• Title/Summary/Keyword: Hybrid Bonding

Search Result 221, Processing Time 0.037 seconds

Development of Amorphous Iron Based Coating Layer using High-velocity Oxygen Fuel (HVOF) Spraying (철계 비정질 분말을 활용한 초고속 용사 코팅층 개발)

  • Kim, Jungjoon;Kim, Song-Yi;Lee, Jong-Jae;Lee, Seok-Jae;Lim, Hyunkyu;Lee, Min-Ha;Kim, Hwi-Jun;Choi, Hyunjoo
    • Journal of Powder Materials
    • /
    • v.28 no.6
    • /
    • pp.483-490
    • /
    • 2021
  • A new Fe-Cr-Mo-B-C amorphous alloy is designed, which offers high mechanical strength, corrosion resistance as well as high glass-forming ability and its gas-atomized amorphous powder is deposited on an ASTM A213-T91 steel substrate using the high-velocity oxygen fuel (HVOF) process. The hybrid coating layer, consisting of nanocrystalline and amorphous phases, exhibits strong bonding features with the substrate, without revealing significant pore formation. By the coating process, it is possible to obtain a dense structure in which pores are hardly observed not only inside the coating layer but also at the interface between the coating layer and the substrate. The coating layer exhibits good adhesive strength as well as good wear resistance, making it suitable for coating layers for biomass applications.

Characteristic Analysis of Resistance Spot Welding between Dissimilar Materials of 1.035mm Laminated Vibration Damping Steel with 35㎛ Viscoelastic Resin (35㎛ 점탄성수지가 적용된 1.035mm 제진강판의 이종소재간 저항점용접 특성분석)

  • Bae, Ki-Man;Baek, Jong-Jin;Shin, Chang-Yeul;Kim, Seung-Kyung;Kang, Myungchang
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.20 no.12
    • /
    • pp.24-29
    • /
    • 2021
  • Recently, owing to the high demand for eco-friendly cars in the automotive industry, noise and vibrations have become major challenges. The use of laminated damping steel is increasing in response to these demands. Laminated damping steel is primarily used in sound insulation plates. The vibration energy is converted into thermal energy due to the viscoelastic resin being located between two steel sheets and being able to damp the vibrations when an external force, such as, noise or vibration is applied to the steel plate. Laminated damping steel is chiefly applied to dash panels in automotive body parts, and because of its structure, junction technology for bonding with other components is necessary. However, there has not been sufficient research conducted on junctions. In this study, regardless of the electrode shape, in the range of 4.0 ~ 8.0 kA welding current, the same welding force and welding time were applied which were 2.8 kN and 200 m/s (12 cycles) and the tensile shear load and nugget size were analyzed after the resistance spot welding between different materials of laminated damping steel with a thickness of 1.035 mm. The results show that in the range of 5 ~ 8 kA welding current, 1.035 mm laminated damping steel meets the MS181-15 standard, which is the technical standard of Hyundai-Kia Motors.

Pomegranate extract on eroded dentin: antioxidant action, bond strength and morphology of the adhesive interface after aging

  • Thiago Vinicius Cortez;Nathalia Mancioppi Cerqueira;Julia Adornes Gallas;Wanderley Pereira Oliveira;Silmara Aparecida Milori Corona;Aline Evangelista Souza-Gabriel
    • Restorative Dentistry and Endodontics
    • /
    • v.49 no.1
    • /
    • pp.9.1-9.14
    • /
    • 2024
  • Objectives: This study aimed to evaluate the effect of pomegranate solution (Punica granatum) on eroded dentin through antioxidant action, shear bond strength (SBS) and interface morphology. Materials and Methods: The 10% pomegranate peel extract was prepared by the lyophilization method. Punicalagin polyphenol was confirmed by high-performance liquid chromatography. Antioxidant activity was evaluated by capturing the 2,2-diphenyl1-picrylhydrazyl (DPPH) radical. For the SBS, 48 dentin fragments were divided into sound or eroded, and subdivided according to the pretreatment (n = 12): water or P. granatum. The surfaces were restored with self-etch adhesive and a bulk-fill resin (Ecosite; DMG). The SBS was done immediately (24 hours) and after thermal cycling + water storage (12 months). For scanning electron microscopy, 48 dentin fragments (24 sound and 24 eroded) received the same treatments as for SBS (n = 6), and they were analyzed after 24 hours and 12 months. Results: The P. granatum had antioxidant action similar (p = 0.246) to the phenolic standard antioxidants. After 24 hours, eroded dentin had lower SBS than sound dentin (p < 0.001), regardless of the pretreatment. After 12 months, P. granatum maintained the SBS of sound dentin (13.46 ± 3.42 MPa) and eroded dentin (10.96 ± 1.90 MPa) statistically similar. The lowest values were found on eroded dentin treated with water (5.75 ± 1.65 MPa) (p < 0.001). P. granatum on eroded dentin caused peritubular demineralization and hybrid layer with resin tags. Conclusions: The pomegranate extract had antioxidant action and preserved the adhesive interface of the eroded dentin.

