  • Spinel $LiMn_2O_4$ and $LiMn_{1.9}Mg_{0.05}Zn_{0.05}O_4$ powders were synthesized by solid-state method at $800^{\circ}C$ for 36h. Crystal structure and electrochemical properties were analyzed by X-ray diffraction, charge-discharge test, cyclic voltammetry and ac impedance to $LiMn_2O_4$ and $LiMn_{1.9}Mg_{0.05}Zn_{0.05}O_4/Li$. All cathode material showed spinel structure in X-ray diffraction. $LiMn_{1.9}Mg_{0.05}Zn_{0.05}O_4/Li$ cell substituted $Mg^{2+}$ and $Zn^{2+}$ showed excellent discharge capacities than other cells, which it presented about 120mAh/g at the 1st cycle and about 73mAh/g at the 250th cycle, respectively. AC impedance of $LiMn_{1.9}Mg_{0.05}Zn_{0.05}O_4/Li$ cells showed the similar resistance of about $65{\sim}110{\Omega}$ before cycling.

  • PDF

$LiMn_{2-y}M_{y}O_{4}$(M=Mg, Zn) 정극의 충방전 용량 및 AC 임피던스 특성 (Charge-discharge capacity and AC impedance of $LiMn_{2-y}M_{y}O_{4}$(M=Mg, Zn) cathode)

  • 정인성;위성동;이승우;구할본
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 하계학술대회 논문집
    • /
    • pp.455-458
    • /
    • 2001
  • Spinel $LiMn_{2-y}$$M_{y}$ $O_4$powder was prepared solid-state method by calcining the mixture of LiOH - $H_2O$, Mn $O_2$, ZnO and MgO at 80$0^{\circ}C$ for 36h. To investigate the effect of substitution with Mg, Zn cation, charge-discharge experiments and initial impedance spectroscopy performed. The structure of $LiMn_{2-y}$$M_{y}$ $O_4$crystallites was analyzed from powder X-ray diffraction data as a cubic spinel, space group Fd3m. all cathode material showed spinel phase based on cubic phase in X-ray diffraction. Ununiform which calculated by (111) face and (222) face was constant in spite of the change of y value, except PUf\ulcorner LiM $n_2$ $O_4$. The discharge capacities of the cathode for the cation subbstitUtes $LiMn_{2-y}$$M_{y}$ $O_4$/Li cell at the 1st cycle and at the 40th cycle were about 120~124 and 108~112mAh/g except LiM $n_{1.9}$Z $n_{0.1}$ $O_4$/Li cell, respectively. This cell capacity is retained by 93% after 40th cycle. AC impedance of $LiMn_{2-y}$$M_{y}$ $O_4$/Li cells revealed the similar resistance of about 65~110$\Omega$ before cycling. before cycling.g.g.

  • PDF

기계적 합금법을 이용한 리튬 2차 전지용 층상 양극물질 $Li[Ni_xCo_{1-2x}Mn_x]O_2$ 의 합성 및 전기화학적 특성에 관한 연구 (Synthesis and electrochemical properties of layered $Li[Ni_xCo_{1-2x}Mn_x]O_2$ materials for lithium secondary batteries prepared by mechanical alloying)

  • 박상호;신선식;선양국
    • 한국결정학회:학술대회논문집
    • /
    • 한국결정학회 2002년도 정기총회 및 추계학술연구발표회
    • /
    • pp.16-16
    • /
    • 2002
  • The presently commercialized lithium-ion batteries use layer structured LiCoO₂ cathodes. Because of the high cost and toxicity of cobalt, an intensive search for new cathode materials has been underway in recent years. Recently, a concept of a one-to-one solid state mixture of LiNO₂ and LiMnO₂, i.e., Li[Ni/sub 0.5/Mn/sub 0.5/]O₂, was adopted by Ohzuku and Makimura to overcome the disadvantage of LiNiO₂ and LiMnO₂. Li[Ni/sub 0.5/Mn/sub 0.5/]O₂ has the -NaFeO₂ structure, which is characteristic of the layered LiCoO₂ and LiNiO₂ structures and shows excellent cycleability with no indication of spinel formation during electrochemical cycling. Layered Li[Ni/sub x/Co/sub 1-2x/Mn/sub x/]O₂ (x = 0.5 and 0.475) materials with high homogeneity and crystallinity were synthesized using a mechanical alloying method. The Li[Ni/sub 0.475/Co/sub 0.05/Mn/sub 0.475/]O₂ electrode delivers a high discharge capacity of 187 mAh/g between 2.8 and 4.6 V at a high current density of 0.3 mA/㎠(30 mA/g) with excellent cycleability. The charge/discharge and differential capacity vs. voltage studies of the Li[Ni/sub x/Co/sub 1-2x/Mn/sub x/]O₂ (x = 0.5 and 0.475) materials showed only one redox peak up to 50 cycles, which indicates that structural phase transitions are not occurred during electrochemical cycling. The magnitude of the diffusion coefficients of lithium ions for Li[Ni/sub x/Co/sub 1-2x/Mn/sub x/]O₂(x = 0.5 and 0.475) are around 10/sup -9/ ㎠/s measured by the galvanostatic intermittent titration technique (GITT).

