Esthetic Rehabilitation of Anterior Dentition by All Ceramic Crowns Using IPS e.max CAD : A Case of Tetracycline Discoloration (전치부 전부도재관을 이용한 테트라싸이클린 착색의 심미보철 회복 증례 (IPS e.max CAD 블록의 이용))

  • Kim, Jae-Hong;Cho, Young-kyu;Kim, Hae-Young
    • Journal of dental hygiene science
    • /
    • v.11 no.4
    • /
    • pp.299-303
    • /
    • 2011
  • The purpose of this case report was to present an example of an esthetic and functional rehabilitation of anterior teeth with tetracycline discoloration and minor morphological abnormality of a 39-year old female. A chairside computer-aided design/computer-aided manufacturing (CAD/CAM) system with CEREC AC was applied for the prosthetic procedure and all ceramic crowns made with lithum disilicate (IPS e.max CAD) restored the esthetic and functional features of sixteen anterior teeth successfully.

Evaluation of marginal fit of 2 CAD-CAM anatomic contour zirconia crown systems and lithium disilicate glass-ceramic crown

  • Ji, Min-Kyung;Park, Ji-Hee;Park, Sang-Won;Yun, Kwi-Dug;Oh, Gye-Jeong;Lim, Hyun-Pil
    • The Journal of Advanced Prosthodontics
    • /
    • v.7 no.4
    • /
    • pp.271-277
    • /
    • 2015
  • PURPOSE. This study was to evaluate the marginal fit of two CAD-CAM anatomic contour zirconia crown systems compared to lithium disilicate glass-ceramic crowns. MATERIALS AND METHODS. Shoulder and deep chamfer margin were formed on each acrylic resin tooth model of a maxillary first premolar. Two CAD-CAM systems (Prettau$^{(R)}$Zirconia and ZENOSTAR$^{(R)}$ZR translucent) and lithium disilicate glass ceramic (IPS e.max$^{(R)}$press) crowns were made (n=16). Each crown was bonded to stone dies with resin cement (Rely X Unicem). Marginal gap and absolute marginal discrepancy of crowns were measured using a light microscope equipped with a digital camera (Leica DFC295) magnified by a factor of 100. Two-way analysis of variance (ANOVA) and post-hoc Tukey's HSD test were conducted to analyze the significance of crown marginal fit regarding the finish line configuration and the fabrication system. RESULTS. The mean marginal gap of lithium disilicate glass ceramic crowns (IPS e.max$^{(R)}$press) was significantly lower than that of the CAD-CAM anatomic contour zirconia crown system (Prettau$^{(R)}$Zirconia) (P<.05). Both fabrication systems and finish line configurations significantly influenced the absolute marginal discrepancy (P<.05). CONCLUSION. The lithium disilicate glass ceramic crown (IPS e.max$^{(R)}$press) had significantly smaller marginal gap than the CAD-CAM anatomic contour zirconia crown system (Prettau$^{(R)}$Zirconia). In terms of absolute marginal discrepancy, the CAD-CAM anatomic contour zirconia crown system (ZENOSTAR$^{(R)}$ZR translucent) had under-extended margin, whereas the CAD-CAM anatomic contour zirconia crown system (Prettau$^{(R)}$Zirconia) and lithium disilicate glass ceramic crowns (IPS e.max$^{(R)}$press) had overextended margins.

Study about shear bond strength of zirconia core used in dental prosthesis (치과 보철물에 사용되는 지르코니아 코어의 전단결합강도에 관한 연구)

  • Sim, Ji-Young;Kim, Jae-Hong;Kim, Woong-Chul;Kim, Hae-Young;Kim, Ji-Hwan
    • Journal of Technologic Dentistry
    • /
    • v.33 no.4
    • /
    • pp.299-306
    • /
    • 2011
  • Purpose: This study aimed to investigate the shear bond strength by manufacturing the veneering porcelain on the IPS e.max $ZirCAD^{(R)}$ zirconia core, using the layering technique and heat-pressing technique, and to evaluate the clinical stability by comparing to the conventional metal ceramic system. Methods: The Schmitz-Schulmeyer test method was used to evaluate the core-veneer shear bond strength of zirconia core ceramic(IPS e.max $ZirCAD^{(R)}$) and their manufacture recommended two veneering ceramic systems(IPS e.max $ceram^{(R)}$, IPS e. max $ZirPress^{(R)}$). A metal ceramic system(Bellabond $plus^{(R)}$, VITA $VM13^{(R)}$) was used as a control group for the two all ceramic system test groups. The maximum loading and shear bond strength was measured. The average shear strength(MPa) was analyzed with the one-way ANOVA and the Tukey's test(${\alpha}$=.05). The fracture specimens were examined using Microscope to determine the failure pattern. Results: The mean shear bond strengths(SD) in MPa were MBSB control 43.62(2.13); ZBSB 18.65(1.76); ZPSB 18.89(1.54). The shear strengths of the zirconia cores were not significantly different(P>.05). Microscope examination showed that zirconia specimens presented mixed failure, and base metal alloy specimens showed adhesive failure. Conclusion: There was no siginificant different between the layering technique and the heat pressing technique in the veneering methods on the zirconia cores. None of the zirconia core and veneering ceramics could attain the high bond strength values of the metal ceramic combination.