  • Rock masses represent natural systems that are inherently complex and in which multiple mechanisms occur. Rock engineering systems such as tunnel and slope interact with surrounding systems through an exchange of both mass and energy. Accordingly the complex nature of rock masses calls for a system approach, and the open nature of rock engineering even requires the engineering to be controlled by a system approach for surrounding environments. However, traditional methods cannot take all variables and their interactions into account and are limited to the system with single mechanisms. Therefore, they are not proper for a complex and open system, and also cannot portray the whole system. Thus, a system approach is indispensable to rock engineering for dealing with the whole of a complex and open system. In this paper Mechanism Path Analysis Methodology (MPAM) Is Introduced for a system approach to rock engineering. The analysis by the methodology gives us all the information of systems behavior in the context of the whole system in order to accomplish the optimum design in accordance with the project objectives and analysis purposes. As an application a conventional model for the evaluation of TBM tunneling performance system is analyzed by MPAM and the result is compared with that by a traditional method.

  • PDF

AE(Acoustic Emission)에 의한 세라믹 복합재료의 고인성화 기구 분석 (Analysis of Toughening Mechanism of Ceramic Composites by Acoustic Emission)

  • 장병국
    • 한국세라믹학회지
    • /
    • 제34권11호
    • /
    • pp.1129-1138
    • /
    • 1997
  • Al2O3/20 vol%YAG composite containing equiaxed grains and Al2O3/20 vol%LaAl11O18 composite containing elongated grains were fabricated using Al2O3-Y2O3 composition and Al2O3-La2O3 composition, respectively, by hot-pressing. In order to investigate the influence of microstructural control of second phase on toughening effect of toughened ceramic composites, AE (acoustic emission) measurements have been coupled with fracture toughness experiments(SENB and SEPB method). A separation of the fracture toughness and analysis of toughening mechanism was possible using the AE technique. The fracture toughness of hot-pressed materials was estimated to be 3.2 MPam0.5 for monolithic alumina, 4.7 MPam0.5 for Al2O3/20 vol%YAG composite and 6.2 MPam0.5 for Al2O3/20 vol%LaAl11O18 composite. In monolithic Al2O3, toughening does not occur as a result of either microcracking or grain bridging, whereas, composites exhibit toughening effects by both microcracking in the frontal zone and gain bridging in the wake zone, resulting in an improvement of fracture toughness as compared with monolithic Al2O3. The fracture toughness of Al2O3/20 vol%LaAl11O18 composite is higher than that of Al2O3/20 vol%YAG composite. It may be attributed to the elongated microstructure of Al2O3/20 vol%LaAl11O18 composite, resulting relatively greater bridging effect.

  • PDF

New Control Strategy for Reducing Switching Losses in Three-Phase Voltage-Source PWM Converters

  • Dong, Xiaopeng;Wang, Zhaoan
    • 전력전자학회:학술대회논문집
    • /
    • 전력전자학회 1998년도 Proceedings ICPE 98 1998 International Conference on Power Electronics
    • /
    • pp.366-373
    • /
    • 1998
  • In this paper, a new control strategy to reduce switching losses in three-phase voltage-source PWM converters is proposed according to Modified-Period-Average-Model (MPAN). The basic concept of this strategy is aimed at calculating the phase control voltages for controlling the source currents to be sinusoidal and in phase with the source voltages, and reducing the number of switching in each period. The phase control voltages of Period-Average-Model(PAM) is obtained according to analyzing the operation of PWM converter. In order to reduce the sensitivity to system parameters in PAM, MPAM is deduced. Then a square wave whose frequency is three times of utility frequency is added to the phase control voltages derived from MPAM. The control strategy reduces the switching losses since there exists about one-third blanking time for every phase in one period. The theoretical derivation and the control strategy are experimentally verified on a 2.5 kW three-phase voltage source converter.