  • PDF

$LiMn_{2-y}M_{y}O_4$ 정극 활물질의 전기화학적 특성 - I. $LiMn_{2-y}Mg_{y}O_4$의 결정 구조 및 AC Impedance 특성 (The Electrochemical Characterization of $LiMn_{2-y}M_{y}O_4$ Cathode Material - I. Crystal Structure and AC Impedance Properties of $LiMn_{2-y}Mg_{y}O_4$)

  • 정인성;김종욱;구할본;김형곤;손명모
    • 한국전기전자재료학회논문지
    • /
    • 제14권4호
    • /
    • pp.309-315
    • /
    • 2001
  • Crystallized $LiMn_{2-y}Mg_{y}O_4$ powder was prepared by calcing the mixture of LiOH.$H_2O$, $MnO_2$ and MgO at $800^{\circ}C$ for 36h in an air atmosphere. The structure of $LiMn_{2-y}Mg_{y}O_4$ crystallites was analyzed from powder X-ray diffraction data as a cubic spinel, space group Fd3m. Though all cathode material showed spinel phase based on cubic phase in X-ray diffraction, other peaks gradually exhibited and became intense with increasing y value in $LiMn_{2-y}Mg_{y}O_4$. However, ununiform which calculated by (111) face and (222) face was constant in spite of the increase of y value, except pure $LiMn_2O_4$. AC impedance of Li/$LiMn_{2-y}Mg_{y}O_4$ cells revealed the similar resistance of about $70\Omega$ before cycling. In addition, The impedance of Li/$LiMn_{1.9}Mg_{0.1}O_4$ cell changed during charge and discharge or after cycling.

  • PDF

Structural Behavior of Mixed $LiMn_2O_4-LiNi_{1/3}Co_{1/3}Mn_{1/3}O_2$ Cathode in Li-ion Cells during Electrochemical Cycling

  • 윤원섭;이상우
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2011년도 춘계학술발표대회
    • /
    • pp.5-5
    • /
    • 2011
  • The research and development of hybrid electric vehicle (HEV), plug-in hybrid electric vehicle (PHEV) and electric vehicle (EV) are intensified due to the energy crisis and environmental concerns. In order to meet the challenging requirements of powering HEV, PHEV and EV, the current lithium battery technology needs to be significantly improved in terms of the cost, safety, power and energy density, as well as the calendar and cycle life. One new technology being developed is the utilization of composite cathode by mixing two different types of insertion compounds [e.g., spinel $LiMn_2O_4$ and layered $LiMO_2$ (M=Ni, Co, and Mn)]. Recently, some studies on mixing two different types of cathode materials to make a composite cathode have been reported, which were aimed at reducing cost and improving self-discharge. Numata et al. reported that when stored in a sealed can together with electrolyte at $80^{\circ}C$ for 10 days, the concentrations of both HF and $Mn^{2+}$ were lower in the can containing $LiMn_2O_4$ blended with $LiNi_{0.8}Co_{0.2}O_2$ than that containing $LiMn_2O_4$ only. That reports clearly showed that this blending technique can prevent the decline in capacity caused by cycling or storage at elevated temperatures. However, not much work has been reported on the charge-discharge characteristics and related structural phase transitions for these composite cathodes. In this presentation, we will report our in situ x-ray diffraction studies on this mixed composite cathode material during charge-discharge cycling. The mixed cathodes were incorporated into in situ XRD cells with a Li foil anode, a Celgard separator, and a 1M $LiPF_6$ electrolyte in a 1 : 1 EC : DMC solvent (LP 30 from EM Industries, Inc.). For in situ XRD cell, Mylar windows were used as has been described in detail elsewhere. All of these in situ XRD spectra were collected on beam line X18A at National Synchrotron Light Source (NSLS) at Brookhaven National Laboratory using two different detectors. One is a conventional scintillation detector with data collection at 0.02 degree in two theta angle for each step. The other is a wide angle position sensitive detector (PSD). The wavelengths used were 1.1950 ${\AA}$ for the scintillation detector and 0.9999 A for the PSD. The newly installed PSD at beam line X18A of NSLS can collect XRD patterns as short as a few minutes covering $90^{\circ}$ of two theta angles simultaneously with good signal to noise ratio. It significantly reduced the data collection time for each scan, giving us a great advantage in studying the phase transition in real time. The two theta angles of all the XRD spectra presented in this paper have been recalculated and converted to corresponding angles for ${\lambda}=1.54\;{\AA}$, which is the wavelength of conventional x-ray tube source with Cu-$k{\alpha}$ radiation, for easy comparison with data in other literatures. The structural changes of the composite cathode made by mixing spinel $LiMn_2O_4$ and layered $Li-Ni_{1/3}Co_{1/3}Mn_{1/3}O_2$ in 1 : 1 wt% in both Li-half and Li-ion cells during charge/discharge are studied by in situ XRD. During the first charge up to ~5.2 V vs. $Li/Li^+$, the in situ XRD spectra for the composite cathode in the Li-half cell track the structural changes of each component. At the early stage of charge, the lithium extraction takes place in the $LiNi_{1/3}Co_{1/3}Mn_{1/3}O_2$ component only. When the cell voltage reaches at ~4.0 V vs. $Li/Li^+$, lithium extraction from the spinel $LiMn_2O_4$ component starts and becomes the major contributor for the cell capacity due to the higher rate capability of $LiMn_2O_4$. When the voltage passed 4.3 V, the major structural changes are from the $LiNi_{1/3}Co_{1/3}Mn_{1/3}O_2$ component, while the $LiMn_2O_4$ component is almost unchanged. In the Li-ion cell using a MCMB anode and a composite cathode cycled between 2.5 V and 4.2 V, the structural changes are dominated by the spinel $LiMn_2O_4$ component, with much less changes in the layered $LiNi_{1/3}Co_{1/3}Mn_{1/3}O_2$ component, comparing with the Li-half cell results. These results give us valuable information about the structural changes relating to the contributions of each individual component to the cell capacity at certain charge/discharge state, which are helpful in designing and optimizing the composite cathode using spinel- and layered-type materials for Li-ion battery research. More detailed discussion will be presented at the meeting.