Interaction of Proline with Cu+ and Cu2+ Ions in the Gas Phase (기체상에서 Cu+ 및 Cu2+ 이온과 proline의 상호작용)

  • Lee, Gab-Yong
    • Journal of the Korean Chemical Society
    • /
    • v.53 no.3
    • /
    • pp.257-265
    • /
    • 2009
  • The structures and metal affinities of the binding configurations of $Cu^{+}$ and $Cu^{2+}$ to proline have been investigated using the hybrid three-parameter Density Functional Theory(DFT/B3LYP). We found that the metal-proline bonding and the energy ordering of several conformers were very different in $Cu^{+}$-proline and $Cu^{2+}$-proline. For $Cu^{+}$-proline, the ground state structure was found to have a bidentated coordination in which $Cu^{+}$ was coordinated to the carbonyl oxygen and imino group nitrogen of neutral proline. On the contrary, the ground state structure of $Cu^{2+}$-proline involves chelation between the two oxygens of the carboxylate group in a zwitterionic proline. The metal ion affinity of proline of the most stable $Cu^{+}$-proline complex was calculated as 76.0 kcal/mol at 6-311++G(d,p) level, whereas the $Cu^{2+}$ ion affinity of proline was calculated as 258.5 kcal/mol.

STUDY ON THE SHEAR BOND STRENGTH OF ALL-IN-ONE DENTIN BONDING SYSTEM (우치에 대한 All-in-one 상아질 결합제의 전단결합강도 비교 연구)

  • Park, Hyung-Joo;Yoo, Seung-Hoon;Kim, Jong-Soo
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.33 no.4
    • /
    • pp.661-672
    • /
    • 2006
  • This study was performed to compare the shear bond strength of AQ Bond $Plus^{TM}$ with AQ $Bond^{TM}$ and Single $Bond^{TM}$. Also by observing the fractured interface under scanning electro-microscope, the fracture pattern and the quality of hybrid layer were analyzed. The possibility of clinical application of all-in-one system which has an advantage to reduce chair time for children with difficult behavior pattern was evaluated, The results obtained are as follows ; 1. There was no significant difference between AQ $Bond^{TM}$ and AQ Bond $Plus^{TM}$ in shear bond strength and Single Bond showed the highest bond strength with statistical significant difference (p<0.05). 2. Adhesive fracture pattern was mainly observed in both enamel/dentin in AQ $Bond^{TM}$ and AQ Bond $Plus^{TM}$ group while Single Bond group showed equal numbers for cohesive and adhesive pattern. 3. Under scanning electro-microscope, resin tags observed in AQ $Bond^{TM}$ and AQ Bond $Plus^{TM}$ were very weak and tangled while strong and thick tags were shown with many lateral branches in Single Bond. Careful case selection and accurate clinical application is recommended when using AQ $Bond^{TM}$ and AQ Bond $Plus^{TM}$considering the result showing its weaker strength than Single $Bond^{TM}$.

