• 제목/요약/키워드: HIPing

검색결과 16건 처리시간 0.023초

Y2O3가 첨가된 Al2O3-TiC복합 소결체의 치밀화와 기계적 성질 (Sintering and Machanical Properties of Y2O3 Added Al2O3-TiC Composite)

  • 최종선;박상엽;김득중;강석중
    • 한국세라믹학회지
    • /
    • 제26권3호
    • /
    • pp.438-444
    • /
    • 1989
  • The role of TiC and the effect of Y2O3 addition on the densification, microstructure and mechanical properties of Al2O3-TiC composite have been studied. The amount of Y2O3 has been varied from 0 to 2 wt.% while keeping the TiC content at 10, 20 or 30 wt.%. The powder compacts have been sintered at 1,75$0^{\circ}C$ for various times in 1 atm Ar atmosphere and hot isostatically pressed (HIPed) at 1,$600^{\circ}C$ for 0.5h under 1,500atm Ar. Considerable increase in sintered density(over 95%) has been achieved by adding 0.5 wt.% Y2O3 in specimens containing high TiC volume. More addition of Y2O3 does not affect the densification. With increasing the sintering time from 0.5 to 4h, slight increase in density results. The growth of Al2O3 grain has been enhanced by Y2O3 addition ; this tendency is reduced with increasing TiC content because of grain boundary dragging effect of TiC particles. The hardness of specimens increases considerably by an addition of 0.5wt.% Y2O3 owing to the density increase. Further addition of Y2O3 has no effect on hardness. Fracture toughness augments with TiC content by crack deflection around the particles. By adding 0.5wt.% Y2O3, all the specimens can be densified to isolated pore stage and thus can be HIPed to full densification and better mechanical property. In particular, the fracture toughness of Al2O3-30 TiC specimen increases about 50% by HIPing. Fully dense Al2O3-30 TiC with good mechanical properties can be prepared by normal Sintering/HIPing process.

  • PDF

열간정수압소결(HIP)시킨 Y-Ba-Cu-O 초전도체의 조직과 특성 (Microstructure and Prooperties of Y-Ba-Cu-O Superconductor Fabricated by Hot Isostatic Pressing)

  • 신미남;백수현;송진태
    • 한국세라믹학회지
    • /
    • 제26권2호
    • /
    • pp.267-275
    • /
    • 1989
  • YBa2Cu3O7-x oxide superconductors were fabricated by sintering and hotisostatic pressing (HIP), and their microstructures and properties were compared with each other. Thougha part of the second phase was observed along grain boundaries, their structures were consisted of single (123) phase and they had many porosities. But, porosities were remakably reduced by Hiping and the densification was brought about. The structure of (123) compound also showed a number of twins, which are typical of high Tc superconductors. The on-set temperature of YBa2Cu3O7-x compound sintered at 96$0^{\circ}C$ in oxygen and hipped at 88$0^{\circ}C$ was highest, but that shwoed 0 resistance at 87$^{\circ}$K, which is a little lower than the compound sintered at 96$0^{\circ}C$. HIP treatment also increased the critical current density of as-sintered compound. However, its value was low, which may be ascribed to the many pores of starting-sintered compact and partially to the second phase along grain boundaries.

  • PDF

Plasma-Sprayed $Al_2O_3-SiO_2$ Multi-Oxide Films on Stainless Steel Substrate

  • Korobova, N.;Soh, Deawha
    • 한국항해항만학회:학술대회논문집
    • /
    • 한국항해항만학회 2000년도 추계학술대회논문집
    • /
    • pp.116-119
    • /
    • 2000
  • The advantage of plasma-sprayed coating is their good resistance against thermal shock due to the porous state of the coated layer with a consequently low Youngs modulus. However, the existence of many pores with a bimodal distribution and a laminar structure in the coating reduces coating strength and oxidation protection of the base metals. In order to counteract these problems, there have been many efforts to obtain dense coatings by spraying under low pressure or vacuum and by controlling particle size and morphology of the spraying materials. The aim of the present study is to survey the effects of the HIP treatment between 1100 and 130$0^{\circ}C$ on plasma-sprayed oxide coating of A1$_2$O$_3$, A1$_2$O$_3$-SiO$_2$on the metal substrate (type C18N10T stainless steel). These effects were characterized by phase identification, Vickers hardness measurement, and tensile test before and after HIPing. These results show that high-pressure treatment has an advantage for improving adhesive strength and Vickers hardness of plasma-sprayed coatings.

