수복재료와 내가동연결장치가 IMZ 임프란트 보철물의 충격흡수효과에 미치는 영향 (A STUDY ON THE SHOCK-ABSORBING BEHAVIOR OF RESTORATIVE MATERIALS AND INTERMOBILE CONNECTOR USEDIN IMZ IMPLANTS)

  • 이수정;정찬목;전영찬
    • 대한치과보철학회지
    • /
    • 제35권1호
    • /
    • pp.118-129
    • /
    • 1997
  • The purpose of this study was to evaluate the shock absorbing effect of 4 restorative materials and intramobile connector. The damping effect of four restorative materials used to veneer test crown rigidly connected to IMZ implant and subjected to an impact force was measured. These materials included a gold alloy(stabilor G) : a noble metal ceramic alloy(Degudent H) : porcelain(Duceram) : composite resin(Dentacolor). In addition, this study compared damping effect of same restoretive materials after using polyoxymethylene intramobile connector(POM IMC). The result of this study suggest that : In case of using metal IMC 1. Veneered composite resin(group IV) reduced the impact force by 75%, when compared to an equivalent thickness of porcelain(group III). Group IV reduced the impact force by 87% and 89%, respectively, when compared to Stabilor G(group I) and Degudent H(group II). 2. The impact force recorded was higher for the alloy with the higher elastic modulus.(Stabilor G, group I, Young's modulus 107 Gpa, versus Degudent H, Group II, Young's modulus 95 Gpa) 3. It took the longest time for composite resin veneered group(IV) to reach to peak force when compared group I, II, III. In case of using POM IMC 4. The mean impact force recorded were reduced by 79%(group I), 78%(group II), 69%(group III), 84%(group IV), respectively, when compared to using metal IMC. 5. The time required to reach the peak force were increased by 78%(group I, II) 87%(group III), 34%(group IV), respectively, when compared to using metal IMC>.

  • PDF

접착재의 종류에 따른 In-Ceram 도재관의 변연적합도와 파절강도에 관한 연구 (MARGINAL FIDELITY AND FRACTURE STRENGTH OF IN-CERAM CROWNS ACCORDING TO VARIOUS RESIN CEMENTS)

  • 임주환
    • 대한치과보철학회지
    • /
    • 제36권6호
    • /
    • pp.888-899
    • /
    • 1998
  • In-Ceram system is one of contemporary esthetic all ceramic restorations and has relatively high flexural strength. The purpose of this study was to evaluate the marginal fidelity according to type of resin cement and measuring position, and to evaluate fracture strength according to type of resin cement. In this study, twenty seven In-Ceram crowns were fabricated on the metal master die of prepared maxillary right central incisor and devided into three groups. All specimens were cemented with Panavia 21 (group PV), Super-bond (group SB) and Lute-it (group LI) on the metal master die. After cementation, specimens were measured marginal gap between the margin of the In-Ceram crown and the finishing line of metal master die by using a stereomicroscope (SZ-ST, Olympus, Japan). Marginal gaps were recorded at the labial, lingual, mesial and distal measuring points on the metal master die. For the mesurement of fracture strength, lingual surfaces of cemented specimens were loaded at a distance of 1mm from incisal edge by using the Autograph S-2000 (Shimadzu, Japan). The results of marginal fidelity and fracture strength were statistically analyzed with the SPSS version 8.0 programs. The results of this study were as follows: 1. In comparison of marginal fidelity according to the measuring points, there was no significant difference. 2. The marginal fidelity according to the type of resin cement was decreased in order of group $LI\;(63.75{\mu}m),\;SB\;(77.78{\mu}m),\;PV\;(86.53{\mu}m)$, and there was significant difference between group LI and PV (p<0.05). 3. The fracture strength according to the type of resin cement was showed descending order of group $LI\;(60.00kg/cm^2),\;SB\;(56.80kg/cm^2),\;PV\;(56.11kg/m^2)$, but there was no significant difference.

