• Title/Summary/Keyword: Iron-Oxide

Search Result 746, Processing Time 0.027 seconds

MBE growth and magnetic properties of epitaxial FeMn2O4 film on MgO(100)

  • Duong, Van Thiet;Nguyen, Thi Minh Hai;Nguyen, Anh Phuong;Dang, Duc Dung;Duong, Anh Tuan;Nguyen, Van Quang;Cho, Sunglae
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2016.02a
    • /
    • pp.318.2-318.2
    • /
    • 2016
  • FeM2X4 spinel structures, where M is a transition metal and X is oxygen or sulfur, are candidate materials for spin filters, one of the key devices in spintronics. Both the Fe and M ions can occupy tetrahedral and octahedral sites; therefore, these types of compounds can display various physical and chemical properties [1]. On the other hand, the electronic and magnetic properties of these spinel structures could be modified via the control of cation distribution [2, 3]. Among the spinel oxides, iron manganese oxide is one of promising materials for applications. FeMn2O4 shows inverse spinel structure above 390 K and ferrimagnetic properties below the temperature [4]. In this work, we report on the structural and magnetic properties of epitaxial FeMn2O4 thin film on MgO(100) substrate. The reflection high energy electron diffraction (RHEED) and X-ray diffraction (XRD) results indicated that films were epitaxially grown on MgO(100) without the impurity phases. The valance states of Fe and Mn in the FeMn2O4 film were carried out using x-ray photoelectron spectrometer (XPS). The magnetic properties were measured by vibrating sample magnetometer (VSM), indicating that the samples are ferromagnetic at room temperature. The structural detail and origin of magnetic ordering in FeMn2O4 will be discussed.

  • PDF

Effect of Fe2+/Fe3+ Ratio on the Crystallization of the Scoria Glass (CaO-MgO-Al2O3-SiO2 System) (Scoria 유리(CaO-MgO-Al2O3-SiO2계)의 결정화에 미치는 Fe2+/Fe3+비 효과)

  • 최병현;지응업
    • Journal of the Korean Ceramic Society
    • /
    • v.26 no.5
    • /
    • pp.705-711
    • /
    • 1989
  • The glass-ceramics was prepared with the scoria(CaO-MgO-Al2O3-SiO2 system) of the locally occurring volcanic ejecta containing 10-13w/o of (FeO+Fe2O3) by melting at 140$0^{\circ}C$ for 4 hours and thermally treated for nucleation and crystallization. The sucrose was added to the scoria to adjust the Fe2+/Fe3+ ratio during the melting process. The addition of 1-2w/o of sucrose showed the glass-ceramics body with the finest particle developed and dispersed over the entire range. It is concluded that the impurity content of iron oxide and titanium oxide play the most-influencial effect on the crystallization. When 1-2w/o of sucrose was added to the scoria, the value of Fe2+/Fe3+ ratio was 0.93-1.32 and showed the best result of crystallization. The nucleation temperature and time were calculated by the measurements of exothermic peak temperatures of DTA for quenched and thermally treated glasses. The nucleation temperature of scoria glass without the addition of sucrose was estimated as 75$0^{\circ}C$, but the addition of sucrose by 2w/o showed the nucleation temperature 6$25^{\circ}C$. The nucleation time was calculated with the same DTA curves. The nucleation times estimated were about 150min. for both of glasses without and with sucrose added. Finally, the activation energies for crystallization were calculated with the DTA data. The calculated activation energies were 143 Kcal/mole for the glass without addition of sucrose and 90Kcal/mole, 87Kcal/mole, 85Kcal/mole and 71Kcal/mole for the glasses of 1w/o, 2w/o, 3w/o and 4w/o addition respectively.

  • PDF

Deterioration Mechanism Interpretation and Surface Contaminant Analysis of the Five-Storied Stone Pagoda in Tapriri, Uiseong (의성 탑리리 오층석탑의 표면오염물 분석 및 손상메커니즘 해석)

  • Lee, Mi Hye;Chun, Yu Gun;Lee, Myeong Seong
    • Economic and Environmental Geology
    • /
    • v.46 no.5
    • /
    • pp.445-453
    • /
    • 2013
  • The Uiseong Tapriri Five-Storied Stone Pagoda (National Treasure No. 77) is typical stone cultural heritage in Unified Silla Dynasty, Korea. The pagoda has been occurred black, brown discoloration and microcrack, exfoliation, granularity decomposition with white discoloration because of continuous weathering. As the results of analysis for the contaminants, chemical weatherings are generated that black contaminant by manganese oxide, brown contaminant by iron oxide, white contaminants by gypsum and taranakite. And physical weatherings, such as microcrack, exfoliation, are occurred by salt(gypsum) crystallization. Therefore, these need to remove the contaminants according to the conservation treatment manual, and regular monitoring using P-XRF to preserve long-term the Five-Storied Stone Pagoda at Tapri-ri, Uiseong.

