• Title/Summary/Keyword: High Alloy Steel

검색결과 446건 처리시간 0.026초

고합금강과 오스테나이트 스테인레스 강의 저사이클 피로 특성 연구 (Study on Characteristics of Low Cycle Fatigue for High Alloy and Austenite Stainless Steel)

  • 김용찬;백세현
    • 동력기계공학회지
    • /
    • 제14권6호
    • /
    • pp.29-34
    • /
    • 2010
  • As the steam temperature of fossil power plant boiler is increasing, the use of 9Cr-1Mo high alloy material is prevalent and it is needed to investigate the characteristics of low cycle fatigue for high alloy and austenite stainless steel that has used up to recently. As a result of test, in 9Cr-1Mo high alloy steel, the relation of strain and fatigue life is non-linear and the crack mode of low cycle fatigue is brittle but in the austenite stainless steel, that of strain and fatigue life is linear and the crack mode of low cycle fatigue is ductile. Comparing the fatigue life between high alloy and austenite stainless steel, there is no consistent characteristics as to strains. But the fatigue life of 9Cr-1Mo steel is longer by 25% than that of STS304 stainless steel in the relatively low, 0.3% strain. In the other strain, the fatigue life of two materials is similar.

초고장력강과 알루미늄 5052 소재의 클린칭 접합특성 (Joint characteristics of advanced high strength steel and A15052 alloy in the clinching process)

  • 이찬주;김재영;이상곤;고대철;;김병민
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2009년도 춘계학술대회 논문집
    • /
    • pp.401-404
    • /
    • 2009
  • The purpose of this study is investigating the joint characteristics of advanced high strength steel DP780 and Al5052 alloy sheet in the clinching process. It is difficult to join the advanced high strength steel with light-weight materials like aluminum alloy, because of low formability of DP780. The defects of clinching joint such as necking of the upper sheet, cracks of the lower sheet and no interlocking were occurred by different ductility between advanced high strength steel and aluminum alloy. The clinching conditions should be optimized to interlock without any defects. In this study, the effect of process parameters of clinching process on joinability of advanced high strength steel with Al5052 alloy was investigated by using FE-analysis. From the result of FE-analysis, the clearance between clinching punch and die, die depth and the shape of die cavity mainly affected the joinability of advanced high strength steel with Al5052 alloy.

  • PDF

용융합금도금 강판 적용 노측용 방호울타리 충돌 안전성 평가 해석 사례 연구 (A Simulation Case Study on Impact Safety Assessment of Roadside Barriers Built with High Anti-corrosion Hot-dip Alloy-coated Steel)

  • 노명현
    • 한국안전학회지
    • /
    • 제31권2호
    • /
    • pp.83-89
    • /
    • 2016
  • As the world's industrial development quickens, the highways and regional expressways have been expanding to serve the logistics and transportation needs of people. The burgeoning road construction has led to a growing interest in roadside installations. These must have reliable performance over long periods, reduced maintenance and high durability. Steel roadside barriers are prone to corrosion and other compromises to their functionality. Therefore, using high anti-corrosion steel material is now seen as a viable solution to this problem. Thus, the objective of this paper is to expand the scope of applications for high anti-corrosion steel material for roadside barriers. This paper assesses the impact safety such as structural performance, occupant protection performance and post-impact vehicular response performance by a simulation review on roadside barriers built with high strength anti-corrosion steel materials named as hot-dip zinc-aluminium-magnesium alloy-coated steel. The simulation test results for the roadside barriers built with high strength anti-corrosion steels with reduced sectional thickness meet the safety evaluation criteria, hence the proposed roadside barrier made by high strength and high anti-corrosion hot-dip zinc-aluminium-magnesium alloy-coated steel will be a good solution to serve safe impact performance as well as save maintenance cost.

TiN 코팅된 고속도강과 합금공구강의 마멸거동 (Wear Behavior of TiN Coatings Deposited on High Speed Steel and Alloy Tool Steel)

  • 김석삼;서창민;박준목
    • 대한기계학회논문집
    • /
    • 제19권3호
    • /
    • pp.705-712
    • /
    • 1995
  • The wear characteristics and wear mechanisms in TiN coating deposited on high speed steel and alloy tool steel by ion plating were investigated. Pin on V-block wear tester was used for a wear test method. The specimen was composed of three kinds of high speed steel and alloy tool steel which had different hardness by changing the heat treating condition. Three kinds of coating thickness were also applied to each specimen. Microscopic observation of worn surfaces was made by SEM. The scratch test of coating surface by the ion plating showed that critical load to break the coating interface was greater than 50N. The critical load increased with both substrate hardness and coating thickness. The wear resistance of TiN coated high speed steel became 10 times greater than that of non-coated ones. SEM observation showed that leading edge of contact was compressive and trailing edge was under maximum tensile stress and then surface cracking broke out perpendicular to sliding direction.

