• 제목/요약/키워드: Nanopowder agglomerate

검색결과 6건 처리시간 0.022초

Consolidation of Iron Nanopowder by Nanopowder-Agglomerate Sintering at Elevated Temperature

  • Lee, Jai-Sung;Yun, Joon-Chul;Choi, Joon-Phil;Lee, Geon-Yong
    • 한국분말재료학회지
    • /
    • 제20권1호
    • /
    • pp.1-6
    • /
    • 2013
  • The key concept of nanopowder agglomerate sintering (NAS) is to enhance material transport by controlling the powder interface volume of nanopowder agglomerates. Using this concept, we developed a new approach to full density processing for the fabrication of pure iron nanomaterial using Fe nanopowder agglomerates from oxide powders. Full density processing of pure iron nanopowders was introduced in which the powder interface volume is manipulated in order to control the densification process and its corresponding microstructures. The full density sintering behavior of Fe nanopowders optimally size-controlled by wet-milling treatment was discussed in terms of densification process and microstructures.

Densification Behavior and Microstructural Development of Nano-agglomerate Powder during Singering

  • Kang, Yun-Sung;Cha, Berm-Ha;Kang, Hyun-Goo;Lee, Jai-Sung
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.282-283
    • /
    • 2006
  • Densification behavior of nano-agglomerate powder during pressureless sintering of Fe-Ni nanopowder was investigated in terms of diffusion kinetics and microstructural development. To understand the role of agglomerate boundary for sintering process, densification kinetics of Fe-Ni nano-agglomerate powder with different agglomerate size was investigated. It was found that activation energy for densification was lower in the small-sized agglomerate powder. The increase in the volume fraction of inter-agglomerate boundary acting as high diffusion path might be responsible for the enhanced diffusion process.

  • PDF

비가압 성형한 Fe 나노분말응집체의 소결거동 (Sintering Behavior of Fe Nanopowder Agglomerates Prepared by Pressureless Compaction)

  • 유우경;정성수;이재성
    • 한국분말재료학회지
    • /
    • 제15권4호
    • /
    • pp.271-278
    • /
    • 2008
  • Sintering behavior of iron nanopowder agglomerate compact prepared by slurry compaction method was investigated. The Fe nanopowder agglomerates were prepared by hydrogen reduction of spray dried agglomerates of ball-milled $Fe_2O_3$ nanopowder at various reduction temperatures of $450^{\circ}C$, $500^{\circ}C$ and $550^{\circ}C$, respectively. It was found that the Fe nanopowder agglomerates produced at higher reduction temperature have a higher green density compact which consists of more densified nanopowder agglomerates with coarsed nanopowders. The sintering behavior of the Fe nanopowder agglomerates strongly depended on the powder packing density in the compact and microstructure of the agglomerated nanopowder. It was discussed in terms of two sintering factors affecting the entire densification process of the compact.

Sintering Behavior of the Net-shaped Fe-8wt%Ni Nanoalloy Powder and Related Mechanical Property

  • Cha, Berm-Ha;Kang, Yun-Sung;Lee, Sung-Ho;Lee, Jai-Sung
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.501-502
    • /
    • 2006
  • The present investigation has been performed on full densification behavior and mechanical property of the powder injection molded Fe-8wt%Ni nanoalloy powder. The net shaping process of the nanopowder was conducted by powder injection molding (PIM) process. The key-process for fabricating fully densified net-shaped nanopowder by pressureless sintering is an optimal control of agglomerate size of nanopowder. Enhanced mechanical property of PIMed Fe-Ni nanopowder is explained by grain refinement and microstructural uniformity.

  • PDF

플라즈마 이온질화에 의한 Fe 나노분말소결체의 표면경화 가능성 연구 (A Feasibility Study on the Surface Hardening of Sintered Iron Nanopowder by Plasma Ion Nitriding)

  • 윤준철;이재성
    • 한국분말재료학회지
    • /
    • 제19권1호
    • /
    • pp.13-18
    • /
    • 2012
  • This study has been performed on the full density sintering of Fe nanopowder and the surface hardening by plasma ion nitriding. The Fe sintered part was fabricated by pressureless sintering of the Fe nanopowder at $700^{\circ}C$ in which the nanopowder agglomerates were controlled to have 0.5-5 ${\mu}m$ sized agglomerates with 150 nm Fe nanopowders. The green compact with 46% theoretical density(T.D.) showed a homogeneous microstructure with fine pores below 1 ${\mu}m$. After sintering, the powder compact underwent full densification process with above 98%T.D. and uniform nanoscale microstructure. This enhanced sintering is thought to be basically due to the homogeneous microstructure in the green compact in which the large pores are removed by wet-milling. Plasma ion nitriding of the sintered part resulted in the formation of ${\gamma}$'-$Fe_4N$ equilibrium phase with about 12 ${\mu}m$ thickness, leading to the surface hardening of the sintered Fe part. The surface hardness was remarkably increased from 176 $H_v$ for the matrix to 365 $H_v$.

산화물 수소환원에 의한 W-Ni-Fe 나노복합분말의 합성과 특성 (Synthesis and Characteristics of W-Ni-Fe Nanocomposite Powder by Hydrogen Reduction of Oxides)

  • 이창우;윤의식;이재성
    • 한국분말재료학회지
    • /
    • 제8권1호
    • /
    • pp.49-54
    • /
    • 2001
  • The synthesis and characteristics of W-Ni-Fe nanocomposite powder by hydrogen reduction of ball milled W-Ni-Fe oxide mixture were investigated. The ball milled oxide mixture was prepared by high energy attrition milling of W blue powder, NiO and $Fe_2O_3$ for 1 h. The structure of the oxide mixture was characteristic of nano porous agglomerate composite powder consisting of nanoscale particles and pores which act as effective removal path of water vapor during hydrogen reduction process. The reduction experiment showed that the reduction reaction starts from NiO, followed by $Fe_2O_3$ and finally W oxide. It was also found that during the reduction process rapid alloying of Ni-Fe yielded the formation of $\gamma$-Ni-Fe. After reduction at 80$0^{\circ}C$ for 1 h, the nano-composite powder of W-4.57Ni-2.34Fe comprising W and $\gamma$-Ni-Fe phases was produced, of which grain size was35nm for W and 87 nm for $\gamma$-Ni-Fe, respectively. Sinterability of the W heavy alloy nanopowder showing full density and sound microstructure under the condition of 147$0^{\circ}C$/20 min is thought to be suitable for raw material for powder injection molding of tungsten heavy alloy.

  • PDF