  • PDF

고강도 시멘트 복합체의 강도특성에 미치는 혼합재료의 영향 (An Effect of Blending Materials on the Strength Characteristics of High Strength Cement Composite)

  • 최일규;김정환;한기성
    • 한국세라믹학회지
    • /
    • 제31권3호
    • /
    • pp.330-336
    • /
    • 1994
  • High strength cement composites (W/C=0.1) were prepared by using various blending materials such as SiC whisker and white carbon (hydrated silica: SiO2·nH2O). The effect of various blending materials on the microstructure and strength of the hardened cement paste were investigated in the view of fracture mechanics. The plain specimen showed 101 MPa of flexural strength, 81 GPa of Young's modulus and 1.32 MPam1/2 of fracture toughness. When the blending materials were added to the composites, their values were enhanced to about 110∼138 MPa, 95∼146 GPa and 1.32∼1.87MPam1/2 respectively. The improvement of the mechanical strength for the hardened cement paste may be due to the removal of macropores, the reduction of total porosity, pozzolanic reaction and the increase of various fracture toughening effect.

  • PDF

반복 사용된 IPS Empress ceramic의 물리적 성질에 관한 연구 Part IV : 경도 및 파괴인성에 관한 연구 (THE PHYSICAL PROPERTIES OF REUSED IPS EMPRESS CERAMIC PART IV : HARDNESS AND FRACTURE TOUGHNESS)

  • 진태호
    • 대한치과보철학회지
    • /
    • 제41권4호
    • /
    • pp.532-537
    • /
    • 2003
  • Statement of the problem : IPS Empress ceramic has been used as one of a esthetic restorative material since it's development, but the broad application of IPS Empress ceramic to clinical prosthodontic field has been limited by its high material cost. Purpose : This study was investigated to evaluate the hardness and fracture toughness after recycling of the IPS Empress ceramic. Material and methods : Reused specimens of IPS Empress were fabricated with repeated pressing. The hardness(Vickers hardness) and fracture toughness of 1st, 2nd and 3rd pressed specimens were measured with Digital Micro Hardness Tester(Model MXT70, Matsuzawa Seiki Co., Ltd, Tokyo, Japan). The obtained data were analyzed using SPSS(Ver 9.5). Result : The mean value of the hardness in the 1st, 2nd and 3rd pressed Empress were $6.23{\pm}0.48MPa,\;5.50{\pm}0.25MPa$, and $5.70{\pm}0.42MPa$. The hardness of the 1st pressing ceramic was higher than those or the 2nd and 3rd pressed ceramics(P<0.05). Hardness of the 3rd pressed ceramic was greater than that of the 2nd pressed ceramic. but there was no significant difference of hardness between those two(P>0.05). The mean value of the fracture toughness was $1.71{\pm}0.16MPam^{1/2}$ in 1st pressed ceramic, $1.78{\pm}0.10MPam^{1/2}$ in 2nd pressed and $1.73{\pm}0.14MPam^{1/2}$ in 3rd pressed IPS ceramic. Fracture toughness of the 2nd pressed ceramic was the highest and that of the 1st pressed ceramic was the lowest. There was no significant difference of fracture toughness among them(P>0.05). Conclusion : Hardness of the 2nd and 3rd pressed IPS Empress ceramics were lesser than that of 1st pressed IPS Empress ceramic(P<0.05), but there was no significant changes of fracture toughness among them(P>0.05).

반복 사용된 IPS Empress 2의 표면경도와 pressing accuracy에 관한 연구 (SURFACE HARDNESS AND PRESSING ACCURACY OF REUSED IPS EMPRESS 2)

