Studies on Relations between High Solid Coating and Quality Changes(II) - Effect of high solid coating on coated paper properties - (고농도 도공과 품질변화의 상관성 연구(2보) -도공지의 품질과 고농도 도공의 효과-)

  • Lee, Yong-Kyu;Yoo, Sung-Jong;Cho, Byoung-Uk;Kim, Yong-Sik
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.39 no.3
    • /
    • pp.52-59
    • /
    • 2007
  • This paper confirms that high solid coating can increase coating speed and reduce drying cost. Low solid coating color with the synthetic thickener and high solid coating color with the rheology modifier and with higher ratio of GCC were prepared. Coated paper was then produced with an industrial coater, varying coating speed and dryer temperature in order to keep the moisture content of the coated paper constant. Coating color concentration was able to be increased from 66% to 69% and from 68% to 71% without an adverse effect on coating color rheology. With a help of the rheology modifier, the increased ratio of GCC in high solid coating did not show harmful effects on the coated paper quality.

Studies on Relations between High Solid Coating and Quality Changes(I) - Effects of major process factors on coating color rheology - (고농도 도공과 품질변화의 상관성 연구(1보) -고농도 도공과 유변학적 인자에 대한 연구-)

  • Lee, Yong-Kyu;Yoo, Sung-Jong;Cho, Byoung-Uk;Kim, Yong-Sik
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.39 no.3
    • /
    • pp.41-51
    • /
    • 2007
  • In order to elucidate the effects of types and mixing ratio of GCC and clay, coating color concentration, and types of rheology modifiers on high solid coating, various coating colors were prepared, high shear viscosity was measured and then rheology of the coating colors was analyzed. Coating color concentration was able to be increased from 67% to 69% and from 68% to 71% with a higher GCC ratio and with the rheology modifier instead of the synthetic thickener, keeping similar or improved coating color rheology and coated paper quality. The rheological properties of high solid coating color were superior with smaller average particle sizes of clay and latex, wider size distribution of GCC and higher added amount of latex.

Effect of Latex Particle Size, Base Paper Grammage and Coating Color Concentration on Printing Quality of Coated Paper (Latex 입경과 원지 평량 및 칼라농도가 도공지의 인쇄품질에 미치는 영향)

  • Lee, Y.K.;Yoo, S.J.;Cho, B.U.;Kim, Y.S.;Nam, B.K.;Choi, S.M.
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.39 no.4
    • /
    • pp.29-37
    • /
    • 2007
  • The effects of latex particle size, basis weight of base paper and coating color concentration on the printing quality of coated paper were investigated. Coating colors were prepared with five types of latexes having different particle sizes. Coated papers were produced with high solid coating colors and with low solid coating colors in a industrial coater, respectively. In high solid coating colors, rheology modifier was used and GCC content was high. It was concluded that, in order to control binder migration and hence print mottle, latex particle sizes shall be controlled as well as formation, sizing degree and roughness of basis paper.

Enhanced Cathode/Sulfide Electrolyte Interface Stability Using an Li2ZrO3 Coating for All-Solid-State Batteries

  • Lee, Jun Won;Park, Yong Joon
    • Journal of Electrochemical Science and Technology
    • /
    • v.9 no.3
    • /
    • pp.176-183
    • /
    • 2018
  • In this study, a $Li_2ZrO_3$ coated $Li[Ni_{0.8}Co_{0.15}Al_{0.05}]O_2$ (NCA) cathode was applied to an all-solid-state cell employing a sulfide-based solid electrolyte. Sulfide-based solid electrolytes are preferable for all-solid-state cells because of their high ionic conductivity and good softness and elasticity. However, sulfides are very reactive with oxide cathodes, and this reduces the stability of the cathode/electrolyte interface of all-solid-state cells. $Li_2ZrO_3$ is expected to be a suitable coating material for the cathode because it can suppress the undesirable reactions at the cathode/sulfide electrolyte interface because of its good stability and high ionic conductivity. Cells employing $Li_2ZrO_3$ coated NCA showed superior capacity to those employing pristine NCA. Analysis by X-ray photoelectron spectroscopy and electron energy loss spectroscopy confirmed that the $Li_2ZrO_3$ coating layer suppresses the propagation of S and P into the cathode and the reaction between the cathode and the sulfide solid electrolyte. These results show that $Li_2ZrO_3$ coating is promising for reducing undesirable side reactions at the cathode/electrolyte interface of all-solid-state-cells.

Effect of High Solid Coating and Water Absorption Uniformity of Base Paper on Print Mottle - Evaluation of print mottle with PEA module - (고농도 도공과 원지의 흡수특성이 인쇄모틀에 미치는 영향 - PEA Module를 이용한 인쇄모틀 평가 -)

  • Yoo, Sung-Jong;Cho, Byoung-Uk;Kim, Yong-Sik;Lee, Yong-Kyu;Lee, Se-Hyun
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.39 no.2 s.120
    • /
    • pp.17-24
    • /
    • 2007
  • PEA(Print Evenness Analyzer) Module can be utilized as a tool to evaluate print mottle. The tester is de-signed to measure the uniformity of liquid penetration into paper at very short contact time. To evaluate effects of base paper properties on print mottle, the experiments were performed with 3 types of base pa-per whose sizing degree, roughness and porosity were varied. Coated papers were produced with high solid coating color (70%) and low solid coating color (67%). Uniformity of water absorption into base paper and coated paper was measured with PEA. It was found that, in order to minimize print mottle, base paper shall be produced with a high sizing degree and low roughness and the concentration of coating color shall be kept as high as possible, providing that it has proper rheology properties for coating process.

