구상흑연주철의 피로수명을 지배하는 내재결함부 크기는 정량적 평가 (Quantitative Evaluation for the Internal Defect Size Governing the Fatigue Life in Ductile Irons)

  • 김진학;김민건
    • 대한기계학회논문집A
    • /
    • 제24권11호
    • /
    • pp.2742-2748
    • /
    • 2000
  • In this study, the quantitative evaluation was performed by examination for gatigue crack origin in two prepared ductile irons specimens which have different microstructures using rotary bending fatigue tester, Series A has mixed microstructure. ferrite plus pearlite, and series B has bainitic microstructure. Obtained main results are as follows. The scatterings of fatigue strength were observed on σ(sub)α-Ν diagram of both specimen series, and it is observed that scatterings of series A were more serious. It is reasonable to evaluate the size of mesocrack range by means of √A(원문참조), where A means the area of mesocrack range including globular graphite nodule. As a result of reconsideration for the fatigue data by introduction of K(sub)α-Ν diagram, the scattrings of fatigue life were, remarkably. reduced. Therefore, it is more reasonable to evaluate of mesocrack range on fatigue life by parameter K(sub)α rather than σ(sub)α.