A Study on Treatment and Recycling of Waste Fluid Sand from the Fluidized Bed Incinerator (유동상식 소각로에서 발생되는 폐유동사(廢流動床) 처리 및 재활용 방안)

  • Lee, Seung-Won
    • Journal of Environmental Science International
    • /
    • v.29 no.11
    • /
    • pp.1015-1024
    • /
    • 2020
  • Using the waste(sand wastr and boiler ash) in fluidized bed inciverator, lightweight aggregate concrete was produced and a recycling plan was prepated. The first, the result of the leaching test shows that the waste fluid sand and boiler ash did not exceed the effluent standard. This indicates that there is no harmful effect for recycling. The second, in the lightweight aggregate test using waste fluid sand and boiler ash, the sample that combined cement, waste fluid sand, and sand showed the highest compressive strength, and the mix proportion was 10: 7: 3. Lightweight aggregate concrete that combined cement, waste fluid sand, boiler ash, and sand had a low compressive strength by and large. The third, the same results were identified in the relation between the content of SiO2 and that of Na2O. As the SiO2 content is lowered, the overall viscosity and plasticity of the concrete also decrease, which is not a good condition to form concrete. As for Na2O, as the content increases, the viscosity of the sample and the viscosity of the cement are remarkably lowered, and the strength of the finished concrete is lowered. Therefore, it was concluded that the higher the content of SiO2 and the lower the content of Na2O, the more suitable it is to mix with cement to produce concrete. Fourth, from the fluidized bed incinerator currently operated by company A in city B, a total of 14,188 tons/year were discharged as of 2016, including 8,355 tons/year of bottom ash (including waste fluid sand) and 5,853 tons/year of boiler ash. The cost for landfill bottom ash and boiler ash discharged is 51,000 won/ton, and the total annual landfill cost is 723,588,000 won/ year. Assuming that the landfill tax to be applied from the year 2018 is about 10,000 won/ton, and if there is no reduction in waste disposal charge, an additional landfill tax of 141,880,000 won/year will be imposed. Consequently, the sum total of the annual landfill cost will be 865,468,000 won/year. Therefore, if the entire amount is used for recycling, the annual savings of about 8.7 billion won can be expected.

A Study on Rheological Properties of Cement Paste using Expansive Additives by Kind & Replacement Ratio (팽창재 종류 및 치환율에 따른 시멘트 페이스트의 레올로지 특성)

  • Park, Chun-Young;Kang, Byeung-Hee
    • Journal of the Korea Institute of Building Construction
    • /
    • v.8 no.2
    • /
    • pp.99-106
    • /
    • 2008
  • To improve concrete tensile strength and bending strength, New plan that have more economical and simple manufacture process is groped. By an alternative plan, chemical pre-stressed concrete is presented. In this study, we analyzed the rheological properties of cement paste with the kind and replacement ratio of k-type CSA type expansive additives that is used mainly in domestic. and we suggested that the algorithm of a mixing plan in the chemical pre-stressed concrete and from this, we presented the basic report for the right mixing plan. From the results, Flow increased more or less according to use of expansive additives. This phenomenon was observed by increasing paste amount that shows as substitution for expansive additives that specific gravity is smaller than that of cement. As linear regression a result supposing paste that mix expansive additives by Bingham plastic fluid. The shear rate and shear stress expressed high interrelationship. therefore, flow analysis of quantitative was available. The plastic viscosity following to replacement ratio of expansive additives is no change almost, the yield value is decreased in proportion to the added amount of expansive additives. Through this experiment, we could evaluate rheological properties of cement paste using the expansive additives. Hereafter by an additional experiment, we must confirm stability assessment of material separation by using the aggregate with the kind and replacement ratio of expansive additives.

The Properties of Flexural Strength and Density of Extrusion Molding Concrete Panel Using Sepiolite (세피올라이트를 이용한 압출성형 콘크리트 패널의 휨강도 및 밀도 특성)

  • Jung, Eun-Hye;Kang, Cheol;Kim, Jae-Won;Lee, Jung-Koo;Choi, Hun-Gug;Kim, Jin-Man
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2006.05b
    • /
    • pp.49-52
    • /
    • 2006
  • Extrusion concrete panel is made by extrusion of high viscosity paste. The high viscosity paste is made by mix of cement, silica, reinforced fiber and thickening agent in the dry mixer and wet mixer subsequently, extrusion in the extruder, and curing in the normal steam curer and high pressure steam curer subsequently. To increase a flexural strength of the panel, it is used inorganic fiber as like asbestos. But it was known that the asbestos was harmful to human being lately, in the domestic area it is restricted usage in the construction materials. So, it is demanded the alternative material for asbestos in the extrusion concrete panel. This study is to investigate that the sepiolite is possible to be the alternative of asbestos. The 3 types of sepiolite is applied to the extrusion concrete panel. To investigate the properties of the panel with sepiolite, it is compared the control with asbestos in the flexural strength, the specific density and the spot compressive strength. From the test results, it was found that the panel with sepiolite B is higher than the control with asbestos in the flexural strength and in the density.

