• 제목/요약/키워드: MPB70

검색결과 11건 처리시간 0.03초

Detection of Mycobacterium bovis in the lymph node of tuberculin positive cattle by guanidium isothiocyanate/silica DNA extraction and polymerase chain reaction

  • Cho, Yun-Sang;Jung, Suk-Chan;Yoo, Han-Sang;Kim, Jong-Man
    • 한국동물위생학회지
    • /
    • 제30권2호
    • /
    • pp.233-241
    • /
    • 2007
  • Tuberculin positive cattle without gross tubercle lesions should be confirmed by the bacteriological examination to determine the state of the infection. To overcome the time-consuming and laborious identification by culture and biochemical tests, polymerase chain reaction (PCR) has been used to identify Mycobacterium bovis. Due to various lipids in the cell wall of Mycobacterium spp, novel methods of DNA extraction from Mycobacterium spp have been developed. In this study, a newly developed guanidium isothiocyanate/silica DNA extraction method was directly applied to specimens from the tuberculin positive cattle. DNAs were directly extracted from the lymph nodes and the major polymorphic tandem repeat (MPTR) and mycobacterial protein of BCG 70 (MPB70) were amplified using PCR. The DNA extraction method using guanidium isothiocyanate/silica was efficient and safe, and the MPTR and MPB70 primers were specific to M bovis. Therefore, MPTR and MPB70 PCRs will be useful for the detection of M bovis in the lymph node from skin-test positive cattle.

피혁폐수의 혐기성 소화시 황산염과 중금속이 메탄균 활성에 미치는 영향 (Effect of Sulfate and Heavy Metals on Methanogenic Activation of in the Anaerobic Digestion of Tannery Wastes)

  • 신항식;오세은
    • 유기물자원화
    • /
    • 제4권1호
    • /
    • pp.13-21
    • /
    • 1996
  • 고농도 황산염과 중금속을 함유한 피혁폐수를 처리하기 위하여, 반응조의 처리도, 황환원균과 메탄균 사이의 기질경쟁 및 크롬농도에 대한 메탄균의 활성을 평가하였다. COD는 $35^{\circ}C$의 반응조 온도에서 유기부하량 2.0 gCOD/l.day와 18시간의 수리학적 체류시간에서 70% 이상의 제거율을 얻을 수 있었다. 황환원균과 메탄균 사이의 기질경쟁에서 황환원균에 의해 이용된 COD는 운전초기 15%에서 실험종료시 43%까지 증가되었다. 이는 유기물 분해로부터 발생되는 대부분의 전자가 황환원균에 의해 이용되어 황산염 환원에 의한 황화물이 생성되므로 메탄균의 활성은 강력히 억제되었다. 전 실험기간 동안 크롬농도는 90% 이상 제거되었으며, 크롬농도의 높은 제거율에도 불구하고 반응조의 처리능력은 거의 감소되지 않았다. 이는 반응조내에서 제거된 3가 크롬이 미생물의 활성에 영향을 미치지 않은 점으로 볼 때 3가 크롬이 6가 크롬에 비해 미생물에 대한 독성영향이 심하지 않다고 볼 수 있다.

  • PDF

2단 소성시간이 7.6/70/30 PLZT 세라믹의 전기적 특성에 미치는 영향 (Electro-optic Characteristics of 7.5/70/30 PLZT Ceramics According to the Second Stage Sintering Time)

  • 박창엽;정익채;정희승
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1987년도 정기총회 및 창립40주년기념 학술대회 학회본부
    • /
    • pp.220-223
    • /
    • 1987
  • In this paper, electro-optic characteristics of PLZT 7.6/70/30 composition in MPB regions, which antiferroelectric and ferroelectric phases coexist together, were studied. As sintering times are increased, Curie temperatures ore linearly decreased. And the antiferroelectric phase becomes more stronger when Curie temperatures are decreased. The crystal structure investigated by lie of X-ray analysis is proved to cubic in the thermally depoled specimen and rhombohedral in the poled specimen. Accordingly, the applicability of 7.6/70/30 specimen as image storage and display device is expected by the method for applying field induced reversible transitions between antiferroelectric(AFE) and ferroelectric(FE) phase.

