• 제목/요약/키워드: Morphotropic phase composition

검색결과 50건 처리시간 0.026초

La 변성 $Pb(Sc_{1/2}Nb_{1/2})O_3-PbTiO_3$계 요업체의 전계유기변위와 분극특성 (Field-Induced Strains and Polarization Switching Mechanisms in La-Modified $Pb(Sc_{1/2}Nb_{1/2})O_3-PbTiO_3$ Ceramics)

  • 장명철
    • 한국세라믹학회지
    • /
    • 제37권1호
    • /
    • pp.63-69
    • /
    • 2000
  • Electrically-induced strain(S) and polarization(P) for Pb(Sc1/2Nb1/2)O3-PbTiO3(1-x)PSN-xPT) crystalline solutions were studied. From the compositional dependence of S and P we could observe two maximum values at x=0.10 and x=0.425. It is considered that PSNT10(x=0.10) composition is the structural phase boundary to indicate the variable order-disorder[VOD] region. PSNT(x=0.425) composition is the morphotropic phase boundary[MPB] to indicate the rhombohedral to tetragonal phase transition. Higher S (0.437%) and P (0.3974$\mu$C/$\textrm{cm}^2$) values were attained by the La substitution (5 wt%) at Pb site in the MPB composition of 57.5PSN-42.5PT.

  • PDF

Piezoresponse Force Microscopy를 이용한 Pb(Zr,Ti)O3 세라믹의 단계적 Poling에 의한 강유전체 도메인 진화 과정 관찰 (Observation of Ferroelectric Domain Evolution Processes of Pb(Zr,Ti)O3 Ceramic Using Piezoresponse Force Microscopy)

  • 김관래
    • 한국전기전자재료학회논문지
    • /
    • 제32권1호
    • /
    • pp.20-24
    • /
    • 2019
  • Ferroelectric material properties are strongly governed by domain structures and their evolution processes, but the evolution processes of complex domain patterns during a macroscopic electrical poling process are still elusive. In the present work, domain-evolution processes in a PZT ceramic near the morphotropic phase-boundary composition were studied during a step-wise electrical poling using piezoresponse force microscopy (PFM). Electron backscatter diffraction was used with the PFM data to identify the grain boundaries in the region of interest. In response to an externally the applied electric field, growth and retreat of non-$180^{\circ}$ domain boundaries wasere observed. The results indicate that ferroelectric polarization-switching nucleates and evolves in concordance with the pattern of the pre-existing domains.

Structural and piezoelectric properties of lead-free (1-x)$(Na_{0.5}\;K_{0.5})NbO_3$-xBa($Ti_{0.9}$, $Sn_{0.1}$)$O_3$ ceramics

  • 차유정;남산;김창일;정영훈;이영진;백종후
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2009년도 춘계학술발표대회
    • /
    • pp.33.1-33.1
    • /
    • 2009
  • Lead-free (1-x)$(Na_{0.5}K_{0.5})NbO_3$-xBa($Ti_{0.9}Sn_{0.1})O_3$ [NKN-BTS-100x] ceramics doped with 1 mol% $MnO_2$ have been prepared by the conventional solid state method and their structural and piezoelectric properties were investigated. The NKN-BTS-100x ceramics exhibited a dense and homogeneous microstructure when they were sintered at $1030-1150^{\circ}C$. Grain growth was observed for the specimen sintered at relatively low temperature of $1050^{\circ}C$. A tetragonal/orthorhombic morphotropic phase boundary (MPB) in the perovskite structure was also appeared for the NKN-BTS-100x ceramics (0.04$1050^{\circ}C$. The enhanced piezoelectric properties in the NKN-BTS ceramics with a MPB composition were obtained. Especially, for the NKN-BTS-6 ceramics, a high dielectric constant (${\varepsilon}^T_3/\varepsilon_0=1,400$), piezoelectric constant ($d_{33}=237$) and electromechanical coupling factor ($k_p=0.42$) were obtained.

