• 제목/요약/키워드: K-R Curve

검색결과 1,128건 처리시간 0.027초

일반구조용강 열간압연 박판의 K와 J 파라미터에 대한 R곡선 거동의 비교 (Comparison with R Curve Behavior fer the K and J Parameter of structural Steel Hot-Rolled Thin Plates)

  • 이계승;이억섭
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2002년도 추계학술대회 논문집
    • /
    • pp.812-815
    • /
    • 2002
  • The shape of K-R curve for an ideally brittle material is flat because the surface energy is an unvaried material property. However, the K-R curve can take on a variety of shapes when nonlinear material behavior accompanies fracture. By the way, a general metallic material is nonlinear, structural steel is such. Therefore, the J-R curve form J-integral value instead of K parameters can be used to evaluate elastic-plastic materials with flaws in terms of ductile fracture that can be significant to design. In this paper, R-curve behaviors form K and J parameter is considered for the precise assessment of fracture analysis, in case of JS-SS400 steels.

  • PDF

일반구조용강 열간압연 박판에 대한 K-R 곡선 결정 (Determination of K-R Curve for Steel Structure Hot-Rolled Thin Plates)

  • 이억섭;이계승;백준호;편장식
    • 한국정밀공학회지
    • /
    • 제19권9호
    • /
    • pp.98-105
    • /
    • 2002
  • Some materials exhibit a rising K-R curve, while the K-R curve for other materials is flat. The shape of the K-R curve depends on material behavior and, to a lesser extent, on the configuration of the cracked structure. The K-R curve for an ideally brittle material is flat because the surface energy is an invariant material property. However, the K-R curve can take on a variety of shapes when nonlinear material behavior accompanies fracture. Five different hot-rolled thin plates are tested to investigate K-R curve behavior. A special experimental apparatus is used to prevent specimens from buckling.

가스압 소결된 질화규소의 R-Curve 거동 (R-Curve Behavior in a Gas-Pressure Sintered Silicon Nitride)

  • 김상섭;김성진;백성기
    • 한국세라믹학회지
    • /
    • 제29권12호
    • /
    • pp.949-955
    • /
    • 1992
  • R-curves, fracture resistance (KR) as a function of crack extension (Δa), of a gas-pressure sintered monolithic Si3N4 were determined by controlled flaw/strength technique. Rising R-curve behavior was observed, confirming the operation of microstructural toughening process during crack growth. The R-curve parameters, k and m in the equation, KR=k(Δa)m, were determined to 30.301 and 0.1146, respectively. Microstructural observation of growing crack revealed that the bridging in the crack wake by unbroken ligament of large elongated ${\beta}$-grains was the mechanism primarily for the rising R-curve behavior.

  • PDF

On geometry dependent R-curve from size effect law for concrete-like quasibrittle materials

  • Zhao, Yan-Hua;Chang, Jian-Mei;Gao, Hong-Bo
    • Computers and Concrete
    • /
    • 제15권4호
    • /
    • pp.673-686
    • /
    • 2015
  • R-curve based on the size effect law previously developed for geometrically similar specimens (geometry type III) is extended to geometries with variable depth (geometry type I) as well as with variable notch (geometry type II), where the R-curve is defined as the envelope of the family of critical strain energy release rates from specimens of different sizes. The results show that the extended R-curve for type I tends to be the same for different specimen configurations, while it is greatly dependent on specimen geometry in terms of the initial crack length. Furthermore, the predicted load-deflection responses from the suggested R-curve are found to agree well with the testing results on concrete and rock materials. Besides, maximum loads for type II specimen are predicted well from the extended R-curve.

원자로 압력용기강 및 Al 합금재의 J-R곡선평가시 Load Ratio 해석의 유효성 검토 (Validity Examination on Evaluation of J-R Curve in the Nuclear Reactor Pressure Vessel Steels and Aluminum Alloys by Load Ratio Analysis)

  • 윤한기;우대호;김연겸;차귀준
    • 동력기계공학회지
    • /
    • 제1권1호
    • /
    • pp.80-90
    • /
    • 1997
  • The purpose of this study is to evaluate the validity examination of the J-R curve characteristics for the nuclear reactor pressure vessel steels and Al alloys by the load ratio analysis. The results of the load ratio analysis are compared with those of the J-R curve which are obtained by the ASTM unloading compliance method. The crack length calculated by the load ratio analysis is agree well with the measured final crack length. The slope of the exponential J-R curve estimated by the load ratio analysis is slightly smaller than that by the ASTM unloading compliance method. The J-R curve obtained by the ASTM unloading compliance method is over-predicted and should be offsetted due to the initial negative crack. On the other hand, the load ratio analysis method can evaluate the J-R curve by only load-displacement curve without particular crack measurement equipment.

