Effects of the Gap and the Speed on the Lap-Joint $CO_2$ Laser Welding of Automotive Steel Sheets (자동차용 강판의 겹치기 $CO_2$ 레이저 용접에서 용접속도와 판재간격에 따른 용접특성 연구)

  • 이경돈;박기영;김주관
    • Journal of Welding and Joining
    • /
    • v.20 no.4
    • /
    • pp.510-516
    • /
    • 2002
  • Recently the laser welding technology has been applied increasingly for the automotive bodies. But the lap joint laser welding for 3 dimensional automotive body is new while the butt joint laser welding is well known as the tailored blank technology. In this study, the process window was found for the full penetration welding of the lap joint of the 1mm-thick high strength steel sheets. The limit curves and characteristic curves were suggested to define the boundaries and the contour lines in a space of the welding speed and the gap size. The characteristics of the weld sectional geometry were used to determine the limit curves. They are bead width, penetration depth and sectional area. After the observed data was analysed carefully, it was noticed that there was a transition point at which the sectional shape was changed and the bead area jumped as the welding speed was increased. Also a new concept of 'input energy Per volume' was suggested to distinguish the difference at the transition Point. The difference of sectional areas at the transition point can be related to the dynamic keyhole phenomena.

Design and Operation Possibility of the Automatic Dynamic Balancer for the High Speed Rotating Chuck at the Friction Welding (마찰 용접용 고속 회전척의 ADB설계 및 작동성 연구)

  • Lee, Jong-Kil
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.18 no.6
    • /
    • pp.148-158
    • /
    • 2001
  • In this paper, Automatic Dynamic Balancer(ADB) was simulated and investigated to use at the high speed rotating chuck for the friction welding. In the limited computer simulations and experiments that have been presently carried out, several conclusions have been found. Above critical speed of the rotating system, ADB can balance the rotating disk. Therefore, it can be predicted that ADB can make an uniform flash during the friction welding.

  • PDF

Development of Laser Vision Sensor with Multi-line for High Speed Lap Joint Welding

  • Sung, K.;Rhee, S.
    • International Journal of Korean Welding Society
    • /
    • v.2 no.2
    • /
    • pp.57-60
    • /
    • 2002
  • Generally, the laser vision sensor makes it possible design a highly reliable and precise range sensor at a low cost. When the laser vision sensor is applied to lap joint welding, however. there are many limitations. Therefore, a specially-designed hardware system has to be used. However, if the multi-lines are used instead of a single line, multi-range data .:an be generated from one image. Even under a set condition of 30fps, the generated 2D range data increases depending on the number of lines used. In this study, a laser vision sensor with a multi-line pattern is developed with conventional CCD camera to carry out high speed seam tracking in lap joint welding.

  • PDF

Control of surface defects on plasma-MIG hybrid welds in cryogenic aluminum alloys

  • Lee, Hee-Keun;Chun, Kwang-San;Park, Sang-Hyeon;Kang, Chung-Yun
    • International Journal of Naval Architecture and Ocean Engineering
    • /
    • v.7 no.4
    • /
    • pp.770-783
    • /
    • 2015
  • Lately, high production rate welding processes for Al alloys, which are used as LNG FPSO cargo containment system material, have been developed to overcome the limit of installation and high rework rates. In particular, plasma-metal inert gas (MIG) hybrid (PMH) welding can be used to obtain a higher deposition rate and lower porosity, while facilitating a cleaning effect by preheating and post heating the wire and the base metal. However, an asymmetric undercut and a black-colored deposit are created on the surface of PMH weld in Al alloys. For controlling the surface defect formation, the wire feeding speed and nozzle diameter in the PMH weld was investigated through arc phenomena with high-speed imaging and metallurgical analysis.

Weldability with Process Parameters During Fiber Laser Welding of a Titanium Plate (II) - The Effect of Control of Heat Input on Weldability - (티타늄 판재의 파이버 레이저 용접시 공정변수에 따른 용접특성 (II) - 입열량 제어에 따른 영향 -)

  • Kim, Jong Do;Kim, Ji Sung
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.40 no.12
    • /
    • pp.1055-1060
    • /
    • 2016
  • Laser welding is a high-density energy welding method. Hence, deep penetration and high welding speed can be realized with lower heat input as compared with conventional welding. The heat input of a CW laser welding is determined by laser power and welding speed. In this study, bead and lap welding of $0.5mm^t$ pure titanium was performed using a fiber laser. Its weldability with laser power and welding speed was evaluated. Penetration, bead width, joining length, and bead shape were investigated, and the mechanical properties were examined through tensile-shear strength tests. Welds with sound joining length were obtained when the laser power and welding speed were respectively 0.5 kW and 2.5 m/min, and 1.5 kW and 6 m/min, and the weld obtained at low output presented better ductility than that obtained at high output.

