• Title/Summary/Keyword: Hydroxyapatite(HAp) sol

Search Result 5, Processing Time 0.018 seconds

Hydroxyapatite+TiO2 Composite Sol Coating on Cp-Ti (Cp-Ti 표면의 Hydroxyapatite+TiO2 복합 Sol 코팅에 관한 연구)

  • Kim, Yun-Jong;Kim, Taik-Nam;Lee, Sung-Ho
    • Korean Journal of Materials Research
    • /
    • v.15 no.7
    • /
    • pp.444-447
    • /
    • 2005
  • In this study, $Hydroxyapatite+TiO_2(HAp+TiO_2)$ composite sol coatings on Cp-Ti substrates were deposited by using a sol-gel derived precursor. Prior to hydroxyapatite coating, the samples were micropolished and divided into three sets. The first set was coated with hydroxyapatite (HAp) directly on Cp-Ti. The second set was first coated with intermediate titania layer and then coated with HAp. The third set samples were coated with $HAp+TiO_2$ (50:50) composite sol. Each samples were predried at $200^{\circ}C$, and heat treated at $600^{\circ}C$. The formation of hydroxyapatite has been confirmed by XRD analyses and the substrate material was found to be oxidized with negligible amount of CaO in the coating. The NaOH treated samples showed the presence of rutile crystal. The SEM studies revealed surface morphologies of each samples. $HAp+TiO_2$ composite sol coating layer was found to be smooth. The bonding strength of each samples were calculated using pull out tests. The bonding strength of the $HAp+TiO_2$ composite sol coating on substrate was 29.35MPa.

Mechanism of Escherichia Coli Removal by Hydroxyapatite

  • Su-Chak Ryu;Dong-Hun Lee;Jae-Hoon Jeong;Sung-Kwang Jo
    • Korean Journal of Materials Research
    • /
    • v.34 no.6
    • /
    • pp.261-266
    • /
    • 2024
  • Although most strains of escherichia coli (E. coli) are harmless, some serotypes can cause serious food poisoning in humans. It is very difficult to eliminate E. coli from our lives. Here we show that E. coli can be eliminated by hydroxyapatite (HAp). Because HAp has a positive charge, the material and E. coli are attracted through electrostatic interactions. Additionally, because the surface of HAp is porous, it enters the pores of the HAp surface removing them from the environment. The amount of adsorption was observed to increase over time, and the zeta potential value of the material tended to be similar to that of E. coli. This phenomenon is thought to have zeta potential similar to that of E. coli as it is adsorbed onto the HAp surface over time. E. coli stained with crystal violet was spread on a glass slide and HAp porous sol powder was dropped to remove the E. coli. We expect that this analysis will open a new direction for antibacterial materials.

A study of hydroxyapatite coating on Ti-6Al-4V dental implant alloy with different surface treatments using a sol-gel derived precursor (Sol-Gel 성형체에 의해 다르게 표면 처리된 치과 Implant용 Ti-6Al-4V합금의 Hydroxyapatite 코팅에 관한 연구)

  • Han, Sok-Yoon
    • Journal of Technologic Dentistry
    • /
    • v.26 no.1
    • /
    • pp.139-144
    • /
    • 2004
  • In the present study, a simple method was successfully used for hydroxyapatite coatings on Ti-6Al-4V substrates deposited by using a sol-gel derived precursor. Prior to hydroxyapatite coating the samples were micropolished (0.1 micron) and divided into three sets. The first set,were the micropolished samples kept as such. The second set were coated with titania sol and the third set was treated with 5M NaOH. After three repetitions of hydroxyapatite coating procedures on each set and heat treatment at 600 $^{\circ}\Delta C$, the formation of hydroxyapatite has been confirmed by XRD analyses and the substrate material was found to be oxidized with negligible amount of CaO in the coating. The SEM studies revealed surface morphology. Hydroxyapatite, calcined at 600$^{\circ}\Delta C$, displaying a porous structure arisen from heating of the bulk. But, it is very meaningful in trying to approach morale management plans with an object of dental technicians. It is necessary that dental technicians should make efforts to control themselves.

  • PDF

A study of hydroxyapatite coating on Ti-6Al-4V alloy with different surface treatments using a sol-gel derived precursor

  • Balakrishnan Avinash;Kim Yun-Jong;Lee Seung-Woo;Kim Taik-Nam
    • The Journal of Engineering Research
    • /
    • v.6 no.1
    • /
    • pp.161-168
    • /
    • 2004
  • In the present study, a simple method was successfully used for hydroxyapatite coatings on Ti-6AL-4V substrates deposited by using a sol-gel derived precursor. Prior to hydroxyapatite coating the samples were micropolished (0.1 micron) and divided into three sets. The first set, were the micropolished samples kept as such. The second set were coated with titania sol and the third set was treated with 5M NaOH. After three repetitions of hydroxyapatite coating procedures on each set and heat treatment at $600^{\circ}C$, the formation of hydroxyapatite has been confirmed by XRD analyses and the substrate material was found to be oxidized with negligible amount of CaO in the coating. The SEM studies revealed surface morphology. Hydroxyapatite, calcined at $600^{\circ}C$, displaying a porous structure arisen from heating of the bulk

  • PDF