• Title/Summary/Keyword: Mg substitution

Search Result 187, Processing Time 0.021 seconds

Effect of Sr Substitution for RE on Microstructure and Tensile Properties in Mg-Al-RE Casting Alloys

  • Jun, Joong-Hwan
    • Journal of Korea Foundry Society
    • /
    • v.31 no.5
    • /
    • pp.284-287
    • /
    • 2011
  • Microstructures and tensile properties at ambient and elevated temperatures were studied by substituting RE for Sr in Mg-6%Al-(3-X)%RE-X%Sr alloys (X = 0~3). With increasing Sr content, $Al_4Sr$ phase with lamellar morphology was newly introduced at interdendritic regions, with a gradual extinction of needle-shaped $Al_4RE$. The Mg-6%Al-3%Sr alloy shows dendritic grains and interdendritic eutectic phases containing bulky Mg-Al-Sr and lamellar $Al_4Sr$ with more continuous manner. The substitution of Sr for RE provided higher YS, UTS and creep resistance at $175^{\circ}C$, which indicates that Sr would be more beneficial in tensile properties and creep resistance at elevated temperature than RE for the Mg-Al based casting alloys.

Occurrence and Chemical Composition of Chlorite and White Mica from Drilling Core (No. 04-1) at Gubong Au-Ag Deposit Area, Republic of Korea (구봉 금-은 광상일대 시추코아(04-1)에서 산출되는 녹니석과 백색운모의 산상 및 화학조성)

  • Bong Chul Yoo
    • Korean Journal of Mineralogy and Petrology
    • /
    • v.36 no.4
    • /
    • pp.273-288
    • /
    • 2023
  • The Gubong Au-Ag deposit, which has been one of the largest deposits (Unsan, Daeyudong, Kwangyang) in Korea, consists of eight lens-shaped quartz veins (a mix of orogenic-type and intrusion-related types) that filled fractures along fault zones within Precambrian metasedimentary rock. Korea Mining Promotion Corporation found a quartz vein (referred to as the No. 6 vein with a grade of 27.9 g/t Au and a width of 0.9 m) at a depth of -728 ML by drilling (No. 90-12) conducted in 1989. Korea Mining Promotion Corporation conducted drilling (No. 04-1) in 2004 to investigate the redevelopment's possibility of the No. 6 vein. The author studied the occurrence and chemical composition of chlorite and white mica using wallrock, wallrock alteration and quartz vein samples collected from the No. 04-1 drilling core in 2004. The alteration of studied samples occurs chloritization, sericitization, silicification and pyritization. Chlorite and white mica from mineralized zone at a depth of -275 ML occur with quartz, K-feldspar, calcite, rutile and pyrite in wallrock alteration zone and quartz vein. Chlorite and white mica from ore vein (No. 6 vein) at a depth of -779 ML occur with quartz, calcite, apatite, zircon, rutile, ilmenite, pyrrhotite and pyrite in wallrock alteration zone and quartz vein. Chlorite from a depth of -779 ML has a higher content of Al and Mg elements and a lower content of Si and Fe elements than chlorite from a depth of -275 ML. Also, Chlorites from a depth of -275 ML and -779 ML have higher content of Si element than theoretical chlorite. Compositional variation in chlorite from a depth of -275 ML was mainly caused by phengitic or Tschermark substitution [Al3+,VI + Al3+,IV <-> (Fe2+ or Mg2+)VI + (Si4+)IV], but compositional variation from a depth of -779 ML was mainly caused by octahedral Fe2+ <-> Mg2+ (Mn2+) substitution. The interlayer cation site occupancy (K+Na+Ca+Ba+Sr = 0.76~0.82 apfu, 0.72~0.91 apfu) of white mica from a depth of -275 ML and -779 ML have lower contents than theoretical dioctahedral micas, but octahedral site occupancy (Fe+Mg+Mn+Ti+Cr+V+Ni = 2.09~2.13 apfu, 2.06~2.14 apfu) have higher contents than theoretical dioctahedral micas. Compositional variation in white mica from a depth of -275 ML was caused by phengitic or Tschermark substitution [(Al3+)VI + (Al3+)IV <-> (Fe2+ or Mg2+)VI + (Si4+)IV], illitic substitution and direct (Fe3+)VI <-> (Al3+)VI substitution. But, compositional variation in white mica from a depth of -779 ML was caused by phengitic or Tschermark substitution [(Al3+)VI + (Al3+)IV <-> (Fe2+ or Mg2+)VI + (Si4+)IV] and direct (Fe3+)VI <-> (Al3+)VI substitution.

