• Title/Summary/Keyword: Liquid forming

Search Result 361, Processing Time 0.026 seconds

A Study on Induction Heating with Forced Surface Cooling in Semi-Solid Forming Process (반용융 성형에서 강제 표면 냉각에 의한 유도 가열 방법에 관한 연구)

  • Park Joon Hong;Choi Young
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.22 no.1
    • /
    • pp.97-102
    • /
    • 2005
  • The procedure of semi-solid forming is composed of heating a billet, forming, compression holding and ejecting step. There are several methods to heat a billet during semi-solid forming process such as electric heating and induction heating. Usually in semi-solid forming process, induction heating has been adopted to achieve more uniform temperature of semi-solid material. Although induction heating is better method than any others, however, there is still difference of temperature between internal part and surface part of semi-solid material. Worse yet, in case of high liquid fraction of semi-solid material, liquid of the billet will flow down though solid of the billet still remains, which is very difficult to handle. In the present study, induction heating of semi-solid material with compulsive surface cooling has been performed to obtain uniform distribution of temperature. Distribution of temperature of the billets was measured and compared with that of conventional distribution of temperature. By this new induction heating method, not only temperature over the whole billet become uniform, but also control of temperature is possible.

A Study on Induction Heating with Compulsive Surface Cooling in Semi-Solid Forming Process (반용융 성형에서 간제 표면 냉각에 의한 유도 가열 방법에 관한 연구)

  • Choi, J. C.;Kim, B. M.;Choi, Y.;Park, J. H.
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2000.11a
    • /
    • pp.465-468
    • /
    • 2000
  • The procedure of semi-solid forming is composed of heating a billet, forming, compression holding and ejecting step. There are several methods to heat a billet during semi-solid forming process such as electric heating and induction heating. Usually in semi-solid forming process, induction heating has been adopted to achieve more uniform temperature of semi-solid material. Although induction heating is better method than any others, however, there is still difference of temperature between internal part and surface part of semi-solid material. Worse yet, in case of high liquid fraction of semi-solid material, liquid of the billet will flow down though solid of the billet still remains, which is very difficult to handle. In the present study, induction heating of semi-solid material with compulsive surface cooling has been performed to obtain uniform distribution of temperature. Distribution of temperature of the billets was measured and compared with that of conventional distribution of temperature. By this new induction heating method, not only temperature over the whole billet become uniform, but also control of temperature is possible.

  • PDF

Design Optimization to achieve an enhanced flatness of a Lab-on-a-Disc for liquid biopsy (액체생검용 Lab-on-a-Disc의 평탄도 향상을 위한 최적화)

  • Seokkwan Hong;Jeong-Won Lee;Taek Yong Hwang;Sung-Hun Lee;Kyung-Tae Kim;Tae Gon Kang;Chul Jin Hwang
    • Design & Manufacturing
    • /
    • v.17 no.1
    • /
    • pp.20-26
    • /
    • 2023
  • Lab-on-a-disc is a circular disc shape of cartridge that can be used for blood-based liquid biopsy to diagnose an early stage of cancer. Currently, liquid biopsies are regarded as a time-consuming process, and require sophisticated skills to precisely separate cell-free DNA (cfDNA) and circulating tumor cells (CTCs) floating in the bloodstream for accurate diagnosis. However, by applying the lab-on-a-disc to liquid biopsy, the entire process can be operated automatically. To do so, the lab-on-a-disc should be designed to prevent blood leakage during the centrifugation, transport, and dilution of blood inside the lab-on-a-disc in the process of liquid biopsy. In this study, the main components of lab-on-a-disc for liquid biopsy are fabricated by injection molding for mass production, and ultrasonic welding is employed to ensure the bonding strength between the components. To guarantee accurate ultrasonic welding, the flatness of the components is optimized numerically by using the response surface methodology with four main injection molding processing parameters, including the mold & resin temperatures, the injection speed, and the packing pressure. The 27 times finite element analyses using Moldflow® reveal that the injection time and the packing pressure are the critical factors affecting the flatness of the components with an optimal set of values for all four processing parameters. To further improve the flatness of the lab-on-a-disc components for stable mass production, a quarter-disc shape of lab-on-a-disc with a radius of 75 mm is used instead of a full circular shape of the disc, and this significantly decreases the standard deviation of flatness to 30% due to the reduced overall length of the injection molded components by one-half. Moreover, it is also beneficial to use a quarter disc shape to manage the deviation of flatness under 3 sigma limits.

