Search Result 241, Processing Time 0.029 seconds

An Experimental Study of Environmental Effects on the Rolling Resistance of Bearing Surfaces Coated by Soft Metallic Films (연금속 박막이 코팅된 베어링 표면의 구름 저항 거동에 미치는 분위기의 영향에 대한 실험적 고찰)

  • 양승호;공호성;윤의성;김대은
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 1998.04a
    • /
    • pp.47-54
    • /
    • 1998
  • An experimental study was performed to discover the effect of environmental conditions on the rolling resistance behavior of pure silver and lead coated 52100 bearing steel. Pure silver and lead coating were produced by a thermal evaporation coating method. Experiments using a thrust ball bearing-typed rolling test-rig were performed under vacuum, dry air and controlled humidity conditions. Results showed that agglomeration of particles were prevented in vacuum environment and as it showed low and stable rolling resistance by shakedown phenomena. Also, humidity relates closely to the agglomeration of particles and increased the rolling resistance after the failure of coated layer.

  • PDF

METALLIC INTERFACES IN HARSH CHEMO-MECHANICAL ENVIRONMENTS

  • Yildiz, Bilge;Nikiforova, Anna;Yip, Sidney
    • Nuclear Engineering and Technology
    • /
    • v.41 no.1
    • /
    • pp.21-38
    • /
    • 2009
  • The use of multi scale modeling concepts and simulation techniques to study the destabilization of an ultrathin layer of oxide interface between a metal substrate and the surrounding environment is considered. Of particular interest are chemo-mechanical behavior of this interface in the context of a molecular-level description of stress corrosion cracking. Motivated by our previous molecular dynamics simulations of unit processes in materials strength and toughness, we examine the challenges of dealing with chemical reactivity on an equal footing with mechanical deformation, (a) understanding electron transfer processes using first-principles methods, (b) modeling cation transport and associated charged defect migration kinetics, and (c) simulation of pit nucleation and intergranular deformation to initiate the breakdown of the oxide interlayer. These problems illustrate a level of multi-scale complexity that would be practically impossible to attack by other means; they also point to a perspective framework that could guide future research in the broad computational science community.

Evaluation of the Environmental Qualification for Non-metallic Parts (비금속부품 내환경검증 수명평가)

  • Bhang, Keug-Jin;Hong, Jun-Hee
    • Journal of Power System Engineering
    • /
    • v.20 no.5
    • /
    • pp.52-59
    • /
    • 2016
  • Environmental Qualification has been almost developed except those of Non-Material Sub-components for valves and pumps though the time has only passed about 10years since EQ test launch of Korea. However EQ test has been performed by a few of engineers under the conditions that experience of EQ test is insufficient and EQ system is not developed completely. In recent years, Strengthen Nuclear Safety Regulation is being done Strictly Nuclear safety components Verification Procedure for Non-Material Sub-components, but the reports contain only performance test results, not Enviro nmental test methods relating to real Aging Degradation. In this Study, there were developed to performance systematically research to acquire EQ technology for five specimens of the Non-Material Sub-components in the Nuclear Power Plant.

Influences of Coatings and Solution Corrosivity on Cathodic Protection of Metallic Materials

  • Yoo, Y.R.;Chang, H.Y.;Jin, T.E.;Kim, Y.S.
    • Corrosion Science and Technology
    • /
    • v.5 no.3
    • /
    • pp.106-111
    • /
    • 2006
  • Painting has protected metallic stack but the paint films may be degraded and corrosion problem can be arisen. To protect the painted metal stack, cathodic protection can be applied. If cathodic protection is applied to bare metal, only small area may be protected. However, if cathodic protection is applied to painted metal surface, large area can be protected and the lifetime of paint films can be extended. High corrosion resistant alloys were corroded at a Flue Gas Desulfurization (FGD) facility of power plant within a short period and thus cathodic protection can be used to protect these metals. On the base of computer simulation, if cathodic protection is applied to bare metal in a FGD environment, it was estimated that applied current could almost be spent to protect area near the anode. However, if cathodic protection is applied to high resistant-coated metal, the much larger area from the anode could be effectively protected.

