• Title/Summary/Keyword: IF Steel Sheet

Search Result 42, Processing Time 0.022 seconds

A Study on the Strengthening Effect of Reinforced Conctete BeamsFlexural Strengthening after Pre-loading (선가력 후 휨 보강한 RC보의 보강 효과에 관한 연구)

  • Kim, Jeong-Sup;Sin, Yong-Seok;Jo, Cheol-Hee;Kim, Kyoug-Ok
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.10 no.6
    • /
    • pp.183-190
    • /
    • 2006
  • From the result of this research above, it may be summed up as follows. As a summary of results from each experiment, as the test body reinforced with the carbon rods was embedded inside the concrete section and made it possible uniform movement, this study has shown that it had excellent characteristics in improving the flexural strength and ductility. Also, it was considered as the carbon-steel sheet composite plate was to exert the strength more if it would complement the adherence with the concrete.

Debonding strain for steel-concrete composite slabs with trapezoidal metal deck

  • Claudio Bernuzzi;Marco A. Pisani;Marco Simoncelli
    • Steel and Composite Structures
    • /
    • v.49 no.1
    • /
    • pp.19-30
    • /
    • 2023
  • Steel-concrete composite slabs represent a very efficient floor solution combining the key performance of two different materials: the steel and the concrete. Composite slab response is governed by the degree of the interaction between these two materials, mainly depending by chemical and mechanical bond. The latter is characterized by a limited degree of confinement if compared with the one of the rebars in reinforced concrete members while the former is remarkably influenced by the type of concrete and the roughness of the profiled surface, frequently lubricated during the cold-forming manufacturing processes. Indeed, owing to the impossibility to guarantee a full interaction between the two materials, a key parameter governing slab design is represented by the horizontal shear-bond strength, which should be always experimentally estimated. According to EC4, the design of the slab bending resistance, is based on the simplified assumption that the decking sheet is totally yielded, i.e., always in plastic range, despite experimental and numerical researches demonstrate that a large part of the steel deck resists in elastic range when longitudinal shear collapse is achieved. In the paper, the limit strain for composite slab, which corresponds to the slip, i.e., the debonding between the two materials, has been appraised by means of a refined numerical method used for the simulation of experimental results obtained on 8 different composite slab types. In total, 71 specimens have been considered, differing for the properties of the materials, cross-section of the trapezoidal profiled metal sheets and specimen lengths.

EVA Sheet and Butyl Rubber based Waterproofing·Anti-Corrosion Sheet for Corrosion Maintenance and Repairing in the Interior Side of the Large Steel Pipes in Water Treatment Facilities (상수도용 대구경 녹 발생 강관 내부의 보수 및 성능 유지를 위한 EVA 시트와 부틸고무를 합지한 자착식 방수방식 시트의 부착성능 평가)

  • An, Ki-Won;Kim, Byoung-Il;Oh, Sang-Keun
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.5 no.3
    • /
    • pp.267-274
    • /
    • 2017
  • This study discusses the applicability of environmental friendly EVA based butyl rubber self-adhesive waterproof sheet designed to prevent corrosion of large scale pipes used in the water treatment facilities during th water treatment process. The experiments conducted tested the waterproofing sheet's adhesion strength on the steel surface of the pipes and checked for whether the material has the proper response properties against the various environmental conditions. In addition, it the sheet adhered to the steel pipe was to see if the adhesion hold against the water pressure due to the ingress of inflow water. Finally, the waterproofing sheet's adhesion strength was tested on a rusted steel surface to confirm whether the material has the necessary properties to secure stable adhesion strength and prevent corrosion of steel pipes at the same time during the process of installation or maintenance. As a result, the self-adhesive waterproof sheets showed that all attachments in the untreated, long term pressuring, immersion in chemical substance (hydrochloric acid, hypochlorous acid, sodium hydroxide), low temperature ($-20^{\circ}C$) conditions showed a adhesion performance of higher than 1.5N/mm, which is the performance standard of KS F 4934. Also, in the testing to check for the adhesion property against inverse water pressure, it was observed that the adhesion failure did not occur even up to $3.0N/mm^2$ pressure. Also, in the process of assessing the adhesion performance on rusted steel surface, specimens after 12 hours of corrosion treatment was shown to have 2.1N/mm, and specimens after 168 hours of corrosion treatment was shown to have 2.0N/mm adhesion strength performance.