  • PDF

Recent Development of 5 V Cathode Materials for Lithium Rechargeable Batteries

  • Kim Hyun-Soo;Periasamy Padikkasu;Moon Seong-In
    • 전기화학회지
    • /
    • 제7권1호
    • /
    • pp.1-8
    • /
    • 2004
  • This paper deals with the recent development of high-voltage cathode materials of mono- and di- metal ions substituted spinel $LiMn_2O_4$ for lithium batteries. $LiCu_xMn_{2-x}O_4(0{\leq}x{\leq}0.5)$ shows reversible intercalation/deintercalation in two potential regions, $3.9\~43\;and\;4.8-5.0V$ and stable electrochemical cycling behavior but with low capacity. $LiNi_{0.5}Mn_{1.5}O_4$ obtained by a sol-gel process delivers a capacity of 127mAh $g^{-1}$ on the first cycle and sustains a value of 124 mAh $g^{-1}$ even after the 60th cycle. The $Li_xCr_yMn_{2-y}O_4(0{\leq}x{\leq}0.5)$ solid-solutions exhibit enhanced specific capacity, larger average voltage, and improved cycling behaviors for low Cr content. $LiCr_yMn_{2-y}O_4$ presents a reversible Li deintercalation process at 4.9V, whose capacity is proportional to the Cr content in the range of $0.25{\leq}x{\leq}0.5$ and delivers higher capacities. $LiM_yCr_{0.5-y}Mn_{1.5}O_4(M=Fe\;or\;Al)$ shows that the capacity retention is lowered compared with lithium manganate. The cumulative capacities obtainable with Al-substitutted materials are less than those with Fe-substituted materials. $LiCr_xNi_{0.5-x}Mn_{1.5}O_4(x=0.1)$ delivers a high initial capacity of 1$152mAh\;g^{-1}$ with excellent cycleability.

리튬 2차 전지용 고용량 스피넬계 양극물질 연구 (A study on the Spinel phase cathode materials with high capacity for lithium secondary batteries)

  • 홍기주;선양국
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2001년도 추계학술대회 논문집 전력기술부문
    • /
    • pp.106-108
    • /
    • 2001
  • As 3V cathode material, a new doping spinel material, LiMn1.6Se0.4O4 powder with a phase-pure polycrystalline was synthesized by a sol-gel method. In spite of Jahn-teller distortion in 3V region($2.4{\sim}3.5V$), the LiMn1.6Se0.4O4 electrode shows no capacity loss. The material in the 3V region initially delivers a discharge capacity of 100mAh/g which increase with cycling to reach 105mAh/g after 90cycles. And 5V cathode material LiNi0.5-xMxMn1.5O4(M=Cr, V, Fe) compounds have been synthesized by sol-gel method. a series of electroactive spinel compounds, LiNi0.5-xMxMn1.5O4(M=Cr, V, Fe) has been studied by crystallographic and electrochemical methods. The material presents only one plateau at around 4.5 V vs. Li/Li+ with a large discharge capacity of 152mAh/g and fairly good cyclability.

