• Title/Summary/Keyword: Microstructure properties

Search Result 4,066, Processing Time 0.032 seconds

A Study on the Control of Microstructures of Polyalphaolefins via Cationic Polymerization (양이온 중합을 이용한 폴리알파올레핀의 미세구조 조절에 관한 연구)

  • Ko, Young Soo;Kwon, Wan-Seop;No, Myoung-Han;Yim, Jin-Heong
    • Polymer(Korea)
    • /
    • v.39 no.2
    • /
    • pp.346-352
    • /
    • 2015
  • Polyalphaolefin (PAO) is a synthetic lubricant that is superior to mineral-based lubricants in the terms of physical and chemical characteristics such as low pour point, high viscosity index (VI), and thermal and oxidation stability. Several kinds of PAOs have been synthesized by using 1-pentene, 1-hexene, 1-octene, or 1-dodecene as monomer with three kinds of aluminum-based Lewis acid catalysts via cationic polymerization. The control of the catalytic performance and physical properties of PAO such like molecular weight, kinematic viscosity, pour point, and viscosity index was done by changing polymerization parameters. The alkyl aluminum halide-based catalysts show better catalytic activity than that of the conventional $AlCl_3$ catalyst. The microstructure of PAO was investigated by means of TOF-MS (time of flightmass spectroscopy) analysis in order to elucidate the correlation between the performances of the lubricant (VI, pour point) and the molecular structure of PAO. The VI of PAO increases with increases in the carbon number of ${\alpha}$-olefin. In other words, the performances of PAO as a lubricant strongly depended on the branch length of PAO.

A Study on the Electromagnetic Property of NiCuZn Ferrite by Additive Bi2O3 and ZrO2 (Bi2O3와 ZrO2가 Ni-Cu-Zn Ferrite의 전자기적 특성에 미치는 영향 연구)

  • Son, Kyung-Ik;Koh, Jae-Gui
    • Journal of the Korean Magnetics Society
    • /
    • v.16 no.4
    • /
    • pp.201-205
    • /
    • 2006
  • The electromagnetic properties and microstructure of the basic composition of $(Ni_{0.2}Cu_{0.2}ZnO_{0.2})_{1.02}(Fe_{2}O_{3})_{0.98}$ were invested, changing the amount of the additives $Bi_2O_3$ and $ZrO_2$ and sintering temperature. The spinel structure of specimen was confirmed by the analysis of XRD patterns. Grain size and its density are increased by increasing the additive and the sintering temperature.However, the permeability increased with decreasing additive. It was also found that $Bi_2O_3$ had more effect on the increase of grain size and permeability rather than $ZrO_2$.

Characteristics of $CO_2$ or Nd:YAG Laser Welded 600MPa Grade TRIP Steel (600MPa급 TRIP강의 $CO_2$ 및 Nd:YAG 레이저 용접부의 특성)

  • Han, Tae-Kyo;Kim, Seung-Jun;Lee, Bong-Keun;Kim, Dae-Up;Kang, Chung-Yun
    • Journal of Welding and Joining
    • /
    • v.24 no.1
    • /
    • pp.56-63
    • /
    • 2006
  • The characteristics of $CO_2$ or Nd:YAG laser welded 600MPa ade TRIP steel was investigated. He or Ar gas was used as a shield gas in case of $CO_2$ laser welding, but the shield gas was not used in case of Nd:YAG laser welding. Bead on plate welding was performed with various welding conditions. Defects in the joints of both welding type occurred at 1.8m/min but were not observed over the welding speed of 2.1m/min in case of Nd:YAG laser welding. However, porosity occurred in $CO_2$ laser welding and the tendency of decreasing with the increase of welding speed. The hardness was the highest at heat affected zone near fusion zone as well as at the fusion zone and decreased on approaching the base metal. In a perpendicular tensile test to the weld line, all specimens that have been welded at optimum conditions were fractured at the base metal, and the tensile properties showed the rather higher than those of raw material. In a parallel tensile test, the strength of the joints was higher than that of the base metal. Elongation was found to be lower than that of the raw material. Forming height by Erichsen test and elongation were deeply related with the ratio of base metal/weld metal and the maximum hardness of the weld metal. Also porosity induced to decrease the strength and the elongation. The maximum formability was recorded at approximately 80% as compared with that of the raw material with the optimum condition.

Crack Path Behavior of SiC Based Tools for Spectacle Lens Cutting (렌즈절삭용 탄화규소계 공구의 크랙전파 거동)

  • Lee, Young-Il
    • Journal of Korean Ophthalmic Optics Society
    • /
    • v.11 no.2
    • /
    • pp.85-89
    • /
    • 2006
  • To research of the improved mechanical properties of materials for spectacle lens cutting, SiC and TiC were used as the main powder. Also, $Al_2O_3$ and $Y_2O_3$ was included as a sintering additive. The weight ratio of the alumina($Al_2O_3$) to yttria($Y_2O_3$) was set to 1:1. The materials for spectacle lens cutting were fabricated by hot-pressing at $1810^{\circ}C$ for 1h and subsequently annealed at $1860^{\circ}C$ for 3, 6 and 12h to initiated grain growth. The longer annealing time is, the bigger the grain size is. The microstructures were observed by scanning electron microscopy (SEM). The SEM images were quantitatively analyzed by image analysis (Image-Pro Plus, Media Cybernetics, Maryland, U.S.A.). Crack deflection by elongated SiC grains was most frequently observed as the dominant toughening mechanism. Crack deflection was generally observed for elongated SiC grains with aspect ratio(AR) > 2.5 and grain thickness < $2.3{\mu}m$. Crack bridging was also observed as one of the operating toughness mechanism.