  • PDF

Effect of Alloying Elements on the Glass Forming Ability of Zr-Ti-Cu-Ni-X Alloys (Zr-Ti-Cu-Ni-X계 합금의 첨가원소에 따른 비정질 형성능)

  • Choi, Chul-Jin
    • Journal of Korea Foundry Society
    • /
    • v.21 no.5
    • /
    • pp.286-289
    • /
    • 2001
  • The glass formation behavior was investigated in the melt spun Zr-Ti-Cu-Ni-X (X=B, P and Si) ribbons. The magnitude of supercooled liquid region of Zr-Ti-Cu-Ni alloy increased with an addition of alloying element. The glass transition temperature and the crystallization temperature increased and the magnitude of supercooled liquid region decreased with increasing the content of alloying elements. The largest supercooled liquid region was observed in the Si containing alloy. This is believed to be due to the dense atom packing with the optimum atomic size ratio of constituent elements.

  • PDF

The Effects of Fabrication Conditions on Forging Limitation and Mechanical Property in Semi-Solid Forming Process (반용융 단조공정에 있어서 제조 조건이 성형성과 기계적 성질에 미치는 영향)

  • 정경득;강충길
    • Transactions of Materials Processing
    • /
    • v.10 no.3
    • /
    • pp.214-222
    • /
    • 2001
  • The homogeneous distribution of solid region without liquid segregation is important in terms of high quality component during thixoforming process. In closed die semi-solid forging process, liquid segregation is strongly affected by injection velocity than solid fraction because the material has to travel relatively long distance to fill the cavity through a narrow gate. The designed die by computer simulation data was used to thixoforging process. The thixoforming velocity to prediction the liquid segregation had been determined with strain rate associated with multistage velocity control during compression test of semi-solid material. The optimal forging velocity and die temperature were investigated to produce the near-net-shape compressor component. The mechanical properties of thixoformed component were tested with various die and material temperatures before and after heat treatment.

  • PDF

The Effect of Pressure on Liquid Segregation in Direct Rheo-Forging Process of Aluminum Alloys (알루미늄 소재의 레오로지 직접단조공정에서 가압력이 액상 편석에 미치는 영향)

  • Oh, S.W.;Bae, J.W.;Kang, C.G.
    • Transactions of Materials Processing
    • /
    • v.16 no.3 s.93
    • /
    • pp.178-186
    • /
    • 2007
  • Rheo-forging process of aluminum alloy is suitable for large parts of net shape without defects and excellent mechanical properties in comparison with conventional die casting and forging process. To control the microstructure of the product with high mechanical properties in rheo-forming, solid fraction is required to prevent porosity and liquid segregation. Therefore, in rheo-forging process, die shape, pressure type and solid fraction are very important parameters. The defects such as porosity, liquid segregation and unfitting phenomena occur during rheo-forging process. To prevent these defects, mechanical properties and microstructure analysis of samples versus the change of pressure are carried out and the problem and its solutions are proposed. Also, the mechanical properties versus various pressures were compared with and without heat treatment. The alloys used for rheo-forming are A356 and 2024 aluminum alloy. The rheology material is fabricated by electromagnetic process with controlling current and stirring time.