  • 손외수;김유리;이경자;진태호
    • 대한치과보철학회지
    • /
    • 제41권5호
    • /
    • pp.596-605
    • /
    • 2003
  • Statement of problem : IPS Empress2 system was developed and used in prosthodontic treatment, but the cost of ingot is expensive for wide application. Purpose : This study was to investigate the possibility on recycling of IPS Empress 2 ceramic for wide application of IPS Empress 2 ceramic in prosthodontic treatment. Material and Method : 1st, 2nd and 3rd pressed disc-shaped($10{\times}1.5mm$) IPS Empress 2 specimens were made with IPS Empress ingot(200, Ivoclar, Liechtenstein) and pressing furnace(IPS Empress EP 500, Ivoclar, Liechtenstein). Vicker's surface hardness and fracture toughness, acid resistance, and pressing accuracy of IPS Empress 2 ceramic were measured and analyzed. Surface hardness was measured by microhardness tester(MTX 70. Matsuzawa, Japan), before and after surface treatment with 0.5% hydrofluoric acid and carbonic acid(Coca cola) for evaluation of acid resistance. Results : The surface hardness of 1st pressed specimen was the higher(5.11 GPa) than those of 2nd pressed(4.89 GPa) and 3rd pressed specimen(4.86 GPa), and the fracture toughness of 1st pressed ($1.58MPam^{1/2}$) and 2nd pressed specimen($1.51MPam^{1/2}$) were higher than that of 3rd pressed specimen($1.39MPam^{1/2}$). The changes of surface hardness of 1st, 2nd, and 3rd pressed specimens after treatment with fluoric acid were 0.17, 0.06, 0.05 (GPa) respectively, and those of 1st, 2nd, and 3rd pressed specimens after treatment with carbonic acid were 0.07, 0.00, 0.05(MPa) respectively. The pressing accuracy of 1st,2nd and 3rd specimen were 77.22%, 85.681%, and 75.05%. The pressing accuracy of 2nd pressed specimen was higher than that of the 3rd specimen. Conclusion : The changes of physical properties according to recycling of IPS Empress 2 from this study were insignificant. Therefore the possibility of recycling of IPS Empress 2 can be suggested from the results.

중석이 첨가된 고분자 유기물 열분해 방법에 의한 신세라믹복합체 개발 (Development of Novel Ceramic Composites by Active Filler Controlled Polymer Pyrolysis with Tungsten)

  • 강건택;김득중
    • 한국세라믹학회지
    • /
    • 제35권9호
    • /
    • pp.939-944
    • /
    • 1998
  • 실리콘함유 고분자(Polysiloxane)의 세라믹변환과정에서의 부피수축효과를 조절하기 위하여 활성화금속으로 중석을 첨가하여 열분해 및 합성반응을 통해 신 세라믹 복합체를 개발하고 이의 세라믹화 과정이나 물성을 조사하였다. 제조된 시편의 미세조직은 고분자로부터 야기된 $S_{1}$-O-C게열의 Glass기지상과, 분해잔여물(고상,기상)등과 활성화금속과의 반응르로 생성된 고경도의 탄호물로 이루어져 있어 향후 내마모재료로서의 응용을 기대할 수 있을 것이다. 제조된 복합체의 물성은 반응조건에 많이 의존함을 알 수 있었다. 1400~$1500^{\circ}C$에서 열분해 시켜 제조한 복합체의 밀도는 95% 이상의 상대밀도와, 경도 값은 7~8GPa 정도이고 탄성률은 220~230 GPa, 파괴인성응ㄴ 6~6.8$MPam^{1/2}$, 파괴강도는 380~470 MPs정도의 값을 나타내었다.

  • PDF

압자압입법에 의한 치과용 도재의 파괴인성 평가 (AN EVALUATION OF FRACTURE TOUGHNESS OF DENTAL CERAMICS BY INDENTATION FRACTURE METHOD)