  • PDF

Bonding efficacy of cured or uncured dentin adhesives in indirect resin (간접 레진수복시 상아질 접착제의 중합 여부에 따른 결합 효능)

  • Jang, Ji-Hyun;Lee, Bin-Na;Chang, Hoon-Sang;Hwang, Yun-Chan;Oh, Won-Mann;Hwang, In-Nam
    • Restorative Dentistry and Endodontics
    • /
    • v.36 no.6
    • /
    • pp.490-497
    • /
    • 2011
  • Objectives: This study examined the effect of the uncured dentin adhesives on the bond interface between the resin inlay and dentin. Materials and Methods: Dentin surface was exposed in 24 extracted human molars and the teeth were assigned to indirect and direct resin restoration group. For indirect resin groups, exposed dentin surfaces were temporized with provisional resin. The provisional restoration was removed after 1 wk and the teeth were divided further into 4 groups which used dentin adhesives (OptiBond FL, Kerr; One-Step, Bisco) with or without light-curing, respectively (Group OB-C, OB-NC, OS-C and OS-NC). Pre-fabricated resin blocks were cemented on the entire surfaces with resin cement. For the direct resin restoration groups, the dentin surfaces were treated with dentin adhesives (Group OB-D and OS-D), followed by restoring composite resin. After 24 hr, the teeth were assigned to microtensile bond strength (${\mu}TBS$) and confocal laser scanning microscopy (CLSM), respectively. Results: The indirect resin restoration groups showed a lower ${\mu}TBS$ than the direct resin restoration groups. The ${\mu}TBS$ values of the light cured dentin adhesive groups were higher than those of the uncured dentin adhesive groups (p < 0.05). CLSM analysis of the light cured dentin adhesive groups revealed definite and homogenous hybrid layers. However, the uncured dentin adhesive groups showed uncertain or even no hybrid layer. Conclusions: Light-curing of the dentin adhesive prior to the application of the cementing material in luting a resin inlay to dentin resulted in definite, homogenous hybrid layer formation, which may improve the bond strength.

Synthesis and characterization of hydrophobic and hydrophilic cellulose derivative by esterification (친수성과 소수성을 동시에 가지는 아세틸화 셀룰로스 에테르의 합성 및 특성 평가)

  • Kim, Taehong;Lee, Sangku;Son, Byunghee;Paik, Hyun-Jjong;Yoon, Sanghyeon;Lee, Heesoo
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.23 no.1
    • /
    • pp.31-36
    • /
    • 2013
  • Acetylated Cellulose Ether (ACE), cellulose-based amphiphilic polymer with hydrophilic and hydrophobic, was synthesized and investigated in terms of its solubility and wettability for organic solvents and water. Acetyl group was substituted to the cellulose ether in a hydrophilic polymer by esterification. As a result of FT-IR, the peak corresponding to the hydroxyl group decreased and carboxyl acid peak increased with increasing reaction time and temperature, which signified the increase in the degree of acetylation of the ACE. There were similar thermal decomposition behaviors before and after esterification reaction until $800^{\circ}C$ so that the reaction occurred without significant structural changes of cellulose backbones. The solubility parameter of the ACE had a range of 18.5~26.4, and its viscosity and turbidity were controlled according to the solubility parameter of organic solvents. The ACE showed the hydrophilicity because the contact angle of the ACE was higher than the cellulose ether. These results confirmed that the ACE had the hydrophobicity and hydrophilicity due to the ether which was glucosidic bonding between the glucose units and un-reacted hydroxyl functional groups in the ACE.

Implementation of Readout IC for $8\times8$ UV-FPA Detector ($8\times8$ UV-PPA 검출기용 Readout IC의 설계 및 제작)

  • Kim, Tae-Min;Shin, Gun-Soon
    • Journal of the Korea Institute of Information and Communication Engineering
    • /
    • v.10 no.3
    • /
    • pp.503-510
    • /
    • 2006
  • Readout circuit is to convert signal occurred in a defector into suitable signal for image signal processing. In general, it has to possess functions of impedance matching with perception element, amplification, noise reduction and cell selection. It also should satisfies conditions of low-power, low-noise, linearity, uniformity, dynamic range, excellent frequency-response characteristic, and so on. The technical issues in developing image processing equipment for focal plane way (FPA) can be categorized as follow: First, ultraviolet (UV) my detector material and fine processing technology. Second, ReadOut IC (ROIC) design technology to process electric signal from detector. Last, package technology for hybrid bonding between detector and ROIC. ROIC enables intelligence and multi-function of image equipment. It is a core component for high value added commercialization ultimately. Especially, in development of high-resolution image equipment ROIC, it is necessary that high-integrated and low-power circuit design technology satisfied with design specifications such as detector characteristic, signal dynamic range, readout rate, noise characteristic, ceil pitch, power consumption and so on. In this paper, we implemented a $8\times8$ FPA prototype ROIC for reduction of period and cost. We tested unit block and overall functions of designed $8\times8$ FPA ROIC. Also, we manufactured ROIC control and image boards, and then were able to verify operation of ROIC by confirming detected image from PC's monitor through UART(Universal Asynchronous Receiver Transmitter) communication.