Preparation of Core-Shell Structured Iron Oxide/Graphene Composites for Supercapacitors Application (코어-쉘 구조의 산화철/그래핀 복합체 제조 및 슈퍼커패시터 응용)

  • Lee, Chongmin;Chang, Hankwon;Jang, Hee Dong
    • Particle and aerosol research
    • /
    • v.14 no.3
    • /
    • pp.65-72
    • /
    • 2018
  • Core-shell structured $Fe_3O_4/graphene$ composites were synthesized by aerosol spray drying process from a colloidal mixture of graphene oxides and $Fe_3O_4$ nanoparticles. The structural and electrochemical performance of $Fe_3O_4/graphene$ were characterized by the field-emission scanning electron microscopy, X-ray diffraction, Raman spectroscopy, cyclic voltammetry, and galvanometric discharge-charge method. Core-shell structured $Fe_3O_4/GR$ composites were synthesized in different mass ratios of $Fe_3O_4$ and graphene oxide. The composite particles were around $3{\mu}m$ in size. $Fe_3O_4$ nanoparticles were encapsulated with a graphene. Morphology of the $Fe_3O_4/graphene$ composite particles changed from a spherical ball having a relatively smooth surface to a porous crumpled paper ball as the content of GO increased in the composites. The $Fe_3O_4/GR$ composite fabricated at the weight ratio of 1:4 ($Fe_3O_4:GO$) exhibited higher specific capacitance($203F\;g^{-1}$) and electrical conductivity than as-fabricated $Fe_3O_4/GR$ composite.

Loess Dyeing of Soybean Fabrics (대두직물의 황토염색)

  • Lee, Sol;Lee, Shin-Hee
    • Fashion & Textile Research Journal
    • /
    • v.17 no.6
    • /
    • pp.1004-1012
    • /
    • 2015
  • The purpose of this study is to investigate the loess dyeability of soybean fabric using loess as colorants. Recent days, various textile products such as inner wears, sheets and interior goods are manufactured using materials dyed with loess emphasizing its improved metabolism, anti-bacterial, deodorizing properties, and far infrared ray emissions. Soybean fabric was dyed with loess solution according to concentration of loess, dyeing temperature and dyeing time. To improve washing fastness, soybean fabric and dyed soybean fabric with loess were mordanted by mordanting agents such as sodium chloride(NaCl), Acetic acid(CH3COOH) and Aluminium Potassium Sulfate(AlK(SO4)2·12H2O). Dyeability and color characteristics of dyed soybean fabric were obtained by CCM observation. Particle size distribution of loess, the dyeability(K/S) of soybean fabric, morphology and washing durability of loess dyed soybean fabric were investigated. The results obtained were as follows; Mean average diameter of loess was 1.08µm. The main components of loess used in this study were silicon dioxide(SiO2), aluminium oxide(Al2O3), and iron oxide(Fe2O3). The content of these three component was above 75 weight %. The dyeability of soybean fabric was increased gradually with increasing concentration of loess. The optimum dyeing temperature and dyeing time were 90℃ and 60minutes expectively. The fastness to washing according to concentration of loess and mordanting method indicated good grade result as more than 4 degree in all conditions.

Skin Corrosion and Irritation Test of Nanoparticles Using Reconstructed Three-Dimensional Human Skin Model, EpiDermTM

  • Kim, Hyejin;Choi, Jonghye;Lee, Handule;Park, Juyoung;Yoon, Byung-Il;Jin, Seon Mi;Park, Kwangsik
    • Toxicological Research
    • /
    • v.32 no.4
    • /
    • pp.311-316
    • /
    • 2016
  • Effects of nanoparticles (NPs) on skin corrosion and irritation using three-dimensional human skin models were investigated based on the test guidelines of Organization for Economic Co-operation and Development (OECD TG431 and TG439). EpiDerm$^{TM}$ skin was incubated with NPs including those harboring iron (FeNPs), aluminum oxide (AlNPs), titanium oxide (TNPs), and silver (AgNPs) for a defined time according to the test guidelines. Cell viabilities of EpiDerm$^{TM}$ skins were measured by the 3-(4, 5-dimethylthiazol-2-yl)-2.5-diphenyltetrazolium bromide based method. FeNPs, AlNPs, TNPs, and AgNPs were non-corrosive because the viability was more than 50% after 3 min exposure and more than 15% after 60 min exposure, which are the non-corrosive criteria. All NPs were also non-irritants, based on viability exceeding 50% after 60 min exposure and 42 hr post-incubation. Release of interleukin 1-alpha and histopathological analysis supported the cell viability results. These findings suggest that FeNPs, AlNPs, TNPs, and AgNPs are 'non-corrosive' and 'non-irritant' to human skin by a globally harmonized classification system.