Various Pattern-Forming States of Nematic Liquid Crystal Based on the Sign Inversion of Dielectric Anisotropy

  • Kang, Shin-Woong;Chien, Liang-Chy
    • Macromolecular Research
    • /
    • v.15 no.5
    • /
    • pp.396-402
    • /
    • 2007
  • The dielectric properties and various pattern-forming states of dual-frequency material in a nematic phase, as well as its mixture containing low concentrations of reactive monomers, are reported. The dielectric relaxation behaviors of nematic MLC 2048 are presented and compared to its mixture containing both mesogenic and nonmesogenic reactive monomers. The sign-inversion frequency of the dielectric anisotropy was significantly shifted on the addition of small amounts of the reactive monomers. However, all three mixtures used in this study essentially exhibited the same field-induced instabilities at different frequencies and voltage domains of the applied electric field. A broad band of modulated states were found to exist above a critical voltage and within a voltage dependent frequency band in the vicinity of the sign-inversion frequency, $f_I$, of the dielectric anisotropy. As the $f_I$ of the mixtures shifted, so did the bands of the modulated state of the different mixtures and the temperatures, which were well matched with the measured $f_I$ value.

Micro Forming of Bulk Metallic Glass using the Deformation Behavior in the Supercooled Liquid Region (과냉각 액체 영역에서의 변형거동을 이용한 벌크 비정질 합금의 미세성형 기술 개발)

  • 옥명렬;서진유;홍경태
    • Transactions of Materials Processing
    • /
    • v.13 no.1
    • /
    • pp.9-14
    • /
    • 2004
  • Recently, various bulk metallic glasses (BMG's) having good mechanical and chemical properties were developed. BMG's can easily be deformed in the supercooled liquid region, via viscous flow mechanism. By using the viscous flow, the very low pressure is needed to deform the materials. In this study, we investigated the structural transition and deformation behavior of Vitreloy 1 (Zr/sub 41.2/Ti/sub 13.8/Cu/sub 12.5/Ni/sub 10/Be/sub 22.5/) using TMA and DSC. We applied the results to the micro forming process. The forming condition was chosen based on the viscosity data from TMA, and Si wafer with micro patterns on the surface was used as a forming die. The deformed surface was analyzed by SEM and 3D Surface Profiling System. The alloy showed good replication of the patterns. Quantitative measurement of roughness was useful to evaluate the replication. Surface condition of the deformed surface was determined by the initial surface condition.

Effect on Formation of Liquid Crystal Pitch (액정핏치 형성에 관한연구)

  • Gwon, Yeong-Bae;Ryu, Hae-Il
    • 한국기계연구소 소보
    • /
    • s.13
    • /
    • pp.15-25
    • /
    • 1984
  • The infrared spectra were determined to discover the characteristics and properties of poff-, PV-, and cc-samples, and studied influence on the formation of mesophase or liquid crystal. The experimental results were as follows; a) Samples with long aliphatic side chain appear cracking texture on temperature forming liquid crystal. b) The fine isotropic microstructure appears in a heterogeneous material containing sulfur, 7.18 w%. c) In the size of molecular weight the lighter than 500 form liquid crystal. d) When poff-sample was treated at $400^{\circ}C$ aliphatic hydrocabon compounds decrease, presented well-oriented bulk liquid crystal.

  • PDF

Studies on the Forming Process for the Bipolar Plate of Fuel Cells

  • Jin, Chul-Kyu;Lee, Jun-Kyoung
    • Journal of the Korean Society of Industry Convergence
    • /
    • v.21 no.4
    • /
    • pp.175-181
    • /
    • 2018
  • Stamping process and rubber pad forming process were performed to manufacture the bipolar plate for fuel cells. For that, a vacuum die casting process and a semi-solid forming process wherein liquid-state materials were used were adopted. After preparing the blank with the stainless steel thin plate having a thickness of 0.1 mm, the bipolar plate channel was formed with the stamping process and rubber pad forming process. The depth of the bipolar plate channel prepared by the stamping method was 0.45 mm and the depth of the bipolar plate channel prepared by the rubber pad forming process was 0.41 mm. Meanwhile, with the vacuum die casting and semi solid forming, the bipolar plate having a channel depth of 0.3 mm, same as the size of the die, could be formed.