Conservation of the Lacquer Artifacts Excavated from Suchon-ri, Gongju, Korea

  • Song, Ji Ae;Jeong, Ah-reum;Kwon, Hyeok-nam;Han, Woo-rim;Lee, Hyun-sang
    • Journal of Conservation Science
    • /
    • v.34 no.6
    • /
    • pp.549-556
    • /
    • 2018
  • In November 2011, various artifacts were excavated from the No. 8 stone-lined tomb in Suchon-ri, Gongju by the Chungnam Institute of History and Culture. These included artifacts with lacquered mainframe and silvery metal ornament. These were recovered together with soil and underwent conservation treatment. In this paper, we discuss the scientific analysis and conservation treatment of the lacquered artifacts excavated from the Suchon-ri site. Among our findings is that the artifacts have three layers of lacquer coating and the metal parts are primarily composed of Ag. As the artifacts were recovered with soil from the site, the soil was removed from underneath and inside the artifacts. The inside of the lacquerware was reinforced with rayon paper using 3% funori, and the metal was treated with acrylic resin after removing the acrylic resin previously used to recover the artifact, followed by cleaning. The metal was also internally reinforced with gauze. Finally, the interior reinforcement was made using PVA and resin in pulp and attached with funori to preserve the shape of the lacquerware, and the exposed rayon was finished with acrylic paint. The main advantages of this study are its review of conservation treatment strategies for lacquer artifacts whose numbers have recently increased, and the application of new conservation treatment methods.

Study on Applying Techniques of Wooden Lacquerware Artifacts Excavated from Imdang-dong Site, Gyeongsan, Korea (경산 임당 유적 출토 칠기유물의 칠기법 연구)

  • Lee, Kwang-Hee;Han, Gyu-Seong
    • Journal of Conservation Science
    • /
    • v.33 no.2
    • /
    • pp.61-73
    • /
    • 2017
  • In order to identify the application techniques of wooden lacquerware artifacts, optical/polarized light microscopy, Fourier transform infrared (FT-IR) spectroscopy, and scanning electron microscopy (SEM) equipped with energy dispersive X-ray analysis (EDX) were conducted on the lacquer films of 61 wooden lacquerware artifacts excavated from the Imdang-dong site, Gyeongsan, Korea. Powdered soil, soot, and charcoal were used as a filler for the undercoat, and iron oxide ($Fe_2O_3$) was used as a red pigment. Five different applying techniques were identified for the undercoat according to the composition of the lacquer. Eight different application techniques were identified for the final coat (on the middle layer and surface layer). Totally seventeen application techniques were identified based on the combination methods of the undercoat and finalcoat. Consequently, the undercoating techniques of Imdang-dong lacquerwares were found to be similar to those of lacquerwares from excavated in other provinces. However, the use of iron oxide as a red pigment at Gyeongsang province is very characteristic compared with others.

Conservation of artifacts excavated from Imdang, Kyǒngsan Province-Metals and Lacquerware (경산시 임당유적 출토 유물 보존처리-금속 및 칠기유물을 중심으로)

  • Yu, Jae-Eun;Shin, Ui-Kyoung;Hwang, Jin-Ju;Goh, Dong-Ha
    • 보존과학연구
    • /
    • s.19
    • /
    • pp.109-132
    • /
    • 1998
  • According to excavation of Imdang site, these sites were excavated place to a various of sites from Early lron period to the Koryo Kingdom. Artifacts to be conserved were excavated from A, D and E district. Metal artifacts were excavated from D and E district and lacquer ware artifacts were excavated from Adistrict. Metal artifacts including lacquer ware iron sword, imitative bronze mirror, Osujen and bronze artifact with letter and so on. Bronze artifacts were covered with soil and rust and performed consolidation after passivation treatment with Benzotriazole solution. Also, iron artifacts performed desalting treatment with 0.1M sesquicarbonate solution. After desalinization, adhesive of these artifacts were processed with Araldite(rapid type) after consolidation with20%∼30% NAD-10 solution. Lacquer ware artifacts remained fragments of lacquer to be all corroded and soiled. Therefore these artifacts retained its original form. Fragments of lacquer joined with Caparol 1%∼3% solution and the soil of relics coated with PSNY 3%∼6% solution. There were many kinds of lacquer were. Lacquer ware artifacts presumed to a string instrument that provide important clues for lacquer ware research. As for lacquer fragments inquire, paints grain size were $2∼5\mum$ and conformed to vanished three times.