Recovery of manganese compounds from electric arc furnace dust by Aluminothermy Process (테르밋 반응을 이용한 페로망간 전기로 분진의 재활용에 관한 연구)

  • Ha, Tae-Young;Jo, Young-Min;Park, Young-Koo;Kim, Youn-Che
    • Journal of the Korean Applied Science and Technology
    • /
    • v.32 no.1
    • /
    • pp.23-30
    • /
    • 2015
  • The properties of dust collected from electric arc furnace of ferro manganese production units was investigated, and also the metallic manganese was recovered from the dust by aluminothermy process. The ferromanganese dust collected from electric arc furnace contained about 15% of manganese oxide ($Mn_3O_4$) and 9% of carbon as the contaminant, and have a 5um of 50% median diameter and irregular particle shape. The carbon contaminant in the dust could be reduced until about 0.1~0.5% level by roasting in the air at a temperature of 600~900C for 60minutes. The recovery of manganese could not be carried out using only ferromanganese dust from electric arc furnace by aluminothermy process, but the ferromanganese which contained manganese of about 92% and iron of about 5% could be obtained from the mixture of ferromanganese dusts from electric arc furnace and converter. The best mixing condition of dust fixed at electric arc furnace dust / converter dust ratio of 1:9 and 2:8, and the mixing rato of 3:7 or more could not separated the metal and slag from the reactant after aluminothermy reaction.

Characteristic of Inorganic Contaminants and Conservation Treatment Materials for the Three-Storied Stone Pagoda of Bulguksa Temple in Gyeongju (경주 불국사 삼층석탑(석가탑)의 무기오염물과 보수물질 특성)

  • Lee, Gemma;Kim, Sa Duk;Park, Sungchul;Kim, Derk Moon
    • Journal of Conservation Science
    • /
    • v.34 no.5
    • /
    • pp.421-431
    • /
    • 2018
  • Analyses of the three-storied stone pagoda at the Bulguksa temple in Gyeongju were carried out in order to identify the cause for material characteristics of inorganic contaminants and conservation treatment materials. Results indicated that foreign soil or weathering soil caused yellow discoloration of the pagoda, reddish-brown contaminants were formed by goethite (FeOOH), an iron oxide mineral, and black pollutants were formed by manganese (Mn) oxide, leading to discoloration of the rock. Among the restoration materials used in the past, cement mortar could cause whitening by reacting with the external environment. The results were used as basic standards to evaluate the material characteristics of the surface contaminants and identify a set of effective conservation treatments. Nevertheless, continuous monitoring is required, as there is a high possibility of regeneration of pollutants in the future because of the continuous exposure of the pagoda to the external environment.

The Evaluation of Hydrogenation Properties on $MgH_x-Fe_2O_3$ Composite by Mechanical Alloying (기계적 합금화법으로 제조된 $MgH_x-Fe_2O_3$ 복합재료의 수소화 특성 평가)

  • Seok, Song;Cho, Kyoung-Won;Hong, Hae-Whan
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.18 no.1
    • /
    • pp.26-31
    • /
    • 2007
  • Hydrogen has a high potential to be a renewable substitute for fossil fuels, because of its high gravimetric energy density and environment friendliness. In particular, Magnesium have attracted much interest since their hydrogen capacity exceeds that of known metal hydrides. One of the approaches to improve the kinetic is addition of metal oxide. In this paper, the effect of $Fe_2O_3$ concentration on the kinetics of Mg hydrogen absorption reaction was investigated. $MgH_x-Fe_2O_3$ composites have been synthesized by hydrogen induced mechanical alloying. The powder synthesized was characterized by XRD, SEM and simultaneous TG, DSC analysis. The hydrogenation behaviors were evaluated by using a sievert's type automatic PCT apparatus. Absorption and desorption kinetics of Mg catalyzed with 5,10 mass% $Fe_2O_3$ are determined at 423, 473, 523, 573, 623K.

Suppression of Methane Emission from Rice Paddy Soils with Fly ash Amendment

  • Ali, Muhammad Aslam;Oh, Ju-Hwan;Kim, Pil-Joo
    • Korean Journal of Environmental Agriculture
    • /
    • v.26 no.2
    • /
    • pp.141-148
    • /
    • 2007
  • Fly ash, a by-product of the coal-burning industry, and a potential source of ferro-alumino-silicate minerals, which contains high amount of ferric oxide and manganese oxide (electron acceptors), was selected as soil amendment for reducing methane $(CH_4)$ emission during rice cultivation. The fly ash was applied into potted soils at the rate of 0, 2, 10, and 20 Mg $ha^{-1}$ before rice transplanting. $CH_4$ flux from the potted soil with rice plants was measured along with soil Eh and floodwater pH during the cropping season. $CH_4$ emission rates measured by closed chamber method decreased gradually with the increasing levels of fly ash applied but rice yield significantly increased up to 10 Mg $ha^{-1}$ application level of the amendment. At this amendment level, total seasonal $CH_4$ emission was decreased by 20% along with 17% rice grain yield increment over the control. The decrease in total $CH_4$ emission may be attributed due to suppression of $CH_4$ production by the high content of active and free iron, and manganese oxides, which acted as oxidizing agents as well as electron acceptors. In conclusion fly ash could be considered as a feasible soil amendment for reducing total seasonal $CH_4$ emissions as well as maintaining higher grain yield potential under optimum soil nutrients balance condition.