Recently, the application of aluminum alloys has been increasing for lightweight and high quality transport vehicles. Therefore, the proposal has been made to apply high speed hybrid welding methods to the marine grade aluminum alloy (A5052) used for shipbuilding by combining a 3-KW CW Nd : YAG laser and the MIG welding process. In this study, the characteristics of the welding parameters were investigated for a hybrid butt joint. This paper also describes the determination of the heat distribution in a weldment and the welding residual stress using a finite element method. Mechanical experimentation was also used to ascertain the reliability of the weldment.
There are some problems when weld gray cast iron which is used well in automobile industry with auto MIG welding. the problems are followed like this 1) Occurrence of porosity and hardening organization. 2) Occurrence of crack due to lower elongation of gray cast iron when restraint stress works on. 3) Occurrence of porosity and unstable bead shape due to unstable arc under low current MIG welding.. especially there is a restraint on chemical composition of weld metal because the weldment demands more than 570Hv hardness. so it is hard to use Fe-Ni wire to prevent cracks occured on weldment and new welding method is needed to resolve that problems. This study shows how to prevent porosity and cracks occurring when weld gray cast iron trimming die and shows a new welding method for press die of gray cast iron
한국마린엔지니어링학회 2001년도 추계학술대회 논문집(Proceeding of the KOSME 2001 Autumn Annual Meeting)
/
pp.88-91
/
2001
New type of vehicles made from thin aluminum alloy are under rapid development and some product are already on the market, but when welding sheet metal joint of aluminum alloy, the main problem are burn-through by the high heat input. The purpose of this study, it is to prevent the burn-through and to shallow penetration that AC pulse welding has diminish the penetration and to lower the droplet temperature at Al sheet metal welding. In this study, we observed the bead appearance and whether it was appeared burn through or not , as the variation of the root gap in the lap and butt-joint welding process.
International Journal of Naval Architecture and Ocean Engineering
/
제7권4호
/
pp.770-783
/
2015
Lately, high production rate welding processes for Al alloys, which are used as LNG FPSO cargo containment system material, have been developed to overcome the limit of installation and high rework rates. In particular, plasma-metal inert gas (MIG) hybrid (PMH) welding can be used to obtain a higher deposition rate and lower porosity, while facilitating a cleaning effect by preheating and post heating the wire and the base metal. However, an asymmetric undercut and a black-colored deposit are created on the surface of PMH weld in Al alloys. For controlling the surface defect formation, the wire feeding speed and nozzle diameter in the PMH weld was investigated through arc phenomena with high-speed imaging and metallurgical analysis.
알루미늄 합금 Al 6082-T6는 최근에 개발되어 북유럽 등의 선진국에서는 그 뛰어난 해양 내식성과 우수한 강도로 인하여 해양구조물의 헬리데크(Helideck), 타워 갱웨이(Tower gangway), 알루미늄 피팅류(Aluminium fitting)등의 해양구조물과 플랫폼(Flatform), 알루미늄 래더(Aluminium ladder)등의 선박부품, 차량, 기계부품 분야에서 전 세계적으로 널리 사용되기 시작하였다. 그러나 전통적으로 용접금속의 기공은 결함으로 분류 되고, Rakesh Kumar 등의 논문에 따르면 용접 시 용접금속 내에 발생되어진 미세기공이 기계적 성질에 악영향을 미치는 것으로 보고되어졌다. 따라서 용접금속내의 발생하는 기공을 방지하는 용접공정의 개발이 반드시 필요하다. 본 연구의 목적은 Al 6082-T6 고속 MIG용접에서 기공방지를 위한 용접공정을 개발하는 것이다. Al 6082-T6의 7t 플레이트에 Al 5356의 와이어를 사용하여 아크길이 변경 및 용접속도를 60cpm과 120cpm으로 변경하여 실험하였고, 용접속도 120cpm의 고속 MIG용접에서 토치 진행각을 변경하여 실험을 진행하였다. 용접공정 파라메터 변경에 따른 기공율 측정은 이미지 분석 소프트웨어를 사용하여 정량적으로 분석하였다.
