• 제목/요약/키워드: Magnetic moment

검색결과 325건 처리시간 0.023초

Template Synthesis and Characterization of Host (Nanocavity of Zeolite Y)-Guest ([Cu([18]aneN4S2)]2+, [Cu([20]aneN4S2)]2+, [Cu(Bzo2[18]aneN4S2)]2+, [Cu(Bzo2[20]aneN4S2)]2+) Nanocomposite Materials

  • Salavati-Niasari, Masoud;Mirsattari, Seyed Nezamodin;Saberyan, Kamal
    • Bulletin of the Korean Chemical Society
    • /
    • 제30권2호
    • /
    • pp.348-354
    • /
    • 2009
  • Copper(II) complexes with tetraoxo dithia tetraaza macrocyclic ligands; [18]ane$N_4S_2$: 1,4,10,13-tetraaza-5,9,14,18-tetraoxo-7,16-dithia-cyclooctadecane, [20]ane$N_4S_2$: 1,5,11,15-tetraaza-6,10,16,20-tetraoxo-8,18-dithia-cyclocosane,Bzo2[18]ane$N_4S_2$: dibenzo-1,4,10,13-tetraaza-5,9,14,18-tetraoxo-7,16-dithia-cyclooctadecane, Bzo2[20]ane$N_4S_2$: dibenzo-1,5,11,15-tetraaza-6,10,16,20-tetraoxo-8,18-dithia-cyclocosane; were entrapped in the nanopores of zeolite-Y by a two-step process in the liquid phase: (i) adsorption of [bis(diamine)copper(II)] (diamine = 1,2-diaminoethane, 1,3-diaminopropane, 1,2-diaminobenzene, 1,3-diaminobenzene); $[Cu(N-N)_2]^{2+}$-NaY; in the nanopores of the zeolite, and (ii) in situ template condensation of the copper(II) precursor complex with thiodiglycolic acid. The obtained complexes and new host-guest nanocomposite materials; $[Cu([18]aneN_4S_2)]^{2+}-NaY,\;[Cu([20]aneN_4S_2)]^{2+}-NaY,\;[Cu(Bzo_2[18]aneN_4S_2)]^{2+}-NaY,\;[Cu(Bzo_2[20]aneN_4S_2)]^{2+}$-NaY; have been characterized by elemental analysis FT-IR, DRS and UV-Vis spectroscopic techniques, molar conductance and magnetic moment data, XRD and, as well as nitrogen adsorption. Analysis of data indicates all of the complexes have been encapsulated within nanopore of zeolite Y without affecting the zeolite framework structure.

강체모델 기반 시스템 안정성을 고려한 자기부상 플라이휠 에너지 저장장치의 최적 설계 (Optimal Design of Magnetically Levitated Flywheel Energy Storage System Based on System Stability Using Rigid-Body Model)

  • 김정완;유승열;배용채;노명규
    • 대한기계학회논문집A
    • /
    • 제34권3호
    • /
    • pp.283-289
    • /
    • 2010
  • 친환경기술과 신재생 에너지 자원에 대한 세계적인 관심이 증가하면서, 플라이휠 에너지 저장 장치는 화학전지나 연료전지와 같은 기존의 에너지 저장 시스템의 대안 중 하나로 부상하고 있다. 플라이휠 에너지 저장장치의 에너지 저장 용량은 극질량 관성모멘트와 회전속도의 제곱에 비례하기 때문에, 가능한 높은 회전속도와 높은 극질량 관성모멘트를 갖도록 설계하는 것이 중요하다. 하지만, 시스템의 운전안정성 확보가 최적설계의 구속조건으로 작용할 수 있다. 본 논문에서는 에너지 저장 용량을 최대화하고 운전안정성 및 외란에 대한 강인성을 확보하는 플라이휠 시스템의 최적설계를 제안한다. 그리고, 기존의 PD 제어에 비교하여 교차궤환제어법이 자이로스코프효과를 줄이고, 에너지 저장밀도를 높이는데 필수적임을 확인하였다.

