Effect of Moulding Conditions on Properties of Table Top for Student Desk Manufactured by Wood Waste Materials (폐기 목질 재료로 제조한 학생용 책상 천판의 성능에 미치는 성형조건의 영향)

  • Roh, Jeang-Kwan;Kim, Jae-Kyung;Kim, Sa-Ick;Jo, Jong-Soo;Yoon, Seung-Lak;Ra, Jong-Bum;Do, Jeong-Lak
    • Journal of the Korean Wood Science and Technology
    • /
    • v.30 no.4
    • /
    • pp.106-113
    • /
    • 2002
  • This research was performed to investigate the effect of moulding conditions on properties of the table top for student desk manufactured by wood waste materials. The table top manufactured using the mat mixed properly with fine particles and coarse particles generally showed better physical properties than those manufactured using either fine particles or coarse particles did/ Especially, highest performance for overlaying was observed when fine particles were used for face layer and coarse particles were used for core layer. The internal bond (IB) strength, the bending strength and thickness swelling increased with the increase of density. Most of physical properties were improved with the increase of hot pressing temperature. The best physical properties were found at 190℃ when the first hot pressing and the second hot pressing times were two minutes. However, the effect of the second hot pressing time of two minutes on the physical properties was not markedly different from that of one minute. This result suggests that the second hot pressing time of one minute is enough to increase the productivity in manufacturing the table top with the least decrease of the physical properties.

Influence of Adhesion Condition on the Laminated Wood of Pinus thunbergii glued with Urea-formaldhyde Resin (요소수지접착제(尿素樹脂接着劑)를 사용(使用)한 곰솔 집성재(集成材)의 제조조건(製造條件)이 접착성질(接着性質)에 미치는 영향(影響))

  • Chung, In-Oh;So, Won-Tek;Lim, Kie-Phy
    • Journal of the Korean Wood Science and Technology
    • /
    • v.12 no.2
    • /
    • pp.35-43
    • /
    • 1984
  • This study was carried out to investigate the block shear strength of the 2ply laminated wood composed of Pinus thunbergii with ureaformaldehyde resin as adhesives according to pressure (6, 9, 12, 15kg/$cm^2$), pressing time(5, 10, 20, 30 hrs.), amount of spread(54, 108, 217, 324g/$cm^2$), hardener(10, 20, 30, 40% of 10% $NH_4CL$ on resin) and extender(0, 5, 10, 15% wheat flour on resin), and the bending strength and bending young's modulus of laminated beam according to the number of ply. The results were summarized as follows; 1. According to pressing pressure with amount of spread 217g/$cm^2$ both dry and wet shear strength of laminated wood showed the highest in 15kg/$cm^2$, and hot-cold soaking treatment showed the highest in 9kg/$cm^2$, while all shear strength of dry, wet and hot-cold soaked laminated wood have been reduced with the increasing of pressing time. 2. According to amount of spread, adhesion strength with the dry, wet and hot-cold soaking treatments revealed the highest in 217g/$cm^2$ and have been reduced under or over 217g/$cm^2$ of spread. 3. According to addition of hardener and extender, all shear strength of laminated block with the dry, wet and hot-cold soaking treatments have been reduced in increasing of addition amount of hardener and extender. The bending strength of beam according to the number of ply showed the highest in 2ply laminated wood and horizontal loading beam to glue line had the higher in strength than the vertical loading.

  • PDF

Microstructure and Thermoelectric Properties of n-Type $\textrm{Bi}_{2}(\textrm{Te}_{0.9}\textrm{Se}_{0.1})_3$ Fabricated by Mechanical Alloying and Hot Pressing Methods (기계적 합금화 공정으로 제조한 n형 $\textrm{Bi}_{2}(\textrm{Te}_{0.9}\textrm{Se}_{0.1})_3$ 가압소결체의 미세구조와 열전특성)

  • Kim, Hui-Jeong;Choe, Jae-Sik;Hyeon, Do-Bin;O, Tae-Seong
    • Korean Journal of Materials Research
    • /
    • v.7 no.1
    • /
    • pp.40-49
    • /
    • 1997
  • $Bi_{2}(Te_{0.9}Se_{0.1})_{3}$ thermoelectric matcrials havc 11et:n fahricxted hy mechanical alloying and hot pressing methods. Microstructure and thermoelectric properties of the hot 11resseii $Bi_{2}(Te_{0.9}Se_{0.1})_{3}$ have been investigated Lvith variations of hot pressing temperature and dopmt atltiition Formation of $Bi_{2}(Te_{0.9}Se_{0.1})_{3}$ alloy powders was completed by mechanical alloying of the as-mixed Ri. Te, arid Sc grmules of ~3.6mm size for 3 hours at ball-to-material weight ratio of 5 : 1. Figure of merit of $Bi_{2}(Te_{0.9}Se_{0.1})_{3}$ was markedly incrcwieti hy hot pressing at temperatures above $450^{\circ}C$, and value of $1.9{\times}10^{-3}/K$ was obtained for the specimen hot pressed at $550^{\circ}C$. With addition of 0.015 wt% Ri as acceptor dopant, figure of merit ol $Bi_{2}(Te_{0.9}Se_{0.1})_{3}$ hot pressed $550^{\circ}C$$2.1{\times}10^{-3}/K$.

