  • This study is to investigate the stress distributions, crystal orientations and magnetic properties during die-upsetting according to working temperature of Nd-Fe-B-Cu alloys. The stress distributions in the specimens during compressing process were calculated by a finite element method program(SPID). The calculated stresses were effective stress (${\sigma}_{eff}$), compression stress(${\sigma}_z$), radial direction stress(${\sigma}_r$) rotational direction stress(${\sigma}_e$) and shear stress(${\tau}_{rz}$). The stress distributions of ${\sigma}_z$, obtained by a computer simulation showed that the stress components causing the magnetic alignment during die-upsetting of the cast magnets were very high at the center-part of a specimen, and decreased toward the periphery-part of a specimen. In view of the above results the magnetic properties should be better at the center-part of a specimen than any other parts. But the measured magnetic properties were better at the mid-part. These results should be due to the fact that the specimens were casted. Normally the magnetic properties are affected by the casting process as well as by the stress levels. ${\sigma}_r$, ${\sigma}_e$ are thought to affect the liquid phase flowing and domain patterns, respectively. The influence of ${\tau}_{rz}$ was trivial, ${\sigma}_{eff}$ distributed similar throughout the specimen. The Nd-rich phase appeared at the peripheral of the specimen where the stress level of ${\sigma}_r$, ${\sigma}_z$, was low or the stress level of ${\sigma}_e$ was high. The Nd-rich phase was squeezed out during die-upsetting. This phase had an effect on the crystal orientation and grain growth. The stress distributions of alloy were irregular at the parts of the specimen where the die contacted with specimen.

  • PDF

Nd-Fe-B-Co계 급냉리본과 Bond 자석의 자기적 성질 (Magenetic Properties of Nd-Fe-B-Co-based Melt-spun Ribbons an dTheir Bonded Magents)

  • 강계명;강기원;오영민;송진태
    • 한국재료학회지
    • /
    • 제3권2호
    • /
    • pp.175-184
    • /
    • 1993
  • Nd-Fe-B계에 Co와 Al을 첨가한 자석합금을 진공유도용해로에서 제조하여 이들 합금을 단롤법으로 melt-spun시켜 급냉리본을 얻었다. 제작된 급냉리본의 냉각속도에 따른 자기적 성질의 변화를 조사하였고, 최적의 급냉속도에서 제작된 리본을 파쇄하여 resin bond 자석을 제조하였으며, 이들 급냉리본 및 bond자석의 자기적 성질, 미세구조, 결정구조에 관하여 연구, 조사하였다. 이들 급냉리본의 자기적 성질은 급냉속도에 따라 크게 변하였으며 20m/sec전후에서 최적의 자기적 성질을 보였다. 이때의 급냉리본의 미세조직은 Nd-rich의 입계상이 미세한 N$d_2$F$e_14$B결정립을 둘러싼 cell 형의 구조였으며, 특히 Al이 2.1at%첨가된 리본시료에서는 iHc=15.5KOe, Br=7.8KG, (BH)max=8.5MGOe의 자기적 성질을 나타내었다. 최적의 급냉속도에서 제작된 리본을 polyamide resin과 2.5wt%의 비율로 혼합하여 상온에서 성형, 결합시켜 제작한 bond자석에서 보다 현저히 향상되었으며 유지시간이 8분인 경우 iHc=10.8KOe, Br=7.3KG, (BH)max=8.0MGOe의 값을 가졌다. 한편, 자구구조는 maze pattern이 주로 관찰되어 자화용이축인 C축이 배열되었으며 bond자석에서보다 hot-press 자석에서 자구폭이 보다 작았다.