최근 전세계적으로 유가 상승 및 배기가스 배출 저감과 관련된 각종 환경규제에 대응하기 위하여 선진 자동차회사들은 $CO_2$ 배출 저감 기술과 기존 내연기관 차량의 연비향상을 위해 엔진성능 개선, 구동시스템의 최적화, 차량 경량화, 공기저항 감소 등에 초점을 맞춰 차량의 연비향상과 배기가스 규제에 대응하고 있다. 특히, 자동차 중량의 30%를 차지하는 차체의 경량화는 엔진효율을 높여 자동차의 성능향상을 극대화시키고, 그로 인해 연비향상을 도모할 수 있으므로 환경오염 방지와 연료절감에 가장 적합하고 효과적인 방법이다. 이에 기존의 강재에 비해 비중이 낮으면서 유사한 강도와 내식성이 뛰어난 알루미늄 합금의 차체 적용에 대한 연구가 진행되고 있다. 본 연구에서는 자동차 Door에 알루미늄 합금(Al 5052)의 적용 가능성을 판단하기 위해 반응표면분석법(Response surface methodology)을 이용하여 저입열 Pulse MIG 용접 공정변수를 최적화하였다. 첫째, 저입열 Pulse MIG 용접에서 용접 공정 변수(용접전압, 용접속도, Gap)의 변화가 비드 형상에 미치는 영향에 대해 평가하였다. 요인분석법을 이용하여 용접 공정 변수와 비드 형상 변수와의 주효과와 교호작용효과를 분석하였고, 이를 통해 비드 형상 변수에 영향을 크게 미치는 용접 공정변수를 선별하여 다중회귀분석을 통해 용접 공정 변수 변화에 따른 비드형상 예측 회귀모델을 제안하였다. 둘째, 자동차 Door 생산 현장에서 박판 알루미늄 합금 겹치기 용접 이음부의 0~1 mm 갭 발생에 대해 강건한 용접조건을 제시하기 위해 반응표면법(Response surface methodology)을 이용하여 저입열 Pulse MIG 용접 공정 변수를 최적화하였고, 그 적용 가능성을 확인하였다.
Electromagnetic force is one of the most important factor that effect on metal transfer mode, short-circuit rate, spatter generation rate and mechanical properties of weld metal etc. Also, shielding gas and welding current have influence on metal transfer mode in GMAW. In this paper, different ways for external electromagnetic forces are applied by attaching cylindrically rounded conducting wire solenoid on touch tip holding. With the applied electromagnetic field, the arc transfer mode changes from normal mode to rotating mode and spatter generation decreased in electromagnetic fields(N-pole). In MIG welding, the influences of electromagnetic force on the spatter generation showed different tendency as in the $CO_2$ welding. It is possible reasons were discussed.
Joining thin aluminum alloy is difficult using most wilding techniques. Many of problems associated burn-through by the high heat input Common welding techniques are TIG, MIG, and MIG-PULSE welding. The VP-GMAW provides more control of the heat balance in the voiding arc by taking advantage of the different arc characteristics obtained with each of the two polarities. In this paper, we proposed new VP_GMA Welding method by control DSP 320C32, and the characteristic and experiment result-voltage, current, welding bead. penentraion by this method are presented
It was attempted to improve the wear resistance of Al alloy under the load condition by making a formation of the thick surface hardening alloy layers. The thick surface hardening alloy layers were formed on 6061 Al alloys overlayed by MIG welding process with WC-12%Co powder addition. Effects of the dispersion of WE-12%Co powders on hardness and wear characteristics of alloys were investigated. The following results were obtained. Most of WE-12%Co powders are dispersed nearly uniform as unmelted particles in the matrix alloy. A part of WC-12%Co powders are melted in the molten pool, and during solidification {TEX}$Al_{9}Co_{2}${/TEX} appeared. With increasing addition of WC-12%Co powders, the hardness and specific wear resistance of the overlay weld alloys increased and reached Hv450 at WC-12%Co powder addition rate of 54g/min. It is considered that excellent wear resistance of the overlayed alloys was due to dispersed WC-12%Co powders and increased 10 times at WC-12%Co powder addition rate of 54 g/min than that of the WC-free overlaying layers.
A laser beam welding and an electric arc welding were combined, and the positive points of each welding method are drawn such as high speed, low thermal load, deep penetration, and high productivity. The fiber laser-MIG conjugated welding. namely the hybrid welding has been studied mainly for the automation industry of a pipeline welding. In this study, the MIG welding was combined with a fiber laser welding to make up the hybrid welding. The weld shapes, microstructures and mechanical properties for weld zones after the hybrid welding or only fiber laser welding were investigated on the 700 MPa grade Ultra Fine Grained(UFG) high strength steel. The amount of acicular ferrite in weld metals and HAZ(heat affected zone) was observed larger after hybrid welding compared with after only laser welding. The Vickers hardness of the top area of the fusion zone after fiber laser welding was higher compared with after hybrid welding.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.