  • PDF

고농도 암모니아를 함유한 돈사폐수의 고율혐기성 소화시 메탄균의 활성연구 (Activity of Methanogens in the High Rate Anaerobic Digestion of Swine Wastewater Containing High Ammonia)

  • 오세은;이채영
    • 대한환경공학회지
    • /
    • 제22권5호
    • /
    • pp.981-987
    • /
    • 2000
  • 축산분뇨에 대한 처리도 및 암모니아에 대한 독성을 평가하기 위하여 UASB 반응조를 운전하였다. 반응조의 운전결과 유기부하량 $2.6kg\;COD/m^3.day$과 수리학적 체류시간 3일에서 70%의 COD 제거효율을 얻을 수 있었으나, 유기부하량과 수리학적 체류시간을 각각 $7kg\;COD/m^3.day$과 2일로 유지한 경우 COD 제거율이 급격히 감소되었다. 반응조 슬러지의 유리암모니아에 대한 독성을 평가하기 위하여 수행된 회분식 실험 결과, 각 단계별 슬러지의 메탄균 활성은 0.5, 0.47 및 $0.3kgCH_4-COD/kgVSS.day$로 반응조내 유리암모니아 농도가 $500mg-N/{\ell}$에서는 메탄균의 활성이 4%, 유리암모니아 농도가 $1000mg-N/{\ell}$에서는 메탄균의 활성이 40% 감소되었다. 이러한 결과로부터 유리암모니아 농도가 $500mg-N/{\ell}$ 이하에서는 반응조 미생물에 미치는 저해정도가 작은 것으로 판단된다. 한편 $1000mgVSS/{\ell}$ 이내의 휘발성 고형물질을 포함하는 폐수는 혐기성균에 의해 쉽게 분해되므로 UASB 반응조를 안정적으로 운영할 수 있다.

  • PDF

성별과 나이에 따른 골반 형태 변화와 골반 변위 -방사선영상을 이용한 골반 계측- (Change of Morphologic Pelvis and Deviation According to Gender, Age -Radiological Pelvimetry-)

  • 강영한;김선칠
    • 대한방사선기술학회지:방사선기술과학
    • /
    • 제34권2호
    • /
    • pp.91-96
    • /
    • 2011
  • 정상인의 골반 정면 영상을 계측하여 성별과 나이에 따라 골반의 형태적 차이가 있는지 알아보고, 나이에 따라 골반의 변위가 발생하는지 남녀 구분하여 분석하였다. 정상인 총 382명(남성 194명, 여성 188명)을 대상으로 골반정면 단순촬영을 시행하여 PACS 영상에서 최대골반너비(MPB), 엉덩뼈너비(SB), 위골반공가로지름(TD), 넙다리뼈머리사이거리(DFH)를 측정하여 골반계측을 시행하였다. 성별에 따른 골반 계측 차이는 평균비교분석, 나이와 계측치의 관계는 상관분석을 하였다. 골반의 변위는 ANOVA test를 시행하였다. 최대골반너비는 성별에 따른 차이는 없었으나, 남성 엉덩뼈너비의 평균은 97.76 mm이었고, 여성은 102.00 mm으로 여성에서 엉덩뼈너비가 유의하게 큰 것으로 나타났다. 위골반공가로지름의 평균은 남성 138.00 mm, 여성 149.79 mm이었고, 넙다리뼈머리사이거리는 남성 141.94 mm, 여성 150.39 mm로 나타났고, 위골반공가로지름과 넙다리뼈머리사이거리는 여성에서 유의하게 더 큰 것으로 나타났다. 나이와 골반계측에서는 넙다리뼈머리 사이거리가 남성(r = -0.280)과 여성(r = -0.207)에서 각각 음의 상관관계가 있었다. 나이에 따른 골반 변위는 남성 50대에서 변위가 크게 나타났고, 여성은 60대, 70대에서 변위가 크게 나타났다. 엉덩뼈너비와 위골반공가로지름, 넙다리뼈머리사이거리는 남성보다 여성에서 더 크게 나타났고, 골반의 크기가 큰 사람은 최대골반너비와 엉덩뼈너비, 위골반공가로지름, 넙다리뼈머리사이거리도 컸다. 나이가 많을수록 변위가 크게 나타났고, 이는 노화의 과정이라고 판단된다.