  • PDF

A STUDY ON THE PHYSICAL CHARACTERISTICS OF THE THREE COMMONLY USED DIE SPACING MATERIALS (여러 가지 Die spacing material의 물리적 성질에 대한 연구)

  • Moon, Hong-Seok;Kim, Jong-Jin
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.37 no.5
    • /
    • pp.640-650
    • /
    • 1999
  • As an optimal quality of the restorations, there should be a least amount of seating discrepancy between the casting and abutment teeth. However, high viscosity of the cementing medium and its resulting thickness may prevent complete seating of the restoration. The use of die spacing material provides adequate internal relief for the cementing medium. The purpose of this study is to compare the thickness of three commonly used die spacing materials. Materials and Methods: Stone plates were fabricated and divided into 12 sections to be painted with die spacers. Tru-Fit, Whip-Mix and Belle do St. Claire die spacer which are commonly used in dental practice were tested in this study. Each die spacers were painted layer by layer according to the manufacturer's recommendation. The average thickness of each die spacers were measured with light microscope(${\times}100$) and compared between them. Results and Conclusions. A silver-colored Tru-Fit die spacer has the lowest value of thickness without statistical significance comparing with a gold-colored Tru-Fit die spacer and a gray layer of Whip-Mix die spacer has the highest value of thickness without any statistical significance comparing with Belle de St. Claire die spacer. Three and four layers of Tru-Fit die spacer and two layers of Whip-Mix and Belle de St. Claire die spacers seem to be in the acceptable range of thickness of 25 to $45{\mu}m$ for optimal seating of the restorations. The standard experimental design and method should be fur thor evaluated for more consistent and objective results.

  • PDF

Evaluation of Field Application for the mix properties of the thixotropic grout (가소성그라우트의 배합특성 및 현장 적용성 평가)

  • Kim, Hak-Moon;Jang, Kyung-Jun
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.12 no.9
    • /
    • pp.4223-4238
    • /
    • 2011
  • The advantages of grouting are the simple instrument, the simple procedure of practice and the simple verification of grouting result. but the more grouting practice there is, the more damages of environment from grouting practice and grouting materials there are. so, the grouting materials and methods with the character of environment friendly are introduced in construction field, recently. This paper is to study of the physical characteristics that has thixotropic character and that consists of inorganic and polycarboxylate co-polymer. In study, various testing methods are performed such as a viscosity, a thixotropy, a compressive strength, a heavy metal detection and pH measurement in lab test and a low pressure injection test and a high pressure injection test in field with different soil type. As a result, a optimum mix ratio is proposed by analyzing the result of lab test. the field applicability is verified by checking a injection pressure, a grout volume and a hardened body of grout by excavating the practice site.

Physical Properties and Low Temperature Resistance of Recycled Binder (재생 아스팔트 바인더의 물리적 특성과 저온균열 저항성 연구)

  • Lee, Young-Gwan;Kim, J.E.;Do, Young-Soo;Kim, Kwang-Woo
    • International Journal of Highway Engineering
    • /
    • v.6 no.4 s.22
    • /
    • pp.1-12
    • /
    • 2004
  • This study evaluated the asphalt binder characteristics for the hot-recycled asphalt mixture in which RAP was added in ambient temperature for surface course as well as for base course. RAPs were collected from four sources and their physical properties were evaluated. Mix designs were performed using 10 and 20% RAP contents for surface courses and 10, 20 and 30% for base courses. A virgin asphalt with the penetration grade of 60-80 was used for mixing recycled mixtures. Physical properties of recycled binders, including penetration, absolute viscosity, GPC, BBR and penetration after TFO were measured. From the results, regression analysis of absolute viscosity versus LMS in GPC showed $R^2$ being over 0.95, showing that GPC results estimate the absolute viscosity with relative accuracy. In BBR test, the resistance of recycled mixtures at low service temperature was inferior to the control, because the low temperature PG of recycled binder was one grade higher than that of the control binder.