Effect of Welding Condition on Microstructure of Transient Zone in Overlay Weld of 3Cr-1Mo Steel/STS-309L (3Cr-1Mo강/STS-309L 오버레이 용접부의 천이영역 조직에 미치는 용접조건의 영향)

  • 김동진;김병훈;지병하;김정태;김성곤;강정윤;박화순
    • Journal of Welding and Joining
    • /
    • v.18 no.2
    • /
    • pp.176-176
    • /
    • 2000
  • Recently developed Austenite stainless steel,309L was to overlay on 3Cr-1Mo-V-Ti-B steels, using Electroslag welding process, which wide electrodes were adopted. Transition region in welding interlayer relating to disbonding crack was investigated. Also. the effect of welding condition on the width of transition region and coarsening grains of the austenite were studied.1) With increasing welding speed the width of martensite at transient region was increased, but the amount of delta ferrite in weld metal was reduced, being fine grained.2) The form of martensite at the transition region was occured by reversible transition region, leading to increasing Ms point.3) With increasing welding speed, the grain of austenite formed at the welding interface was finer. With increasing welding current under the same welding speed, the grain size of the austenite was finer. At high current, original grain size of the austenite is coarse, but the austenite has fine grains because the austenite was transformed to martensite during cooling.4) In the case of high welding speed, the width of martensite at the welding interface was increased, but the grain size of austenite at the welding interface was finer. This indicates that the inhibition of disbonding crack may be achieved through dispersening fine carbides in the grain boudary.(Received August 3, 1999)

Effect of Welding Condition on Microstructure of Transient Zone in Overlay Weld of 3Cr-1Mo Steel/STS-309L (3Cr-1Mo강/STS-309L 오버레이 용접부의 천이영역 조직에 미치는 용접조건의 영향)

  • 김동진;김병훈;지병하;김정태;김성곤;강정윤;박화순
    • Journal of Welding and Joining
    • /
    • v.18 no.2
    • /
    • pp.49-56
    • /
    • 2000
  • Recently developed Austenite stainless steel, 309L was used to overlay on 3Cr-1Mo-V-Ti-B steels, using Electroslag welding process, which wide electrodes were adopted. Transition region in welding interlayer relating to disbonding crack was investigated. Also, the effect of welding condition on the width of transition region and coarsening grains of the austenite were studied. 1) With increasing welding speed the width of martensite at transient region was increased, but the amount of delta ferrite in weld metal was reduced, being fine grained. 2) The form of martensite at the transition region was occurred by reversible transformation during cooling since the interdiffusion of Cr and Ni from weld metal and Fe and C from base metals at the transition region, causes to lowering the concentration of Cr and Ni at the transition region, leading to increasing Ms point. 3) With increasing welding speed, the grain of austenite formed at the welding interface was finer. With increasing welding current under the same welding speed, the grain size of the austenite was finer. At high current, original grain size of the austenite is coarse, but the austenite has fine grains because the austenite was transformed to martensite during cooling. 4) In the case of high welding speed, the width of martensite at the welding interface was increased, but the grain size of austenite at the welding interface was finer. This indicates that the inhibition of disbonding crack may be achieved through dispersening fine carbides in the gain boundary.

  • PDF

A Study on the Feasibility of Partial Penetration Laser Welding for the Lap Joint of 390MPa High Strength Steel Sheets (390MPa급 고장력강판의 경치기 레이저 용접에서 부분용입 용접의 적용 가능성에 대한 연구)

  • 이경돈;박기영;김주관
    • Journal of Welding and Joining
    • /
    • v.20 no.2
    • /
    • pp.95-101
    • /
    • 2002
  • After high power lasers are avaliable in the commercial market, the number of applications of the laser welding has been increased in manufacturing industries. Although the tailored blank laser welding of butt jointed steel sheets is well known recently in the automotive industries, the lap joint laser welding is a new technology to the automotive manufacturing people as well as the design people. But the deep penetration laser welding seems to be preferred to the partial penetration welding for the lap joint welding in the automotive manufacturers because the partial penetration is a serious deflect for the butt joint. In this study, the feasibility of partial penetration welding fur the lap joint $CO_2$ laser welding was studied fur the 1mm thick 390MPa high strength steel sheets for automotive bodies. The process window of the lap joint partial penetration welding was obtained from experiments with the gap size and the welding speed as process parameters. The partial penetration welding was found excellent on the basis of the tensile shear strength and sectional geometry. The bead width, input energy Per volume, tensile-shear strength, deformation energy and the sectional geometries after tensile-shear tests of partial penetration welded specimens are compared with those of full penetration welded specimens with a series of gaps and welding speeds.

The Development of Welding Process to Prevent Porosity in MIG Welding of Al 6082-T6 (Al 6082-T6 MIG 용접에서 기공방지를 위한 용접공정 개발)

  • Baek, Sang-Yeub;Jung, Yon-Ho;Kim, Won-Il;Cho, Sang-Myung
    • Journal of Welding and Joining
    • /
    • v.28 no.6
    • /
    • pp.28-34
    • /
    • 2010
  • This paper was described on investigation to prevent porosity in high speed MIG Welding of Al 6082-T6. Porosity measurement was carried out by using image analysis of micrographs with the help of an analysis software. The main parameter was arc length and torch progressive angle. The porosity ratio was increased as arc length was increased. The arc length was increased depending upon the output voltage. By proper selection of pulse waveform parameter, the stable arc of one pulse one drop was generated. The porosity ratio of optimum condition in one pulse one drop was lower than high voltage condition. When torch progressive angle was an angle of advance $10^{\circ}$, porosity ratio was minium.