  • PDF

PZT 세라믹스의 전기기계결합계수 온도 안정성에 관한 연구 (Temperature Stability of Electro-mechanical Coupling Factors of PZT Ceramics)

  • 이개명
    • 한국전기전자재료학회논문지
    • /
    • 제27권1호
    • /
    • pp.27-32
    • /
    • 2014
  • In this paper, PZT piezoelectric ceramic specimens with 4 compositions (Zr/Ti=50/50, 53/47, 56/44, 58/42) in $Pb(Zr,Ti)O_3$ system were fabricated. We studied effects of poling strength and thermal aging on the temperature characteristics of eletromechanical coupling factor k31 of the specimens, which were poled with the DC electric fields, 1.5, 2.5 and 3.5 kV/mm respectively and thermally aged for an hour at $200^{\circ}C$. The eletromechanical coupling factor k31 of the specimen with the composition Zr/Ti= 53/47, nearest to the morphotropic phase boundary decreased the most greatly, irrelevant to the intensity of poling field, due to 1st thermal aging. And the temperature coefficient of eletromechanical coupling factor k31 was (-) in the tetragonal phase composition and (+) in the rhombohedral phase composition, which is reverse in the temperature coefficient of resonance frequency. It is interesting that eletromechanical coupling factor k31 of PZT ceramics is shown to be able to increase as temperature increase in the interval $-20{\sim}80^{\circ}C$.

액츄에이터 응용을 위한 Pb(Ni1/3Nb2/3)O3-PbTiO3 세라믹스의 압전 특성에 미치는 Fe2O3 첨가 영향 (Effects of Fe2O3 Addition on Piezoelectric Properties of Pb(Ni1/3Nb2/3)O3-PbTiO3 Ceramics for Actuator Applications)

  • 임은경;김창일;이영진;임종인;백종후
    • 한국전기전자재료학회논문지
    • /
    • 제19권10호
    • /
    • pp.935-941
    • /
    • 2006
  • In this paper, the dielectric and piezoelectric properties of $0.4Pb(Ni_{1/3}Nb_{2/3})O_3+0.6Pb(Zr_{405}Ti_{595})O_3+X\;wt%\;Fe_2O_3$ ceramics were investigated with the addition of $Fe_2O_3$ and sintering temperature. Dielectric constant and piezoelectric constant increased with amount of $Fe_2O_3$ to 0.25 wt% and then decreased the further addition of $Fe_2O_3$. It seems that $Fe_2O_3$ acts as a sintering aid at the sintering temperature of $1150^{\circ}C$. By the addition of $Fe_2O_3$., sintering temperature of the system was lowered from $1250^{\circ}C\;to\;1100^{\circ}C$. The piezoelectric properties showed the maximum value of ${\varepsilon}r=4669,\;d_{33}=810(10^{-12}m/V)$, kp = 77 %, Qm = 55, in $0.4Pb(Ni_{1/3}Nb_{2/3})O_3\;-0.6Pb(Zr_{0.405}Ti_{0.595})O_3+0.25wt%\;Fe_2O_3$ ceramics having composition near the morphotropic phase boundary. The composition may be appropriate for actuator materials because of high piezoelectric constant and electromechanical coupling factor.

PZT 세라믹스의 강도에 미치는 내부응력의 영향 (Effect of internal Stress on the Strength of PZT Cermics)

  • 태원필;윤여범;김송희
    • 한국세라믹학회지
    • /
    • 제33권1호
    • /
    • pp.49-55
    • /
    • 1996
  • The aim of this study is to investigate the change of bending strength and fatigue strength in the unpoled and poled Pb(Zr, Ti)O3 ferroelectrics of tetragonal morphotropic phase boundary (MPM) and rhombohedral com-position in terms of internal stress which is measured by XRD method. Before poling treatment the highest bending strength was found in rhombohedral composition. After poling treatment the bending strength decreas-ed in all compositions but it decreased most remarkably in tetragonal composition. The most prominent de-crease of bending strength after poling treatment in tetragonal was attributed to the occurrence of microcracks due to highanisotropic internal stress around grain boundary which was induced of bending strength after poling in MPB and rhombohedral composition was not due to the occurrence of microcracks but to the increase in tensile internal stress perpendicular to the direction of crack propagation by domain alignment. Fatigue strength was higher before poling treatment than after poling treatment for various compositions.

  • PDF

PZT 압전세라믹스 공진자의 공진주파수의 경시변화 (Aging of Resonant Frequency of PZT Piezoelectric Ceramic Resonantors)

  • 이개명;강찬호;김병효;황충구;고승우
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 하계학술대회 논문집
    • /
    • pp.109-114
    • /
    • 2002
  • Aging stabilities of the operating frequency of piezoelectric devices such as filter, oscillator and discriminator are very important. In this study it was studied aging stabilities of the length-extensional vibration mode of Pb(Zr$\_$y/Ti$\_$1-y/)O$_3$+x[wt%]Cr$_2$O$_3$ ceramics. PZT ceramics in Morphotropic phase boundary have higher aging rates of k$\_$31/ and resonant frequency than those in tetragonal phase or rhombohedral phase. Thermal aging moves the composition with maximum aging rate to Zr-rich side in Cr not added PZT system. Aging rate of resonant frequency of the ceramics with x=0.1, y=0.53 and x=0.3, y=0.53 increased by thermal aging.

