Comparison of Welding Characteristics of Austenitic 304 Stainless Steel and SM45C Using a Continuous Wave Nd:YAG Laser (오스테나이트계 스테인리스강과 SM45C의 연속파형 Nd:YAG 레이저 용접특성비교)

  • 유영태;오용석;노경보;임기건
    • Transactions of the Korean Society of Machine Tool Engineers
    • /
    • v.12 no.3
    • /
    • pp.58-67
    • /
    • 2003
  • Welding characteristics of austienite 304 stainless and SM45C using a continuous wave Nd:YAG laser n experimentally investigated Laser beam welding is increasingly being used in welding of structural steels. The laser welding process is one of the most advanced manufacturing technologies owing to its high speed and deep penetration. The thermal cycles associated with laser welding are generally much Inter than those involved in conventional welding processes, leading to a rather small weld zone. Experiments are performed for 304 stainless steel plates changing several process parameter such as laser power, welding speed, shielding gas flow rate, presence of surface pollution, with fixed or variable gap and misalignment between the similar and dissimilar and plates, etc. The Nd:YAG laser welding process is one of the most advanced manufacturing technologies owing to its high speed and penetration. This paper describes the weld ability of SM45C carbon steel for machine structural use by Nd:YAG laser. The follow conclusions can be drawn that laser power and welding speed have a pronounced effect on size and shape of the fusion zone. Increase in welding speed resulted in an increase in weld depth/aspect ratio and hence a decrease in the fusion zone size. The penetration depth increased with the increase in laser power.

An analysis of Cutting Characteristic of Multilayer FPCB using Nd:YAG UV Laser System (Nd:YAG UV 레이저를 이용한 연성회로 다층기판 절단특성에 대한 연구)

  • Choi, Kyung-Jin;Lee, Young-Hyun
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.27 no.3
    • /
    • pp.9-17
    • /
    • 2010
  • The FPCB is used for electronic products such as LCD display. The process of manufacturing FPCB includes a cutting process, in which each single FPCB is cut and separated from the panel where a series of FPCBs are arrayed. The most-widely used cutting method is the mechanical punching, which has the problem of creating burrs and cracks. In this paper, the cutting characteristics of the FPCB have been experimented using Nd:YAG DPSS UV laser as a way of solving this problem. To maximize the industrial application of this laser cutting process, test samples of the multilayered FPCB have been chosen as it is actually needed in industry. The cutting area of the FPCB has four different types of layer structure. First, to cut the test sample, the threshold laser cut-off fluence has been found. Various combinations of laser and process parameters have been made to supply the acquired laser cut-off fluence. The cutting characteristics in terms of the variation of the parameters are analyzed. The laser and process parameters are optimized, in order to maximize the cutting speed and to reach the best quality of the cutting area. The laser system for the process automation has been also developed.

Effects of Acid-etching, CO2 and Nd:YAG Lasing on the Dentin Surface (산부식과 CO2 및 Nd:YAG 레이저 조사에 따른 상아질 표면의 변화)

  • Lee, Jae-Hak;Park, June-Sang;Ko, Myung-Yun
    • Journal of Oral Medicine and Pain
    • /
    • v.25 no.1
    • /
    • pp.129-144
    • /
    • 2000
  • The purpose of this study was to examine dentin surface changes of extracted sound third molar specimens which were etched with 10% maleic acid and irradiated at $7-140J/cm^2$ with $CO_2$ and at $156-280J/cm^2$ with Nd:YAG laser. The results were as follows. 1. Dentin surfaces etched with 10% maleic acid and then irradiated at below of $42J/cm^2$ with $CO_2$ laser showed the retentive morphology for resin restoration. 2. Dentin surfaces irradiated at below of $42J/cm^2$ with $CO_2$ laser showed the increased acid-resistance. 3. Dentin surfaces irradiated at $218-280J/cm^2$ with Nd:YAG laser showed the retentive morphology. 4. Dentin surfaces irradiated at $218-280J/cm^2$ with Nd:YAG laser and etched 10% maleic acid and then $218-280J/cm^2$ with Nd:YAG laser showed the increased acid-resistance.

  • PDF

Experimental Study for Removing Artificial Patinas of Bronze Sculpture by Nd:YAG Laser Cleaning System (청동 조형물의 인공 파티나 제거를 위한 Nd:YAG 레이저 적용 실험 연구)

  • Park, Chang-Su;Cho, Nam-Chul
    • Journal of Surface Science and Engineering
    • /
    • v.46 no.5
    • /
    • pp.197-207
    • /
    • 2013
  • In the midst of increasing importance of modern cultural assets, especially, most modern bronze objects are exposed to outdoor environment, and as the objects are corroded steadily due to environmental factors the objects lost their original colors on the surface. We performed artificial patinas on the bronze sample per each color of red, black and green and checked cuprite and tenorite which are detected from actual bronze corrosion by analyzing the components. In addition, we applied the existing corrosion removal methods of grinder and sand blaster on a similar sample of bronze mirror per injection pressure and performed comparative analysis on the result with Nd:YAG laser. As a result of Nd:YAG laser cleaning artificial patina from bronze samples, all of the patinas were removed by laser wavelength 1064 nm better than 532 nm. Upon applying to a similar sample of bronze mirror, the artificial patina could be selectively removed from substrates without surface damage when Nd:YAG laser was conducted other than the existing removal method, and so it showed the possibility of application.

Intracavity frequency doubling of a single-mode Nd:YAG laser using a nonplanar ring cavity (비평면 고리형 공진기를 이용한 단일 모드 Nd:YAG 레이저의 내부 공진기 주파수 배가)

  • 박종락;윤태현
    • Korean Journal of Optics and Photonics
    • /
    • v.14 no.1
    • /
    • pp.85-91
    • /
    • 2003
  • Intracavity frequency doubling of a single-mode Nd:YAG laser by using a nonplanar ring cavity is demonstrated. The nonplanar ring cavity consists of a Brewster-angled Nd:YAG crystal placed in a magnetic field, a KTP crystal, and two spherical mirrors. In this design the Nd:YAG block acts as both a nonreciprocal polarization rotator and a partial polarizer, and the nonplanar portion of the ring cavity, which is formed by a relative twist angle between the Brewster-angled end surfaces of the Nd:YAG block, serves as a reciprocal polarization rotator. An eigenpolarization theory for the cavity configuration is presented and suitable values of the relative twist angle for unidirectional operation are estimated. A single-mode output power of 22 ㎽ at 532 nm and an optical to optical conversion efficiency of 1.8% are obtained with a 1.2 W diode laser at 809 nm.

A Study on the Welding Behavior of A3003 Aluminium Alloy Thin Sheet by Nd : YAG Laser Beam (박판 A3003 Al합금의 Nd : YAG 레이저빔 용접에 관한 연구)

  • 허인석;김병철;김도훈;김진수;이한용
    • Laser Solutions
    • /
    • v.4 no.1
    • /
    • pp.29-38
    • /
    • 2001
  • This work was carried out to investigate the welding behavior of thin A3003 Al alloy sheets by Nd : YAG laser beam. Considering bead shape and mechanical properties, the laser pulse shapes selected were two kinds of 2-division and 3-division by varying power level and pulse duration. In order to obtain optimum conditions, the factorial design method and central composite design method were applied. Tensile test, optical microscopy, micro hardness test and TEM analysis were performed. Due to the annealing caused by thermal effect during laser welding, precipitates were coarsended. The HAZ was softened and failed during tensile test. The hardness of HAZ was lower than that of base metal, since the heat input relieved the work hardening effect and caused grain growth.

  • PDF