• 제목/요약/키워드: Mg-Al alloys

검색결과 350건 처리시간 0.024초

대전류 및 용가재 직경에 따른 Al5083 아크 용접부 마그네슘 기화 및 기계적 성질 (Effects of High Current and Welding Wire Diameter on the Magnesium Vaporization and Mechanical Properties of Al5083 Arc Welds)

  • 권혜미;박철호;홍인표;강남현
    • Journal of Welding and Joining
    • /
    • 제31권6호
    • /
    • pp.84-89
    • /
    • 2013
  • The demand of LNG tank and the constituting material, i.e., the Al5083 thick plate, increased due to the rapid growth LNG market. To weld the Al5083 thick plate, the gas metal arc welding (GMAW) of high current is necessary to increase manufacturing productivity incurred by the multi pass welding. However, the arc welding vaporizes the volatile element such as magnesium (Mg). This phenomenon changes the Mg composition of the weld metal and the mechanical properties. The study investigated the weldability of Al5083 alloys after conducting high current GMAW. The Al5083 alloy was welded by using different size of welding wires and high current (800-950A). As the arc current increased from 800A to 950A, the mechanical strength decreased and the secondary dendrite arm spacing (SDAS) increased. Even though the arc current increased SDAS, the mechanical strength decreased due to the Mg loss in the weldment. The large diameter of welding wire decreased the dilution of the weld, therefore increasing the Mg content and the strength of the weld. For the reason, the content of Mg in welds was a major parameter to determine the mechanical property for the high current GMAW. For the arc current between 800A and 950A, the yield strength of the weldments showed a relationship with the weight percent of Mg content ($X_{Mg}$): Y.S = 27.9($X_{Mg}$)-11.

Al-Si-Cu계 합금의 주조법과 용체화처리 조건이 기계적 특성변화에 미치는 영향 (Effects of the Solid Solution Treatment Conditions and Casting Methods on Mechanical Properties of Al-Si-Cu Based Alloys)

  • 문민국;김영찬;김유미;최세원;강창석;홍성길
    • 한국주조공학회지
    • /
    • 제38권6호
    • /
    • pp.111-120
    • /
    • 2018
  • In this study, the effects of two different casting methods (gravity casting and, diecasting) and various solid-solution conditions on the mechanical properties of ASC (Al-10.5wt%Si-1.75wt%Cu) and ALDC12 (Al-10.3wt%Si-1.72wt%Cu-0.76wt%Fe-0.28wt% Mn-0.32wt%Mg-0.9wt%Zn) alloys were investigated. A thermodynamic solidification analysis program (PANDAT) was used to predict the liquidus, solidus, and phases of the used alloys. In the results of an XRD analysis, ${\beta}$-AlFeSi peaks were observed only in the ALDC12 alloy regardless of the casting method or SST (solid-solution treatment) conditions. However, according to the results of a FE-SEM observation, both ${\theta}(Al_2Cu)$ and ${\beta}$-AlFeSi were found to exist besides ${\alpha}$-Al and eutectic Si in the gravity-casted ASC alloy at $500^{\circ}C$ after a SST of 120min. The ${\alpha}$-AlFeSi and ${\beta}$-AlFeSi phases including the eutectic phases were also found to exist in the ALDC12 alloy. The results of a microstructural observation and analyses by XRD, FE-SEM and EDS were in good agreement with the PANDAT results. The gravity-casted ALDC12 and ASC specimens showed the highest Y.S. and UTS values after aging for three hours at $180^{\circ}C$ after a SST at $500^{\circ}C$ for 30min. At longer solid-solution treatment times at $500^{\circ}C$ in the gravity-casted ALDC12 and ASC specimens, the elongations of the ASC alloys increased, whereas they decreased slightly in the ALDC12 alloys.

해양환경용 알루미늄 합금 재료의 전기화학적 부식 손상 특성 (Electrochemical Corrosion Damage Characteristics of Aluminum Alloy Materials for Marine Environment)

  • 김성진;황은혜;박일초;김성종
    • 한국표면공학회지
    • /
    • 제51권6호
    • /
    • pp.421-429
    • /
    • 2018
  • In this study, various electrochemical experiments were carried out to compare the corrosion characteristics of AA5052-O, AA5083-H321 and AA6061-T6 in seawater. The electrochemical impedance and potentiostatic polarization measurements showed that the corrosion resistance is decreased in the order of AA5052-O, AA5083-H321 and AA6061-T6, with AA5052-O being the highest resistant. This is closely associated with the property of passive film formed on three tested Al alloys. Based on the slope of Mott-Schottky plots of an n-type semiconductor, the density of oxygen vacancies in the passive film formed on the alloys was determined. This revealed that the defect density is increased in the order of AA5052-O, AA5083-H321 and AA6061-T6. Considering these facts, it is implied that the addition of Mg, Si, and Cu to the Al alloys can degrade the passivity, which is characterized by a passive film structure containing more defect sites, contributing to the decrease in corrosion resistance in seawater.

