Thermal Shock Tests and Thermal Shock Parameters for Ceramics

  • Awaji, Hideo;Choi, Seong-Min
    • 한국세라믹학회지
    • /
    • 제49권4호
    • /
    • pp.385-396
    • /
    • 2012
  • Thermal shock test methods and thermal shock parameters for ceramics were reviewed from the following viewpoints: (1) The test methods should be based on the precise estimation of both temperature and thermal stress distributions in a specimen taking into account the temperature-dependent thermo-mechanical properties; (2) The thermal shock parameters must be defined as a physical property of the materials and described as a function of temperature at the fracture point of the specimen; (3) The relation between the strength and fracture toughness of brittle ceramics under a thermal shock load must be the same as the relation under a mechanical load. In addition, appropriate thermal shock parameters should be defined by the thermal shock strength and thermal shock fracture toughness based on stress and energy criteria, respectively. A constant heat flux method is introduced as a testing technique suitable for estimating these thermal shock parameters directly from the electric power charged.

765 kV용 400 kN 현수애자 개발 (Development of Extra High Voltage(400kN) Porcelain Insulator for Transmission Lines)

  • 최인혁;최장현;이동일;최연규
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제52권8호
    • /
    • pp.348-353
    • /
    • 2003
  • This paper was the research of high voltage suspension insulator (400 [kN]) including pottery stone, feldspar, clay and alumina of 17 [wt%]. The slurry was fabricated after ball milling mixed raw materials. Green compacts were made by the extrusion of jiggering method and were sintered at 1300[$^{\circ}C$] for 50 [min.] in the tunnel kiln. The sintered density was reached to 97% of theoretical density, and the bending strength was 1658 [k $g_{f}$/$\textrm{cm}^2$] and hardness and fracture toughness which was measured by ICL( indentation crack length ) method were 1658 (kgf/$\textrm{cm}^2$) and 27.5 [Gpa], respectively. In measurement of tana and insulation break voltage of 400 (kN) porcelain, tan$\delta$ took some numerical value between 17${\times}$10$_{-3}$ and 61${\times}$10$_{-3}$ and insulation break voltage value was 19.9$\pm$1.4 [㎸/mm]. The test was performed to research whether the shape of pin affect a overvoltage break load or not As a consequence, when a pin was designed a pin diameter 51 [mm] with the bottom form of two-step constructed with straight in the suspension insulator, Insulator showed overvoltage break load 52 [ton] of the highest value and reflected a fine characteristic in aged deterioration test which is one of the accelerated aging test. Also it could be confirmed a fine characteristic through performing the test that electrical property of insulator was established correctly in accordance with IEC 60383-1 standards.s.

건물의 외주부 존에 대한 동적 부하모델 이용 피크냉방부하 저감효과 분석 (Evaluation on Reducing Peak Cooling Load Based on Dynamic Load Model of Building Perimeter Zones)

  • 이경호
    • 한국태양에너지학회 논문집
    • /
    • 제31권4호
    • /
    • pp.1-8
    • /
    • 2011
  • In this paper, inverse building modeling was applied to building perimeter zones which have different window orientation. Two test zones of east-facing and west-facing zones in ERS(Energy Resource Station) building, which is representative of small commercial building, was used to test performance of cooling load calculation and peak cooling load reduction. The dynamic thermal load model for the east and west zone was validated using measured data for the zones and then it was used to investigate the effect of peak cooling load reduction by adjustment of indoor cooling temperature set points during on-peak time period. For the east zone, the peak load can be reduced to about 60% of the peak load for conventional control even without any precooling. For the west zone, PLR is nearly independent of the start of the on-peak period until a start time of 1pm. Furthermore, PLR has a small dependence on the precooling duration. Without any precooling, the peak cooling load can be reduced to about 35% of the peak load associated with conventional control.

J적분에 의한 SB41강의 피로균열 진전 특성 평가 (Description of crack growth behavior of SB41 steel in terms of J integral)

  • 배원호;김상태;이택순
    • 대한기계학회논문집
    • /
    • 제14권6호
    • /
    • pp.1568-1575
    • /
    • 1990
  • 본 연구에서는 중앙균열을 가진 SB41강의 평판이 하중제어와 변형률제어 피로 상태에서 소규모 항복, 대규모 항복, 또는 전면 항복의 각 응력에서 피로균열 진전 속 도와 J적분 범위, .DELTA.J와의 관계를 조사하는 한편, 피로균열 진전 속도를 지배하는 국 소적 역학 인자인 균열선단 개구변위, COD와 균열 진전 속도와 관계 및 그 특성을 고 찰하였다.

세라믹 코팅 Al 부스바의 열적·기계적 특성 (Thermal and Mechanical Properties of Ceramic Coated Al Bus Bar)

  • 곽동순;백승명;곽민환
    • 전기학회논문지
    • /
    • 제66권11호
    • /
    • pp.1651-1656
    • /
    • 2017
  • This paper deals with the thermal and mechanical properties of ceramic coating material for bus bars. A ceramic coated samples were prepared for the mechanical properties test. There are two types of samples. One is a square shape and the other is a busbar shape. Each sample was deteriorated for 30 days to compare the thermal and mechanical properties with the non-degraded samples. Two thermal properties tests are TGA and flammability tests, and four mechanical properties tests are drop impact test, cross cut, tensile test, and bend test. The ceramic coating material was never damaged by impact and did not separate from aluminum in the cross cut test. In the tensile test, the breakage of the insulating material did not occur until aluminum fractured, and the breakage of the insulating material did not occur until the maximum load in the bending test. The decomposition temperature (melting point) of the ceramic coating material was higher than that of other epoxy insulators. This ceramic coating material is nonflammable and it has excellent fire stability.

