Jahant M. Sarwar;Chowdhury D.A. Nasima;Islam M. Khalidul;Mun Sung Phil
Journal of Korea Technical Association of The Pulp and Paper Industry
/
v.37
no.5
s.113
/
pp.41-49
/
2005
This paper deals the effect of anthraquinone (AQ) on the contribution of sulphidity in kraft pulping of sapwood. The pulping conditions namely- active alkali concentration, pulpingtime, temperature and liquor ratio were varied in low ($15\%$) and high ($30\%$) sulphidity. $0.1\%$ AQ was added in the low and high sulphidity pulping with varying active alkali concentration and cooking time. At optimum conditions, low sulphidity kraft process produced about $44\%$ pulp yield with kappa number of about 23. But in high sulphidity kraft process kappa number was reduced to about 20 at the same yield. An addition of AQ reduced alkali requirement by $2\%$ on oven dried raw material and cooking time by 1 hour to produce pulp yield of about $44\%$ at kappa number 20. AQ is more effective in low sulphidity pulping than the high sulphidity pulping. The breaking length of kraft-AQ pulp was slightly higher than that of kraft pulp.
Fig. 8 summarizes the present status of high yield pulp production and the directions of research on modification. A thick line indicates pulping process presently in use. As mentioned previously, one kind of modification is to introduce hydrophilic groups onto the pulp. Still unsolved is whether or not the introduction of hydrophilic groups should be restricted to lignin only. Goring (28) reported that middle lamella lignin has fewer phenolic hydroxyl groups than cell wall lignin and suggested that such a difference in the lignin may be useful in the removal of middle lamella lignin. The introduction of hydrophilic groups onto pulp may not be enough to modify high yield pulp. The removal of some portion of carbohydrate may be also necessary from the standpoint of softening of pulp fibers. There is no information at what lignin and carbohydrate, and how much should be removed. The combination with synthetic high polymers may also be important in modifying high yield pulp. Prof. C. Schuerch of the State University of New York who was a visiting professor at the University of Tokyo in 1974, mentioned that the hydrophilicity of lignin would be promoted, if phenolic hydroxyl or carboxyl groups could be introduced into the aromatic nucleus of lignin. If this were possible. this process would also mean a pulp yield of more than 100%. This idea is just one example of the expectation made possible through lignin chemistry. Instead of the introduction of hydrophilic group, the oxidative degradation of aromatic nucleus of lignin may also be useful in promoting the hydrophilicity of pulp. In this case, ozone may be an excellent chemical. However, there are a lot of problems to be solved such as homogeneity of reaction and selectivity of ozone for lignin. The above ideas are summarized in Fig. 9. There are many problems to be solved in the production of an excellent high yield pulp which is comparable to chemical pulp. The information from wood chemistry hopefully will elucidate some of the problems mentioned above.
Fines in high-yield sulfite pulp have much higher water retention value as compared with fines in Stone groundwood pulp. Therefore, they are apt to adhere partially or entirely onto the fiber surface during the paper making. This tendency is greatly enhance with decrease of the pretreated yield and increase of the water retention value of fines. Fines, which adhere onto the fiber surface in paper, contribute to the light scattering of the paper. Accordingly, the specific scattering coefficient of fines in high-yield sulfite pulp is considerably lower than that of fines in stone groundwood pulp, which hardly adhere onto the fiber surface. The fact that high-yield sulfite pulp is inferior to stone groundwood pulp in opacity is explained on the basis of the high degree of swelling of fined in addition to the softening of fiber fraction.
Proceedings of the Korea Technical Association of the Pulp and Paper Industry Conference
/
2006.06b
/
pp.295-303
/
2006
The pulp yield was improved by about 4.5-5% when polysulfide (PS) and anthraquinone (AQ) were added to the kraft cooking liquor (white liquor). The exchange of the black liquor with fresh white liquor further increased the yield. The highest pulp yield was obtained when the PS cooking liquor containing 70% of total active alkali (AA) and 100% of AQ was used from the beginning of the reaction and the black liquor was exchanged with fresh white liquor containing the residual 30% of AA just after temperature reached $135^{\circ}C$. There was a good correlation between kraft pulp yields of a hardwood species and the ratios of the amount of xylose to glucose (X/G ratio), liberated by an acid hydrolysis of the pulps. However, the correlation was dependent on raw material wood species. Therefore, it is required in advance to establish a correlation between the yields and X/G ratios for raw material wood species of a target pulp in order to estimate pulp yield using X/G ratio. The X/G ratios of relatively high yield pulps showed higher values than those expected from the correlation. In a mill trial, the superiority of the PS-AQ isothermal cooking (ITC) process over the kraft ITC process was confirmed by examining X/G ratio of pulps obtained. The pulp yield in the PS-AQ ITC process was estimated at about 57.0%. This yield is very high, which indicates that reaction conditions of the PS-AQ ITC process are optimal.
El-Sakhawy Mohamed;El-Ghorab Ahmed;El-Gendy Ahmed;El-Sabour Mona A.;El-Sayed Essam S. A.