  • PDF

Measurement of Hardness of Constituent Phases in Ti(C0.7N0.3)-NbC-Ni Cermets Using Nanoindentation (나노인덴테이션을 이용한 Ti(C0.7N0.3)-NbC-Ni 써멧 구성상의 경도평가)

  • Kim, Seong-Won;Kim, Dae-Min;Kang, Shin-Hoo;Ryu, Sung-Soo;Kim, Hyung-Tae
    • Journal of Powder Materials
    • /
    • v.15 no.6
    • /
    • pp.482-488
    • /
    • 2008
  • The indentation technique has been one of the most commonly used techniques for the measurement of the mechanical properties of materials due to its experimental ease and speed. Recently, the scope of indentation has been enlarged down to the nanometer range through the development of instrumentations capable of continuously measuring load and displacement. In addition to testing hardness, the elastic modulus of submicron area could be measured from an indentation load-displacement (P-h) curve. In this study, the hardness values of the constituent phases in Ti($C_{0.7}N_{0.3}$)-NbC-Ni cermets were evaluated by nanoindentation. SEM observation of the indented surface was indispensable in order to separate the hardness of each constituent phase since the Ti($C_{0.7}N_{0.3}$)-based cermets have relatively inhomogeneous microstructure. The measured values of hardness using nanoindentation were ${\sim}20$ GPa for hard phase and ${\sim}10$ GPa for binder phase. The effect of NbC addition on hardness was not obvious in this work.

The Influence of Heat Treatment Temperature on Microstructure and Corrosion Behavior of SDSS Tube (SDSS (Super Duplex Stainless Steel) 강관의 미세조직 및 부식특성에 미치는 열처리 온도의 영향)

  • Lee, Insup;Cheon, Chang-seok;Yim, Tai-Hong;Han, Yoon-Ho;Lee, Myon-Hag
    • Journal of the Korean institute of surface engineering
    • /
    • v.48 no.6
    • /
    • pp.329-334
    • /
    • 2015
  • The aim of this paper is to determine the proper heat treatment temperature for SDSS tube production without ${\sigma}$-phase precipitation. When Mother steel tube was heat treated at $800^{\circ}C$ temperature, relatively a large amount of ${\sigma}$-phase precipitated and grain refinement of ferrite phase occurred simultaneously. However, in Pilgered and Drawn steel tubes, grain refinement of the ferrite phase did not occur and a small amount of ${\sigma}$-phase precipitated. For all three types of steel tubes, the pitting potential was reduced to 2/5 or less compared with the untreated one and corrosion also occurred in the salt spray test due to the precipitation of ${\sigma}$-phase. When heat treatment temperature was $900^{\circ}C$, grain refinement of the ferrite phase occurred and very little ${\sigma}$-phase precipitated in Pilgered and Drawn steel tubes. But when heat treatment was done at $1,000^{\circ}C$ temperature, all three types of steel tubes had a similar corrosion properties of that of untreated one and also corrosion did not occur in the salt spray test, as ${\sigma}$-phase did not precipitate. Therefore, the optimum heat treatment temperature range is determined to be more than $1000^{\circ}C$ for the SDSS at which corrosion does not occur.

Fabrication Process and Forming Analysis of Fuel Cell Bipolar Plate by Injection Condition of Vacuum Die Casting (진공 다이캐스팅 공법의 사출조건에 따른 연료전지용 분리판 성형 해석 및 제조 공정)

  • Jin, Chul-Kyu;Jang, Chang-Hyun;Kim, Jae-Sung;Choi, Jae-Won;Kang, Chung-Gil
    • Journal of Korea Foundry Society
    • /
    • v.31 no.5
    • /
    • pp.274-283
    • /
    • 2011
  • The vacuum die casting is a promising candidate of the stamping process for fabrication of fuel cell bipolar plate due to its advantages, such as precision casting, mass production and short production time. This study proposes vacuum die casting process to fabricate bipolar plates in fuel cell. Bipolar plates were fabricated under various injection conditions such as molten metal temperature and injection velocity. Also, according to injection velocity conditions, simulation results of MAGMA soft were compared to the experimental results. In case of melt temperature $650^{\circ}C$, misrun occurred. When the melt temperature was $730^{\circ}C$, mechanical properties were low due to dendrite microstructure. Injection velocity has to set at more than 2.0 m/s to fabricate the sound sample. When melt temperature, injection velocity (Fast shot), and vacuum pressure are $700^{\circ}C$, 2.5 m/s and 30 kPa respectively, sample had good formability and few casting defects. Simulation results are mostly in agreement with experimental results.

