Load Ratio 해석에 의한 알루미늄 5083 합금 용접부의 J-R곡선 평가 (Evaluation of J-R Curve for Aluminum 5083 Alloy Weldment by Load Ratio Analysis)

  • 윤한기;김연겸
    • Journal of Welding and Joining
    • /
    • 제15권4호
    • /
    • pp.178-186
    • /
    • 1997
  • The purpose of this study is to evaluate the J-R curve characteristics for the 5083 aluminum alloy weldment by the load ratio analysis. The results of the load ratio analysis are compared with those of the J-R curve which are obtained by the ASTM unloading compliance method. The crack length calculated by the load ratio analysis is agrees well with the measured final crack length. The slope of the exponential J-R curve estimated by the load ratio analysis is slightly smaller than that by the ASTM unloading compliance method. The exponential correlation of the J-R curve for the 5083 aluminum alloy base metal by the load ratio analysis is J = 93.88 ${\Delta}{\alpha}^{0.375}$. That for the weld metal and HAZ is J = 69.87 ${\Delta}{\alpha}^{0.389}$ and J = 70.59 ${\Delta}{\alpha}^{0.359}$ respectively. The J-R curve obtained by the ASTM unloading compliance method is overpredicted and should be offsetted due to the initial negative crack. On the other hand, the load ratio analysis method can evaluate the J-R curve by only load displacement curve without particular crack measurement equipment.

  • PDF

원자로 압력용기강 및 Al 합금재의 J-R곡선평가시 Load Ratio 해석의 유효성 검토 (Validity Examination on Evaluation of J-R Curve in the Nuclear Reactor Pressure Vessel Steels and Aluminum Alloys by Load Ratio Analysis)

  • 윤한기;우대호;김연겸;차귀준
    • 동력기계공학회지
    • /
    • 제1권1호
    • /
    • pp.80-90
    • /
    • 1997
  • The purpose of this study is to evaluate the validity examination of the J-R curve characteristics for the nuclear reactor pressure vessel steels and Al alloys by the load ratio analysis. The results of the load ratio analysis are compared with those of the J-R curve which are obtained by the ASTM unloading compliance method. The crack length calculated by the load ratio analysis is agree well with the measured final crack length. The slope of the exponential J-R curve estimated by the load ratio analysis is slightly smaller than that by the ASTM unloading compliance method. The J-R curve obtained by the ASTM unloading compliance method is over-predicted and should be offsetted due to the initial negative crack. On the other hand, the load ratio analysis method can evaluate the J-R curve by only load-displacement curve without particular crack measurement equipment.

  • PDF

일반구조용강 열간압연 박판의 K와 J 파라미터에 대한 R곡선 거동의 비교 (Comparison with R Curve Behavior fer the K and J Parameter of structural Steel Hot-Rolled Thin Plates)

  • 이계승;이억섭
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2002년도 추계학술대회 논문집
    • /
    • pp.812-815
    • /
    • 2002
  • The shape of K-R curve for an ideally brittle material is flat because the surface energy is an unvaried material property. However, the K-R curve can take on a variety of shapes when nonlinear material behavior accompanies fracture. By the way, a general metallic material is nonlinear, structural steel is such. Therefore, the J-R curve form J-integral value instead of K parameters can be used to evaluate elastic-plastic materials with flaws in terms of ductile fracture that can be significant to design. In this paper, R-curve behaviors form K and J parameter is considered for the precise assessment of fracture analysis, in case of JS-SS400 steels.

  • PDF

SA508-3재의 제하컴플라이언스법과 하중비해석을 이용한 파괴저항곡선 평가 (J-R Curve Characterization by Load Ratio Analysis and Unloading Compliance Method for SA508 C-3 steel)

  • 임만배;차귀준;윤한기;안원기
    • 한국해양공학회지
    • /
    • 제12권1호
    • /
    • pp.65-75
    • /
    • 1998
  • The fracture resistance curve is one of most important and design techniques employed in nuclear pressure vessel structures. This study is to evaluate the J-R curve characteristics for the SA508C-3 by the unloading compliance method and load rato analysis. The effect of strain aging for the exponential correlation of the J-R curve in this metal are investigated at room temperature, 20$0^{\circ}C$ and 30$0^{\circ}C$. The load ratio analysis method can evaluate the J-R curve by using the simple tension load-displacement curve only without the repeat of the unloading and loading. Therefore, the analysis by the proposed load ratio method has a merit, in comparison with the unloading compliance method, which can measure the crack length without the precision measurement equipment.

  • PDF

Load Ratio 해석에 의한 Al 5083 알루미늄합금 용접부의 J-R곡선 평가 (Evaluation on J-R Curve of 5083 aluminum Alloy Weldment by Load Ratio analysis)

  • 윤한기;김연겸;우대호
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 1997년도 특별강연 및 춘계학술발표 개요집
    • /
    • pp.91-98
    • /
    • 1997
  • This research is to evaluate of the J-R curve characteristic in 5083 aluminum alloy weldment by utilizing the load ratio analysis. This analysis method can be evaluated the J-R curve only with load-displacement curve without any particular precision instrument equipment in CT specimen. For validity, the results of the load ratio analysis are compared with the those of the J-R curve, which are obtained by the ASTM standard unloading compliance method. The calculated crack length of the load ratio analysis is well appropriate that the measured final crack length. And the J-R curve slope estimated by the load ratio analysis is slightly smaller than that by the ASTM unloading compliance method.