  • PDF

전악수복환자에서 Shilla system을 이용한 교합평면 재구성 증례 (Reestablishing the occlusal plane in full mouth rehabilitation patient, using Shilla system)

  • 양민수;방몽숙;박상원;임현필;윤귀덕;양홍서
    • 대한치과보철학회지
    • /
    • 제51권1호
    • /
    • pp.33-38
    • /
    • 2013
  • 교합평면은 시상면적인 치열궁 형태를 나타내는 것으로, 악구강계를 구성하는 요소의 하나인 교합을 형태적으로 구성한다. 본 증례에서는 생체의 정중 시상면에 대한 수평, 측방좌표를 교합기상에 재현하여 상하악 치아 및 결손부 치조제에 대한 좌우 동적인 위치관계 얻기 위해 Shilla system (Hamans, Tokyo, Japan)을 이용하여 교합평면을 재구성 하였다. 본 증례의 환자는 41세의 남자 환자로 상악 전치부 10본금속-도재 고정성국소의치 파절 및 탈락과 전반적인 치료를 주소로 내원하였다. 임상 검사, 방사선 검사, 모형분석을 통해 임플란트 식립을 동반한 완전구강회복술을 하기로 결정하였다. Gothic Arch device (Centrofix; AmannGirrbach GmbH, Germany)를 이용하여 악간관계를 채득하고 마운팅 후, Shilla system을 이용하여 기존 교합평면을 평가, 분석하여 진단 납형을 제작하였다. 이를 토대로 방사선 스텐트를 제작하여 임플란트 식립하였고, 진단 납형을 이용하여 임시수복물을 제작하였다. 임시 수복물의 형태 및 교합 양식을 재현하기 위해 맞춤 전방유도판을 제작하고, 교차 마운팅을 시행하였으며 최종 수복물은 지르코니아 코핑을 이용한 완전 도재관으로 제작하였다. 이상과 같이 전악수복환자에서 진단과 치료 과정에서 Shilla system을 이용하여 적절한 심미적, 기능적 수복 결과를 얻을 수 있었다.

접착치의학 개념에 따른 최소 침습적 치아 삭제법을 적용한 심미적인 치은 연상 변연 도재 부분피개관 수복 증례 (Clinical performance of esthetic ceramic partial-coverage restorations with supra-gingival margin using minimally invasive tooth preparation method according to the concept of adhesive dentistry)

  • 홍명식;최유성;이종혁;하승룡
    • 대한치과보철학회지
    • /
    • 제59권3호
    • /
    • pp.319-332
    • /
    • 2021
  • 심미적인 도재 재료와 레진 시멘트의 비약적인 발전으로 임상에서 금속도재관에서 전부도재관으로의 전환이 활발히 이루어지고 있으며, 도재 수복물 제작 시 그에 적합한 형태와 기술을 이용하여야 그 장점을 최대화할 수 있다. 최근 법랑질을 최대한 보존하고 접착 효율을 높이는 최소 침습적 치아 삭제법을 적용하여 치은 연상 변연을 가진 심미적인 도재 부분피 개관 수복방법이 소개되었는데, 이를 통해 치질 삭제의 최소화, 시멘트 제거의 용이성 등 여러 장점들을 얻을 수 있다고 보고된다. 또한 이 제작법은 치은 압배사의 삽입이 불필요하여 치은 압배사 삽입에 소요되는 시간을 절약할 수 있으며 환자의 불편감도 감소시킬 수 있다. 더 나아가 치은 열구액이나 혈액의 개입 없이 명확하게 변연을 채득할 수 있어 더 정확한 수복물 제작이 가능하다고 보고된다. 본 증례에서는 각각 해당 치아 부위에 부분적인 결함이 있는 환자에서 통상적인 전부피개관이 아닌 접착치의학 개념에 따른 최소 침습적 치아 삭제법을 적용한 치은 연상 변연 도재 부분피개관으로 다양한 제작 방법을 활용하여 수복함으로써 불필요한 치아 삭제를 방지하고 잔존 치질을 최대한 보존할 수 있었다. 치료 후 환자와 술자 모두 심미적, 기능적으로 만족할 만한 결과를 얻었기에 이를 보고하는 바이다.

