B content and was 263 kA/m at x=18. On the contrary, the remanence has shown an opposite trends. The increase of Nd content in $Nd_{x}{(Fe_{0.9}Co_{0.1})}_{86-x}B_{10}Mo_{3}Cu_{1}$ nanocrystalline containing ${\alpha}-Fe$ as main phase had no effect on the structure and improved coercivity up to 256 kA/m. However, the remanence was decreased from 1.4 T to 1.15 T according to the increase of Nd content.

  • PDF

Ga 첨가가 $\alpha$-Fe기 Nd-Fe-B 합금의 자기특성에 미치는 영향 (Influence of Ga-Addition on the Manetic Properties of $\alpha-Fe$ Based Nd-Fe-B Alloy)

  • 조덕호;이병엽;조용수
    • 한국자기학회지
    • /
    • 제7권1호
    • /
    • pp.44-48
    • /
    • 1997
  • 약 30 nm의 미세결정립으로 구성된 ( .alpha. -Fe)-(Nd$_{2}$Fe$_{14}$B$_{1}$)형 저 Nd함유 Nd-Fe-B계 합금이 급속응고법으로 제조된 비정질상으로 부터 결정화하여 제조되었다. Nd$_{4}$Fe$_{82}$B$_{10}$Mo$_{3}$Cu$_{1}$ 조성에 Ga의 첨가는 각형성 개선효과와 함께 잔류자화를 1.29 T까지 증가시킨다. Nd의 함유량을 증가시킨 초미세결정립 Nd$_{5}$Fe$_{81}$B$_{9}$Mo$_{3}$Cu$_{1}$Ga$_{1}$ 합금의 Nd$_{2}$Fe$_{81}$B$_{9}$Mo$_{3}$Cu$_{1}$Ga$_{1}$ 합금의 잔류자화, 보자력 및 최대자기에너지적은 각각 1.24 T, 257.4 kA/m(3.23 kOe), and 100.3 kJ/m$^{3}$(12.6 MGOe)이다.다.

  • PDF

Co 치환이 α-Fe기 초미세결정립 Nd-Fe-B계 합금의 자기특성에 미치는 영향 (The Effects of Co-substitution on the Magnetic Properties of Nanocrystalline Nd-Fe-B based Alloy Containing α-Fe as Main Phase)

  • 조덕호;조용수
    • 한국자기학회지
    • /
    • 제12권1호
    • /
    • pp.30-33
    • /
    • 2002
  • 초미세결정렵 Nd-Fe-B-Mo-Cu합금에서 Co 치환이 미세조직과 자기특성에 미치는 영향을 조사 하였다. 급속응고법으로 제조된 비정질 Nd-(Fe, Co)-B-Mo-Cu합금은 결정화에 의하여 $\alpha$-Fe기 초미세결정립 Nd-(Fe, Co)-B-Mo-Cu합금이 제조되었다. Co로의 Fe치환은 결정립 미세화에 기여하며, 이로 인하여 경자기특성이 개선되었다. 최적열처리된 초미세결정립 N $d_4$(F $e_{0.85}$ $Co_{0.15}$)$_{82}$ $B_{10}$M $o_3$Cul합금의 잔류자화, Curie온도는 Co가 치환되지 않은 합금에 비하여 개선된 우수한 특성을 나타내었다. 64$0^{\circ}C$, 10분 열처리된 초미세결정립 N $d_4$(F $e_{0.85}$ $Co_{0.15}$)$_{82}$ $B_{10}$M $o_3$Cu 합금의 평균결정립 크기는 약 15 nm이며, 이때 보자력, 잔류자화 및 최대에너지적은 각각 239kA/m, 1.4 T 및 103.5 kJ/ $m^3$이었다.