구멍확장시험의 변형특성 및 활용성 연구 (Study on Deformation Characteristics of Hole Expansion Test and Its Applicability)

  • 한수식;이현영
    • 소성∙가공
    • /
    • 제28권3호
    • /
    • pp.154-158
    • /
    • 2019
  • The hole expansion tests using conical punch, flat punch or hemispherical punch are widely used for stretch flangeability verification of HSS. In this study, we investigate the strain distribution on the shear edges of the hole expansion test using grid marking and a projector. A small crack at the edge is distributed, resulting in a large gap between the HER and the crack strain. The strain distribution at the edges is irregular due to anisotropy of sheet metal. While an edge perpendicular to the rolling direction indicate a lower strain level compared to an edge parallel to the rolling direction, edge cracks occur at the edge perpendicular to the rolling direction. To predict the manifestation of edge cracks in FE analysis, the result of the hole expansion test with a crack strain measurement may well be a better tool than FLD. In this case, the level of strain and the direction of the edge relative to the rolling direction should be well considered.

내열강 용접부의 파괴강도 평가를 위한 Advanced Small Punch 시험에 관한 연구 (A Study on Advanced Small Punch Test for Evaluation of Fracture Strength in Heat Resisting Stell Weldment)

  • 이동환;이송인;권일현;유효선
    • Journal of Welding and Joining
    • /
    • 제20권6호
    • /
    • pp.99-99
    • /
    • 2002
  • In order to evaluate the proper fracture strength of microstructures in a steel weldment, smaller size loading ball than used for a conventional small punch(CSP) testing is required due to regional limitation on constitutive structures. In this study, the minimized loading ball(φ 1.5mm) and bore diameter of lower die(φ 3mm) were designed for an advanced small punch(ASP) test. The results obtained from the ASP test were compared with those from a CSP testing for a X20CrMoV121 steel weldment. It was found that the ASP test clearly showed the microstructural dependance on fracture strength and ductile-brittle transition behavior of the weldment. In the ASP test, especially, the cracks tend to initiate for various directions within hemispherical indentation region of an objective structure in SP test. This indicates that the evaluation of more proper fracture strength for F.L+CGHAZ, FGHAZ and ICHAZ can be performed by means of the ASP test in a steel weldment.

내열강 용접부의 파괴강도 평가를 위한 Advanced Small Punch 시험에 관한 연구 (A Study on Advanced Small Punch Test for Evaluation of Fracture Strength in Beat Resisting Steel Weldment)

  • 이동환;이송인;권일현;유효선
    • Journal of Welding and Joining
    • /
    • 제20권6호
    • /
    • pp.823-829
    • /
    • 2002
  • In order to evaluate the proper fracture strength of microstructures in a steel weldment, smaller size loading ball than used for a conventional small punch(CSP) testing is required due to regional limitation on constitutive structures. In this study, the minimized loading ball(${\varphi}1.5mm$) and bore diameter of lower die(${\varphi}3mm$) were designed for an advanced small punch(ASP) test. The results obtained from the ASP test were compared with those from a CSP testing for a X20CrMoV121 steel weldment. It was found that the ASP test clearly showed the microstructural dependance on fracture strength and ductile-brittle transition behavior of the weldment. In the ASP test, especially, the cracks tend to initiate for various directions within hemispherical indentation region of an objective structure in SP test. This indicates that the evaluation of more proper fracture strength for F.L+CGHAZ, FGHAZ and ICHAZ can be performed by means of the ASP test in a steel weldment.

유한요소법을 이용한 disk-brake piston의 공정설계 (Application of FEM to the Forming Process of Disk-Brake Piston)

  • 황병복;이호용
    • 소성∙가공
    • /
    • 제3권2호
    • /
    • pp.178-188
    • /
    • 1994
  • A design methodology is applied for manufacturing a disk-brake piston component. The design criteria are the limit drawing ratio and the forging load within the available press limit. Also, the final product should not have any geometrical defect. The rigid-plastic FEM has been applied to simulate the conventional four stage manufacturing processes, which include deep drawing and forging process. Simulation of one stage process from a selected stock to the final product shape is performed for generating information on additional requirements for metal flow. Two stage forming processes with different punch corner and nose geometries are also simulated to identify the possible best solutions. Finally, the best manufacturing process is selected, which is using a hemispherical punch int he deep drawing process.

  • PDF

금속판재의 성형성 평가를 위한 실험 및 유한요소해석에 관한 고찰 (Some Remarks on the Experiment and Finite Element Analysis to Evaluate to Forming Limit of Sheet Metals)

  • 곽인구;신용승;김형종;김헌영
    • 소성∙가공
    • /
    • 제9권4호
    • /
    • pp.379-388
    • /
    • 2000
  • This study aims to examine the influence of experimental and numerical factors on the results of the test and finite element simulation to evaluate the formability of sheet metals. The stretch-forming test with a hemispherical punch is carried out to obtain the limiting dome height (LDH) and forming limit diagram (FLD) for several kinds of aluminium and steel sheet. The results of the LDH and FLD tests are analysed to find any correlation with the uniaxial tensile properties. It proves that the size of the prescribed grid has great influence on the measured value of strain. The finite element analysis of the punch stretching process is also carried out and the result is compared with the experimental data. The influence of the numerical parameters such as friction coefficient, element size and anisotropy model on the simulation results tms out to be very considerable.

