The Effect of Trivalent Cation Doping on the Low Temperature Phase Stability of 2Y-TZP (3가 양이온 산화물이 첨가된 2Y-TZP의 저온 상안정성)

  • Jang, Ju-Woong;Kim, Hak-Kwan;Lee, Deuk-Yong;Kim, Dae-Joon;Park, Sun-Min
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.11
    • /
    • pp.1055-1062
    • /
    • 2002
  • The phase stability and the Low Temperature Degradation(LTD) mechanism of Tetragonal Zirconia Polycrystals(TZP), sintered specimens of $Y_2O_3$-Stabilized Zirconia(2Y-TZP), doped with trivalent cations, were evaluated by investigating meachnical properties, Raman spectra, lattice parameter variation and the oxygen vacancy behavior under applied electric field. XRD observation was put forward on 2Y-TZP doped with trivalent cation whose ionic radii were larger than $Zr^{4+}(Sc^{3+},\;Yb^{3+},\;Y^{3+},\;Sm^{3+},\;Nd^{3+},\;La^{3+})$ up to 2 mol% and sintered at 1500 h for 1h. For $La^{3+}$ doping, the stability of tetragonal phase was degraded due to the formation of the pyrochlore phase $(La_2Zr_2O_7)$ as the dopant content increased above exceeded 0.5 mol%. As the dosage increased, tetragonal phase maintained for the case of $Sc^{3+}$, whose radius was similar to $Zr^{4+}$, on the other hand, the cubic phase was formed for the cases of $Yb^{3+},\;Y^{3+},\;Sm^{3+},\;Nd^{3+}$. As the radii of dopant cation increased, c/a ratio increased and it was experimentally observed that the amount of monoclinic phase decreased when the specimens were annealed at $220{\circ}C$ for 500 h.

A Study on Improvement of Fire-resistant and Flame-retardant Properties of Silicone Rubber Composites Containing Perlite (펄라이트를 첨가한 실리콘 고무 복합체의 내화 및 난연 특성 향상에 관한 연구)

  • Lee, Byung-Gab;Lee, Jong-Hyeok;Bang, Dae-Suk;Won, Jong-Pil;Jang, Il-Young;Park, Woo-Young;Jhee, Kwang-Hwan
    • Elastomers and Composites
    • /
    • v.46 no.2
    • /
    • pp.164-170
    • /
    • 2011
  • In this study, silicone rubber filled with environmentally-friendly perlite was prepared by mechanical mixing in order to improve thermal properties, such as heat and fire resistances. We found that the properties of silicone rubber composites depended on perlite concentration by various characterization methods. Thermogravimetric analysis(TGA) indicated that the initial degradation temperature of silicone/perlite composite was higher than that of pristine silicone rubber. The gas torch test showed that the opposite side temperature of composite materials was remarkably low as compared to that of pristine silicone rubber. In addition, the composites containing 5 wt% and 10 wt% of perlite showed remarkable thermal stability at elevated temperatures according to the results of both fireproof furnace tests under the RABT condition and carbonization furnace tests. The images from a scanning electron microscope(SEM) showed the degree of dispersion of perlite in silicone rubber. Finally, it was confirmed that limited oxygen index(LOI) was increased with perlite concentration.