Characteristics of Bulk and Coating in Gd2-xZr2+xO7+0.5x(x = 0.0, 0.5, 1.0) System for Thermal Barrier Coatings

  • Kim, Sun-Joo;Lee, Sung-Min;Oh, Yoon-Suk;Kim, Hyung-Tae;Jang, Byung-Koog;Kim, Seongwon
    • Journal of the Korean Ceramic Society
    • /
    • v.53 no.6
    • /
    • pp.652-658
    • /
    • 2016
  • Gadolinium zirconate, $Gd_2Zr_2O_7$, is one of the most versatile oxides among the new thermal-barrier-coating (TBC) materials for replacing conventional yttira-stabilized zirconia (YSZ). $Gd_2Zr_2O_7$ exhibits excellent properties, such as low thermal conductivity, high thermal expansion coefficient comparable with that of YSZ, and chemical stability at high temperature. In this study, bulk and coating specimens with $Gd_{2-x}Zr_{2+x}O_{7+0.5x}$ (x = 0.0, 0.5, 1.0) compositions were fabricated in order to examine the characteristics of this gadolinium zirconate system with different Gd content for TBC applications. Especially, coatings with $Gd_{2-x}Zr_{2+x}O_{7+0.5x}$ (x = 0.0, 0.5, 1.0) compositions were produced by suspension plasma spray (SPS) with suspension of raw powder mixtures prepared by planetary milling followed by ball milling. Phase formation, microstructure, and thermal diffusivity were characterized for both sintered and coated specimens. Single phase materials with pyrochlore or fluorite were fabricated by normal sintering as well as SPS coating. In particular, coated specimens showed vertically-separated columnar microstructures with thickness of $400{\sim}600{\mu}m$.

Growth and characterization of oxide buffer layer on IBAD_MgO template for HTS coated conductors (박막형 고온초전도 선재를 위한 산화물 완충층의 IBAD_MgO 기판에서의 성장과 특성)

  • Ko, Rock-Kil;Jang, Se-Hoon;Ha, Hong-Soo;Kim, Ho-Sup;Song, Kyu-Jeong;Ha, Dong-Woo;Oh, Sang-Soo;Park, Chan;Moon, Seung-Hyun;Kim, Young-Cheol
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.06a
    • /
    • pp.297-297
    • /
    • 2008
  • Buffer layers play an important role in the development of high critical current density coated conductor. $LaMnO_3$, $SrTiO_3$ and $BaZrO_3$ buffer layers were compatible with MgO surfaces and also provide a good template for growing high current density REBCO(RE=Rare earth) films. Systematic studies on the influences of pulsed laser deposition parameters (deposition temperature, deposition pressure, processing gas, laser energy density, etc.) on microstructure and texture properties of $LaMnO_3$, $SrTiO_3$ and $BaZrO_3$ films as buffer layer deposited on ion-beam assisted deposition MgO (IBAD_MgO) template by pulse laser deposition method, were carried out. These results will be presented together with the discussion on the possible use of this material in HTS coated conductor as buffer.

  • PDF

Effect of Transition Metal on Properties of SiC Electroconductive Ceramic Composites (SIC 도전성 세라믹 복합체의 특성에 미치는 천이금속의 영향)

  • 신용덕;오상수;주진영
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.53 no.7
    • /
    • pp.352-357
    • /
    • 2004
  • The composites were fabricated, respectively, using 61vol.% SiC - 39vol.% TiB$_2$ and using 61vo1.% SiC - 39vo1.% WC powders with the liquid forming additives of 12wt% $Al_2$O$_3$+Y$_2$O$_3$ by pressureless annealing at 180$0^{\circ}C$ for 4 hours. Reactions between SiC and transition metal TiB$_2$, WC were not observed in this microstructure. The result of phase analysis of composites by XRD revealed SiC(6H), TiB$_2$ and YAG(Al$_{5}$Y$_3$O$_{12}$) crystal phase on the SiC-TiB$_2$, and SiC(2H), WC and YAG(Al$_{5}$Y$_3$O$_{12}$) crystal phase on the SiC-WC composites. $\beta$\$\longrightarrow$$\alpha$-SiC phase transformation was ocurred on the SiC-TiB$_2$, but $\alpha$\$\longrightarrow$$\beta$-SiC reverse transformation was not occurred on the SiC-WC composites. The relative density, the vicker's hardness, the flexural strength and the fracture toughness showed respectively value of 96.2%, 13.34GPa, 310.19Mpa and 5.53Mpaㆍml/2 in SiC-WC composites. The electrical resistivity of the SiC-TiB$_2$ and the SiC-WC composites is all positive temperature coefficient resistance(PTCR) in the temperature ranges from $25^{\circ}C$ to 50$0^{\circ}C$. 2.64${\times}$10-2/$^{\circ}C$ of PTCR of SiC-WC was higher than 1.645${\times}$10-3/$^{\circ}C$ of SiC-TiB$_2$ composites.posites.