  • PDF

소결체 및 전극의 크기와 조성이 $Pb(Mn_{1/3}Nb_{2/3})O_3 PbTiO_3-PbZrO_3$계 압전세라믹스의 공진특성에 미치는 영향 (Effect of Composition Size of Sintered Body and Electrode on Resonant Characteristics of $Pb(Mn_{1/3}Nb_{2/3})O_3 PbTiO_3-PbZrO_3$ Piezoelectric Ceramics)

  • 류영대;조상희
    • 한국세라믹학회지
    • /
    • 제23권1호
    • /
    • pp.60-66
    • /
    • 1986
  • The effect of composition size of sintered body and electrode on resonant characteristics of the system $Pb(Mn_{1/3}Nb_{2/3})O_3 PbTiO_3-PbZrO_3$ has been decribed. Composition ranged from X=40 to X=55 diameter of sintered body ranged from D=6.5 to D=12.5(mm) and diameter of electrode ranged from De=5.5 to De=11 (mm) In the composition of morphotropic phase boundary antiresonant frequency (fa) dcreased slowly whereas resonant frequency (fr) decreased rapidly on the ground of this Δf(fa-fr) and electromechanical coupling fractor Kp increased and Qm showed low value. On the contrary in toward the composition of tetragonal and rhombo-hedral fa increased slowly whereas fr increased rapidly on the ground of this Δf and Kp decreased and Qm increased abruptly. Substance of the above statements have no concern with size of sintered body and ele-ctrode. The other side as the size of electrode decreased Qm fr, fa and Δf increased. Cm and Co dominantly affect the resonant frequency and antiresonant frequency.

  • PDF

Pb(Zn, Nb)$O_3$-Pb(Ni, Nb))$O_3$-$PbTiO_3$-$PbZrO_3$계 세라믹스의 소결 및 전기적 특성 (Sintering and Electric Prooperties of Pb(Zn, Nb)$O_3$-Pb(Ni, Nb))$O_3$-$PbTiO_3$-$PbZrO_3$ System)

  • 박재성;이기태;남효덕
    • 한국세라믹학회지
    • /
    • 제27권7호
    • /
    • pp.934-942
    • /
    • 1990
  • The quarternary system ceramics 0.5[yPb(Zn1/3Nb2/3)O3-(1-y)Pb(Ni1/3Nb2/3)O3]-0.5[xPbTiO3-(1-x)PbZrO3](PZN-PNN-PT-PZ) was fabricated by the columbite precursor method to obtain a stabilized perovskite structure and by conventional method to evaluate the efficiency of the former methd. Dielectric and piezoelectric properties were investigated and the stability of the perovskite phase was studied as a function of PZN and PT contents and firing temperature. In the samples prepared by the columbite precursor method, the pyrochlore phase, which is detrimental to both the dielectric and piezoelectric properties, was not observed in the absence of PZN, and electric properties were improved even when fabricated at low temperature. By adding PZN, some pyrochlore phase appeared and the morphotropic phase boundary of the samples shifted to more Zr-rich composition. The temperature dependence of piezoelectric constant decreased with the addition of PZN, due to the rising of the Curie point.

  • PDF

PZT 세라믹스에 있어서 길이진동모드의 경시변화 (Aging of Length-Extensional Vibration Modes in PZT Ceramics)

  • 이개명;김병효;황충구;강찬호;현덕수
    • 한국전기전자재료학회논문지
    • /
    • 제15권10호
    • /
    • pp.858-864
    • /
    • 2002
  • Aging stabilities of the operating frequency of piezoelectric devices such as filter, oscillator and discriminator are very important. In this study it was studied aging stabilities of the length-extensional vibration mode of Pb(Zr$\^$y/O$_3$+ x[wt%]Cr$_2$Co$_3$ ceramics. PZT ceramics in morphotropic phase boundary have higher aging rates of k$\_$31/ and resonance frequency than those in tetragonal phase or rhombohedral phase. Thermal aging moves the composition with maximum aging rate to Zr-rich side in Cr$_2$O$_3$ not added PZT system. In the PZT system, aging rates of k$\_$31/ and resonance frequency for first 30 days are bigger than those for the following 90 days. Thermal aging decrease those for first 30 days. Aging rate of resonance frequency of the ceramics with x=0.1, y=0.53 and x=0.3, y=0.53 increased by thermal aging.