Formation Conditions of Na-cellulose II with Three Fold Helix (3회나선축을 갖는 Na-cellulose II의 형성조건에 관한 고찰)

  • Kim, Nam-Hun;Lee, Myoung-Ku
    • Journal of the Korean Wood Science and Technology
    • /
    • v.27 no.1
    • /
    • pp.18-23
    • /
    • 1999
  • The formation conditions of Na-cellulose II with three fold helix were investigated by an x-ray diffraction method. Na-cellulose II was formed through Na-cellulose I. It seems that the concentration of sodium hydroxide in Na-cellulose II is higher than both those of Na-cellulose I and Na-cellulose III. Na-cellulose II was formed well by different rinsing and drying methods even though the sample treatment was carried out in very short periods of time. Metal-complexed Na-cellulose swollen in the mixture of $Cu(OH)_2$ and sodium hydroxide is stable in wet state, and changed to a different polymorph by drying.

  • PDF

Adsorption Behavior of Metal ions by Na-Cellulose (Na-셀룰로스에 대한 금속이온들의 흡착성에 관한 연구)

  • Lee, Tack-Hyuck;Yoon, Koog-Joong
    • Analytical Science and Technology
    • /
    • v.7 no.3
    • /
    • pp.271-276
    • /
    • 1994
  • A Na-cellulose adsorbent was prepared by treating Sigma S-5504 cellulose with 2M NaOH and examined the adsorption behavior between metal ions and Na-cellulose in aqueous solution with batch method. Considering ion exchange capacity of Na-cellulose, the adsorption ratio of the Na-cellulose to metals charge equivalent indicated that the adsorption result from ion exchanging between metal ions and Na-cellulose. The enthalpy for the metal adsorption on the Na-cellulose was calculated to -18kcal/mol, which value was compared to those of carboxymethylcellulose(CMC) and Dowex 50W-X8, these result suggested that the adsorption on Na-cellulose resulted from ion exchange adsorption.

  • PDF

Fine Structure and Physical Properties of Cotton Fibers and their Fabrics Treated with Liquid Ammonia, NaOH, and NaOH/Liquid Ammonia (액체암모니아, 수산화나트륨, 수산화나트륨/액체암모니아 처리한 면의 미세구조 및 물성)

  • 배소영;이문철;김홍성;이영희;김경환
    • Textile Coloration and Finishing
    • /
    • v.6 no.2
    • /
    • pp.47-54
    • /
    • 1994
  • Cotton fiber, NaOH-mercerized cotton fiber, cotton fabric, and NaOH-mercerized cotton fabric have been treated by liquid ammonia at -33.4$^{\circ}C$. The fine structures, bending properties, tensile strengthes, shrinkages for laundering, and wrinkle recoveries were studied. The treatment of cottons with liquid ammonia brought about the transition of crystal lattice ; transforming cellulose I crystal of original cotton to cellulose I and III crystal, and cellulose II crystal of mercerized cotton to cellulose II and III crystals. The degree of crystallinities were decreased in the order of liquid ammonia>NaOH/liquid ammonia>NaOH-treated cotton. However moisture regain and water absorbency for liquid ammonia-treated cotton were lower than that of NaOH-treated cotton because of a difference in swelling actions of the agents. It seems caused by intermicrofibrillar pores produced in swelling processes. The bending rigidity and bending hysteresis were decreased remarkly by liquid ammonia treatment. Therefore softness and dimensional stability were improved. The liquid amminia and NaOH/liquid ammonia-treated cottons moreover show excellent properties in tensile strength, anti-shrinkage for laundering, and wrinkle recovery.

  • PDF

Radiation-Induced Grafting of Acrylic Acid onto Cellulose: III. The Water Absorption Characteristics (셀룰로오스에 아크릴산의 방사선 그라프트 반응: III. 셀룰로오스의 흡수특성)

  • Kwon, Oh Hyun;Nho, Young Chang
    • Applied Chemistry for Engineering
    • /
    • v.9 no.4
    • /
    • pp.516-522
    • /
    • 1998
  • In this study, a water adsorbent was synthesized by radiation grafting of acrylic acid and multifunctional monomers such as 1,2-propanediol dimethacrylate (PDMA) and 1,1,1-trimethylolethane triacrylate (TMETA) onto cellulose and its subsequent treatment with 5% NaOH. Its absorbency on $H_2O$ and 0.9 % NaCl aqueous solution was examined. The highest absorbency on water and on 0.9% NaCl aqueous solution was obtained from the addition of 0.75 vol % PDDMA and of 1.0 vol % TMETA onto acrylic acid solution, respectively. The absorbency of commercial hygienic band on water and NaCl aqueous solution was 21 g/g and 22 g/g, respectively. However, that for acrylic acid-grafted cellulose including TMETA was 298 g/g and 54 g/g, respectively.