(CrAs)3(MnAs)3(110) 초격자의 전자구조와 자성에 대한 제일원리 연구 (First-principles Study on the Magnetism and Electronic Structure of (CrAs)3(MnAs)3(110) Superlattice)

  • 이재일;홍순철
    • 한국자기학회지
    • /
    • 제16권2호
    • /
    • pp.111-114
    • /
    • 2006
  • Zinc-blonde 구조를 가지는 CrAs와 MnAs에서 (110)면 원자층으로 이루어진 초격자의 자성을 제일원리 방법을 이용하여 연구하였다. 이를 위해 CrAs와 MnAs의 (110)층이 각기 세 층씩 교대로 반복되는 $(CrAs)_3(MnAs)_3(110)$ 초격자계의 전자구조를 총 퍼텐셜 선형보강평면파동(FLAPW) 에너지띠 방법을 이용하여 계산하였다. Cr-As로 이루어진 층과 Mn-As로 이루어진 층이 접합되는 계면에 있는 Cr과 Mn원자의 자기모멘트를 계산한 결과 각기 $3.07\;\mu_B$$3.74\;\mu_B$로 가운데 층의 Cr과 Mn의 자기모멘트 값인 $3.06\;\mu_B$$3.76\;\mu_B$보다 약간 크거나 작았다. 계산된 상태밀도로부터 이 계의 전자구조와 반쪽금속성을 고찰하였다.

Tc and Jc distribution in in situ processed MgB2 bulk superconductors with/without C doping

  • Kim, C.J.;Kim, Y.J.;Lim, C.Y.;Jun, B.H.;Park, S.D.;Choo, K.N.
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제16권2호
    • /
    • pp.36-41
    • /
    • 2014
  • Temperature dependence of magnetic moment (m-T) and the magnetization (M-H) at 5 K and 20 K of the in situ processed $MgB_2$ bulk pellets with/without carbon (C) doping were examined. The superconducting critical temperature ($T_c$), the superconducting transition width (${\delta}T$) and the critical current density ($J_c$) were estimated for ten test samples taken from the $MgB_2$ bulk pellets. The reliable m-T characteristics associated with the uniform $MgB_2$ formation were obtained for both $MgB_2$ pellets. The $T_cs$ and ${\delta}Ts$ of all test samples of the undoped $MgB_2$ were the same each other as 37.5 K and 1.5 K, respectively. The $T_cs$ and ${\delta}Ts$ of the C-doped $MgB_2$ were 36.5 K and 2.5 K, respectively. Unlike the m-T characteristics, there existed the difference among the M-H curves of the test samples, which might be caused by the microstructure variation. In spite of the slight $T_c$ decrease, the C doping was effective in enhancing the $J_c$ at 5 K.

제어모멘트자이로 김블의 토크 외란 모델링 검증 및 피드포워드 제어를 이용한 토크 리플 저감 (Verification of Torque Disturbance Modeling of CMG Gimbal and Its Torque Ripple Reduction using Feed-Forward Control)

  • 이준용;오화석
    • 항공우주시스템공학회지
    • /
    • 제12권1호
    • /
    • pp.27-34
    • /
    • 2018
  • CMG의 발생 토크는 김블의 각속도에 비례하고 위성의 자세제어에 직접적인 영향을 미치기 때문에 김블의 토크 리플 저감이 필요하다. 본 논문에서는 토크 리플의 발생 원인을 베어링에 의한 마찰 불균형, 모터의 자기장과 상전류 불균형으로 가정하여 이를 수학적으로 모델링한다. 김블의 정속 구동 데이터를 통해 모델링의 파라미터를 추정하고 이를 이용하여 피드포워드 제어로 적용할 경우 영향성을 분석한다. 시뮬레이션을 통해 토크 리플과 각속도 변동이 저감되는 것을 확인하여 외란 모델링을 이용한 외란 저감 기법을 제시한다.

