Properties of EMNC According to Addition Contents Variation for Nanosilica (2) -For Mechanical, Electrical Properties (나노 실리카 충진함량 변화에 따른 EMNC의 특성 연구 (2) -기계적, 전기적 특성 중심으로-)

  • Park, Jae-Jun
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.25 no.11
    • /
    • pp.886-894
    • /
    • 2012
  • In order to develop electrical insulation materials, epoxy-nanosilica-microsilica mixture composites (ENMC) was synthesized, and mechanical properties such as their tensile and flexural strength, and AC insulation breakdown strength were investigated. Properties of mechanical strength and AC insulation breakdown strength are analyzed as scale and shape parameter with respect to weibull plot. Their tensile and flexural strength, AC insulation breakdown strength were compared original epoxy or EMC to ENMC. The 4 phr nano-silica addition and the 65 wt% micron-silica mixture composite (ENMC) was found to have the highest tensile and flexural strength. In the tensile strength was improved 29%, and flexural strength was improved 60.9% higher than those of the original epoxy. In the insulation breakdown strength, ENMC_4 phr was improved 17% and ENMC_5 phr was improved 15.8% higher than those of the EMC.

Enhancing mechanical and durability properties of geopolymer concrete with mineral admixture

  • Jindal, Bharat Bhushan;Singhal, Dhirendra;Sharma, Sanjay;Parveen, Parveen
    • Computers and Concrete
    • /
    • v.21 no.3
    • /
    • pp.345-353
    • /
    • 2018
  • This paper approaches to improve the mechanical and durability properties of low calcium fly ash geopolymer concrete with the addition of Alccofine as a mineral admixture. The mechanical and durability performance of GPC was assessed by means of compressive strength, flexural strength, permeability, water absorption and permeable voids tests. The correlation between compressive strength and flexural strength, depth of water penetration and percentage permeable voids are also reported. Test results show that addition of Alccofine significantly improves the mechanical as well as permeation properties of low calcium fly ash geopolymer concrete. Very good correlations were noted between the depth of water penetration and compressive strength, percentage permeable voids and compressive strength as well as between compressive strength and flexural strength.

Evaluation of polymethyl methacrylate resin mechanical properties with incorporated halloysite nanotubes

  • Abdallah, Reham M.
    • The Journal of Advanced Prosthodontics
    • /
    • v.8 no.3
    • /
    • pp.167-171
    • /
    • 2016
  • PURPOSE. This study inspects the effect of incorporating halloysite nanotubes (HNTs) into polymethyl methacrylate (PMMA) resin on its flexural strength, hardness, and Young's modulus. MATERIALS AND METHODS. Four groups of acrylic resin powder were prepared. One group without HNTs was used as a control group and the other three groups contained 0.3, 0.6 and 0.9 wt% HNTs. For each one, flexural strength, Young's modulus and hardness values were measured. One-way ANOVA and Tukey's test were used for comparison (P<.05). RESULTS. At lower concentration (0.3 wt%) of HNT, there was a significant increase of hardness values but no significant increase in both flexural strength and Young's modulus values of PMMA resin. In contrast, at higher concentration (0.6 and 0.9 wt%), there was a significant decrease in hardness values but no significant decrease in flexural strength and Young's modulus values compared to those of the control group. CONCLUSION. Addition of lower concentration of halloysite nanotubes to denture base materials could improve some of their mechanical properties. Improving the mechanical properties of acrylic resin base material could increase the patient satisfaction.

Effect of Mixing Method on Mechanical Properties of Fiber Reinforced Concrete

  • Kim, Hyun Wook;Lee, Chang Joon
    • Journal of the Korea Institute of Building Construction
    • /
    • v.15 no.3
    • /
    • pp.351-357
    • /
    • 2015
  • Fiber reinforced concrete (FRC) has been successfully used to enhance the flexural toughness of concrete. As fibers are randomly oriented in FRC, they sometimes produce clumps that reduce the mechanical performance, and a properly chosen mixing protocol can be a way to minimize this problem. In this research, the effects of mixing method on the mechanical properties of FRC were investigated. The compressive strength, flexural strength, and flexural toughness were measured using three different mixing methods. It was shown from the results that the compressive strength and peak flexural load were not affected by changes in mixing method. However, in terms of flexural toughness, the changes in mixing method clearly affected the flexural toughness of FRC. The truck-mixed FRC outperformed two pan-mixed FRCs.

Mechanical strengths of self compacting concrete containing sawdust-ash and naphthalene sulfonate

  • Elinwa, Augustine U.;Mamuda, Mamuda;Ahmed, M.
    • Advances in concrete construction
    • /
    • v.2 no.4
    • /
    • pp.301-308
    • /
    • 2014
  • The present research work is on the effect of sawdust ash (SDA) on the mechanical strengths of self compacting concrete (SCC) using naphthalene sulfonate (NS) as a plasticizer. Experiments on compressive, flexural and splitting tensile strengths are conducted and the data analyzed using the Minitab 15 software. The results showed that SDA can defer the reaction of cement hydration and prolong the setting times of cement paste. This was very much pronounced on the flexural and splitting tensile strengths at 90 days of curing which are 36 % and 33 % higher than the control strengths, respectively. The study has proposed strength relations of mortar compressive strength with the flexural and splitting tensile strengths and these are, 5 and 7 times respectively. The flexural strength is 1.5 times that of the splitting tensile. Finally, linear models were developed on these relationships.