Piezoelectric and Electric Field Induced Strain Properties of PMW-PNN-PZT Ceramics with the Substitution of Ba (Ba 치환에 따른 PMW-PNN-PZT 세라믹스의 압전 및 전계유기왜형 특성)

  • 윤광희;김규수;최병수
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.14 no.1
    • /
    • pp.20-25
    • /
    • 2001
  • To develop the piezoelectric actuator, the structural, dielectric and piezoelectric properties and electric fieldinduced strain of the ceramics(Pb$\_$1-2/Ba$\_$x/)[Mg$\_$1/2/W$\_$1/2/)$\_$0.03/-Ni$\_$1/3/Nb$\_$2/3/)$\_$0.12/-(Zr$\_$0.5/Ti$\_$0.5/)$\_$0.85/]O$_3$(x=0, 0.01, 0.03, 0.05, 0.07, 0.1) were investigated with the substitution of Ba. The tetragonality of crystal structure and grain size decreased by the substitution of Ba. Curie temperature decreased due to the decrease of the tetragonality, and dielectric constants increased with the substitution of Ba. The coercive field, remnant polarization and electromechanical coupling factor also decreased, whereas the piezoelectric constatns d$\_$33/ and d$\_$31/ were showed the highest value of 430 and 209(x10$\^$-12/C/N), respectively, because of the increase of dielectric constant. The strain induced by 60Hz AC electric field had the maximum value of 204x10$\^$-6/Δℓ/ℓ at the substitution of Ba 3mol%. As the applied electric field approaches to the coercive field, the piezoelectric element is depolarized and the electric field induced strain revealed non-linearity.

  • PDF

Effects of Nano FexC Addition on Superconducting Properties of MgB2 (MgB2 초전도 특성에 대한 나노 FexC 첨가 효과)

  • Lee, Dong-Gun;Lee, Ji-Hyun;Jun, Byung-Hyuk;Park, Soon-Dong;Uhm, Young-Rang;Park, Hai-Woong;Kim, Chan-Joong
    • Journal of Powder Materials
    • /
    • v.19 no.2
    • /
    • pp.146-150
    • /
    • 2012
  • The effects of nano $Fe_xC$ addition to superconducting properties of $in$ $situ$ processed $MgB_2$ superconductors was examined. 0.1 wt.% and 1 wt.% nano $Fe_xC$ powders were mixed with boron and magnesium powders by ball milling. The powder mixtures were made into pellets by uniaxial pressing. The pellets were heat-treated at $700^{\circ}C-900^{\circ}C$ in argon atmosphere for $MgB_2$ formation. It was found by powder X-ray diffraction that the raw powders were completely converted into $MgB_2$ after the heat treatment. The superconducting transition temperature ($T_c$) and critical current density ($J_c$), estimated from susceptibility-temperature and $M-H$ curves, were decreased by nano $Fe_xC$ addition. The $T_c$ and $J_c$ decrease by nano $Fe_xC$ addition are attributed to the incorporation of iron and carbon with $MgB_2$ lattices (Fe substitution for Mg and C substitution for B) due to the high reactivity of the nano $Fe_xC$ powder.