Al-Cu-Mg합금의 일방향응고시 로온도에 따른 응고거동변화 (Effects of the Furnace Temperature on the Growth Behavior of Directionally Solidified Al-Cu-Mg Alloy)

  • 문철희
    • 한국주조공학회지
    • /
    • 제17권6호
    • /
    • pp.545-551
    • /
    • 1997
  • 14 cm length Al-15Cu-1Mg alloys have been directionally solidified in 3 mm diameter alumina tubes in a furnace moved with a constant velocity V=12 cm/hr under various furnace temperatures of 660, 710 and $760^{\circ}C$. By analysing the evolution of the temperature profiles along the alloy length during the solidification, the growth characteristics such as the position of the solid/liquid interface, the local growth velocity (R) and the temperature gradient at the solid/liquid interface (G) have been determined. The effects of the furnace temperature on the growth behavior have been investigated by the comparison of R and G values for each temperature. Under the furnace temperature of $760^{\circ}C$, steady state growth region was observed for the latter half of the growth period.

  • PDF

Al-10%Si-0.3%Mg 합금에서 Sr첨가가 미세조직 및 기계적 성질에 미치는 영향 (Effects of Sr Additions on Microstructures and Mechanical Properties in Al-10%Si-0.3%Mg Alloy)

  • 김경현;이정무;정신검
    • 한국주조공학회지
    • /
    • 제13권1호
    • /
    • pp.94-101
    • /
    • 1993
  • The effects of strontium content as modifier on microstructure and mechanical properties were studied in Al-10%Si-0.3%Mg cast alloys. There were not big differences in the form of eutectic Si particle and its morphology depending on adding amount of strontium, but the alloy modified by 0.012%Sr had shown the higher values than the alloy modified 0.038%Sr in strength, elongation and impact value.

  • PDF

레이저 용접시 분광학적 수법에 의한 증발입자의 거동과 플라즈마 물성의 계측 (Evaporating Particle Behaviors and plasma Parameters by Spectroscopic Method in laser Welding)

  • 김윤해
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제23권4호
    • /
    • pp.514-522
    • /
    • 1999
  • The laser-induced plasma affects greatly on the results of welding process. moreover selective evaporation loss of alloying elements leads to change in chemical composition of weld metal as well as the mechanical properties of welded joint. this study was undertaken to obtain a fundamental knowledge of pulsed laser welding phenomena especially evaporation mechanism of different aluminum alloys. The intensities of molecular spectra of AlO and MgO were different each other depeding on the power density of a laser beam Under the low power density condition the MgO band spectrum was predominant in intensity while the AlO spectra became much stronger with an increase in the power density. These behaviors have been attributed to the difference in evaporation phenomena of Al and Mg metals with different boiling points and latent heats of vaporization. The time-averaged plasma temperature and electron number density were determined by spectroscopic methods and consequently the obtained temperature was $3,280{\pm}150K$ and the electron number density was $1.85{\times}10^{19}\;l/m^3$.

  • PDF

반응고 Al-Zn-Mg 합금의 고온 압출 시 특성 평가 (Characteristics on the Hot Extrusion of Semi-Solid Al-Zn-Mg Alloy)

  • 조국래;김정한;염종택;심성용;임수근;박노광
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2007년도 춘계학술대회 논문집
    • /
    • pp.405-408
    • /
    • 2007
  • Semi-solid Al-Zn-Mg alloys were produced using a cooling plate method in order to investigate the extrudability. Al melt was poured on cooling plate which was adjusted at $60^{\circ}$ with respect to the horizontal plane, and the melt was cooled by water circulation underneath. Obtained Semi-solid feedstock has globular microstructure but also contains considerable amount of gas pore. Due to the pore, tensile elongation of the semi-solid feedstock was very low and it doesn't show yield point phenomenon. Isothermal hot extrusion was carried out using at $400^{\circ}C$ with a ram speed of 1mm/sec and an extrusion ratio of 25:1. The extruded bar show noticeably improved tensile ductility and strength because pore volume fraction decreased from 5% to 0.8% after extrusion. Mechanical properties of the semi-solid extruded bar were compared with that of commercial casting alloy..