Effects of Heating Conditions in the Straightening of Sheet Metal Distortion (박판재 변형의 가열교정에서 가열면적의 영향)

  • Park, Jun-Hyoung;Kim, Jae-Woong;Kim, Ki-Chul;Jun, Joong-Hwan
    • Journal of Welding and Joining
    • /
    • v.26 no.4
    • /
    • pp.79-84
    • /
    • 2008
  • Use of sheet metal structure is increased in various fields such as automobile, aerospace and communication equipment industry. When this structure is welded, welding distortion is generated due to the non-uniformity of temperature distribution. Recently welding distortion becomes a matter of great importance in the structure manufacture industry because it deteriorates the product's quality by bringing about shape error. Accordingly many studies for solving the problems by controlling the welding distortion are being performed. However, it is difficult to remove all kinds of distortion by welding process, though various kinds of methods for reducing distortion are applied to production. Consequently, straightening process is operated if the high precision quality is requested after welding. The local heating method induces compression plastic deformation by thermal expansion in the heating stage and then leaves constriction of length direction in the cooling stage. Accordingly, in the case of sheet metal structure, straightening effect is expected by heating for the part of distortion. This study includes numerical analysis of straightening effect by the local heating method in distortion comes from production of welded sheet metal structure. Particularly straightening effect followed by dimensions of heating area is analyzed according to the numerical analysis. The numerical analysis is performed by constructing 3-dimensional finite element model for 0.4mm stainless steel-sheet metal. Results of this study confirm that straightening effect changes as heating area increases and the optimum value of heating area that proves the maximum straightening effect exists.

Design of a Stainless Steel Insert for Mechanical Joining of Long Fiber-reinforced Composite Structures (장섬유강화 복합재료 구조물의 기계적 접합을 위한 스테인레스 강 인서트 설계)

  • Lee, Sung-Woo;Chang, Seung-Hwan
    • Composites Research
    • /
    • v.31 no.4
    • /
    • pp.139-144
    • /
    • 2018
  • Long Fiber-reinforced composites have advantages of excellent production efficiency and formability of complex shapes compared to conventional continuous fiber reinforced composite materials. However, if we need to make complicated composite shapes or to assemble parts made of different materials, a variety of joining methods are needed. In general, long fiber prepreg sheet (LFPS) contains mold release agent to facilitate demolding after thermoforming. Therefore, mechanical fastening is required in addition to the adhesive bonding to get proper joining strength. In this study, we proposed a stainless steel insert for co-cure bonding which cures LFPS and bonds the stainless steel insert through thermoforming process. The wing of the insert which is spread during the thermoforming process induces adhesion and mechanical wedging effect and serves as a hook to resist the pulling force. The burn-out method was used to confirm the unfolded state of the stainless steel insert wings inserted into the composite material. The static pull-out test was performed to quantitatively evaluate the joining strength. From these experimental results, the condition which guarantees the most appropriate joining strength was derived.

Effect of Process Parameters on Condenser Discharge Weldability of Thin Gauge Steel (박판 강재의 컨덴서 용접성에 미치는 용접변수의 영향)

  • 김기철;이목영;임태진
    • Journal of Welding and Joining
    • /
    • v.15 no.6
    • /
    • pp.49-56
    • /
    • 1997
  • Effect of process parameters on the quality of condenser discharge weld for coated sheet steels was discussed. The welding specimens were coated with pure Zn of 20/20 g/m2 in the production line. Direct measurements of welding parameters such as the discharge current, the pressures and the voltage drop across the electrodes were carried out with welding process monitoring system. High speed camera was also utilized to analyze the weld formation process. Test results indicated that the relation between weld strength and applied energy was stabilized at the acceptable welding heat input range. It was thought that the acceptable welding heat input should be redefined based on the monitored data because the calculated value of the welding heat input could hardly be utilized if the discharge condition was changed. Mechanical test results and high speed photographs showed that expulsion deteriorated the weld quality and the strength at the same time especially when the size of the spatter was large enough to carry the molten metal, which should form the nugget, out of the welding spot. Results also demonstrated that the discharge current should be applied at the appropriate time during the process because sufficient nugget was not produced if the time was deviated from the optimum range.

  • PDF

Evaluation of Local Damages and Residual Performance of Blast Damaged RC Beams Strengthened with Steel Fiber and FRP Sheet (폭발 손상을 입은 강섬유 및 FRP 시트 보강 철근콘크리트 보의 국부손상 및 잔류성능 평가)