  • PDF

$LiZn_xMn{2-x}O_4(0\leqq x \leqq$ 0.15) 정극 활물질의 결정 성장 변화와 전기 화학적 특성 (The crystal growth and the electrochemical property of $LiZn_xMn{2-x}O_4(0\leqq x \leqq$ 0.15) cathode material)

  • 정인성;구할본;이진;박계춘
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1999년도 춘계학술대회 논문집
    • /
    • pp.133-136
    • /
    • 1999
  • We report on the electrochemical properly of LiZ $n_{x}$Mn $_{2-x}$ $O_4$ for different degrees of Zn substitution(x) Though all cathode material showed spinel phase based on cubic phase in X-ray diffraction, other peaks(M $n_2$ $O_3$ or M $n_3$ $O_4$) gradually exhibited and became intense with the increase of x vague in LiZ $n_{x}$Mn $_{2-x}$ $O_4$. In addtion, TG-DTA analysis exhibited that both LiM $n_2$ $O_4$ and LiZ $n_{0.1}$ M $n_{1.9}$ $O_4$ occurred the weight loss(TG) and the endothermic and exothermic reaction(DTA) until 80$0^{\circ}C$ When x=0.1 in LiZ $n_{x}$Mn $_{2-x}$ $O_4$ cathode materials showed the charge and discharge capacity of about 100mAh/g at first cycle and about 70mAh/g after tooth cycle.cle.e.cle.e.e.e.

  • PDF

니켈 치환된 스피넬 LiMn2O4 박막의 구조적, 광학적 성질 (Structural and optical properties of Ni-substituted spinel $LiMn_2O_4$ thin films)

  • 이중한;김광주
    • 한국진공학회지
    • /
    • 제15권5호
    • /
    • pp.527-533
    • /
    • 2006
  • 졸-겔(sol-gel) 방법을 이용하여 스피넬(spinel) 구조를 가지는 $LiNi_xMn_{2-x}O_4$ 박막을 x = 0.9까지 합성하였다. 니켈 치환된 박막은 작은 x 값에서는 cubic 구조가 유지되지만, $x{\geq}0.6$ 범위에서는 tetragonal 구조로 상전이가 일어남이 발견되었다. 이와 같은 cubic-tetragonal 상전이는 low-spin $(t_{2g}^6,e_g^1)$ 상태를 가지는 $N^{3+}(d^7)$ 이온이 팔면체 자리를 차지하게 됨으로써 나타나는 Jahn-Teller 효과에 의한 것으로 해석된다. 이와 같은 Ni 이온들은 +3 및 +2의 원자가를 가지고 존재함이 X-ray photoelectron spectroscopy 분석을 통하여 확인되었다. $LiNi_xMn_{2-x}O_4$ 박막들에 대하여 가시광선-자외선 영역에서 spectroscopic ellipsometry(SE)를 이용하여 광학적 성질을 조사하였고, 그 결과 분석을 통하여 화합물 전자구조에 대하여 고찰하였다. SE 측정된 유전함수 스펙트럼은 주로 전하이동(charge-transfer, CT) 전이(transition)에 의한 넓은 에너지 영역을 가지는 1.9, 2.3, $2.8{\sim}3.0$, $3.4{sim}3.6eV$ 근처의 흡수구조 들로 이루어져 있는데, $O^{2-}$에서 $Mn^{4+}$ 이온의 $t_{2g}$ (1.9 eV)와 $e_g$ $(2.8{\sim}3.0\;eV)$로의 전이 즉, $O^{2-}(2p){\rightarrow}Mn^{4+}(3d)$$O^{2-}$에서 $Mn^{3+}$ 이온의 $t_{2g}$ (2.3 eV)와 $e_g$ ($3.4{\sim}3.6$ eV)로의 전이 즉, $O^{2-}(2p){\rightarrow}Mn^{3+}(3d)$ 등에 의한 것으로 해석된다. 또한, 1.6, 1.8, 1.9 eV 부근에서 관측된 좁은 에너지 영역의 흡수구조 들은 팔면체 $Mn^{3+}$ 이온 내에서의 d-d 결정장(crystal-field) 전이에 의한 것으로 해석된다. 이러한 흡수구조는 Ni 치환량이 증가함에 따라 그 강도가 감소한다. x = 0.6의 경우 $e_g$ 상태와 관련된 CT 전이구조 들이 $t_{2g}$ 상태와 관련된 전이구조 들에 비하여 큰 폭으로 감소하는데 이것은 Jahn-Teller 효과에 의해서 격자상수가 tetragonal 구조로 확장됨에 따라 $e_g$ 상태와 $O^{2-}(2p)$ 상태 간의 파동함수 중첩이 감소한 것에 기인하는 것으로 해석된다.