  • PDF

Development of Powder Injection Molding Process for Fabrication of Glass Component

  • Lin, Dongguo;Lee, Junghyun;Park, Seong Jin
    • 한국분말재료학회지
    • /
    • 제23권1호
    • /
    • pp.26-32
    • /
    • 2016
  • Powder injection molding (PIM), which combines the advantages of powder metallurgy and plastic injection molding technologies, has become one of the most efficient methods for the net-shape production of both metal and ceramic components. In this work, plasma display panel glass bodies are prepared by the PIM process. After sintering, the hot isostatic pressing (HIP) process is adopted for improving the density and mechanical properties of the PIMed glass bodies. The mechanical and thermal behaviors of the prepared specimens are analyzed through bending tests and dilatometric analysis, respectively. After HIPing, the flexural strength of the prepared glass body reaches up to 92.17 MPa, which is 1.273 and 2.178 times that of the fused glass body and PIMed bodies, respectively. Moreover, a thermal expansion coefficient of $7.816{\times}10^{-6}/^{\circ}C$ is obtained, which coincides with that of the raw glass powder ($7.5-8.0{\times}10^{-6}/^{\circ}C$), indicating that the glass body is fully densified after the HIP process.

Plasma-Sprayed $Al_{2}O_{3}-SiO_{2}$ Multi-Oxide Films on Stainless Steel Substrate

  • Korobova, N.;Soh, Deawha
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 추계학술대회 논문집
    • /
    • pp.116-119
    • /
    • 2000
  • The advantage of plasma-sprayed coating is their good resistance against thermal shock due to the porous state of the coated layer with a consequently low Youngs modules. However, the existence of many pores with a bimodal distribution and a laminar structure in the coating reduces coating strength and oxidation protection of the base metals. In order to counteract these problems, there have been many efforts to obtain dense coatings by spraying under low pressure or vacuum and by controlling particle size and morphology of the spraying materials. The aim of the present study is to survey the effects of the HIP treatment between 1100 and 130$0^{\circ}C$ on plasma-sprayed oxide coating of A1$_2$O$_3$, A1$_2$O$_3$-SiO$_2$ on the metal substrate (type C18N10T stainless steel). These effects were characterized by phase identification, Vickers hardness measurement, and tensile test before and after HIPing, These results show that high-pressure treatment has an advantage for improving adhesive strength and Vickers hardness of plasma- sprayed coatings.

  • PDF

IN738LC 초내열합금에서 미세조직과 고온 피로수명에 미치는 고온등압압축(HIP) 공정의 영향 (Effects of Hot Isostatic Pressing on the Microstructure and High-Temperature Fatigue Life of the Ni-base Superalloy IN738LC)

  • 최철;김두수;이영찬;박영규;김길무;김재철
    • 한국재료학회지
    • /
    • 제10권2호
    • /
    • pp.128-137
    • /
    • 2000
  • 가스터빈 블레이드 재료로 사용되는 IN738LC 니켈기 초합금 주조재에 대하여 고온등압압축(HIP) 공정에 의한 미세조직 변화와 고온 피로수명에 미치는 영향을 조사하였다. 세부적으로 HIP 처리에 따른 주조결함 제거와 피로변형 열화재의 물성재생효과 확인에 중점을 두었으며, 이를 위하여 회전굽힘 피로시험을 실시하고 변형전후의 미세조직을 광학 및 주사전자현미경으로 관찰하였다. HIP 처리 전후의 미세조직과 피로수명을 비교, 평가한 결과, 주조재와 열처리재의 피로수명 차는 크지 않았으나 HIP 처리재의 피로수명은 이들과 비교하여 평균 60배 이상 증가한 것으로 나타났다. 또한 인위적으로 고온 피로변형을 가한 열화재를 대상으로 반복 HIP 처리한 결과, 열화 변형조직이 신재 상태로 거의 완전히 재생될 뿐만 아니라, 재료내에 미세하게 잔존하던 주조결함까지 부가적으로 제거됨에 따라 반복 HIP 처리에 의한 피로수명 연장 효과가 크게 나타났다.

  • PDF