PLD 공정으로 제조된 LSM-YSZ 나노복합체층이 포함된 경사구조 박막 공기극을 적용한 SOFC의 성능 분석 (Performance of Solid Oxide Fuel Cell with Gradient-structured Thin-film Cathode Composed of Pulsed-laser-deposited Lanthanum Strontium Manganite-Yttria-stabilized Zirconia Composite)

  • 명두환;홍종일;황재연;이종호;이해원;김병국;조성걸;손지원
    • 한국세라믹학회지
    • /
    • 제48권6호
    • /
    • pp.487-492
    • /
    • 2011
  • The effect of the application of lanthanum strontrium manganite and yttria-stabilized zirconia (LSM-YSZ) nano-composite fabricated by pulsed laser deposition (PLD) as a cathode of solid oxide fuel cell (SOFC) is studied. A gradient-structure thin-film cathode composed of 1 micron-thick LSM-YSZ deposited at an ambient pressure ($P_{amb}$) of 200 mTorr; 2 micron-thick LSM-YSZ deposited at a $P_{amb}$ of 300 mTorr; and 2 micron-thick lanthanum strontium cobaltite (LSC) current collecting layer was fabricated on an anode-supported SOFC with an ~8 micron-thick YSZ electrolyte. In comparison with a 1 micron-thick nano-structure single-phase LSM cathode fabricated by PLD, it was obviously effective to increase triple phase boundaries (TPB) over the whole thickness of the cathode layer by employing the composite and increasing the physical thickness of the cathode. Both polarization and ohmic resistances of the cell were significantly reduced and the power output of the cell was improved by a factor of 1.6.

고에너지 밀링을 통한 Ni-BaCe0.9Y0.1O3-δ 서멧 멤브레인의 미세구조 균질성 향상 (Improved Microstructural Homogeneity of Ni-BCY Cermets Membrane via High-Energy Milling)

  • 김혜진;안기용;김보영;이종흔;정용재;김혜령;이종호
    • 한국세라믹학회지
    • /
    • 제49권6호
    • /
    • pp.648-653
    • /
    • 2012
  • Hybridization of dense ceramic membranes for hydrogen separation with an electronically conductive metallic phase is normally utilized to enhance the hydrogen permeation flux and thereby to increase the production efficiency of hydrogen. In this study, we developed a nickel and proton conducting oxide ($BaCe_{0.9}Y_{0.1}O_{3-{\delta}}$: BCY) based cermet (ceramic-metal composites) membrane. Focused on the general criteria in that the hydrogen permeation properties of a cermet membrane depend on its microstructural features, such as the grain size and the homogeneity of the mix, we tried to optimize the microstructure of Ni-BCY cermets by controlling the fabrication condition. The Ni-BCY composite powder was synthesized via a solid-state reaction using $2NiCO_3{\cdot}3Ni(OH)_2{\cdot}4H_2O$, $BaCeO_3$, $CeO_2$ and $Y_2O_3$ as a starting material. To optimize the mixing scale and homogeneity of the composite powder, we employed a high-energy milling process. With this high-energy milled composite powder, we could fabricate a fine-grained dense membrane with an excellent level of mixing homogeneity. This controlled Ni-BCY cermet membrane showed higher hydrogen permeability compared to uncontrolled Ni-BCY cermets created with a conventionally ball-milled composite powder.

내산화성 Cr-Si-Al합금의 주조상태 및 고온가열 후의 미세조직 특성 (Microstructural Characteristics of Oxidation Resistant Cr-Si-Al alloys in Cast State and after High Temperature Heating)