Sintered $Fe_3Al$ Intermetallic - A New Filter Element for Hot Gas Filtration

  • Xing, Y.;Kuang, X.;Wang, F.;Kuang, C.;Fang, Y.
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.597-598
    • /
    • 2006
  • Gas filtration at high temperature from industrial processes offers various advantages such as increasing process efficiency, improving heat recovery and materials resource recovery, etc. At the same time, it is an advanced environment protection technology. This paper describes a newly developed metallic filter element. The manufacturing process of sintered $Fe_3Al$ metallic powder and the mechanical and filtration characteristics of this filter element were investigated. In this work, the phase constituent changes of the $Fe_3Al$ powder during sintering were studied. The newly developed filter elements were found to have excellent corrosion resistance, good thermal resistance, high strength and high filtration efficiency.

  • PDF

Monitoring of Lead and Antimony in Metallic Kitchenware (국내 유통 금속제 주방기구 중 납 및 안티몬 모니터링)

  • Lee, Sun-Hee;Jung, Kyu-Jin;Lee, Yoong-Kook;Sung, Jun-Hyun;Eom, Mi-Ok;Lee, Yong-Ja;Lim, Joung-Gyoon
    • Journal of Food Hygiene and Safety
    • /
    • v.22 no.1
    • /
    • pp.52-56
    • /
    • 2007
  • In order to offer monitoring data about standard and specification of metallic kitchenware, we carried out the material test and migration test of lead and antimony in 71 kinds of kitchenwares. As a result of this study, Pb was detected less than 0.06% at the material test and Sb was not defected in 71 kinds of kitchenwares. Pb was also detected less than 0.41 mg/L at the migration test. Currently according to the Food Code of Korea, Pb and Sb in metal product shall not exceed 10% and 5%, respectively and Pb migrated from metal product shall not exceed 1.0 mg/L. Therefore, our all data are not exceeding the standard and specification of metal product and show that all the kitchenwares in domestic circulation may be safe.

A Study on collection efficiency of two-stage electrostatic precipitator using PET-coated non-metallic electrode with respect to relative humidity (PET 코팅된 비금속 집진판을 사용한 2단 전기집진기의 상대습도에 따른 집진효율 연구)

  • Haneol Lee;Gwangtaek Lee;So-Hee An;Ye Won Park;Gunhee Lee;Kee Jung Hong;Inyong Park;Sang Bok Kim;Daehoon Park;Yeawan Lee;Dong-Keun Song;Yong-Jin Kim;Bangwoo Han;Hak-Joon Kim
    • Particle and aerosol research
    • /
    • v.19 no.3
    • /
    • pp.53-62
    • /
    • 2023
  • This study compared the collection efficiency of a two-stage electrostatic precipitator (ESP) with a lightweight PET film-coated carbon electrode collector plate, depending on the relative humidity of the exhaust gas and the applied voltage to the pre-charger. It was confirmed that the onset voltage at which corona discharge occurs decreases and the discharge current decreases at the same voltage as the relative humidity increases. On the other hand, even though there was almost no change in the diameter of the particles generated depending on the relative humidity, the efficiency was higher at the same voltage as the relative humidity increased. In addition, by applying a two-stage ESP structure, the collection efficiency was higher than that of a single-stage electrostatic precipitator under the same conditions. The ESP using the carbon electrode coated with PET film used in this study is expected to be effective in various aspects such as weight and in the current situation where environmental regulations are rapidly tightening.

Development of Surface Coating Technology fey Metallic Bipolar Plate in PEMFC : I. Study on Surface and Corrosion Properties (PEMFCB금속분리판 코팅 기술 개발 : I. 표면 및 부식 특성 평가)

  • Chung, Kyeong-Woo;Kim, Se-Yung;Yang, Yoo-Chang;Ahn, Seung-Gyun;Jeon, Yoo-Taek;Na, Sang-Mook
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 2006.11a
    • /
    • pp.348-351
    • /
    • 2006
  • Bipolar plate, which forms about 50% of the stack cost, is an important core part with polymer electrolyte membrane in PEMFC. Bipolar plates have been commonly fabricated from graphite meterial having high electrical conductivity and corrosion resistance. Lately, many researchers have concentrated their efforts on the development of metallic bipolar plate and stainless steel has been considered as a potential material for metallic bipolar plate because of its high strength, chemical stability, low gas permeability and applicability to mass production. However, it has been reported that its inadequate corrosion behavior under PEMFC environment lead to a deterioration of membrane by dissolved metal ions and an increase in contact resistance by the growth of passive film therefore, its corrosion resistance as well as contact resistance must be improved for bipolar plate application. In this work, several types of coating were applied to 316L and their electrical conductivity and corrosion resistance were evaluated In the simulated PEMFC environment. Application of coating gave rise to low interfacial contact resistances below $19m{\Omega}cm^2$ under the compress force of $150N/cm^2$. It also made the corrosion potential to shift in the posit ive direct ion by 0.3V or above and decreased the corrosion current from ca. $9{\mu}A/cm^2$ to ca. $0.5{\mu}A/cm^2$ in the mixed solution of $0.1N\;N_2SO_4$ and 2ppm HF A coat ing layer under potentiostatic control of 0.6V and $0.75V_{SCE}$ for 500 hours or longer showed some instabilities, however, no significant change in coat Ing layer were observed from Impedance data. In addition, the corrosion current maintained less than $1{\mu}A/cm^2$ for most of time for potentiostatic tests. It indicates that high electrical conductivity and corrosion resistance can be obtained by application of coatings in the present work.