Effects of cement dosage and steel fiber ratio on the mechanical properties of reactive powder concrete

  • Erdogdu, Sakir;Kandil, Ufuk;Nayir, Safa
    • Advances in concrete construction
    • /
    • v.8 no.2
    • /
    • pp.139-144
    • /
    • 2019
  • In this study, the mechanical properties of reactive powder concrete (RPC) with a constant cement to silica fume ratio of 4 were investigated. In the experimental program, reactive powder concretes with steel fiber at different ratios were produced. Five productions using quartz sand with a maximum grain size of 0.6 mm were performed. A superplasticizer with a ratio of 3% of the cement was used for all productions. $40{\times}40{\times}160mm$ prismatic specimens were prepared and tested for flexural and compression. The specimens were exposed to two different curing conditions as autoclave and standard curing condition. Autoclave exposure was performed for 3 hours under a pressure of 2 MPa. It was observed that the compressive strength of concrete, along with the flexural strength exposed to autoclave was quite high compared to the strength of concretes subjected to standard curing. The results obtained indicated that the compressive strength, along with the flexural strength of autoclaved concrete increased as the amount of cement used increases. Approximately 15% increase in flexural strength was achieved with a 4% steel fiber addition. The maximum compressive strength that has been reached is over 210 MPa for reactive powder concrete for the same steel fiber ratio and with a cement content of $960kg/m^3$. The relationship between compressive strength and flexural strength of reactive powder concrete exposed to both curing conditions was also identified.

Analysis of the Mechanical Properties of High-Tension Performance Biochar Concrete Reinforced with PVA Fibers Based on Biochar Cement Replacement Ratio

  • Kim, Sangwoo;Lee, Jihyeong;Hong, Yeji;Kim, Jinsup
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.44 no.5
    • /
    • pp.603-613
    • /
    • 2024
  • This study evaluated the mechanical properties of high-tension performance biochar concrete, focusing on the effects of varying biochar cement replacement ratios (0 %, 1 %, 2 %, 3 %, 4 %, and 5 %). Mechanical properties, including compressive strength, tensile strength, and flexural strength, were tested. The results showed a general decrease in compressive strength with increasing biochar replacement, with significant reductions at 1 % to 3 % levels. PVA fiber reinforcement improved long-term compressive strength, particularly at higher biochar levels. Tensile and flexural strength also showed initial reductions with low biochar levels but improved at higher replacement levels. PVA fibers consistently enhanced tensile and flexural strength. SEM images confirmed the integration of biochar and PVA fibers into the cement matrix, enhancing microstructural density and crack resistance.

Variation of Mechanical Properties in Polyacetal with Melamine (멜라민 함량에 따른 폴리아세탈의 기계적 특성 변화)

  • 박광석;서광석
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1999.11a
    • /
    • pp.498-500
    • /
    • 1999
  • Polyacetals with melamine were investigated in terms of mechanical properties. It was found that tensile strength, impact strength and elongation were decreased with the increase of melamine content up to 30 par, flexural strength had no remarkable changes. For master-batch using polyurethane as carrier resin, in which the ratio of polyurethane to melamine was 2:1, tensile strength and flexural strength were decreased and impact strength remained unchanged with melamine me content.

  • PDF

A Study on Mechanical, Electrical Properties of Epoxy/MICA Composites with MICA Filled Contents (Epoxy/MICA 복합체의 MICA 충진함량 변화에 대한 기계적, 전기적 특성연구)

  • Park, Jae-Jun
    • The Transactions of The Korean Institute of Electrical Engineers
    • /
    • v.62 no.2
    • /
    • pp.219-227
    • /
    • 2013
  • This paper reported a study on the thermal, mechanical and electrical insulation properties of epoxy/mica composites. To investigate the effect of mica content, glass transition temperature, mechanical properties such as tensile and flexural strength, and insulation breakdown properties for epoxy composites with various contents of mica. The effect of insulation thickness on insulation breakdown property was also studied. It was observed that tensile and flexural strength decreased with increasing mica content, while elastic modulus increased as the mica content increased. AC insulation breakdown strength for all epoxy/mica composites was higher than that of neat epoxy and that of the system with 20 wt% mica was 14.4% improved. As was expected, insulation breakdown strength at $30^{\circ}C$ was far higher than that at $130^{\circ}C$, and it was also found that insulation breakdown strength was inversely proportion to insulation thickness.

Mechanical Properties of $Al_2O_3-AlN$ Particulate Composite ($Al_2O_3-AlN$계 입자복합체의 기계적 성질)

  • 김영우;박홍채;오기동
    • Journal of the Korean Ceramic Society
    • /
    • v.33 no.1
    • /
    • pp.101-109
    • /
    • 1996
  • The mechanical propertieso f sintered AlN with the addition of alumina were investigated The flexural strength of the AlN dispersed ALON specimens was higher than that of ALON and fracture toughness showed similar tendency. The high-temperature flexural strength of specimens which 50 and 64.3 mol% alumina was added to AlN was constant up to 100$0^{\circ}C$ with about 290 and 420 MPa respectively but abruptly decreased at 120$0^{\circ}C$ In the specimens which contained 5 and 30mol% alumina the flexural strength increased to about 14% at 100$0^{\circ}C$ and did not decrease at 120$0^{\circ}C$ compared to at room temperature.

  • PDF