30 MN 스트레인 게이지 방식 힘 센서의 제작 및 특성 (Fabrication and Characteristics of 30 MN Strain Gage Type Force Sensor)

  • 강대임;송후근;이정태
    • 센서학회지
    • /
    • 제3권2호
    • /
    • pp.24-32
    • /
    • 1994
  • 힘 증강기법을 이용하여 10 MN 로드셀 3개로 30 MN 힘 센서를 설계 제작하였다. 로드셀은 스트레인 게이지방식으로서 기둥형 감지부로 설계되었으며 오차를 줄이기 위하여 온도보상회로등이 내장되어 있다. 특성실험 결과 제작된 힘 센서의 총오차는 0.1 %이내로 추정되어 4.5 MN 이상의 대용량 재료시험기의 교정 및 시험에 유용하게 사용될 것으로 기대된다.

  • PDF

고무차륜형 AGT 경량전철 차량용 알루미늄 차체의 개발 (Development on the Aluminum Carbody for Rubber-Tired AGT Vehicle)

  • 김연수;박성혁;백남욱;김동승
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2003년도 춘계학술대회
    • /
    • pp.1118-1123
    • /
    • 2003
  • Based on the design requirements(size, strength, structure, weight, and etc.) for the rubber-tired AGT vehicle, carbody made of aluminum alloy is designed. The analysis of strength and stiffness is performed in the designed carbody, which results in the modification for optimal shapes and structures. It consists of a under frame, side frame, roof frame, end frame and forehead frame. After the carbody manufactured, tests are performed, which are vertical load test, longitudinal compressive load test, twisting load test, twisting natural frequency measurement, bending natural frequency measurement and 3 points supporting test. Results of them can guarantee a structural safety.

  • PDF

사각 관 구조물의 충격에 의한 좌굴특성 (Buckling Behavior of a Square Tube Structure by Lateral Impact Load)

  • 윤경호;송기남;강흥석
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2001년도 춘계학술대회논문집A
    • /
    • pp.812-818
    • /
    • 2001
  • The drop type impact test and finite element analysis are established for examining the buckling behavior of a square tube under the lateral impact load. Based on these results, the effects by the boundary conditions for supporting the structure are reviewed, which are as follows. One is pinned condition by screw; the other is fixed by welding. The critical impact force and acceleration by test are nearly same between two cases. However, the critical impact velocity of the pinned condition is higher than that of the fixed case. Therefore, the dynamic buckling behavior of a pinned structure is better than the fixed condition in view of critical impact velocity. These test and analysis results will be adaptable for predicting the dynamic structural integrity of a tube structure not only the axial impact event but the lateral impact event.

  • PDF

SI 엔진의 텀불 유동과 화염전파 (Tumble flow motion and flame propagation in a SI engine)

  • 지명석
    • 한국산업융합학회 논문집
    • /
    • 제2권2호
    • /
    • pp.155-163
    • /
    • 1999
  • In this study, single cylinder engines with different tumble ratio were made to find out in-cylinder fluid motion and flame propagation. Tumble ratio derived from the steady state flow rig test. Flame propagation speed was obtained using cylinder head gasket ionization probe and the piston ionization probe. And the combustion pressure in cylinder was measured to analyze the combustion characteristics. In case of high tumble engine, BSFC and BSHC were decreased and BSNOx was increased at part load test. Also BMEP and combustion peak pressure was increased at full load test. Tumble flow motion had an great effects on initial burning period rather than main burning period in part load test.

  • PDF

소형 압전유압펌프 브레이크 시스템의 성능해석 및 실험 (Performance Analysis and Test of the Small Piezoelectric-Hydraulic Pump Brake System)

  • 황용하;황재혁;응위웬 안 푹;배재성
    • 항공우주시스템공학회지
    • /
    • 제12권4호
    • /
    • pp.49-56
    • /
    • 2018
  • 본 논문에서는 소형 압전유압펌프 브레이크 시스템의 성능해석 및 실험을 수행하였다. 먼저 브레이크 시스템의 구성을 위해 브레이크 부하 구성품의 3-D 모델링을 수행하였고, 상용 프로그램인 AMESim을 이용한 모델링을 진행하였다. 브레이크 시스템 모델링에는 플로팅 타입의 캘리퍼를 부하로 활용하였다. AMESim 시뮬레이션을 통해, 부하 압력과 체크밸브 변위 및 무부하 상태에서의 유량을 계산하였으며 브레이크 부하의 추가에 따른 성능해석 및 동특성 변화를 확인하였다. 브레이크 시스템의 성능 실험을 위해 부하를 고정시키는 치구를 제작하였고, 무부하 상태에서의 유량 및 부하 압력 형성 실험을 수행하고 시뮬레이션 결과와 비교하였다. 실험 결과, 최대 부하압력은 130Hz에서 약 73bar, 최대 유량 발생은 145Hz에서 약 203cc/min로, 중소형 무인기 브레이크 시스템에 적용가능성을 확인하였다. 또한 시뮬레이션 결과와 실험결과의 오차는 부하 압력과 토출 유량에서 각각 6%, 5% 정도이며, 모델링이 브레이크 성능해석에 효과적으로 활용될 것으로 판단된다.