Fiber Laser Welding in the Car Body Shop - Laser Seam Stepper versus Remote Laser Welding -

  • Kessler, Berthold
    • Journal of Welding and Joining
    • /
    • v.31 no.4
    • /
    • pp.17-22
    • /
    • 2013
  • The excellent beam quality of high power fiber lasers are commonly used for remote welding applications in body job applications. The Welding speed and productivity is unmatched with any other welding technology including resistance spot welding or traditional laser welding. High tooling cost for clamping and bulky safety enclosures are obstacles which are limiting the use. With the newly developed Laser stitch welding gun we have an integrated clamping in the process tool and the laser welding is shielded in a way that no external enclosure is needed. Operation of this laser welding gun is comparable with resistance spot welding but 2-times faster. Laser stitch welding is faster than spot welding and slower than remote welding. It is a laser welding tool with all the laser benefits like welding of short flanges, weld ability of Ultra High Strength steel, 3 layers welding and Aluminium welding. Together with low energy consumption and minimum operation cost of IPG fiber laser it is a new and sharp tool for economic car body assembly.

The Effects of GMAW Parameters on Penetration, Hardness and Microstructure of AS3678-A350 High Strength Steel

  • Kaewsakul, Nut;Putrontaraj, Rungsuk;Kimapong, Kittipong
    • International Journal of Advanced Culture Technology
    • /
    • v.3 no.1
    • /
    • pp.169-178
    • /
    • 2015
  • This research aims to study the effects of various welding parameters in gas metal arc welding (GMAW) process on welding penetration, microstructure and hardness of AS3578-A350 high strength steel with the thickness of 10 mm. The welding process parameters were a welding current of 100-200A, an arc voltage of 20-30V, a welding speed of 20-60 cm/min and a gas shielding type of Ar and $Ar+CO_2$. The summarized experimental results are as follows. An increase of the welding current and voltage affected to increase the penetration depth of the joint. However, when the welding speed was decreased, it increased the penetration depth of the joint. Using the Ar gas for shielding the weld area, produced the higher penetration depth and the less narrow weld bead than the joint that was shielded by the mix gas of $Ar+CO_2$. The variation of the welding process parameters affected to produce the various microstructures of weld metal and heat affected zone and also showed the various kind of hardness along the weld joint.

Laser Weldability and Formability of Hot Rolled Steels for Hydroforming Applications (하이드로포밍용 열연 강재의 레이저 용접성 및 성형 특성)

  • Lee Won-Beam;Lee Jong-Bong
    • Journal of Welding and Joining
    • /
    • v.22 no.6
    • /
    • pp.19-24
    • /
    • 2004
  • The laser welding and its analysis of thin-sheet carbon steels were carried out with high power $CO_{2}$ laser. The main factor of weld quality of laser welding is gap and edge quality. This work was preformed to focus on the gap tolerance problem during laser welding. First, bead on plate welding of thin sheet was examined to investigate the effect of laser welding variables, and to obtain optimum welding condition. Butt welding was also carried out to show the effect of gap on the laser weldability of thin sheet. In order to investigate the effect of gap on formability of welded thin sheet, LDH test was caried out. At high welding speed, the partial penetration was obtained by low heat input. Otherwise, porosity was formed in the bead at low weld speed because of too much heat input. The optimum welding condition of welding was derived from bead width, penetration and hardness property. The maximum gap tolerance on laser welding was observed to be about 0.2mm. This gap size has good relationship with beam size of laser spot(about 0.3mm). The formability of welded sheet was about $80{\%}$ value of base metal and the gap size has not affected on the formability, although weld quality is dependent on the gap size.

Observation of Nugget Formation Mechanism by using High Speed Camera (고속카메라를 이용한 저항 점 용접의 너겟 형성 메커니즘 관찰)

  • 조용준;이세헌
    • Proceedings of the KWS Conference
    • /
    • 2000.10a
    • /
    • pp.43-45
    • /
    • 2000
  • Resistance Spot Welding has been one of the important process in the sheet metal fabrication of auto-body industry It is well known that the nugget formation of RSW is the major factor for the strength of the body. A high speed camera was used to consider initial melting and growth of the weld nugget in order to find out the nugget formation mechanism. It was observed that such mechanism had an effect on the dynamic resistance, which was a process parameter of resistance spot welding. Also, the relationship between the mechanism and process parameter was considered for the industrial application.

  • PDF

Microstructure Evolution of UFG Steel Weld by Hybrid and Laser Welding (하이브리드 용접과 레이저 용접에 의한 세립강 용접부의 미세조직변화에 관한 연구)

  • Dong, H.W.;Lee, M.Y.;Ahn, Y.S.
    • Journal of Power System Engineering
    • /
    • v.14 no.3
    • /
    • pp.58-63
    • /
    • 2010
  • A laser beam welding and an electric arc welding were combined, and the positive points of each welding method are drawn such as high speed, low thermal load, deep penetration, and high productivity. The fiber laser-MIG conjugated welding. namely the hybrid welding has been studied mainly for the automation industry of a pipeline welding. In this study, the MIG welding was combined with a fiber laser welding to make up the hybrid welding. The weld shapes, microstructures and mechanical properties for weld zones after the hybrid welding or only fiber laser welding were investigated on the 700 MPa grade Ultra Fine Grained(UFG) high strength steel. The amount of acicular ferrite in weld metals and HAZ(heat affected zone) was observed larger after hybrid welding compared with after only laser welding. The Vickers hardness of the top area of the fusion zone after fiber laser welding was higher compared with after hybrid welding.