  • PDF

반용융 Al-Zn-Mg합금의 고온 압출 시 특성 평가 (Characteristics on the Hot Extrusion of Semi-Solid Al-Zn-Mg Alloy)

  • 조국래;염종택;심성용;임수근;박노광;김정한
    • 소성∙가공
    • /
    • 제16권5호통권95호
    • /
    • pp.391-395
    • /
    • 2007
  • Semi-solid Al-Zn-Mg alloys were produced by using a cooling plate method in order to investigate the extrudability. Al melt was poured on cooling plate which was adjusted at $60^{\circ}$ with respect to the horizontal plane, and the melt was cooled by water circulation underneath. Obtained Semi-solid feedstock has globular microstructure but also contains considerable amount of gas pore. Due to the pore, tensile elongation of the semi-solid feedstock was very low and it doesn't show yield point phenomenon. Isothermal hot extrusion was carried out using at $400^{\circ}C$ with a ram speed of 1mm/sec and an extrusion ratio of 25:1. The extruded bar show noticeably improved tensile ductility and strength because pore volume fraction decreased from 5% to 0.8% after extrusion. Mechanical properties of the semi-solid extruded bar were compared with that of commercial casting alloy.

시효 열처리 된 Al-Si-Mg-Cu-(Ti) 합금의 고온 열팽창 계수 변화 (Changes in High-temperature Coefficient of Thermal Expansion of Artificial Aging Heat-treated Al-Si-Mg-Cu-(Ti) Alloys)

  • 최세원
    • 열처리공학회지
    • /
    • 제34권5호
    • /
    • pp.226-232
    • /
    • 2021
  • The relationship between precipitation and coefficient of thermal expansion of Al-6%Si-0.4%Mg-0.9%Cu-(Ti) alloy (in wt.%) after various heat treatments were studied by the thermodynamic analyzer (TMA) and differential scanning calorimetry (DSC). Solution heat treatment of the alloy was carried out at 535℃ for 6 h followed by water quenching, and the samples were artificially aged in the air at 180℃ and 220℃ for 5 h. The coefficient of thermal expansion (CTE) curve showed some residual strain and decreased with increasing aging temperature. The CTE curves changed sharply in the temperature range of 200℃ to 400℃, and the corresponding peak shifted for the aged samples due to the change in the precipitation behavior of the secondary phase. These transformation peaks in the aged sample are related to the volume of the precipitation of the Si phase as determined by DSC analysis. The change in CTE is mainly caused by the precipitation of the Si phase in the Al-Si alloy, and the size of the change occurs simultaneously with the size of the precipitate.

Surface Observation of Mg-HA Coated Ti-6Al-4V Alloy by Plasma Electrolytic Oxidation

  • Yu, Ji-Min;Choe, Han-Cheol
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2016년도 추계학술대회 논문집
    • /
    • pp.198-198
    • /
    • 2016
  • An ideal orthopedic implant should provide an excellent bone-implant connection, less implant loosening and minimum adverse reactions. Commercial pure titanium (CP-Ti) and Ti alloys have been widely utilized for biomedical applications such as orthopedic and dental implants. However, being bioinert, the integration of such implant in bone was not in good condition to achieve improved osseointegraiton, there have been many efforts to modify the composition and topography of implant surface. These processes are generally classified as physical, chemical, and electrochemical methods. Plasma electrolytic oxidation (PEO) as an electrochemical route has been recently utilized to produce this kind of composite coatings. Mg ion plays a key role in bone metabolism, since it influences osteoblast and osteoclast activity. From previous studies, it has been found that Mg ions improve the bone formation on Ti alloys. PEO is a promising technology to produce porous and firmly adherent inorganic Mg containing $TiO_2$($Mg-TiO_2$ ) coatings on Ti surface, and the amount of Mg introduced into the coatings can be optimized by altering the electrolyte composition. In this study, a series of $Mg-TiO_2$ coatings are produced on Ti-6Al-4V ELI dental implant using PEO, with the substitution degree, respectively, at 0, 5, 10 and 20%. Based on the preliminary analysis of the coating structure, composition and morphology, a bone like apatite formation model is used to evaluate the in vitro biological responses at the bone-implant interface. The enhancement of the bone like apatite forming ability arises from $Mg-TiO_2$ surface, which has formed the reduction of the Mg ions. The promising results successfully demonstrate the immense potential of $Mg-TiO_2$ coatings in dental and biomaterials applications.

  • PDF