Analysis of Image Distortion on Magnetic Resonance Diffusion Weighted Imaging

  • Cho, Ah Rang;Lee, Hae Kag;Yoo, Heung Joon;Park, Cheol-Soo
    • Journal of Magnetics
    • /
    • 제20권4호
    • /
    • pp.381-386
    • /
    • 2015
  • The purpose of this study is to improve diagnostic efficiency of clinical study by setting up guidelines for more precise examination with a comparative analysis of signal intensity and image distortion depending on the location of X axial of object when performing magnetic resonance diffusion weighted imaging (MR DWI) examination. We arranged the self-produced phantom with a 45 mm of interval from the core of 44 regent bottles that have a 16 mm of external diameter and 55 mm of height, and were placed in 4 rows and 11 columns in an acrylic box. We also filled up water and margarine to portrait the fat. We used 3T Skyra and 18 Channel Body array coil. We also obtained the coronal image with the direction of RL (right to left) by using scan slice thinkness 3 mm, slice gap: 0mm, field of view (FOV): $450{\times}450mm^2$, repetition time (TR): 5000 ms, echo time (TE): 73/118 ms, Matrix: $126{\times}126$, slice number: 15, scan time: 9 min 45sec, number of excitations (NEX): 3, phase encoding as a diffusion-weighted imaging parameter. In order to scan, we set b-value to $0s/mm^2$, $400s/mm^2$, and $1,400s/mm^2$, and obtained T2 fat saturation image. Then we did a comparative analysis on the differences between image distortion and signal intensity depending on the location of X axial based on iso-center of patient's table. We used "Image J" as a comparative analysis programme, and used SPSS v18.0 as a statistic programme. There was not much difference between image distortion and signal intensity on fat and water from T2 fat saturation image. But, the average value depends on the location of X axial was statistically significant (p < 0.05). From DWI image, when b-value was 0 and 400, there was no significant difference up to $2^{nd}$ columns right to left from the core of patient's table, however, there was a decline in signal intensity and image distortion from the $3^{rd}$ columns and they started to decrease rapidly at the $4^{th}$ columns. When b-value was 1,400, there was not much difference between the $1^{st}$ row right to left from the core of patient's table, however, image distortion started to appear from the $2^{nd}$ columns with no change in signal intensity, the signal was getting decreased from the $3^{rd}$ columns, and both signal intensity and image distortion started to get decreased rapidly. At this moment, the reagent bottles from outside out of 11 reagent bottles were not verified from the image, and only 9 reagent bottles were verified. However, it was not possible to verify anything from the $5^{th}$ columns. But, the average value depends on the location of X axial was statistically significant. On T2 FS image, there was a significant decline in image distortion and signal intensity over 180mm from the core of patient's table. On diffusion-weighted image, there was a significant decline in image distortion and signal intensity over 90 mm, and they became unverifiable over 180 mm. Therefore, we should make an image that has a diagnostic value from examinations that are hard to locate patient's position.

졸-겔 방법을 이용하여 제작된 (Mn, Cr)xCo1-xFe2O4 박막의 구조적, 자기적 특성 (Structural and Magnetic Properties of (Mn, Cr)xCo1-xFe2O4 Thin Films Prepared by Sol-gel Method)