A study on Dielectric Properties using PMN Ceramics with La substitution (La치환된 PMN계 세라믹스의 유전특성에 관한 연구)

  • Ji, S.H.;Lee, N.H.;Kim, Y.H.;Kim, J.S.;Lee, D.C.
    • Proceedings of the KIEE Conference
    • /
    • 1995.07c
    • /
    • pp.1242-1244
    • /
    • 1995
  • The dielectric and polarizable properties of $0.9Pb_{1-x}La_x({Mg}_{1/3}Nb_{2/3})O_3-0.1PbTiO_3$ (x=0,1,2,3,4,5) have been investigated. The temperature-dependant electrostictive characteristics of 0.9PMN-0.1PT relaxor ferroelectric system were improved by enhencing the extent of the diffuse phase transition(DPT). This was achieved using PMN-PTceramics by the partial substitution of La at the Pb site. The curie temperature and the maximum dielectric permittivity decreased by substituting La and the electric field-related hysteresis phenomena decreased with increasing La substitution amount.

  • PDF

Effects of Polyacrylic Acid Doping on Microstructure and Critical Current Density of $MgB_2$ Bulk ($MgB_2$ bulk의 미세구조와 임계전류밀도에 미치는 polyacrylic acid doping 효과)

  • Lee, S.M.;Hwang, S.M.;Lee, C.M.;Joo, J.;Kim, C.J.
    • Progress in Superconductivity
    • /
    • v.11 no.2
    • /
    • pp.87-91
    • /
    • 2010
  • We fabricated the polyacrylic acid (PAA)-doped $MgB_2$ bulks and characterized their lattice parameters, actual C substitutions, microstructures, and critical properties. The boron (B) powder was mixed with PAA using N,N-dimethylformamide as solvent and then the solution was dried out at $200^{\circ}C$ and crushed. The C treated B powder and magnesium powder were mixed and compacted by uniaxial pressing at 500 MPa, followed by sintering at $900^{\circ}C$ for 1 h in high purity Ar atmosphere. We observed that the PAA doping increased the MgO amount but decreased the grain size, a-axis lattice constant, and critical temperature ($T_c$), which is indicative of the C substitution for B sites in $MgB_2$. In addition, the critical current density ($J_c$) at high magnetic field was significantly improved with increasing PAA addition: at 5 K and 6.6 T, the $J_c$ of 7 wt% PAA-doped sample was $6.39\;{\times}\;10^3\;A/cm^2$ which was approximately 6-fold higher than that of the pure sample ($1.04\;{\times}\;10^3\;A/cm^2$). This improvement was probably due to the C substitution and the refinement of grain size by PAA doping, suggesting that PAA is an effective dopant in improving $J_c$(B) performance of $MgB_2$.

Preparation and Luminescent Properties of (Zn1-xMgx)2SiO4:mn Phosphors ((Zn1-xMgx)2SiO4:mn 형광체의 제조와 발광특성)

  • Lee, Ji-Young;Yu, Il
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.22 no.5
    • /
    • pp.415-418
    • /
    • 2009
  • $Zn_{2}SiO_{4}$:Mn green phosphors doped with Mg for PDP were synthesized by solid state reaction method. $Zn_{2}SiO_{4}$:Mn, Mg phosphors with increasing Mg concentration were changed from Rhombohedral to Orthorhombic structure. Photoluminescence intensity of $Zn_{2}SiO_{4}$:Mn phosphors doped with Mg 0.5 mol was definitely higher than that of Mg non-doped sample. The enhanced luminescence with doping Mg in the $Zn_{2}SiO_{4}$:Mn phosphors was interpreted by the increase of energy transfer from host to Mn ions with substitution Mg for Zn in the $Zn_{2}SiO_{4}$:Mn host.