임상가를 위한 특집 3 - 심하게 흡수된 치조제를 가진 환자에서 CAD/CAM을 이용한 임플란트 고정성 보철치료 (Implant fixed prosthetic treatment using CAD/CAM system in a patient with severe alveolar resorption)

  • 최유성
    • 대한치과의사협회지
    • /
    • 제50권3호
    • /
    • pp.126-139
    • /
    • 2012
  • Loss of dentition can lead to not only compromised esthetics and functions of the patient, but also alveolar bone resorption. Bone grafting with prosthetic reconstruction of the gingiva can be selected for the treatment, and it provides many benefits as prosthetic gingival reconstruction does not require a complicated surgical process and is available within a short period of time, with stable clinical results. However, conventional porcelain fused to metal prosthesis has certain limits due to its size, and deformation after several firing procedures. In this clinical report, the author would like to introduce a patient with severe alveolar resorption who was treated with gingiva-shaped zirconia/titanium CAD/CAM implant fixed prosthesis for esthetic and functional rehabilitation. Clinical reports Clinical report 1, 2 : A case of loss of anterior dentition with atrophied alveolar bone. Implant retained zirconia bridge applied with Procera implant bridge system to simulate the gingiva. Upper structure was fabricated with zirconia all ceramic crown. Clinical report 3, 4 : A case of atrophied maxillary alveolus was reconstructed with fixed implant prosthesis, a CAD/CAM designed titanium structure covered wi th resin on its surface. Anterior dentition was reconstructed with zirconia crown. Conclusion and clinical uses. All patients were satisfied with the outcome, and maintained good oral hygiene. Zirconia/titanium implant fixed prosthesis fabricated by CAD/CAM system was highly accurate and showed adequate histological response. No critical failure was seen on the implant fixture and abutment overall. Sites of severe alveolar bone loss can be rehabilitated by implant fixed prosthesis with CAD/CAM system. This type of prosthesis can offer artificial gingival structure and can give more satisfying esthetics and functions, and as a result the patients were able to accept the outcome more fondly, which makes us less than hard to think that it can be a more convenient treatment for the practitioners.

관교의치 및 금속 도재 보철물용 Ni-Cr 합금과 Ag-Pd 합금의 재사용에 따른 주조 재현성의 변화 (Castability of Some Repeatedly Used Ni-Cr Alloys and Ag-Pd Alloys for Crown and Bridge and Metal-Ceramic Restorations)

  • 김웅철
    • 대한치과기공학회지
    • /
    • 제8권1호
    • /
    • pp.37-43
    • /
    • 1986
  • The purpose of this study is to evalute the effects of melting and casting procedures on the castability of some N-Cr and Ag-Pd alloys. One Ag-Pd alloy and two Ni-Cr alloys were chosen for study, and the first casting group of these alloys were used as the control, and with which the castability of the first recase group and the mixture group of the first recast and as much amount of the first casting alloy was compared. The results of this study were as follows: 1. The castability of the first recast alloys veried significantly depending upon the presence or abscence of the first casting alloy and the kind of alloys. 2. When the first recast alloy was mixed with as much amount of the first casting alloy, there was no significant difference in castabilityh between the first recast group and the first casting group. 3. When the first recast alloy was used alone, the castability veried significantly depending upon the kind of alloys, i.e., the castability of Rexillium III and Palliag M was decreased significantly when compared with that of the first casting groups, while that of C & B Alloy was not.