Improvement of the Strength Properties and Impact Resistance of the Cement Composite Materials by the use of Surface Modification of the Aramid Fibers (아라미드섬유의 표면개질에 의한 시멘트 복합재료의 강도특성 및 내충격성능의 향상효과)

  • Nam, Jeong-Soo;Yoo, Jae-Chul;Kim, Gyu-Yong;Kim, Hong-Seop;Jeon, Joong-Kyu
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.19 no.1
    • /
    • pp.100-108
    • /
    • 2015
  • The purpose of this study is to evaluate the effect of improvement on the impact resistance and strength properties of cement composites by surface modification of aramid fiber. For aramid fiber reinforced cement composites, therefore, dispersion capability and the bonding efficiency between the fibers and the cement composite material need to be improved. It is possible by modifying surface properties to hydrophobic, it is considered that oiling agent ratio of 1.2 % and improvement of performance is in need to be investigated. In this study, short aramid fibers were mixed by different fiber length and oiling agent ratio. And improvement of strength properties and impact resistance performance of hybrid cement composites were evaluated under the influence of steel fiber. As a result, strength properties of aramid fiber reinforced cement composites are different by mixing ratio of fiber, oiling agent ratio and length of fiber. In case of cement composites which have same volume fraction and fiber length, tensile strength and flexural strength were improved with increase of the emulsions throughput of the fiber surface. The results of evaluation on the static strength properties had effects on impact resistance performance by high-velocity impact. And it was observed that the scabbing of rear was suppressed with increase of the oiling agent ratio.

Influence of Sodium Hypochlorite on Bond Strength of Dual-cured Core Build-up Resin Composite (이원중합형 코어 축조용 복합레진의 결합강도에 대한 NaOCI의 영향에 대한 연구)

  • Lee, Jun-Bong;Park, Jong-Duk;Kwon, Su-Mi;Yu, Mi-Kyung;Lee, Kwang-Won
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.23 no.4
    • /
    • pp.283-292
    • /
    • 2007
  • Two-step or one-step bonding systems generally inhibit curing process of dual-cured core build-up resin composite for their adhesive acidity. In addition this dual-cured core build-up resin composite can be applied to dentin of pulp chamber and root at the time that complete the endodontic treatment. The purpose of this investigation was to determine the influence of sodium hypochlorite on rnicrotensile bond strength of dual-cured core build-up resin composite. Extracted human molars were horizontally sectioned with 1mm thickness using low speed diamond saw. After the sectioned specimens were divided into 8 groups, adhesive systems (Clearfil SE-Bond, Prime&Bond NT[2-step, 1-step], Adper Prompt L-Pop) were then applied with or without sodium hypochlorite pretreatment. The treated specimen was filled with dual-cured core build-up resin composite (Luxacore, DMG corp., German). Then light cured for 40 seconds and soaked in $37^{\circ}C$ water bath for 24 hours. After the treated specimen was grinded with 1mm width and measured rnicrotensile bond strength by testing machine. Additionally 8 teeth were prepared for SEM evaluation. The results were as follows. : NaOCl treated groups generally had lower rnicrotensile bond strength but did not show any difference statistically except Adper Prompt L-Pop. When the teeth were treated by NaOCl, though the difference of applied adhesive system, it had no statistically significant difference within the NaOCl treated groups except the relation of between ClearFil SE-Bond adhesive system and Adper Prompt L-Pop adhesive system. In the SEM evaluation, NaOCl treated groups presented relatively long resin tags and incomplete hybrid layer formation generally.