Evaluation of Protective Ability of High Solid Novolac Clear Coatings Through Electrochemical Techniques

  • Ramesh, D.;Shakkthivel, P.;Manickam, A. Susai;Kalpana, A.;Vasudevan, T.
    • Corrosion Science and Technology
    • /
    • v.5 no.2
    • /
    • pp.62-68
    • /
    • 2006
  • Solvent free high solid coatings are increasingly used as they posses number of advantages such as, lower cost per unit film thickness, better performance and eco-friendliness. In the present study polymeric film-forming materials such as aniline-novolac (ANS), cresol-novolac (CNS) and acrylic copolymer blended cresol-novolac (ACNS) coating materials have been prepared. The corrosion resistance properties of the prepared high solid coating materials have been evaluated through potential-time, potentiodynamic polarization and electrochemical impedance studies (EIS). Among the three coating systems, cresol-novolac polymer coated substrates offer better corrosion resistance property and the order of the performance was found as CNS > ACNS > ANS. We can recommend these systems for use in automobile applications.

Effect of Drying Condition of High Solid Coating on the Coated Paper Properties (고농도 도공의 건조조건이 도공지의 품질에 미치는 영향)

  • Yoo, Sung-Jong;Cho, Byoung-Uk;Lee, Yong-Kyu
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.42 no.1
    • /
    • pp.26-34
    • /
    • 2010
  • Effects of drying condition (IR radiation) on the optical properties and the printability of coated paper were elucidated at various latex sizes and low and high coating color concentrations. It was found that the smaller latex provided better rheology and higher dry and wet pick strength than the larger one. The high solids coating resulted in higher paper gloss and smaller roughness than the low solids coating, even though the clay addition was reduced by 20 parts in the high solids coating. Increasing IR radiation prohibited binder migration into the base paper. Thus it improved binder distribution and decreased pores in the coated layer, resulting in the increased dry and wet pick strength and the improved printing gloss. On the other hand, the color trapping and ink set-off was impaired with increasing IR radiation. Print mottle index passed through a maximum with increasing IR radiation.

Curing Reaction and Physical Properties of High-Solid Acrylic/Isocyanate Coatings (하이솔리드 아크릴/이소시아네이트 도료의 경화반응과 도막물성)

  • Park, Hong-Soo;Shim, Il-Woo;Jo, Hye-Jin;Kim, Seong-Kil;Kim, Myung-Soo
    • Journal of the Korean Applied Science and Technology
    • /
    • v.22 no.4
    • /
    • pp.371-378
    • /
    • 2005
  • In the previous study, three kinds of monomers and the functional monomer, acetoacetoxyethyl methacrylate (AAEM), which could improve the film property and cross-linkage, were polymerzied into acrylic resin copolymers (HSA-98-20, HSA-98-0, HSA-98+20) containing 80% solid content. In this study, the high-solid coatings(HSA-98-20C, HSA-98-0C, HSA-98+20C) were prepared by the curing reaction between acrylic resins containing 80% solid content and isocyanate at room temperature. Various properties were examined for the film coated with the prepared high-solid coatings. The introduction of AAEM in the coatings enhanced the abrasion resistance and solvent resistance of coatings, which indicated the possible use of high-solid coatings for top-coating materials of automobile. The curing times measured by viscoelastic measurement were 350, 264, and 212 min for HSA-98-20C, HSA-98-0C, and HSA-98+20C, respectively. This shows that the curing times become shorter with increasing $T_g$ values.

Conjugate Heat Transfer Analysis of High Pressure Turbine with Secondary Flow Path and Thermal Barrier Coating (2차유로 및 열차폐 코팅을 고려한 고압터빈의 열유동 복합해석)

  • Kang, Young-Seok;Rhee, Dong Ho;Cha, Bong Jun
    • The KSFM Journal of Fluid Machinery
    • /
    • v.18 no.6
    • /
    • pp.37-44
    • /
    • 2015
  • Conjugate heat analysis on a high pressure turbine stage including secondary flow paths has been carried out. The secondary flow paths were designed to be located in front of the nozzle and between the nozzle and rotor domains. Thermal boundary conditions such as empirical based temperature or heat transfer coefficient were specified at nozzle and rotor solid domains. To create heat transfer interface between the nozzle solid domain and the rotor fluid domain, frozen rotor with automatic pitch control was used assuming that there is little temperature variation along the circumferential direction at the nozzle solid and rotor fluid domain interface. The simulation results showed that secondary flow injected from the secondary flow path not only prevents main flow from penetrating into the secondary flow path, but also effectively cools down the nozzle and rotor surfaces. Also thermal barrier coating with different thickness was numerically implemented on the nozzle surface. The thermal barrier coating further reduces temperature gradient over the entire nozzle surface as well as the overall temperature level.

Tribological characteristics of WC/C multilayer films with various environments (WC/C 박막 코팅의 환경변화에 따른 트라이볼로지적 특성)

  • 이은성;김석삼;김종국
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 2001.11a
    • /
    • pp.78-87
    • /
    • 2001
  • The friction and wear behaviors of WC/C multilayer coating were investigated by using a pin on disk type tester. The experiment was conducted by using silicon nitride (S $i_{3}$ $N_{4}$) as a pin material and WC/C multilayer coating on bearing steel (STB2) as a disk material, under various environments that are atmospheric conditions of high vacuum( 1,3$\times$10$^{-4}$ Pa), medium vacuum( 1.3$\times$10$^{-l}$Pa). ambient air( 10$^{5}$ pa)(3 types) and relative humidity(2~98%) conditions. The results showed that WC/C coating fracture was suddenly increased with increasing degree of vacuum, because of high adhesion. So, WC/C coating could not be displayed their ability as solid lubricant. WC/C coating could be displayed better abilitv as solid lubricant with increasing relative humidity. because of oxide film, size and shape of wear debris. The friction coefficient and specific wear rate became better about RH 50%.%.