  • PDF

R-Curve Behavior of Silicon Nitride at Elevated Temperatures

  • Sakaguchi, Shuji
    • The Korean Journal of Ceramics
    • /
    • 제4권4호
    • /
    • pp.331-335
    • /
    • 1998
  • R-curve, of three kinds of silicon nitride-based ceramics were measured, using single edge notched beam (SENB) method at room and at elevated temperatures, up to $1200^{\circ}C$. Stable fraacture was seen on ceramic materials with SENB specimens if the machined notch is deep enough, even though the crack resistance did not increase with crack length. Hot pressed silicon nitride did not show the rising R-curve behavior at room temperature, but it showed some rising at $1000^{\circ}C$ and above. Si3N4 reinforced with SiC whiskers showed no rising behavior at room and elevated temperatures, as it has smaller grain size, compare to the monolithic specimen. Gas pressure sintered silicon nitride had very large and elongated grains, and it showed rising R-curve even at room temperature. However, it showed some creep behavior at $1200^{\circ}C$ and the calculated R-curve on this condition did not show a good result. We cannot apply this technique on this condition for obtaining the R-curve.

  • PDF

부균열을 가진 J-R곡선의 수정옾셋방법에 의한 평가 (Evaluation by modified offset method on J-R curve with negative crack growth)

  • 안광주;최재강
    • 한국안전학회지
    • /
    • 제12권3호
    • /
    • pp.45-51
    • /
    • 1997
  • To evaluate the elastic-plastic fracture toughness by this modified offset method, the origin of J-R curve is set with drawing the blunting line on the maximum point of the negative crack growth and R curve is modified by adding the blunting factor of the experimented point on the R curve. The elastic-plastic fracture toughness $J_{IC]$ of A5083-H112 material by the modified offset method we 44kN/m on the smooth CT specimens.

  • PDF

CONNECTIONS ON REAL PARABOLIC BUNDLES OVER A REAL CURVE

  • Amrutiya, Sanjay
    • 대한수학회보
    • /
    • 제51권4호
    • /
    • pp.1101-1113
    • /
    • 2014
  • We give analogous criterion to admit a real parabolic connection on real parabolic bundles over a real curve. As an application of this criterion, if real curve has a real point, then we proved that a real vector bundle E of rank r and degree d with gcd(r, d) = 1 is real indecomposable if and only if it admits a real logarithmic connection singular exactly over one point with residue given as multiplication by $-\frac{d}{r}$. We also give an equivalent condition for real indecomposable vector bundle in the case when real curve has no real points.

전력분석 공격에 대응하는 타원곡선 상의 결합 난수 스칼라 곱셈 알고리즘 (A Combined Random Scalar Multiplication Algorithm Resistant to Power Analysis on Elliptic Curves)

  • 정석원
    • 사물인터넷융복합논문지
    • /
    • 제6권2호
    • /
    • pp.25-29
    • /
    • 2020
  • 타원곡선 암호 알고리즘은 RSA 공개키 알고리즘에 비해 짧은 키의 길이와 적은 통신 부하 때문에 IoT 환경에서 인증용으로 많이 사용되고 있다. 타원곡선 암호 알고리즘의 핵심연산인 스칼라 곱셈이 안전하게 구현되지 않으면, 공격자가 단순 전력분석이나 차분 전력분석을 사용하여 비밀 키를 찾을 수 있다. 본 논문에서는 스칼라 난수화와 타원곡선점 가리기를 함께 적용하고, 연산의 효율성이 크게 떨어지지 않으며 전력분석 공격법에 대응하는 결합 난수 타원곡선 스칼라 알고리즘을 제안한다. 난수 r과 랜덤 타원곡선 점 R에 대해 변형된 Shamir의 두 배 사다리 알고리즘을 사용하여 타원곡선 스칼라 곱셈 kP = u(P+R)-vR을 계산한다. 여기에서 위수 n=2l±c일 때, 2lP=∓cP를 이용하여 l+20 비트 정도의 u≡rn+k(modn)과 ν≡rn-k(modn)를 구한다.

$Al_2O_3-ZrO_2-SiC$ Whisker 복합재료에서의 R-curve 거동에 관한 연구 (Study on the R-curve Behaviour in $Al_2O_3-ZrO_2-SiC$ Whisker Comosite)

  • 김현하;박현;최성철
    • 한국세라믹학회지
    • /
    • 제30권9호
    • /
    • pp.731-739
    • /
    • 1993
  • R-curve measurements were performed on Al2O3(matrix)-ZrO2-SiC whisker composite and Al2O3-ZrO2, Al2O3-SiC whisker composites in the favor of comparing the effect of ZrO2 and SiC whisker, as a second phase, to Al2O3 matrix. Al2O3-SiC whisker and Al2O3-ZrO2-SiC whisker were fabricated by hot pressing at 1$700^{\circ}C$, 15MPa and Al2O3-ZrO2 by pressureless sintering at 1$600^{\circ}C$. A controlled flaw/strength technique was utilized to determine fracture resistance as a function of crack extension and R-curve behaviour was determined from the relationship which is KR=K0(Δa)m. R-curveresults were KR=6.173$\times$Δa0.031 for Al2O3-ZrO2, KR=18.796$\times$Δa0.172 for Al2O3-SiC whisker and KR=11.96$\times$Δa0.110 for Al2O3-ZrO2-SiC whisker composite. From the analysis of R-curve and expeirmental data above three composites, it is found that R-curve behaviour of Al2O3-ZrO2-SiC whisker composite was dominated initially by the strengthening effect of ZrO2 and after, some extended crack were influenced by the effect of SiC whisker. Analysis of SEM and X-ray data revealed that whisker bridging in the crack wake and whisker pull-out mechanisms were the main mechanism for the R-curve behaviour.

  • PDF