  • PDF

Effects of Alkali Concentration on Fiber Characteristics of SwBKP during Alkali Treatment in Cosolvent System (알칼리 공용매 팽윤처리 시 알칼리 농도가 SwBKP 섬유 특성에 미치는 영향)

  • Seo, Ji-Hye;Choi, Kyoung-Hwa;Cho, Byoung-Uk
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.48 no.3
    • /
    • pp.37-43
    • /
    • 2016
  • Various mechanical and chemical pretreatment methods including alkali treatment, pre-beating, enzyme treatment and oxidation treatment have been used to reduce the production energy of the microfibrillated cellulose (MFC). Among them, alkali swelling can be helpful to reduce the energy consumption because the internal bonding between fibrils could be weakened. In this study, dimethyl sulfoxide (DMSO) was used as a cosolvent to improve alkali pretreatment efficiency and the effects of NaOH concentration during NaOH-DMSO swelling on changes in fiber characteristics of softwood bleached kraft pulp (SwBKP) were elucidated. For alkali treatment in H2O-DMSO solvents, fiber length were decreased with increasing NaOH concentration while fiber width, curl and WRV were increased. WRV began to increase at 8% NaOH solution. In addition, above 8% concentration of NaOH, crystalline structure of pulp fibers converted from cellulose II to cellulose III by DMSO cosolvent. Comparing the previous results with this study, it was shown that DMSO cosolvent could promote swelling of pulp fibers and thus reduce NaOH concentration for the maximum swelling of fibers.

Effect of gamma irradiation on the size of cellulose nanocrystals with polyethylene glycol and sodium hydroxide/Gd2O3 nanocomposite as contrast agent in magnetic resonance imaging (MRI)

  • Fathyah Whba;Faizal Mohamed;Mohd Idzat Idris;Rawdah Whba;Noramaliza Mohd Noor
    • Nuclear Engineering and Technology
    • /
    • v.56 no.5
    • /
    • pp.1803-1812
    • /
    • 2024
  • The attractive properties of gadolinium-based nanoparticles as a positive contrast agent for magnetic resonance imaging (MRI) have piqued the interest of both researchers and clinicians. Nonetheless, due to the biotoxicity of gadolinium (III) ions' free radicals, there is a need to address this issue. Therefore, this research aimed to develop a biocompatible, dispersible, stable, hydrophilic, and less toxic cellulose nanocrystals/gadolinium oxide nanocomposite as contrast agent properties for MRI purposes. This study aimed to synthesize gadolinium oxide nanoparticles coated with cellulose nanocrystals with polyethylene glycol and sodium hydroxide (CNCs-PEG/NaOH)/Gd2O3 using the gamma irradiation method to reduce the particle size. The results showed that using a gamma irradiation dose of 10 kGy, quasi-spherical morphology with a size of approximately 5.5 ± 0.65 nm could be produced. Furthermore, the cytocompatibility of (CNCs-PEG/NaOH)/Gd2O3 nanocomposite synthesized was assessed through MTT assay tests on Hep G2 cells, which demonstrated good cytocompatibility without any cytotoxic effects within a concentration range of (10 ㎍/mL - 150 ㎍/mL) and had sufficient cellular uptake. Moreover, the T1-weighted MRI of (CNCs-PEG/NaOH)/Gd2O3 nanocomposite revealed promising results as a positive contrast agent. It is envisaged that the gamma irradiation method is promising in synthesizing (CNCs-PEG/NaOH)/Gd2O3 nanocomposite with nanoscale for different applications, especially in the radiotherapy field.

Physical Properties and Dyeability of Cotton Fabrics Treated with Liquid Ammonia (액체암모니아 처리 면직물의 물성 및 염색성)

  • Jeon, Sung-Ki;Lee, Chang-Soo;Im, Yong-Jin;Lee, Chung;Kim, Tae-Kyung;Lee, Hye-Jung
    • Textile Coloration and Finishing
    • /
    • v.15 no.4
    • /
    • pp.73-79
    • /
    • 2003
  • It is generally known that cotton treated with liquid ammonia has better soft handle, wrinkle recoveries and stability of appearance as compared with the alkali mercerized cotton. In this study, the various cotton fabrics treated with liquid ammonia$(NH_3)$, sodium hydroxide(NaOH) and sodium hydroxide(NaOH)/liquid ammonia$(NH_3)$ and untreated cotton fabric were investigated and compared in terms of physical properties and dyeing behavior. As the result, the strength of four kinds of cotton fabrics were similar. But the elongation of cotton treated with liquid ammonia increased slightly. Liquid ammonia treatment reduced the crystallinity of cotton and the crystalline structure of cotton transformed from cellulose 1 to mixed structure of celluloseIand III. In dyeing, dyeing rate decreased but equilibrium dye uptake increased by liquid ammonia treatment of cotton fabrics.