  • 김정민;김채영;양원철;박준식
    • 한국재료학회지
    • /
    • 제31권3호
    • /
    • pp.156-161
    • /
    • 2021
  • Cr-Si based alloys are not only excellent in corrosion resistance at high temperatures, but also have good wear resistance due to the formation of Cr3Si phase, therefore they are promising as metallic coating materials. Aluminum is often added to Cr-Si alloys to improve the oxidation resistance through which stable alumina surface film is formed. On the other hand, due to the addition of aluminum, various Al-containing phases may be formed and may negatively affect the heat resistance of the Cr-Si-Al alloys, so detailed investigation is required. In this study, two Cr-Si-Al alloys (high-Si & high-Al) were prepared in the form of cast ingots through a vacuum arc melting process and the microstructural changes after high temperature heating process were investigated. In the case of the cast high-Si alloy, a considerable amount of Cr3Si phase was formed, and its hardness was significantly higher than that of the cast high-Al alloy. Also, Al-rich phases (with the high Al/Cr ratio) were not found much compared to the high-Al alloy. Meanwhile, it was observed that the amount of the Al-rich phases reduced by the annealing heat treatment for both alloys. In the case of the high temperature heating at 1,400 ℃, no significant microstructural change was observed in the high Si alloy, but a little more coarse and segregated AlCr phases were found in the high Al alloy compared to the cast state.

Self-Cleaning and Photocatalytic Performance of TiO2 Coating Films Prepared by Peroxo Titanic Acid

  • Yadav, Hemraj M.;Kim, Jung-Sik
    • 한국재료학회지
    • /
    • 제27권11호
    • /
    • pp.577-582
    • /
    • 2017
  • Self-cleaning and photocatalytic $TiO_2$ thin films were prepared by a facile sol-gel method followed by spin coating using peroxo titanic acid as a precursor. The as-prepared thin films were heated at low temperature($110^{\circ}C$) and high temperature ($400^{\circ}C$). Thin films were characterized by X-ray diffraction(XRD), Field-emission scanning electron microscopy(FESEM), UV-Visible spectroscopy and water contact angle measurement. XRD analysis confirms the low crystallinity of thin films prepared at low temperature, while crystalline anatase phase was found the for high temperature thin film. The photocatalytic activity of thin films was studied by the photocatalytic degradation of methylene blue dye solution. Self-cleaning and photocatalytic performance of both low and high temperature thin films were compared.

고온 이산화탄소 분위기에서 316 L 스테인리스강의 부식 거동 (High-Temperature Corrosion Behavior of 316 L Stainless Steel in Carbon Dioxide Environment)

  • 채호병;서석호;정용찬;이수열
    • 한국재료학회지
    • /
    • 제27권10호
    • /
    • pp.552-556
    • /
    • 2017
  • Evaluation of the durability and stability of materials used in power plants is of great importance because parts or components for turbines, heat exchangers and compressors are often exposed to extreme environments such as high temperature and pressure. In this work, high-temperature corrosion behavior of 316 L stainless steel in a carbon dioxide environment was studied to examine the applicability of a material for a supercritical carbon dioxide Brayton cycle as the next generation power plant system. The specimens were exposed in a high-purity carbon dioxide environment at temperatures ranging from 500 to $800^{\circ}C$ during 1000 hours. The features of the corroded products were examined by optical microscope and scanning electron microscope, and the chemical compound was determined by x-ray photoelectron spectroscopy. The results show that while the 316 L stainless steel had good corrosion resistance in the range of $500-700^{\circ}C$ in the carbon dioxide environment, the corrosion resistance at $800^{\circ}C$ was very poor due to chipping the corroded products off, which resulted in a considerable loss in weight.

TiC-Mo 고용체 단결정의 고온 압축변형 특성 (Deformation Property of TiC-Mo Solid Solution Single Crystal at High Temperature by Compression Test)

  • 신순기
    • 한국재료학회지
    • /
    • 제24권11호
    • /
    • pp.625-631
    • /
    • 2014
  • To investigate the deformation properties of TiC-(5-20) mol% Mo solid solution single crystals at high temperature by compression testing, single crystals of various compositions were grown by the radio frequency floating zone technique and were deformed by compression at temperature from 1250K to 2270K at strain rates from $5.1{\times}10^{-5}$ to $5.9{\times}10^{-3}/s$. The plastic flow property of solid solution single crystals was found to be clearly different among a three-temperature range (low, intermediate and high temperature ranges) whose boundaries were dependent on the strain rate. From the observed property, we conclude that the deformation in the low temperature range is controlled by the Peierls mechanism, in the intermediate temperature range by the dynamic strain aging and in the high temperature range by the solute atmosphere dragging mechanism. The work softening tends to become less evident with an increasing experimental temperature and with a decreasing strain rate. The temperature and strain rate dependence of the critical resolved shear stress is the strongest in the high temperature range. The curves are divided into three parts with different slopes by a transition temperature. The critical resolved shear stress (${\tau}_{0.2}$) at the high temperature range showed that Mo content dependence of ${\tau}_{0.2}$ with temperature and the dependence is very marked at lower temperature. In the higher temperature range, ${\tau}_{0.2}$ increases monotonously with an increasing Mo content.