  • PDF

3D printing으로 제작된 금속 코어와 치과용 도재 간의 전단결합강도 평가 (Evaluation of shear bond strength between metal core fabricated by 3D printing and dental porcelain)

  • 정재관;이수옥;김기백
    • 한국산학기술학회논문지
    • /
    • 제16권4호
    • /
    • pp.2585-2592
    • /
    • 2015
  • 3D 프린팅 기술은 최근 치과용 보철물 제작 기술로 도입이 되었다. 본 연구의 목적은 3D 프린팅 기술에 의해 제작된 금속 코어와 상부 도재와의 전단결합강도를 평가하는 것이다. 본 연구를 위해 30개의 금속 코어를 제작하였다(cast 15개, 3D printing 15개). 금속 코어에 치과용 도재를 축성하여 시편 제작을 완료하였다. 완성된 시편의 전단결합강도는 crosshead speed 1mm/min으로 하중을 가하여 측정하였으며, 두 그룹의 전단결합강도 값 사이에는 통계적으로 유의한지 알아보기 위하여 Mann-Whitney test를 이용하였다(유의수준 0.05). 측정이 끝난 후 시편을 대상으로 파절양상을 분석하였다. 본 연구를 위한 실험 설계, 금속 코어 제작, 도재 축성 등의 시편 제작부터 실험 수행과 수행 후 실험 데이터 분석과 통계 분석 그리고 파절된 시편을 대상으로 한 파절 양상 분석까지 총 6개월이 소요되었다. 실험 결과 cast 50.14, 3D printing 54.36 MPa를 갖는 것으로 조사되었고, 통계적으로도 유의하였다. 파절양상은 두 집단 모두 시편의 대부분이 혼합형 파절양상을 보였다. 이와 같은 결과들로 미루어볼 때 3D 프린팅에 의해 제작된 금속도재관 제작을 위한 금속 코어는 임상적으로 허용이 가능할 것으로 사료된다.

치과용 지르코니아 코어 가공후의 잔여물을 활용하여 주입성형법으로 제조한 소결체의 특성 (The Properties of Sintered Body by Using the Slip Casting Process with Remained Dental Zirconia Block after Machining)

  • 김상수;이동윤;서정일;배원태
    • 대한치과기공학회지
    • /
    • 제34권2호
    • /
    • pp.75-81
    • /
    • 2012
  • Purpose: All ceramic crown, made from zirconia instead of metal for core material, is recognized the best esthetical prosthesis. Recently, high-priced zirconia blocks and expensive CAD/CAM machines come into use for making zirconia core. In this study, slip casting process is adapted to evaluate the possibility of the recycling the remained parts of zirconia block after machining. Methods: Remained zirconia blocks were reduced to powders with zirconia mortar, and screened with 180 mesh sieve. Passed powders were ball milled under various conditions to obtain the optimum zirconia slip for casting. Solid casting method was used for casting the specimens with plaster mold. Formed specimens were dried and biscuit fired at $1,000^{\circ}C$ for 1 hour. Biscuit fired specimens were finished with exact shape of square pillar. Finished specimens were fired from $1,200^{\circ}C$ to $1,550^{\circ}C$ at $50^{\circ}C$ intervals for 1 hour. Linear shrinkage, apparent porosity, water absorption, bulk density, and flexural strength were tested. Microstructures were observed by SEM. Results: Above examinations indicated that the optimum firing temperture was $1,500^{\circ}C$, and when fired at this temperature for 1 hour, apparent porosity was 0% and flexural strength was 680MPa. SEM photomicrographs showed uniform 200~300nm grain size, which is equal with microcture of sintered commercial zirconia block. when compare 24% linear shrinkage of cast specimen with 20% linear shrinkage of CAD/CAM machined block, it was estimated that the size controlling of cast core was not so difficult. Conclusion: According to the all of this experimental results, the cast zirconia core produced from the remained parts of zirconia block was possible to use for all ceramic denture.