  • PDF

원통드로잉 성형에 있어서 Puckering 억제조건과 FEM-Simulation 해석 (On the Critical Tension Force and Analysis by the FEM for Puckering in the Cylindrical Cup-Drawing)

  • 후등학;임철록;정태훈
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1994년도 추계학술대회 논문집
    • /
    • pp.80-94
    • /
    • 1994
  • As for axisymmetirc sheet metal forming, a kind of pick-up apparatus for body-wrinkling is deviced. Experiments with both hemispherical and flat headed punches, with various clearances between punch and die, with respect to three kinds of materials each of which has two thicknesses, are performed. Firstly the process of evolution of body-wrinkling is observed. Then the critical blank-holding force (or meridional tensile force) for suppression of body-wrinkling at a specified punch-stroke is measured for all cases mentioned above. An empirical formula for it is proposed. Deformation patterns and stress distributions are analysed by the use of FEM. A simplified critical condition for body-wrinkling is formulated and introduced into the FEM program. And its effectiveness is checked by comparison with the experimental results. Using this FEM system, the governing factors of body-wrinkling are cleared up.

  • PDF

비대칭 시편의 딥드로잉 실험에 의한 박판금속의 성형한계도 (Identification of Forming Limits of Sheet Metals for Automobile Parts by Asymmetric Deep-drawing Experiments)

  • 허훈;이충호;정재웅
    • 소성∙가공
    • /
    • 제7권1호
    • /
    • pp.81-93
    • /
    • 1998
  • Identification of forming limits of sheet metals is an important task to be done before the sheet metal forming processes. The information of the forming limit is indispensable for design of deformed shapes and related forming processes. This procedure becomes more important than ever as the auto-body becomes complicated and the number of auto-body parts is reduced for lower production cost. To identify the forming limit of sheet metals stretching with a hemispherical punch has gained popularity because of the convenient experimental procedure. The stretching experiment however has localized deformation or the shear band is originated from the non-unifrom deformation in the critical circum-stance instead of the absolute criterion. More accurate information of the forming limit therefore could be obtained by a more appropriate experiment to the real process. In this papaer an experiment program is devised to practivally identify the forming limits of sheet metals for auto-body parts. The experiment program contains not only stretching but deep-drawing Both forming experiments use the same hemispherical punch while they use different specimens. Deep-drawing experiments use speci-mens cut out in circular arc on both sides of circular blank to make it torn during the deep-drawing They also use speciments cut out straight in one side of a circular blank to make it deformed unevenly which causes local deformation during the deep-drawing. The experimental result demonstrates that the forming limit diagrams in the two cases show difference in their effective magnitude. The forming limit curve from deep-drawing is located lower than that from stretching. It is noted from the result that the deep-drawing process causes acceleration of localized deformation in comparison with the stretching process. From the experimental result the maximum value of forming limit could be pre-dicted for safe design.

  • PDF

국소 가열 방법을 이용한 2단계 축대칭 디프 드로잉 공정의 해석 및 설계 (Finite Element Analysis Design of Axisymmetric Deep Drawing Process by Local Heating)

  • 이동우;송인섭;양동열
    • 한국정밀공학회지
    • /
    • 제10권3호
    • /
    • pp.198-204
    • /
    • 1993
  • The study is concerned with finite element analysis and design of axisymmetric deep drawing by local heating. When the bottom shape of a cup is not flat but in complex-shaped, i.e., hemispherical, the cup cannot be drawn in one or two processes in the conventional deep drawing process and the limit drawing ratio is limited as well. By introducing local heating selectively with regards to the heating position, the formability of the sheet metal can be greatly increased with the reduced number of processes. In the Process analysisthe rigid- viscoplastic finite element method is employed and the temperature effect is incorporated. Bishop's step-wise decoupled method is employed to analyze the thermomechanical interaction between deformation and heat transfer. Axisymmetric deep drawing of a hemisphere-bottomed cup has been analyzed for various combinations of heat application in the punch and the die. At the first stage of deep drawing stretch forming is practically carried out by firmly pressing the blankholder with the punch and the die heated at various levels of temperature. Then at the second stage the same cup is drawn for the saame or different combination of temperature. From the computation, it has thus been shown that the fromability of a cup is greatly increased in two-stage deep drawing with increased limet drawing ratio.

  • PDF

아몰퍼스 판재 성형의 스프링 백에 관한 연구 (A Study on Spring Back in Sheet Forming of Amorphous Alloys)

  • 윤상헌;이용신
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2005년도 춘계학술대회 논문집
    • /
    • pp.1757-1760
    • /
    • 2005
  • This paper is concerned with spring back after sheet forming of bulk amorphous alloys in the super cooled liquid state. The temperature-dependence and strain-rate dependence of Newtonian/non-Newtonian viscosities as well as the stress overshoot/undershoot behavior of amorphous alloys are reflected in the thermo-mechanical Finite Element simulations. Hemispherical deep drawing operations are simulated for various forming conditions such as punch velocity, die corner radius, friction, blank holder force, clearance and initial forming temperature. Here, spring back by an instantaneous elastic unloading was followed by thermal deformation during cooling and two modes of spring backs are examined in detail. It could be concluded that the superior sheet formability of an amorphous alloy can be obtained by taking the proper forming conditions for loading/unloading.

  • PDF

디프드로잉이 포함된 소성가공의 공정설계에 관한 연구 (A Study on the Process Sequence Design in Metal Forming including Deep Drawing)

  • 황병복;임중연;이호용
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1994년도 추계학술대회 논문집
    • /
    • pp.107-117
    • /
    • 1994
  • A design methodology is applied for manufacturing a disk-brake piston component and a washing machine container. The design criteria are the limit drawing ratio and the forging load within the available press limit. Also, the final product should not have any geometrical defect. The rigid-plastic and elastic-plastic FEM have been applied to simulate both of the conventional manufacturing processes, respectively, which include deep drawing and forging process. Simulations of one stage process from a selected stock to the final product shape are performed for generating information on additional requirements for metal flow. The best manufacturing processes are selected, which is using a hemispherical punch in the deep drawing process for both disk-brake piston component and washing machine container.

  • PDF