Electricity Generation Coupled with Wastewater Treatment Using a Microbial Fuel Cell Composed of a Modified Cathode with a Ceramic Membrane and Cellulose Acetate Film

  • Seo, Ha-Na;Lee, Woo-Jin;Hwang, Tae-Sik;Park, Doo-Hyun
    • Journal of Microbiology and Biotechnology
    • /
    • v.19 no.9
    • /
    • pp.1019-1027
    • /
    • 2009
  • A noncompartmented microbial fuel cell (NCMFC) composed of a Mn(IV)-carbon plate and a Fe(III)-carbon plate was used for electricity generation from organic wastewater without consumption of external energy. The Fe(III)-carbon plate, coated with a porous ceramic membrane and a semipermeable cellulose acetate film, was used as a cathode, which substituted for the catholyte and cathode. The Mn(IV)-carbon plate was used as an anode without a membrane or film coating. A solar cell connected to the NCMFC activated electricity generation and bacterial consumption of organic matter contained in the wastewater. More than 99% of the organic matter was biochemically oxidized during wastewater flow through the four NCMFC units. A predominant bacterium isolated from the anode surface in both the conventional and the solar cell-linked NCMFC was found to be more than 99% similar to a Mn(II)-oxidizing bacterium and Burkeholderia sp., based on 16S rDNA sequence analysis. The isolate reacted electrochemically with the Mn(IV)-modified anode and produced electricity in the NCMFC. After 90 days of incubation, a bacterial species that was enriched on the Mn(IV)-modified anode surface in all of the NCMFC units was found to be very similar to the initially isolated predominant species by comparing 16S rDNA sequences.

Autohydrolysis and Enzymatic Saccharification of Lignocellulosic Materials(III) - Recycling and Reutilization of Cellulase Enzyme - (목질 재료의 자기가수분해 및 효소당화에 관한 연구 (Ⅲ) - Cellulase 효소의 회수 및 재사용 -)

  • Cho, Nam-Seok
    • Journal of the Korean Wood Science and Technology
    • /
    • v.17 no.3
    • /
    • pp.45-51
    • /
    • 1989
  • A major problem in the enzymatic hydrolysis of lignocellulosic substrates is the very strong bonding of cellulase to lignin and even cellulose in the hydrolysis residues. This phenomenon inhibits recycle of the cellulase which is a major expense of the enzymatic hydrolysis process. In this paper, autohydrolyzed wood was delignified by two-stage with a 0.3% Na OH extraction and oxygen-alkali bleaching and was subjected to enzymatic hydrolysis with cellulase. Also, an improved almost quantitative recycle process of cellulase enzyme was discussed. In enzyme recovery by affinity method. the first recycling showed relatively high hydrolysis rate of 97.4%. Even at the third recycle. hydrolysis rate was 86.7 percents. In the case of cellulase recovery by ultrafiltration method, first 2 recycling treatments resulted very high hydrolysis rate(97.0-97.7%). Even the third recycling showed about 94.2%. Authoydrolysis of oak wood followed by 2-stage delignification with alkali and oxygen-alkali produced a substrate for enzymatic hydrolysis that allowed almost quantitative recycle of cellulase.

  • PDF

Studies on the Grassland Development in the Foerst III. Effect of fertilizer level on quality , mineral constituents and tree growth of grass-clover mixtures grown under pine trees (임간초지 개발에 관한 연구 III. 임간혼파초지에서 3요소 시비수준이 목초의 품질과 무기성분함량 및 나무생장에 미치는 영향)

  • Seo, S.;Han, Y.C.;Park, M.S.;Lee, J.Y.
    • Journal of The Korean Society of Grassland and Forage Science
    • /
    • v.5 no.3
    • /
    • pp.187-194
    • /
    • 1985
  • This field experiment was carried out to determine the effects of thirteen different fertilizer levels of nitrogen(N), phosphorus($P_2O_5$) and potassium($K_2O$) on the content of crude protein, crude fiber, mineral constituents of product and tree growth forest pasture with 40-50% shading. The experiment was arranged as a randomized block design and performed in the suburban forest of Suweon in 1984. The results obtained are summarized as follows: 1. Crude protein content and total protein yield were higher in the plot of 28 and 42kg $N/_{10a}$, regardless of $P_2O_5\;and\;K_2O$ level, while those were the lowest in zero fertilizer and N-zero fertilizer plots. 2. The contents of lignin and silica were significantly low in the high N fertilizer level, and the contents of NDF, ADF, cellulose and hemicellulose were not affected by different fertilizer levels. However, the content of crude fiber tended to be low with high N, regardless of $P_2O_5\;and\;K_2O$. 3. The contents of N,K and $SiO_2$ of grasses were influenced by different fertilizer levels. However, those of P,Ca,Ma and Na showed little differences. 4. The recovery percentage of NPK was higher in the plot of standard fertilizer level with 28-20-24 kg/10a, and higher recovery percentage was observed in $K_2O$, followed by N and $P_2O_5$ in that order. 5. The growth of tree was increased as the level of N fertilizer was increased, but no such trend was noted by $P_2O_5\;and\;K_2O$ levels. 6. Crude protein, crude fiber, some mineral contituents of grasses, and growth of tree were influenced by N level, regardless of $P_2O_5\;and\;K_2O$. And the optimum fertilizer level of $N-P_2O_5-K_2O$ seemed to be 28-20-24 kg/10a for the production of grasses with higher quality and more yield in the forest.

  • PDF