  • PDF

SA 508C-3강의 고온에서 J-R Curve 및 Tmat의 평가 (Evaluation of J-R Curve and Tmat of SA 508C-3 Steel at Elevated Temperature)

  • 임만배;차귀준
    • 한국해양공학회지
    • /
    • 제12권3호통권29호
    • /
    • pp.60-67
    • /
    • 1998
  • In this study, the J-Resistance Curve and material tearing modulus of SA508-C3 steel, which is one of the used nuclear pressure vessel steel, are measured ar room temperature, $200^{circ}C$ and $300^{circ}C$ according to load ratio analysis and ASTM E813, ASTM E1152, respectively. It is observed that J-R curve and Tmat value decrease as the temperature level increase. Applicability of $T_j$ proposed by Paris et al as instability parameter for ductile material is investigated. It is concluded that results are the $T_j$ parameter may be used as a crack instability parameter.

  • PDF

J-적분을 이용한 균열 찢어짐 불안정성에 관한 연구 (Traring instability of crack based on J-integral)

  • 이홍서;김희송
    • 한국정밀공학회지
    • /
    • 제6권3호
    • /
    • pp.78-89
    • /
    • 1989
  • Applicability of tearing modulus based on J-integral proposed by Paris et al is investigated using compact tension specimens of strutural alloy steel (SCM4). Both general fracture test and instability fracture test are performed. The applied tearing modulus, ( $T_{j}$)app estimated from the real load vs. crack growth curve measured from experiments are compared with that estimated from the limit load vs. crack growth curve. The results are : (1) the $T_{j}$parameter could be applied to predict crack growth instability : (2) The use of ( $T_{j}$)app estimated from the load vs. crack growth curve, proposed in this study could be well predicted crack growth instability instead of that estimated form the limit load vs. crack growth curve.e.

  • PDF

한국의 대중국 항만 무역에서 J-curve 효과는 존재하는가? (Is There a J-Curve Effect in the Trade with China via Korean Ports?)

  • 김창범
    • 한국항만경제학회지
    • /
    • 제27권3호
    • /
    • pp.1-12
    • /
    • 2011
  • 본 논문은 금융위기 이후 대중 수출증가가 경기회복에 주도적 역할을 하고, 우리경제의 중국경제 의존도가 크게 상승하는 상황에서 J-curve 효과가 우리나라 대중국 항만 수출입 흐름에 적용되는가를 월별자료를 이용하여 2000년부터 2010년까지의 기간에 대해 실증분석 하였다. 오차수정모형을 추정한 결과 단기적인 조정역할은 실질실효환율이 수행하는 것으로 나타났으며, 분산분해 결과 대중국 항만 무역수지에 대한 영향력이 국내경기보다 실질실효 환율과 세계경기가 더 크게 나타남을 알 수 있었다. 이와 더불어 수준변수로 구성된 VAR과 오차수정항을 포함한 VECM을 이용한 충격반응 분석을 실시한 결과 대중국 항만 무역수지는 환율 충격에 대하여 시차를 두고 반응을 보이는 것으로 나타나 J-curve 효과가 존재함을 알 수 있었다.

표준 CT시험편을 이용한 실배관 파괴저항 곡선 예측 (Estimation of the Fracture Resistance Curve for the Nuclear Piping Using the Standard Compact Tension Specimen)

  • 박홍선;허용;구재민;석창성;박재실
    • 대한기계학회논문집A
    • /
    • 제33권9호
    • /
    • pp.930-937
    • /
    • 2009
  • The estimation method of the fracture resistance curve for the pipe specimen was proposed using the load ratio method for the standard specimen. For this, the calculation method of the load - CMOD curve for the pipe specimen with the common format equation(CFE) was proposed by using data of the CT specimen. The proposed method agreed well with experimental data. The J-integral value and the crack extension were calculated from the estimated load - CMOD data. The fracture resistance curve was estimated from the calculated J-integral and the crack extension. From these results, it have been seen that the proposed method is reliable to estimate the J-R curve of the pipe specimen.

부균열을 가진 J-R곡선의 수정옾셋방법에 의한 평가 (Evaluation by modified offset method on J-R curve with negative crack growth)

  • 안광주;최재강
    • 한국안전학회지
    • /
    • 제12권3호
    • /
    • pp.45-51
    • /
    • 1997
  • To evaluate the elastic-plastic fracture toughness by this modified offset method, the origin of J-R curve is set with drawing the blunting line on the maximum point of the negative crack growth and R curve is modified by adding the blunting factor of the experimented point on the R curve. The elastic-plastic fracture toughness $J_{IC]$ of A5083-H112 material by the modified offset method we 44kN/m on the smooth CT specimens.