  • 안승근;이주형;배태성
    • 대한치과보철학회지
    • /
    • 제34권2호
    • /
    • pp.309-319
    • /
    • 1996
  • This study was performed to evaluate the fracture toughness of seven commercially available dental ceramics by indentation fracture method. All specimens were fabricated to the final dimensions of approximately 12mm in diameter 2mm in thickness. The characte-ristic indentation dimensions of Vickers or Knoop indentation were measured to calculate the fracture toughness values and Young’s moduli. The results obtained were summarized as follows; 1. Young’s modulus and Vickers hardness of Vita In-Ceram showed the maximum values of $154.4{\pm}49.2$ Gpa and $12.60{\pm}0.71$Gpa, respectively. Results of Scheff test exhibited the significant difference between Vita In-Ceram group and others(p<0.01). 2. Maximum fracture toughness of $2.562{\pm}0.37 MPam^{1/2}$ for Vita In-Ceram and the maxi-mum one of $0.908{\pm}0.132MPam^{1/2}$ for Vitadur-N were calculated. Results of Scheff test showed the significant difference between Vita In-Ceram group and Vita Hi-Ceram(p<0.05) : also between Vita In-Ceram or Vita Hi-Ceram and others(p<0.01). 3. The alumina-based core ceramics showed the aspect of Palmqvist crack for the indentation load of 49.0N, but others showed the median/lateral crack for the indentation load of 9.8N.

  • PDF

$Y-Nb-TZP/Al_2O_3$ 복합체의 저온 상안정성 및 기계적 특성 (Low-temperature phase stability and mechanical properties of $Y-Nb-TZP/Al_2O_3$ compoites)

  • 이득용;김대준;조경식;장주웅
    • 한국결정성장학회지
    • /
    • 제8권4호
    • /
    • pp.634-639
    • /
    • 1998
  • $Y_2O_3$$Nb_2O_5$가 첨가된 지르코니아에 입자 크기가 다른 두종류의 Al2O3를 부피비로 10~30% 첨가한 복합체를 155$0^{\circ}C$ 온도에서 5시간 소결하여 $250^{\circ}C$ 온도의 공기 분위기하에서 1000시간 혹은 $180^{\circ}C$ 온도의 0.3MPa H2O vapor pressure 분위기하에서 5시간 열처리를 하여 X-ray 회절분석 방법을 이용하여 저온 상안정성을 조사하였다. 복합체 전부 열처리 후에 정방정 상에서 단사정 상으로 상전이가 발생하지 않는 우수한 저온 상안정성이 관찰되었다. 복합체의 상아정성에 Nb 첨가가 $Al_2O_3$의 첨가보다 더 효과적이었다. 2.8$\mu$m 입자크기를 가진 Al2O3를 부피비로 20% 첨가한 복합체에서 최적의 조건이 관찰되었으며 강도와 인성값은 각각 670MPa와 7.1MPam1/2이었다. Al2O3 입자 크기가 2.8$\mu$m에서 0.2$\mu$m로 감소함에 따라 강도는 다소 증가하였으나 파괴인성값은 감소하였다.

  • PDF

금속 알콕사이드로부터 PSZ-seeding Mullite 복합체의 합성 및 소결체의 특성 (Synthesis of PSZ-seeding Mullite Composite from Metal Alkoxides and Its Characteristics of Sintered Body)

  • 임굉;임재석;김영호
    • 한국재료학회지
    • /
    • 제17권1호
    • /
    • pp.18-24
    • /
    • 2007
  • Mullite-PSZ composite was prepared by sol-gel method using $Al(sec-OC_4H_9)_3,\;Si(OC_2H_5)_4,\;ZrOCl_2\;8H_2O\;and\;Y_2O_3$. The sinterability ana mechanical properties of powder compacts sintered at $1,650^{\circ}C$ for 4 hrs were investigated for various PSZ contents. In result Al-Si spinel formed at $980^{\circ}C$ from amorphous dried gel, and zirconia as well as mullite crystal formed above $1,200^{\circ}C$. The sintered body was densified to $97{\sim}98%$ except the specimen containing 25vol% PSZ which showed the relative density of about 95% obtained by sintering at $1,650^{\circ}C$ for 4 h. The flexural strength of the sintered body was a maximum value of 290 MPa in 20 vol% PSZ, which was also considerably larger than the value of 200 MPa without PSZ. The value of the fracture toughness increased linearly with increase of PSZ content and showed a maximum value of $4.3MPam^{1/2}$ in 25 vol% PSZ, Namely this value was remarkably larger than the $value(2.6MPam^{1/2})$ of pure mullite without PSZ.