MnO2 첨가가 0.985[Li0.04(Na0.545K0.46)0.96(Nb0.81Ta0.15Sb0.04)]O3+0.015KNbO3 세라믹스의 유전 및 압전 특성에 미치는 영향 (Effect of MnO2 Addition on Dielectric and Piezoelectric Properties of 0.985[Li0.04(Na0.545K0.46)0.96(Nb0.81Ta0.15Sb0.04)]O3 Ceramics)

  • 김유석;류주현
    • 한국전기전자재료학회논문지
    • /
    • 제27권6호
    • /
    • pp.361-366
    • /
    • 2014
  • $MnO_2$-doped $0.985[Li_{0.04}(Na_{0.545}K_{0.46})_{0.96}(Nb_{0.81}Ta_{0.15}Sb_{0.04})]O_3+0.015KNbO_3(0.985LNKNTS+0.015KNbO_3)$ lead-free ceramics were fabricated by conventional solid state method to develop excellent dielectric and piezoelectric properties. The result of X-ray diffraction patterns obviously indicated that all of the specimen has pure perovskite structure without secondary phase. In addition, orthorhombic phase and coexistance region of orthorhombic-tetragonal phase (MPB) were observed with amount of $MnO_2$. The optimal values of ${\rho}$=4.70 $g/cm^3$, $d_{33}=238$ pC/N, $k_P=0.46$, $Q_m=121$, ${\varepsilon}_r=849$, and $T_C=225^{\circ}C$ were obtained at 0.01 mol% $MnO_2$ doped $0.985LNKNTS+0.015KNbO_3$ ceramics sintered at $990^{\circ}C$ for 5 h, respectively. Hence, it was indicated that the suitable amount of $MnO_2$ could improve the electrical properties of $0.985[Li_{0.04}(Na_{0.545}K_{0.46})_{0.96}(Nb_{0.81}Ta_{0.15}Sb_{0.04})]O_3+0.015KNbO_3$ ceramics.

RAINBOW 압전 액츄에이터의 제조와 물성 (Processing and Properties of RAINBOW Piezoelectric Actuator)

  • 백종후;임은경;김창일;이미재;지미정;최병현;김세기
    • 한국전기전자재료학회논문지
    • /
    • 제19권3호
    • /
    • pp.222-227
    • /
    • 2006
  • RAINBOW(Reduced And Internally Biased Oxide Wafers) are a new class of high-displacement, piezoelectric actuator produced by selectively removing oxygen from one surface of ceramic using a high-temperature chemical reduction process. In this paper, RAINBOW actuator materials of $0.4Pb(Ni_{1/3}Nb_{2/3})O_3-0.6Pb(Zr_{x}Ti_{1-x})O_3$ ceramics were prepared. Its dielectric and piezoelectric properties were investigated in the vicinity of MPB. The piezoelectric properties showed the maximum value of ${\epsilon}r$ = 4871, $d_{33}$ = 610 ($10^{-12}$ m/V), $d_{31}$ = -299 ($10^{-12}$ m/V), $k_{33}$ = $71\%$, Qm = 70, in $0.4Pb(Ni_{1/3}Nb_{2/3})O_{3}-0.6Pb(Zr_{405}Ti_{595})O_3$ composition sintered at $1250^{\circ}C$. The strain - electric field characteristics of RAINBOW actuator were significantly improved comparison with the conventional bulk actuator. The prepared RAINBOW actuator showed about $390\;{\mu}m/100\;V$ displacement.

$Ba(La_{1/2}Nb_{1/2})O_3$의 고용량과 Zr/Ti 조성비가 $Ba(La_{1/2}Nb_{1/2})O_3-Pb(Zr, Ti)O_3$ 세라믹의 전기광학 특성에 미치는 영향 (Effects of $Ba(La_{1/2}Nb_{1/2})O_3$ content and Zr/Ti composition ratio on electrooptic properties of the $Ba(La_{1/2}Nb_{1/2})O_3-Pb(Zr, Ti)O_3$ ceramics)

  • 류기원;이성갑;배선기;이영희
    • 대한전기학회논문지
    • /
    • 제44권5호
    • /
    • pp.644-648
    • /
    • 1995
  • Transparent xBa(La$_{1}$2/Nb$_{1}$2/)O$_{3}$-(1-x)Pb(Zr, Ti)O$_{3}$ (x=8.5, 9.0[mol.%], Zr/Ti=70/30~40/60) ceramics were fabricated by the two-stage sintering method, the electrooptic properties were investigated with Ba(La$_{1}$2/Nb$_{1}$2/)O$_{3}$ content and Zr/Ti composition ratio. Decreasing the Zr/Ti ratio, the electrooptic property was changed from a quadratic electrooptic effect to a linear electrooptic effcet. In the BLN-PZT 9.0/50/50 specimen having the tetragonal structure, the linear electrooptic coefficient had the highest value of 6.01*10$^{-10}$ [m/V] and in the BLN-PZT 9.0/55/45 specimen which located near the MPB region, the quadratic electrooptic coefficient had the highest value of 10.53*10$^{-16}$ [m$^{2}$/V$^{2}$].