  • PDF

Preparation and Toughening of Hot-Pressed SiC-AIN Solid Solutions

  • Lim, Chang-Sung
    • The Korean Journal of Ceramics
    • /
    • v.5 no.3
    • /
    • pp.224-229
    • /
    • 1999
  • The preparation and toughening of SiC-AIN solid solution from powder mixtures of $\beta$-SiC, AIN and $\alpha$-SiC by hot-pressing were studied in the 1870 to $2030^{\circ}C$ temperature range. The reaction of AIN and $\beta$-SiC(3C) powders causing transformation to the 2H(wurtzite) structure appeared to depend on hot-pressing temperatures and an additive of $\alpha$-SiC. For the composition of 49wt% SiC with 2 wt% $\alpha$-SiC and 47.5 wt% AIN47.5wt% SiC with 5 wt % $\alpha$-SiC at 203$0^{\circ}C$ for 1 h, th complete solid solutions with a single phase of 2H could be obtained. The appreciable amount of $\alpha$-SiC could develop the columnar inter-grains of 4H phase and the stable 2H phase with the relatively uniform composition and grain size distributions. The effect of $\alpha$-SiC on the phases present and compositional microstructures with columnar inter-grains was invetigated using X-ray diffraction, scanning electron microscopy and transmission electron microscopy. The fracture toughness and Vickers hardness of the hot-pressed solid solutions wre examined by the indentation-fracture-test method.

  • PDF

Cold Rolling Process for the Matrix Fabrication of the Mcfc (용융탄산염형 연료전지의 전해질 매트릭스에 관한 연구)

  • Park, Sang-Kill;Rho, Chang-Joo
    • Journal of the Korean Society of Fisheries and Ocean Technology
    • /
    • v.27 no.2
    • /
    • pp.125-131
    • /
    • 1991
  • Electrolyte matrix fabrication process can be classifed as hot pressing, tape casting, callendering, electrophoretic deposition. however, these have limits in practice. Hot pressing is cumbersome method, because of careful heating and cooling. Furthermore, the perfected tile is so fragile that it is difficult to fit in a cell. Therefore this method is not adequate for mass production of the electrolyte matrix. Using electrophoretic deposition method, a very thin matrix can be made, but many attempts of the electrolyte embeding were found to be failure. Tape casting and callendering methods are employed in most of the matrix fabrication for the present. But these methods require lots of water as a solvent, so that coating of the LiAlO sub(2) with electrolyte is difficult. Recently, hot roll milling method has been developed and the perfected matrix was proved to be free from crack. The method, however, needs a roller to make a matrix and a perfected matrix is carefully striped off from the cooled roller. Therefore, this method requires a long time due to the cooling process. The author proposes a cold rolling process. On this method, heated slurry of the LiAlO sub(2) mixed with binder, is rolled with a cold roller. The heated slurry dose not adhere to the roller, since contacted hot slurry is rapidly solidified. Therefore fabrication speed is increased, without getting rid of merits of the hot rolling process.

  • PDF

Phenol-Formaldehyde (PF) Resin Bonded Medium Density Fiberboard

  • Park, Byung-Dae;Riedl, Bernard;Park, Sang-Jin
    • Journal of the Korean Wood Science and Technology
    • /
    • v.27 no.1
    • /
    • pp.64-71
    • /
    • 1999
  • This study was conducted to manufacture MDF panels bonded with PF resins which provide excellent durability and dimensional stability with panels, and to identify benefits and weaknesses of using PF resins for MDF panels that have been manufactured with urea-formaldehyde (UF) resins for interior applications due to its low dimensional stability under moisture conditions. The results showed that the performance of PF-bonded MDF panels satisfied the performance requirement. A six-cycle aging test also revealed that PF-bonded MDF panels had high durability. Thickness swelling after 24 hours submersion in cold water was less than 2 percent, showing good dimentioanl stability. The identified weaknesses of using PF resins were relatively high resin content and long hot-pressing time. An acceptable resin content appeared to be 8 percent which can increase the production cost of PF-bonded MDF panels. The hot-pressing time (7 minutes) used in this study is relatively long compared to that of UF-bonded MDF panels. This result also indicates that hot-pressing process has to be optimized to control various pressing variables.