Fundamental Study on the Weld Defects and Its Real-time Monitoring Method (레이저 용접시 용접결함의 실시간 모니터링법 개발에 관한 연구)

  • 김종도
    • Journal of Welding and Joining
    • /
    • v.20 no.1
    • /
    • pp.26-33
    • /
    • 2002
  • This study was undertaken to obtain the fundamental knowledges on the weld deflects and it's realtime monitoring method. The paper describes the results of high speed photography, acoustic emission (AE) detection and plasma light emission (LE) measurements during $CO_2$ laser welding of STS 304 stainless steel and A5083 aluminum alloy in different welding condition. The characteristic frequencies of plasma and keyhole fluctuations at different welding speed and shield gases were measured and compared with the results of Fourier analyses of temporal AE and LE spectra, and they had considerably good agreement with keyhole and plasma fluctuation. Namely, the low frequency peaks of AE and LE shifted to higher frequency range with the welding speed increase, and leer the argon shield gas it was higher than that in helium and nitrogen gases. The low frequencies dominating in fluctuation spectra of LE probably reflect keyhole opening instability. It is possible to monitor the weld bead deflects by analyzing the acoustic and/or plasma light emission signals.

Mechanical properties of fine grained steel weldments formed with low heat input (세립강 저입열 용접부의 기계적 성질)

  • 윤중근;박태동;김광수;박영수
    • Proceedings of the KWS Conference
    • /
    • 2003.11a
    • /
    • pp.227-229
    • /
    • 2003
  • Low heat input welding methods have been investigated in order to minimize the HAZ softening of the 600MPa grade fine grained steel weldment. The welding processes of interest were a high speed FCA welding with a multi-torch welding system, laser welding with filler feeding and hybrid laser welding. No HAZ softening was found for all the weldments formed with low heat input less than 10kJ/cm. Tensile strength of the weldments was high enough to satisfy the required value. Impact toughness of the weldments was also good even at -20$^{\circ}C$.

  • PDF

Process Parameters of Butt Welding of SM45C using a Continuous Wave Nd:YAG Laser Beam (연속파형 Nd:YAG 레이저를 이용한 SM45C 맞대기 용접의 공정 변수)

  • 유영태;노경보;오용석;김종신;임기건
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.20 no.7
    • /
    • pp.44-55
    • /
    • 2003
  • The Nd:YAG laser process is known to have high speed and deep penetration capability to become one of the most advanced welding technologies. This paper describes the machining characteristics of SM45C carbon steel welding by use of an Nd:YAG laser. In spite of its good mechanical characteristics, SM45C carbon steel has a high carbon contents and suffers a limitation in the industrial application due to the poor welding properties. The major process parameters studied in the present laser welding experiment were position of focus, travel speed and laser power. Optical microscope and SEM were used to investigate the microstructures of the welded zone. The experimental results showed that penetration depth of the welding process increases with laser power. Both the microstructural investigation and the theoretical calculations indicated that materials undergoes a very high heating and cooling cycle during welding process. It was also found that the austenite nucleation takes place at the initial stage and the completion temperature of austenite transformation is much higher than in the case of the arc welding.

Effect of Process Parameters on Condenser Discharge Weldability of Thin Gauge Steel (박판 강재의 컨덴서 용접성에 미치는 용접변수의 영향)

  • 김기철;이목영;임태진
    • Journal of Welding and Joining
    • /
    • v.15 no.6
    • /
    • pp.49-56
    • /
    • 1997
  • Effect of process parameters on the quality of condenser discharge weld for coated sheet steels was discussed. The welding specimens were coated with pure Zn of 20/20 g/m2 in the production line. Direct measurements of welding parameters such as the discharge current, the pressures and the voltage drop across the electrodes were carried out with welding process monitoring system. High speed camera was also utilized to analyze the weld formation process. Test results indicated that the relation between weld strength and applied energy was stabilized at the acceptable welding heat input range. It was thought that the acceptable welding heat input should be redefined based on the monitored data because the calculated value of the welding heat input could hardly be utilized if the discharge condition was changed. Mechanical test results and high speed photographs showed that expulsion deteriorated the weld quality and the strength at the same time especially when the size of the spatter was large enough to carry the molten metal, which should form the nugget, out of the welding spot. Results also demonstrated that the discharge current should be applied at the appropriate time during the process because sufficient nugget was not produced if the time was deviated from the optimum range.

  • PDF

A Study on the $CO_2$ Laser Beam Welding of Thin Steel Sheets and Tailored Blanks - Between Similar Thin Sheet Materials - (박판의 $CO_2$레이저 빔 용접과 소재접합일체성형에 관한 연구- 동질 박판재간 -)

  • 이희석;배동호
    • Journal of Welding and Joining
    • /
    • v.15 no.2
    • /
    • pp.54-63
    • /
    • 1997
  • For the purpose of establishing laser welding condition (laser power, welding speed and beam focus) and of evaluating tailored blanks for two kinds of thin steel sheets SPCC and SK5M using in the thin plate structure such as automobile, train, and so on, investigated their $CO^2$ laser weldability under various initial welding conditions. SPCC thin sheet showed good weldability under some welding conditions. But, high carbon steel sheet SK5M needed heat treatment after welding to obtain ductility of the welded joint. And next, tailored blank was tested through deep drawing to evaluate reliability of their obtained laser welding conditions. The forming depths by tailored blank were SPCC+SPCC=22-25mm and SK5M+SK5M=13-25mm.

  • PDF