  • PDF

Effect of AP Particle Size on the Physical Properties of HTPB/AP Propellant (AP 입자가 HTPB/AP 추진제의 물리적 특성에 미치는 효과)

  • Yim, Yoo Jin;Park, Eun Ji;Kwon, Tae Ha;Choi, Seong Han
    • Journal of the Korean Society of Propulsion Engineers
    • /
    • v.20 no.1
    • /
    • pp.14-19
    • /
    • 2016
  • The viscosity and mechanical property of HTPB/AP composite solid propellant are profoundly affected by particle size of AP. In HTPB/AP propellant formulated by two mode of AP size such as $190{\mu}m$ and $7{\mu}m$, the propellant was found to be much less viscose at end of mix when coarse/fine AP ratio is ranged from 70/30 to 60/40 due to high solid packing fraction. It was shown that the toughness of tensile strength test for HTPB/AP propellant increased with the increase in coarse AP. Considering both lower viscosity and better tensile strength, the optimum ratio of AP coarse/fine was estimated to be 70/30.

Development of inorganic thixotropic-grout for backfilling of shield TBM tail voids and its compatibility (쉴드 TBM 뒤채움용 무기계 가소성 그라우트의 개발 및 적합성 평가)

  • Kim, Dae-Hyun;Jung, Du-Hwoe;Jeong, Gyeong-Hwan
    • Journal of Korean Tunnelling and Underground Space Association
    • /
    • v.11 no.3
    • /
    • pp.277-286
    • /
    • 2009
  • A suitability of a thixotropic grout developed in this study has been examined through laboratory tests on strength, segregation, and viscosity. The thixotropic grout is a mixture of two types of liquid components. The A-liquid component consists of cement, water, and MG-A and the B-liquid component consists of scarlet, water, and MG-B. Unconfined compressive strength of specimens prepared with a prefer mix-proportion satisfied a design criteria for the backfilling of tail voids. A material segregation phenomenon under water condition was not observed in the thixotropic grout whereas it was observed in the existing silica-type grout. In addition, viscosity tests have been rallied out on the thixotropic grout to verify the capability of a long-distance delivery in the field. Both the A-liquid component and the B-liquid component maintained a viscosity of below 2,000 cP for 120 minutes. This experimental result confirms that two liquid components guarantees a long-distance delivery in tile field application.

Effect of Antioxidants on the Oxidative Stability of Biodiesel Fuels (항산화제가 바이오디젤유의 산화안정성에 미치는 영향)

  • Ryu, Kyung-Hyun
    • Transactions of the Korean Society of Automotive Engineers
    • /
    • v.15 no.6
    • /
    • pp.81-86
    • /
    • 2007
  • Biodiesel fuel that consists of saturated and unsaturated long-chain fatty acid alkyl esters is an alternative diesel fuel produced from vegetable oils or animal fats. However, air causes autoxidation of biodiesel fuel during storage, which can reduce fuel quality by adversely affecting its properties, such as the kinematic viscosity and acid value. One approach for improving the resistance of fatty derivatives to autoxidation is to mix them with antioxidants. This study investigated the effectiveness of five such antioxidants in mixtures with biodiesel fuels produced by three biodiesel manufacturers : tert-butylhydroquinone (TBHQ), butylated hydroxyanisole (BHA), butylated hydroxytoluene (BHT), propyl gallate (PrG) and $\alpha$-tocopherol. Oxidation stability was determined using Rancimat equipment. The results show that TBHQ, BHA, and BHT were the most effective and $\alpha$-tocopherol was the least effective at increasing the oxidation stability of biodiesel. This study recommends that TBHQ and PrG be used for safeguarding biodiesel fuel from the effects of autoxidation during storage.

Experimental studies on rheological properties of smart dynamic concrete

  • Bauchkara, Sunil D.;Chore, H.S.
    • Advances in concrete construction
    • /
    • v.5 no.3
    • /
    • pp.183-199
    • /
    • 2017
  • This paper reports an experimental study into the rheological behaviour of Smart Dynamic Concrete (SDC). The investigation is aimed at quantifying the effect of the varying amount of mineral admixtures on the rheology, setting time and compressive strength of SDC containing natural sand and crushed sand. Ordinary Portland cement (OPC) in conjunction with the mineral admixtures was used in different replacement ratio keeping the mix paste volume (35%) and water binder ratio (0.4) constant at controlled laboratory atmospheric temperature ($33^{\circ}C$ to $35^{\circ}C$). The results show that the properties and amount of fine aggregate have a strong influence on the admixture demand for similar initial workability, i.e., flow. The large amounts of fines and lower value of fineness modulus (FM) of natural sand primarily increases the yield stress of the SDC. The mineral admixtures at various replacement ratios strongly contribute to the yield stress and plastic viscosity of SDC due to inter particle friction and cohesion.