  • PDF

The Study on the Weathering Characteristics about Epoxy Adhesive for the Adhesion and Restoration of Metallic Cultural Assets (금속문화재 접합 복원용 에폭시 접착제의 내후성 연구)

  • Lee, Ji-Hyun;Wi, Koang-Chul
    • Journal of Conservation Science
    • /
    • v.26 no.1
    • /
    • pp.61-67
    • /
    • 2010
  • After selecting five types of adhesive epoxy resin for metallic cultural assets such as $Araldite^{(R)}$ rapid type, $Devcon^{(R)}$, $Araldite^{(R)}$ SV427+HV427, $CDK^{(R)}$520, $Araldite^{(R)}$ AW106+HV953 which had already been studied, this paper approached more closely the problem of yellowing and the signal of aging with time passing by connecting the problems with the safety of metallic cultural assets. The change of physical properties according to the change of state of epoxy adhesives was investigated through the change of flexural strength and the change of surface hardness by artificially providing the possible environmental change factors such as ultra-violet ray, and acid base, and how the epoxy chemically changes in its ingredients by the environment was analyzed through FT-IR. As a result of the experiment, for the most part of adhesives brought about the physical change of flexural strength, the change of surface hardness, and the chemical change of chemical ingredients as the product of alcohol, which were respectively different according to the time of ultraviolet irradiation, and acid base change. Under most of the conditions, SV427+HV427 and $CDK^{(R)}$520 were fairly stabilized under each condition of weatherability, but it seems that they should be refrained from being applied in case that the area to restore is thin and wide because the degree of flexural strength of themselves is low. Also, it is found that the preservation environment is very important not only for artifacts but also for the preservation of resins sused for preservation treatment.

Sedimentary Geochemical Characteristics and Environmental Impact of Sediments in Tamjin River and Doam Bay (탐진강 및 도암만 지역 퇴적물의 퇴적지구화학적 특성과 환경영향)

  • Hong, Jin-Taek;Na, Bum-Soo;Kim, Joo-Yong;Koh, Yeong-Koo;Youn, Seok-Tai;Shin, Sang-Eun;Kim, Hai-Gyoung;Moon, Byoung-Chan;Oh, Kang-Ho
    • Journal of Environmental Impact Assessment
    • /
    • v.16 no.6
    • /
    • pp.393-405
    • /
    • 2007
  • To examine the sedimentary geochemical characteristics of sediment in the Tamjin River and Doam bay, the analysis was conducted, using the sample obtained in February 2000, on the grain size and the contents of metallic elements and organic carbon. The factors that influence the geochemical behavior of metallic elements in the surface sediment are grain size, organism, surrounding soil and $CaCO_3$. To find out the pollution level of metallic elements, the enrichment factor (EF) and the index of geoaccumulation ($I_{geo}$) were researched. The majority of metallic elements sustain their values in natural state. The elements such as K, Ba, Zr, etc. appear to be rich in some places. The EF and $I_{geo}$ of P, Cu, Zn, and Pb, which belong to toxic heavy metals, are partly related with man-made pollution. P and Cu have a high EF, Pb has a high $I_{geo}$ and Zn is high in both EF and $I_{geo}$. The low contents of P and Cu are not likely to be related with the pollution of water environment. However, given the development of relative pollution, the research and the management regarding the pollutants are needed. Because Pb, naturally enriched by geological characteristics, has a large influence on water environment along with Zn, the adequate measures against man-made pollution should be worked out.