Constitutive Relation of Alloy Steels at High Temperatures

  • Lee, Young-Seog
    • International Journal of Precision Engineering and Manufacturing
    • /
    • 제6권4호
    • /
    • pp.55-59
    • /
    • 2005
  • This paper presents a feasibility study whether Shida's constitutive equation being widely used for plain carbon steel in steel manufacturing industry can be extended to alloy steels with a due carbon equivalent model. T,he constitutive relation of the alloy steels (SAE9254, AISI52100 and AISI4140) is measured using hot deformation simulator (GLEEBLE 3500C) at high temperatures ($800^{\circ}C{\~}1000^{\circ}C$) within strain rates of $0.05{\~}40\;s^{-1}$. It has been found the predicted flow stress behavior (constitutive relation) of AISI52100 steel is in agreement with the measured one. On the other hand, the measured flow stress behavior of SAE9254 and AISI4140 steel partly concords with the predicted one when material experiences relatively high strain rate ($10{\~}40\;s^{-1}$) deformation at low temperature ($800^{\circ}C$). It can be deduced that, for AISI52100 steel, Shida's equation with the carbon equivalent model can be applicable directly to the roughing and intermediate finishing stand in hot rolling process for calculating the roll force and torque.

Surface modification and induced ultra high surface hardness by nitrogen ion implantation of low alloy steel

  • Olofinjana, A.O.;Bell, J.M.;Chen, Z.
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2002년도 proceedings of the second asia international conference on tribology
    • /
    • pp.157-158
    • /
    • 2002
  • A surface hardenable low alloy carbon steel was implanted with medium energy (20 - 50KeV) $N_2^+$ ions to produced a modified hardened surface. The implantation conditions were varied and are given in several doses. The surface hardness of treated and untreated steels were measured using depth sensing ultra micro indentation system (UMIS). It is shown that the hardness of nitrogen ion implanted steels varied from 20 to 50GPa depending on the implantation conditions and the doses of implantation. The structure of the modified surfaces was examined by X-ray photoelectron spectroscopy (XPS). It was found that the high hardness on the implanted surfaces was as a result of formation of non-equilibrium nitrides. High-resolution XPS studies indicated that the nitride formers were essentially C and Si from the alloy steel. The result suggests that the ion implantation provided the conditions for a preferential formation of C and Si nitrides. The combination of evidences from nano-indentation and XPS, provided a strong evidence for the existence of $sp^3$ type of bonding in a suspected $(C,Si)_xN_y$ stoichiometry. The formation of ultra hard surface from relatively cheap low alloy steel has significant implication for wear resistance implanted low alloy steels.

  • PDF

Simultaneous Co-deposition of Zn-Mg Alloy Layers on Steel Strip by PVD Process

  • Kim, Tae-Yeob;Goodenough, Mark
    • Corrosion Science and Technology
    • /
    • 제10권6호
    • /
    • pp.194-198
    • /
    • 2011
  • This is the first release of an interim report on the development of coating technology of Zn-Mg alloy layers on steel strip by EML-PVD (electromagnetic levitation - physical vapor deposition) process in an air-to-air type continuous PVD pilot plant. It intends to introduce a basic principle of the EML-PVD process together with the high speed PVD pilot plant built in Posco. Due to the agitation effect provided by the high frequency induction coil, simultaneous evaporation of Zn and Mg from a droplet could produce alloy coating layers with Mg content of 6% to 12% depending on the composition of the droplet inside the coil. For its superior corrosion resistance, Zn-Mg alloy coated steel would be a very promising material for automotive, electrical appliances, and construction applications.

베어링강의 개발동향 (The Current Status of the Development of Bearing Steels)

  • 유선준
    • 소성∙가공
    • /
    • 제12권2호
    • /
    • pp.88-93
    • /
    • 2003
  • Several alloy bearing steels have been starting to replace for conventional high carbon and high chromium bearing steel since 1980. In this paper the global bearing developing trends were summarized in several important aspects- developments in alloy bearing steels for improved service life, development of inclusion rating method in bearing steel and developments in bearing service life testing.

알루미늄 합금의 미끄럼마모 특성에 미치는 상대재 경도의 영향 (Analysis of Sliding Wear Properties for Aluminum Alloy According to the Hardness Values of the Mating Tool Steel)

  • 이한영;조용재;김태준;박원규
    • Tribology and Lubricants
    • /
    • 제26권2호
    • /
    • pp.105-110
    • /
    • 2010
  • In order to investigate the wear behavior of aluminum alloy depended on different hardness of the mating tool steel, sliding wear tests were conducted. It was found that the wear characteristics pattern of aluminum alloy for sliding speed was not affected by the hardness of the mating tool steel. However, the effects of the hardness of the mating tool steel exhibited only in relatively low sliding speed ranges. At these ranges, the wear rate of aluminum alloy decreased when increasing the hardness of the mating tool steel. This was attributed by the fact that $Al_2O_3$ particles released from the aluminum worn surface were crushed and embedded on the mating worn surface with high hardness level. At the high sliding speed ranges, wear of aluminum alloy was hardly occurred by the formation of thick $Al_2O_3$ film on the worn surface, regardless of the hardness of the mating tool steel.

Mn-B 합금계 고강도 강의 동적 물성 (Dynamic Material Property of Mn-B Alloy High-Strength Steel)

  • 최창;홍성인
    • 한국정밀공학회지
    • /
    • 제13권11호
    • /
    • pp.124-131
    • /
    • 1996
  • The dynamic material property of Mn-B ally high-strength steel is investigated through the rod impact test which is one of simple test methods for the analysis of the material behavior under high-strain-rate. Rod impact test is performed to produce the deformed shape of rod and analyzed by the one-dimensional theory based on conservation law and the two-dimensional hydrocode AUTODYN-2D. The dynamic yield stress is determined and compared with the static yield stress to investigate the strain-rate sensitivity of Mn-B alloy high-strength steel.

  • PDF