The interest of austenitic heat resistant stainless steels containing high Si has increased because they have higher resistance of oxidation and higher strength at high temperature than STS 310. This study carried out Varestraint test for evaluation of solidification cracking sensitivity of 14 different stainless steels. As a result of Varestraint test, all specimens solidified as primary ferrite, and solidification crack sensitivity increased with adding $N_2$ to shielding gas. Nb and W had beneficial effect on solidification crack resistance in case of less than FN 2 containing, but crack sensitivity increased with Nb and W in case of more than FN 2. Ce had beneficial effect on solidification crack resistance but impaired weld bead appearance.
The crystallization kinetics of $Fe_{73.5}Si_{13.5}B_{9}Cu_{1}Nb_{3}$ amorphous alloy has been investigated using differential scanning calorimetry (DSC). The crystallization process had two stages, i.e. precipitation of the $\alpha$-Fe(Si) solid solution and the tetragonal borides. The isothermal transformation data of the amorphous alloy has been fitted successfully to the generalized Johnson-Mehl-Avrami equation. The mean time exponent, n, obtained is close to 2.5. The value of n=2.5 may be interpreted as being due to a diffusion-controlled transformation process with a constant nucleation rate, one likely transformation mode for the crystallization of metallic amorphous alloys. The activation energy of the overall crystallization process deduced from the time to 50% crystallization are about 81 kcal/mole. The value is of the same order as those estimated from viscous flow.
공냉에 의한 중탄소 비조질강은 페라이트와 펄라이트의 미세구조를 갖는다. 기존의 조질강과 비교하여 이재료는 V, Nb, Ti을 첨가하여 강도는 거의 동등한 반면 인성에 있어서 조질강에 비해 취약하다. 본 연구에서는 직접 소입 저탄소 비조질강의 기계적 성질에 미치는 몰리브덴의 영향을 조사하였다. 몰리브덴 첨가 직접 소입 비조질강은 고강도와 고인성을 나타내었다. 몰리브덴은 변태 온도를 저하시켜 미세한 구조와 균일한 석출 구조를 효과적으로 생성시킨ㄷ. 본 실험의 결과로 0.15C+0.11V+0.035Nb+1.81Mo의 재료를 유냉시켜 121MPo의 강도와 127.5J의 인성을 얻었다.
The effect of the Mo addition on the high temperature creep properties of the 9Cr-3W steel was also evaluated. Two experimental steels, (9Cr-3W and 9Cr-3W-0.5Mo), were prepared using a vacuum induction melting process, followed by hot rolling and heat treatment processes. Three types of precipitates, ($M_{23}C_6$, Nb-rich MX and V-rich MX) were observed in a typical tempered martensitic matrix. Significant effects of the Mo addition on the tensile properties were not observed. However, the creep properties at $650^{\circ}C$ under applied stresses of 140 and 150 MPa were considerably enhanced by the Mo addition. The microstructural observation after the creep test indicated that the addition of Mo could function to retain the recovery of the martensitic matrix, thus resulting in the enhanced creep properties of the 9Cr-3W-0.5Mo steel. Furthermore coarsening of the $M_{23}C_6$ carbides and formation of Laves phases were observed in both samples after the creep tests.
In the case of hull material. large sized merchant ships are made of steel, on the other hand FRP or wood are used for small sized fishing boats. At present in Korea approximately 88,500 fishing boats are in operation of which 70% are made of FRP
In the meantime, stainless steel is frequently used as shaft materials of the small-size FRP fishing boat. Namely, the kinds of shaft materials are STS 304(18Cr-8Ni), STS 316(18Cr-12Ni-2.5Mo steel) and STS 630(17Cr-Ni-Nb steel)etc. Among these things, STS 304 which is the cheapest and having ordinary corrosion resistance is most widely used as 2nd class shaft material. But, using STS 304 for shaft system material of the small-size FRP fishing boat on seawater environments entails a severe corrosion which causes shaft system troubles. Particularly, the corrosions tend to be concentrated of the stern and bow side, propeller shaft surface of inside of stern tube and the boat having no stern cooling pipe line system. As a solution for those problems, research on the ways to mitigate corrosion on the part of 2nd class stainless steel shaft have been undertaken. In the result, not only clarification for the reason of corrosion of the part of stainless steel shaft used mainly for the small-size FRP fishing boat was done, but also most optimal corrosion protection system was developed by experimenting shaft's protection simulation based of the electrochemical cathodic protection principle. In addition, verification through the field test on the optimal cathodic corrosion protection method by means of aluminum sacrificial anode was carried out. In this study, effective and economical shaft's protection system is suggested to the small-size FRP fishing boat operator by substantiating the results obtained from the research on the optimal cathodic protection.
Al과 Mn을 활용한 저비중 경량 스테인리스강에 관한 연구가 진행되고 있다. 경제적으로 고가의 Cr을 대체하거나 소량 첨가함으로써 유해성 6가 크롬발생을 감소시킬 수 있는 기술이다. Ti, Al, Nb을 첨가하여 비중을 낮추고 경량화 함으로써 자동차, 산업플랜트, 해양선박, 플랜트에 사용할 수 있으며 에너지 연료를 절감할 수 있다. 열처리 냉각속도가 빠를수록 미세한 ferrite조직으로 된다. 본고에서는 Al, Mn을 활용한 Cr-free경량-저비중 스테인리스강의 기술동향을 중점 분석하였다.
The structure and properties of HSLA steel obtained by Osprey forming process were investigated. The porosities were generated at the bottom of specimen due to the quenching effect of cold substrate during forming. The steel had a bainitic structure. The grain size were different among positions due to the cooling rates. The elements such as Mn, S, Si, Cr, Mo and etc. were contained in inclusions. They were formed at grain boundries. The size of them was $1{\sim}2{\mu}m$ and has nothing to do with the chemical composition. MnS and NbC were precipitated during rolling and aging.
The effects of casting variables and alloying elements on the fluidity of thin wall cast stainless steels were investigated. Melts were poured into the sand molds to produce thin wall test castings. The length of it was 245 mm and the thickness varied at the interval of 0.5 in the range of 1.6 to 2.6 mm. For the same casting condition, the fluidities of austenitic stainless steel, ferritic, precipitation hardenable and martensite ones were better in the order. The higher the pouring temperature, the shorter the pouring rate and the better the fluidity were. The fluidity was increased with the addition of Cr and decreased with W and Nb.
In this study, actual scale welding were conducted at the USC thermal power plant turbine and main steam pipe casting candidate mock up material 9Cr-1.5Mo-CoVNbNB steel(CB2) and 9Cr-0.5Mo-MVNbN steel(P92). And to evaluate the welding process for the actual production, mechanical property testes were conducted for the weld metal. The Mock-up welding condition successfully led to an excellent structural welding joint between casting and pipe material.
In metal cutting at the tool-chip interface, friction generates considerable amount of heat. Thus, tile .knowledge of wear properties or the cutting tool material in high temperature has been known as one of tile important factors in need of clarification. The authors presented the wear properties of 5%V-5%Co-1%Nb high speed steel, fabricated by powder metallurgy, in room temperature in a previous article. The objective of this paper is to clarify tile effects of temperature ell its wear properties. Wear tests in sliding conditions under various temperatures have been conducted. The results indicate that tile wear properties of tile tool material in high temperature as well as in room temperature are excellent. It may be deduced that the oxide layer formed on the vol-n surface at high temperature is stable enough to prevent wear due to tile high temperature strength of its matrix.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.