  • Lee, Jin-Young;Jang, Dae-Sung;Kwon, Ki-Yeon;Yoon, Young-Soo
    • Journal of the Korea Concrete Institute
    • /
    • v.26 no.5
    • /
    • pp.627-634
    • /
    • 2014
  • In this study, standoff detonation tests and static beam tests on $160{\times}290{\times}2200mm$ RC beams were conducted to investigate the effect of local damage on the flexural strength and ductility index. And also, blast resistance of RC beams strengthened with steel fiber and FRP sheet were evaluated by these tests. The standoff detonation tests were performed with charge weight of 1kg and standoff distance of 0.1m. After the tests, crater diameters and loss weights of specimens were measured to evaluate the local damage of specimens. Flexural strength and ductility index were measured by conducting the static beam tests on the damaged and undamaged specimens. As a test results, normal concrete specimen(NC) showed relatively large crater and spall diameters that caused weight loss of 23.5kg as a local damage. Whereas, steel fiber reinforced concrete specimen(SFRC) and FRP sheet retrofitted specimens(NC-F, NC-FS) showed higher blast resistance than NC by reducing crater size and weight loss. Flexural strength and ductility index were decreased in case of local damaged specimens by detonation. Especially, large decrease of flexural strength was shown in NC as compared with intact specimen and brittle failure was occurred due to buckling of compressive reinforcement. In case of specimens strengthened with steel fiber and FRP sheet, residual flexural strength and ductility index were increased as compared with NC. In these results, it is concluded that critical local damage can be occurred unless enough standoff distance can be assured even if the charge weight is small. and it is verified that strengthening method using steel fiber and FRP sheet can increase blast resistance.

The study on salt injury and carbonation of concrete (도심지 상업 건축물의 리모델링 조사.연구)

  • 김동훈;이해진;김진호;임남기
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2001.11a
    • /
    • pp.136-141
    • /
    • 2001
  • If we build new building after demolition of commercial building that is located in the downtown, it will be caused a social and environmental problem as wasting of resources and generating of waste. In this study, I investigated about remodel ins, this conclusion is given below. 1. Reconstruction cost is 2.1 times, and construction period is 1.4 times as much remodeling. So remodeling has an advantage. 2. For repairing and reinforcing timeworn building, we reinforced it as using carbon fiber sheet (girder, slab) and injecting method steel plate bonding Also, we tried to maintain efficiency of new building as using epoxy to protect concrete crack. 3. In the side of waste products and cost, remodeling has much more advantage than reconstruct. But demolition used construction period much. Because it had to be reused as repairing and reinforcing. And there was no difference between remodeling cost and reconstruct cost. If we develop research with enterprise.university.laboratory to exploit material and equipment and to train specialized engineer who will has a capacity to know construct repair and reinforce, it can be attribute to prevail remodeling in new construct market.

  • PDF

Corrosion resistance at high temperature condition of Cr Films Formed on hot-dip Al-Si plated steel sheet (용융Al-Si도금 강재에 형성한 Cr 막의 고온 환경 중 내식특성)

  • Gang, Min-Ju;Lee, Seung-Hyo;Lee, Myeong-Hoon
    • Journal of the Korean institute of surface engineering
    • /
    • v.55 no.6
    • /
    • pp.448-459
    • /
    • 2022
  • Generally, steel is the most commonly used in the industry because of good strength, processability and cost-effectiveness. Steel can be surface-treated such as coating or used as an alloy by adding elements such as Cr, Ni, Zr, and Al to increase corrosion resistance. However, even if steel is used in same environment corrosion resistance is sharply lowered when it is exposed to a high temperature for a fixed or extended period of time due to an overload or other factors. In particular, the use of hot-dip aluminized plated steel, which is used in high-temperature atmospheres, is increasing due to the surface Al2O3 oxide film. This steel necessitates an urgent solution as issues of corrosion resistance limitations often appear. It is an important issue that not only cause analysis but also the research for the surface treatment method that can be solved. Thus, in this study, Cr in which it is expected to be effective in corrosion resistance and heat resistance attempted to deposit on hot dip aluminized plated steel with PVD sputtering. And it was possible to present the surface treatment application of various types of industrial equipment exposed to high temperature and basic design guidelines for use by confirming the corrosion resistance of hot dip Al-Si plated steel with Cr film deposited at high temperature.

Correlation Between Mechanical and Magnetic Properties for Cold Rolled Carbon Steel Sheet (냉연강판의 기계적 물성과 자기적 특성의 상관관계)

  • Park, S.Y.;Ryu, K.S.;Yi, J.K.;Park, J.S.
    • Journal of the Korean Magnetics Society
    • /
    • v.16 no.4
    • /
    • pp.211-215
    • /
    • 2006
  • Measurement methods in order to measure the mechanical properties nondestructively have been studied. The mechanical properties of the structural and turbine rotor steels are related with their magnetic properties. If the magnetic properties of the cold rolled carbon steel sheet (CR) for a car are measured nondestructively, its mechanical properties are analogized by their magnetic properties. And then the mechanical properties are monitored on-line by measuring the magnetic properties. We prepared three CR materials, CBQ 3060, CBQ 3041, and CBQ 3036, were prepared in order to measure their mechanical and magnetic properties. The Vickers hardness,yield strength, and tensile strength were measured by ASTM E 8M, and the reversible magnetic permeability was measured by the surface type probe. The coercivity calculated by the peak interval of reversible magnetic permeability increased linearly with the increase of Vickers hardness, yield strength, and tensile strength. The amplitude of the peak interval of reversible magnetic permeability drastically decreased when the lift-off was increased.