  • PDF

초음파 진동자용 MnO2가 Doping된 PZT-PSN 세라믹스의 구조 및 압전 특성 (Structural and Piezoelectric Properties of MnO2-Doped PZT-PSN Ceramics for Ultrasonic Vibrator)

  • 차유정;김창일;김경준;정영훈;이영진;이해근;백종후
    • 한국재료학회지
    • /
    • 제19권4호
    • /
    • pp.198-202
    • /
    • 2009
  • For use in ultrasonic actuators, we investigated the structural and piezoelectric properties of $(1\;-\;x)Pb(Zr_{0.515}Ti_{0.485})O_3$ - $xPb(Sb_{1/2}Nb_{1/2})O_3$ + 0.5 wt% $MnO_2$ [(1 - x)PZT - xPSN + $MnO_2$] ceramics with a variation of x (x = 0.02, 0.04, 0.06, 0.08). All the ceramics, which were sintered at $1250^{\circ}C$ for 2 h, showed a typical perovskite structure, implying that they were well synthesized. A homogeneous micro structure was also developed for the specimens, and their average grain size was slightly decreased to $1.3{\mu}m$ by increasing x to 0.8. Moreover, a second phase with a pyrochlore structure appeared when x was above 0.06, which resulted in the deterioration of their piezoelectric properties. However, the 0.96PZT-0.04PSN+$MnO_2$ ceramics, which corresponds with a morphotropic phase boundary (MPB) composition in the (1 - x)PZT - xPSN + $MnO_2$ system, exhibited good piezoelectric properties: a piezoelectric constant ($d_{33}$) of 325 pC/N, an electromechanical coupling factor ($k_p$) of 70.8%, and a mechanical quality factor ($Q_m$) of 1779. The specimens with a relatively high curie temperature ($T_c$) of $305^{\circ}C$ also showed a significantly high dielectric constant (${\varepsilon}_r$) value of 1109. Therefore, the 0.96PZT - 0.04PSN + $MnO_2$ ceramics are suitable for use in ultrasonic vibrators.

압전복합센서용 PZT 세라믹스의 미세구조 및 압전특성에 미치는 $Cr_2O_3$$Nb_2O_5$ 첨가효과 (Effect of $Cr_2O_3$ and $Nb_2O_5$ Additives on the Microstructure and Piezoelectric Properties of PZT Ceramics for Piezoelectric Composite Sensor)

  • 백종후;엄형근;임은경;김창일;이미재;최병현;김세기
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 추계학술대회 논문집 Vol.18
    • /
    • pp.27-28
    • /
    • 2005
  • 본 연구에서는$Cr_2O_3$$Nb_2O_5$ 를 첨가한 $Pb(Zr_{0.54}Ti_{0.48})O_3$ 세라믹스에서 $Nb_2O_5$ 첨가량에 따른 소결 및 압전, 유전특성을 조사하였다. $Pb(Zr_{0.54}Ti_{0.48})O_3$ + 0.2 wt% $Cr_2O_3$ + wt% $Nb_2O_5$ ($0.{\sim}2wt.%$)의 첨가량에 따른 압전, 유전특성 및 미세구조에 관해 연구하였다. 본조성에서 $Nb_2O_5$ 첨가량이 증가함에 따라 입경의 크기는 증가하였으며, 0.5 wt% $Nb_2O_5$ 첨가조성에서 $4\sim5\mu m$의 최대 평균입경을 보이다가 그 이상의 첨가 조성에서 급격히 감소하였다. 유전상수와 kp 는 $Nb_2O_5$ 첨가량이 1.0 wt% 조성까지 증가하였다가 그 이상 조성에서 감소하였다. $Nb_2O_5$ 첨가량이 증가함에 따라 삼방정(rhombohedral)구조에서 정방정(tetragonal)구조로 상전이 일어났으며, 본 조성의 상경계 영역인 0.5 wt% 조성에서 $\varepsilon_r$ = 730, $k_p$ = 0.72, $d_{33}$ = 450, $g_{33}$ = 70의 우수한 압전 특성을 나타내었다. 이러한 조성은 접촉센서용 복합압전소재의 실용가능성을 제시하였다.

  • PDF