Effect of metal ions on the secondary structure and activity of calf intestine phosphatase

  • Chen, Fengjuan;Liu, Guoqi;Xu, Zhihong;Zeng, Zhengzhi
    • BMB Reports
    • /
    • v.41 no.4
    • /
    • pp.305-309
    • /
    • 2008
  • Cobalt is an essential microelements in many biological processes involving enzymatic activity. We found that $Zn^{2+}$ and $Mg^{2+}$, which are in the active site of native calf intestine alkaline phosphatase (CIP), can be replaced by $Co^{2+}$ directly in solution. The effect of $Co^{2+}$ concentration on the substitution reaction was examined at ratios of [$Co^{2+}$]/[CIP] from 0:1 to 8:1. The quantity of $Zn^{2+}$ in CIP decreased progressively as the ratio was increased, but the amount of $Mg^{2+}$ changed in irrregular fashion. A series of active site models of the reaction mechanism of CIP are proposed. Low pH was found to promote the replacement of $Mg^{2+}$ by $Co^{2+}$. To understand how the substitution affects the enzyme, we also solved the secondary structure of CIP after reaction with $Co^{2+}$ in different conditions.

Electromagetic Wave Absorbing Properties of $Ni_{0.5}-Zn_{0.4}-X_{0.1}{\cdot}Fe_2O_4$(X=Cu, Mg, Mn)-Rubber Composite ($Ni_{0.5}-Zn_{0.4}-X_{0.1}{\cdot}Fe_2O_4$(X=Cu, Mg, Mn)-Rubber Composite의 전파흡수특성에 관한 연구)

  • Im, Hui-Dae;Yun, Guk-Tae;Lee, Chan-Gyu
    • Korean Journal of Materials Research
    • /
    • v.9 no.12
    • /
    • pp.1234-1239
    • /
    • 1999
  • Electromagnetic wave asorbing properties of the $Ni_{0.5}-Zn_{0.4}-X_{0.1}{\cdot}Fe_2O_4$, where X was replaced by substitution elements Cu, Mg, Mn, have been studied. The structure, shape, size and magnetic properties of the $Ni_{0.5}-Zn_{0.4}-X_{0.1}{\cdot}Fe_2O_4$ were analyzed by XRD, SEM, VSM. The relative complex permittivity, permeability, and electromagnetic wave absorbing properties were measured by Network Analyzer. The structure, shape, size and magnetization value of the $Ni_{0.5}-Zn_{0.4}-X_{0.1}{\cdot}Fe_2O_4$ were found to be similar in spite of substitution elements. The coercive force and hysteresis-loss showed maximum value when Mg was substituted for X. The dielectric loss(${\varepsilon}_r"/{\varepsilon}_r'$) was found to be maximum value when Mn was substituted for X. Also the magnetic loss(${\mu}_r"/{\mu}_r'$} was found to be maximum with Cu substitution. The electromagnetica wave absorbing property of the $Ni_{0.5}-Zn_{0.4}-X_{0.1}{\cdot}Fe_2O_4$-Rubber composite with 4mm thickness was excellent as over - 40dB at 9GHz, and the $Ni_{0.5}-Zn_{0.4}-X_{0.1}{\cdot}Fe_2O_4$-Rubber composite with 8mm thickness was over-40dB at 2GHz. Those composites also showed superior microwave absorbing properties.

  • PDF

Enhanced superconducting properties of MgB2 by doping the carbon quantum dots

  • K.C., Chung;S.H., Jang;Y.S., Oh;S.H., Kang
    • Progress in Superconductivity and Cryogenics
    • /
    • v.24 no.4
    • /
    • pp.55-58
    • /
    • 2022
  • Carbon-based doping to MgB2 superconductor is the simplest approach to enhance the critical current densities under magnetic fields. Carbon quantum dots is synthesized in this work as a carbon provider to MgB2 superconductors. Polyvinyl Pyrrolidone is pyrolyzed and dispersed in dimethylfomamide solvent as a dopant to the mixture of Mg and B powders. Doped MgB2 bulk samples clearly show the decrease of a-axis lattice constant, grain refinements, and broadening of FWHM of diffraction peaks compared to un-doped MgB2 possibly due to the carbon substitution and/or boron vacancy at the boron site in MgB2 lattice. Also, high-field Jc for the doped MgB2 is enhanced significantly with the crossover about 3 T at 5 & 20 K when increasing the doping of carbon quantum dots.