Journal of Korea Technical Association of The Pulp and Paper Industry
/
v.37
no.5
s.113
/
pp.15-24
/
2005
Different types of antioxidants compounds were prepared economically from natural sources. Application of these compounds towards photo stabilization of high yield bagasse pulp has been investigated. It was found that potato peel antioxidant followed by clove volatile oil provides lower brightness reversion and better photo stabilization effect for paper made from high yield bagasse pulp after exposure to UV lights in comparison with butyl hydroxy anisol or chamomile volatile oil.
Journal of Korea Technical Association of The Pulp and Paper Industry
/
v.33
no.3
/
pp.75-83
/
2001
The potential of oxygen delignification is a powerful tool to reduce detrimental environmental effects. This study was performed to investigate the effect of steam explosion treatment of chemically treated oak wood on oxygen-alkali pulping. Pulp yield during steam explosion treatment by ${Na_2}{O_3}$-NaOH impregnation was higher than the other impregnation chemicals. Also, NaOH extraction at room temperature after steam explosion treatment improved the kappa number from 140~116 to 90~64. Oxygen-alkali pulping of chemical steam explosion treated woods affected to pulp yields. ${Na_2}{O_3}$-NaOH impregnation was very effective to higher carbohydrate yields at same delignification level. Its carbohydrate yield seemed to be highly related to the effluent pH. Oxygen-alkali pulping after steam explosion treatment of ${Na_2}{O_3}$-NaOH impregnated wood was shown that carbohydrate yield was very high because its effluent pH was increase from natural to mild alkali. Even if oxygen bleaching limit the delignification to 50% in order to avoid unacceptable yield and viscosity losses, oxygen-alkali pulping after steam explosion by ${Na_2}{O_3}$-NaOH impregnation was possible to extend the delignification more than 80%. Considering high pulp yield with lower lignin content from steam explosion treated wood, it might be profitable to end the cook at a high kappa number instead of a low kappa number, and continuously apply the oxygen delignification, in order to better quality pulp.
Journal of Korea Technical Association of The Pulp and Paper Industry
/
v.34
no.4
/
pp.22-29
/
2002
This research was conducted to investigate the morphological characteristics of fine fibers produced during beating process of high yield pulp treated with ozone and the distribution of lignin in the produced fine fibers. Thermomechanical(TMP) pulp and chemithermomechanical(CTMP) pulp of spruce and CTMP of white birch were beaten to reach 200$m\ell$ CSF, and then the fine fibers were observed using ultraviolet microscope. The fine fibers produced from TMP and CTMP of spruce using treated with ozone for 15 minutes were fragments of fiber surfaces or cell corners, and most of them contained lignin. However, lignin was not observed in the fibers after 15 minutes of ozone treatment. The fine fibers produced from CTMP of white birch were broken pieces or fragments of fiber surfaces or cell corners. The lignin was observed in the fibers until 5min of ozone treatment but no lignin was observed after 5 minutes of ozone treatment. Different morphological characteristics of TMP and CTMP explained both the different morphological characteristics and the distribution of lignin observed in the fine fibers produced from the beating process of TMP and CTMP treated with ozone.
This research has been examined to measure the degree of the fiber damage of ozonenation high yield pulp in the beating process. Ozone treated the TMP(Thermomechanical Pulp) and CTMP(Chemithermomechanical Pulp) of spruce and the CTMP of birch has been beaten to be reached 200ml(freeness) of its content. It had been studied the forming of fiber distribution by treatment for long fiber, short fiber, fine with the above method. As ozone treatment time gets longer, the pulp has showed the tendency of increasing the fiber content of 28, 48mesh. Ozone treated fiber has been increased long fiber content by being added softness. By given longer ozone treatment time, the TMP and CTMP of spruce has showed the decreasing of fiber content. On the contrary, CTMP of birch has showed the increasing its fiber content. It had proved that the results of difference are rather closer to the species of tree than closer to the kinds of pulp. The fiber content of over 200mesh which has created in beating process demonstrates the decreasing of its fiber content by getting longer ozone treatment time. The softness of fiber can be extracted by the lignin of fiber surface that had been formed by ozone treatment. Thus we assume that the fiber in the process of beating obtains less physical damage.
Journal of Korea Technical Association of The Pulp and Paper Industry
/
v.31
no.3
/
pp.77-82
/
1999
The delignification, and optical and strength properties were determined to compare the ozone treatment effect in hardwood and softwood CTMPs. During ozone treatment, the delignificantion was much higher in hardwood pulp than in softwood pulp . The optical and strength properties which were very dependent upon the lignin content in pulp were significantly improved in the case of hardwood pulp . The ozone treatment of high yield pulp was more effective in hardwood pulp than that of softwood pulp.
Enzymatic hydrolysis of cellulose was studied with emphasis on the effect of cellulase loading and pulp sludge concentration on glucose yield. Enzyme loading appeared to have a significant effect on glucose yield. Chemical pretreatment had no effect on enzymatic hydrolysis of pulp sludge. High glucose yield was obtained from enzymatic hydrolysis, especially at sludge concentrations lower than twenty percent. The optimum concentrations of crude cellulase and ${\beta}-glucosidase$ were 5 U/mL and 8 U/mL, respectively, considering the amount of enzymes used and glucose produced.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.