  • 김광주;김희경;박영란;박재윤
    • 한국자기학회지
    • /
    • 제16권1호
    • /
    • pp.23-27
    • /
    • 2006
  • 역스피넬 산화물 $CoFe_2O_4$에서 Co를 Mn 또는 Cr클 치환하여 얻어지는 $Mn_xCo_{1-x}Fe_2O_4$$Cr_xCo_{1-x}Fe_2P_4$ 박막시료 들을 졸-겔 방법을 이용하여 제작하고 그 구조적, 자기적 특성들을 비교분석 하였다. X-ray diffraction 측정 결과, Mn 치환의 경우는 치환량의 증가에 따라 격자상수가 증가하였지만 Cr치환의 경우는 격자상수가 거의 변화하지 않음이 관측되었다. 이와 같은 결과는 Mn 치환의 경우 팔면체 자리의 Co이온과 같은 원자가 +2를 가지게 되는 것으로 설명 가능하며 Cr치환의 경우는 +3을 가지게 되어 같은 양의 $Fe^{3+}$이온들의 $Fe^{2+}$로의 환원이 발생하는 것으로 설명되어질 수 있다. $Cr_Co_{1-x}Fe_2O_4$박막들에 대한 Mossbauer 스펙트럼 측정 결과 사면체 자리에 $Fe^{2+}$이온의 존재가 관측되었으며 이는 $Cr^{3+}$이온의 팔면체 자리 치환에 의하여 야기되는 사면체 자리의 $Fe^{3+}{\rightarrow}Fe^{2+}$ 환원에 의한 것으로 해석된다. 반면에 $Mn_xCo_{1-x}Fe_2O_4$ 박막들에 대한 Mossbauer스펙트럼 측정 결과, $Fe^{2+}$ 이온의 존재는 관측되지 않았으며 Mn 치환량이 큰 경우 (>0.47)팔면체 자리의 $Fe^{3+}$이온들의 사면체 자리로의 이동이 관측되었다. 박막들에 대한 진동시료자화(vibrating sample magnetometry)측정 결과, Mn, Cr 치환의 경우 모두 $CoFe_2O_4$와 비교하여 포화자화량이 증가함이 나타났으며 치환에 관여한 이온들 간의 스핀 자기 능률 크기의 비교를 통하여 그 정성적인 설명이 가능하다.

3-Benzylidine/Furfurylidine/(Pyridyl/Thienyl-2'-methylene) imino-5-p-sulphonamido phenyl azo-2-thiohydantoins와 UO2(VI), ZrO(IV) 및 Th(IV) 이온의 동종이핵 착물에 대한 합성 및 특성 (Synthesis and Characterization of Homobinuclear Complexes of UO2(VI), ZrO(IV) and Th(IV) ions with 3-Benzylidine/Furfurylidine/(Pyridyl/Thienyl-2'-methylene) imino-5-p-sulphonamido phenyl azo-2-thiohydantoins)

  • Dash, D.C.;Mahapatra, A.;Naik, P.;Mohapatra, R.K.;Naik, S.K.
    • 대한화학회지
    • /
    • 제55권3호
    • /
    • pp.412-417
    • /
    • 2011
  • [$M_2L(NO_3)_n(H_2O)_m$]의 일반식을 갖는 일련의 동종이핵 착물을 합성하여 원소분석, 열분석, 몰 전기전도도, 자기모멘트 및 분광학적 방법(IR, UV-vis 및 $^1H$-NMR)을 통해 특성을 조사하였다. 이 경우, 일반식에 있어서 M=$UO_2$(VI), ZrO(IV), Th(IV); L=3-benzylidine-imino-5-p-sulphonamido phenyl azo-2-thiohyatoin(bispt), 3-furfurylidine-imino-5-psulphonamido phenyl azo-2-thiohydantoin(fispt),3-pyridyl-2'-methylene-imino-5-p-sulphonamido phenyl azo-2-thiohydantoin (pmispt) 및 3-thienyl-2'-methylene-imino-5-p-sulphoanamido phenyl azo-2-thiohydantoin(tmispt); Th(IV)에 대해서 n=8 그 외의 것에 대해서는 n=4, bispt에 대해서는 m=4 그 외의 것에 대해서는 m=3을 의미한다. 이러한 결과에서 얻은 정보를 통해 리간드들은 4배위를 하는 것으로 확인되었는데, 즉 한 중심금속은azomethine 질소 및 카르보닐 산소에 배위되는 반면, 또 다른 중심금속은 아조 질소 및 thioimido 질소에 배위되어 위의 조성을 갖는 동종이핵 착물을 이룬다. 몇 가지 병원균에 대한 리간드와 그들의 지르코닐 착물의 독성 연구도 수행하였다.