Marginal accuracy and fracture strength of Targis/Vectris Crowns prepared with different preparation designs

  • Song, Ho-Yong;Cho, Lee-Ra
    • 대한치과보철학회지
    • /
    • 제38권6호
    • /
    • pp.791-799
    • /
    • 2000
  • Statement of problem. Targis/Vectris restorations provide excellent esthetics. Marginal accuracy is significantly influenced by the preparation design. There were no studies to examine the effect of preparation design on the marginal discrepancy and fracture strength of Targis / Vectris crowns. Purpose. This study evaluated the marginal accuracy before and after cementation, and the fracture strength of FRC/Ceromer(Targis / Vectris) crowns according to different preparation design. Material and method. Three metal dies with different convergence angles($6^{\circ},\;10^{\circ},\;15^{\circ}$) were prepared. Total 30 (10 for each angle) Targis/Vectris crowns were made. The restorations were evaluated for adaptation of the margin before and after cementation, then were compressively loaded to failure. Fracture surfaces of the crowns were examined using a SEM. Results. The mean marginal gap was $49{\yen}m\;for6^{\circ},\;55{\S}>for\;10^{\circ}\;and\;70{\S}>for\;15^{\circ}$ and in clinically acceptable level. The mean marginal gap increased significantly after cementation. The increasing amount during cementation was the largest in the $6^{\circ}$ group. The crowns on 60 convergence angle had a significantly higher fracture strength than the crowns on $15^{\circ}$ angle. Mean fracture strength of total crowns regardless of convergence angle was 1390 N, which was higher than all-ceramic crowns. SEM observation showed two-mode fracture pattern. Conclusion. From the results of this study, all of the FRC/Ceromer crowns had clinically acceptable marginal accuracy and could withstand the bite force. Moreover, less convergent angle than all-ceramic crown might be recommended for preparation procedure.

  • PDF

유기조성물을 이용한 페이스트형 일반도재 시스템 (Development of Organic Paste Porcelain for Fixed Prostheses)

  • 한중석;이명현;김대현;정헌영
    • 구강회복응용과학지
    • /
    • 제20권2호
    • /
    • pp.109-120
    • /
    • 2004
  • 덴틴, 에나멜, 투명 일반도재를 페이스트화 하여 치아의 색상, 투명도 및 구조를 고려한 복합층구성물을 미리 제조하여 심미수복물을 용이하게 제작하는 공정을 개발하였다. 페이스트 상태에서 성형성과 유동특성이 확보되고, 소성 후 색도, 및 강도 등의 제특성들을 만족시킬 수 있는 결합제 시스템으로서 UV (creation universal liquid)를 선정하였고 조성 및 최적화가 이루어졌다. 페이스트는 24시간까지도 점성 및 작업성이 유지되었고, 이를 이용하여 복합층 구성물의 용이한 성형이 가능하였다. 소성수축률은 15.2%로 기존의 방법으로 제조한 시편에 비해 0.8% 낮았으나 유의차는 없었다. spectrophotometer에 의한 색도특성 관찰결과 덴틴재를 기존 제조방식으로 제조한 시편과 페이스트형 도재 시스템으로 제조한 시편에서 $L^*$, $a^*$, $b^*$가 각각 60~80, -1.5~+1.5, 5~20 사이의 값을 나타냄을 확인하였다. 측정값으로부터 구해진 제조방식에 따른 시편 간의 색차(${\Delta}E^*$)는 0.156으로 극히 근소한 차이를 나타냄을 확인하였다. 유기물 첨가에 따른 소성 후 잔류물 함량은 검출오차범위 내에 있었으며, 기존의 제조방식으로 제조한 소성체와 페이스트형 도재 시스템을 이용한 소성체의 강도는 각각 $70{\pm}4MPa$, $74{\pm}3MPa$으로 유의차가 없이 근사한 물성을 나타내었다. 페이스트형 도재를 이용한 도재축성법을 기존방법과 비교분석한 결과, 기계적 또는 광학적 특성의 변화없이 적용이 가능하였다.