Improved Temperature Stability in Dielectric Properties of 0.8BaTiO3-(0.2-x)NaNbO3-xBi(Mg1/2Ti1/2)O3 Relaxors

  • Goh, Yumin;Kim, Baek-Hyun;Bae, Hyunjeong;Kwon, Do-Kyun
    • 한국세라믹학회지
    • /
    • 제53권2호
    • /
    • pp.178-183
    • /
    • 2016
  • Ferroelectric relaxor ceramics with $BaTiO_3-NaNbO_3-Bi(Mg_{1/2}Ti_{1/2})O_3$ ternary compositions (BT-NN-BMT) have been prepared by sol-gel powder synthesis and consequent bulk ceramic processing. Through the modified chemical approach, fine and single-phase complex perovskite compositions were successfully obtained. Temperature and frequency dependent dielectric properties indicated typical relaxor characteristics of the BT-NN-BMT compositions. The ferroelectric-paraelectric phase transition became diffusive when NN and BMT were added to form BT based solid solutions. BMT additions to the BT-NN solid solutions affected the high temperature dielectric properties, which might be attributable to the compositional inhomogeneity of the complex perovskite and resulting weak dielectric coupling of the Bi-containing polar nanoregions (PNRs). The temperature stability of the dielectric properties was good enough to satisfy the X9R specification. The quasi-linear P-E response and the temperature- stable dielectric properties imply the high potential of this ceramic compound for use in high temperature capacitors.

자전연소합성법에 의해 제조된 BaTiO3 분말의 소결특성에 미치는 첨가제의 영향 (The Effect of Adittives on the Sintering Properties of Barium Titanate Powder Prepared by Self-propagating High-temperature Synthesis)

  • 임성재;신창윤;원형일;원창환
    • 한국분말재료학회지
    • /
    • 제13권2호
    • /
    • pp.129-137
    • /
    • 2006
  • In this study, high purity fine $BaTiO_3$ powders were prepared by SHS (Self-propagating High-temperature Synthesis). We would examinate the study of sintering properties and characteristics as a function of temperature with various additives (binder, sintering agent). In separately binder addition, the green and sintered density of specimen were increased as binder content increases. The increased porosity resulted in fine grain size due to the inhibition of grain boundary moving. The $Al_{2}O_{3},\;TiO_{2}$ and MgO playa role of increasing dielectric constants at room temperature. These values were decreased at curie temperature. In case of $SiO_2$, the Curie temperature was decreased. In this study, a high dielectric ceramic capacitor material with temperature stability was synthesized by using various additives.

초고압을 이용한 나노급 마그네시아 분말의 저온 소결 연구 (Low Temperature Processing of Nano-Sized Magnesia Ceramics Using Ultra High Pressure)

  • 송정호;엄정혜;노윤영;김영욱;송오성
    • 한국세라믹학회지
    • /
    • 제50권3호
    • /
    • pp.226-230
    • /
    • 2013
  • We performed high pressure high temperature (HPHT) sintering for the 20 nm MgO powders at the temperatures from $600^{\circ}C$ to $1200^{\circ}C$ for only 5 min under 7 GPa pressure condition. To investigate the microstructure evolution and physical property change of the HPHT sintered MgO samples, we employed a scanning electron microscopy (SEM), density and Vickers hardness measurements. The SEM results showed that the grain size of the sintered MgO increased from 200 nm to $1.9{\mu}m$ as the sintering temperature increased. The density results showed that the sintered MgO achieved a more than 95% of the theoretical density in overall sintering temperature range. Based on Vickers hardness test, we confirmed that hardness increased as temperature increased. Our results implied that we might obtain the dense sintered MgO samples with an extremely short time and low temperature HPHT process compared to conventional electrical furnace sintering process.