Ba-Ferrite 단결정의 자기적 특성에 관한 뫼스바우어 분광학적 연구 (Mössbauer Studies of the Magnetic Properties in Ba-ferrite Single Crystal)

  • 서정철;지성훈;홍양기
    • 한국자기학회지
    • /
    • 제17권2호
    • /
    • pp.60-64
    • /
    • 2007
  • Ba-ferrite 단결정을 제조하여 자기적 성질을 Mossbauer 분광법으로 연구하였다. 단결정 시료를 c-축 방향으로 얇게 절단하고 그 면에 감마선을 조사한 결과 결정 전체에 걸쳐 Fe 이온의 스핀 방향이 c-축과 일치함을 확인하였다. 온도에 따른 초미세자기장의 감소 추세는 입자상태와 거의 비슷하였으며 결정 내 Fe원자의 이온 상태 역시 일치하였다. 결정구조는 Magnetoplumbite로서 결정상수는 $a_0=5.892{\AA},\;b_0=5.892{\AA},\;c_0=23.198{\AA}$로 정되었으며 그 외의 다른 상은 존재하지 않는 것으로 나타났다. $M\"{o}ssbauer$ spectrum은 결정 내에 존재하는 Fe의 자리에 따라 5의 각각의 다른 subspectrum이 존재하였는데 감마선의 방향이 c-축과 일치하여 모든 자리에서 4개의 공명흡수선 만이 존재하였다. 따라서 결정의 형태는 전체적으로 단일상으로 형성되었음을 확인하였고 여분의 ${\alpha}-Fe_2O_3$ 등은 존재하지 않음을 명확히 하였다. 자기이력곡선을 통하여 실온상태에서 포화자기모멘트는 70.71 emu/g, 보자력이 320 Oe의 값으로 측정되었다.

나노 옥사이드 층을 가진 스펙큘라 스핀밸브의 자기저항 특성 및 교환바이어스의 열처리 온도 의존성 (The Dependences of Magnetoresistance and Exchange Biasing on Annealing temperature in Top and Bottom Type Specular Spin Valves with Nano-oxide Layers)

  • 장성호;강탁;김희중;김광윤
    • 한국자기학회지
    • /
    • 제12권3호
    • /
    • pp.103-108
    • /
    • 2002
  • 나노옥사이드(nato-oxide layer, NOL) 층이 고정층에 첨가된 스펙큘라 스핀밸브(specular spin valve)와 NOL이 없는 기본 스핀 밸브를 UHV 스퍼터 시스템에서 FeMn 반강자성층을 사용하여 탑 및 바텀 형 스핀밸브를 제조하였으며, 제조한 시료의 열처리 온도에 따른 자기저항 특성 및 교환바이어스 특성을 비교 분석하였다. 탑 형 스핀밸브에서는 NOL이 있는 경우 25$0^{\circ}C$ 열처리에서 9.2%의 자기저항비를 얻을 수 있었으며, 바텀 형 스핀밸브에서는 25$0^{\circ}C$ 열처리에서 10.1%의 자기저항비를 얻을 수 있었다. 따라서 바텀 형 스핀밸브가 탑 형 스핀밸브보다 고정층에 첨가된 NOL의 스펙큘라 반사 효과가 높아 자기저항비가 증가함을 확인하였다. 또한 바텀 형 스핀밸브에서 25$0^{\circ}C$ 이상의 열처리시 NOL이 있는 경우가 NOL이 없는 경우보다 28 % 이상의 교환바이어스 증가를 보였다. 이와 같은 원인은 NOL이 첨가된 고정층의 자기모멘트의 감소와 X-선 회절 분석 결과로부터 NOL의 첨가에 따른 강화된 (111) FeMn집합조직 때문이라고 판단된다.