• 제목/요약/키워드: Glazed zirconia

검색결과 6건 처리시간 0.017초

Resin bonding of metal brackets to glazed zirconia with a porcelain primer

  • Lee, Jung-Hwan;Lee, Milim;Kim, Kyoung-Nam;Hwang, Chung-Ju
    • 대한치과교정학회지
    • /
    • 제45권6호
    • /
    • pp.299-307
    • /
    • 2015
  • Objective: The aims of this study were to compare the shear bond strength between orthodontic metal brackets and glazed zirconia using different types of primer before applying resin cement and to determine which primer was more effective. Methods: Zirconia blocks were milled and embedded in acrylic resin and randomly assigned to one of four groups: nonglazed zirconia with sandblasting and zirconia primer (NZ); glazed zirconia with sandblasting, etching, and zirconia primer (GZ); glazed zirconia with sandblasting, etching, and porcelain primer (GP); and glazed zirconia with sandblasting, etching, zirconia primer, and porcelain primer (GZP). A stainless steel metal bracket was bonded to each target surface with resin cement, and all specimens underwent thermal cycling. The shear bond strength of the specimens was measured by a universal testing machine. A scanning electron microscope, three-dimensional optical surface-profiler, and stereoscopic microscope were used to image the zirconia surfaces. The data were analyzed with one-way analyses of variance and the Fisher exact test. Results: Group GZ showed significantly lower shear bond strength than did the other groups. No statistically significant differences were found among groups NZ, GP, and GZP. All specimens in group GZ showed adhesive failure between the zirconia and resin cement. In groups NZ and GP, bonding failed at the interface between the resin cement and bracket base or showed complex adhesive and cohesive failure. Conclusions: Porcelain primer is the more appropriate choice for bonding a metal bracket to the surface of a full-contour glazed zirconia crown with resin cement.

Orthodontic bracket bonding to glazed full-contour zirconia

  • Kwak, Ji-Young;Jung, Hyo-Kyung;Choi, Il-Kyung;Kwon, Tae-Yub
    • Restorative Dentistry and Endodontics
    • /
    • 제41권2호
    • /
    • pp.106-113
    • /
    • 2016
  • Objectives: This study evaluated the effects of different surface conditioning methods on the bond strength of orthodontic brackets to glazed full-zirconia surfaces. Materials and Methods: Glazed zirconia (except for the control, Zirkonzahn Prettau) disc surfaces were pre-treated: PO (control), polishing; BR, bur roughening; PP, cleaning with a prophy cup and pumice; HF, hydrofluoric acid etching; AA, air abrasion with aluminum oxide; CJ, CoJet-Sand. The surfaces were examined using profilometry, scanning electron microscopy, and electron dispersive spectroscopy. A zirconia primer (Z-Prime Plus, Z) or a silane primer (Monobond-S, S) was then applied to the surfaces, yielding 7 groups (PO-Z, BR-Z, PP-S, HF-S, AA-S, AA-Z, and CJ-S). Metal bracket-bonded specimens were stored in water for 24 hr at $37^{\circ}C$, and thermocycled for 1,000 cycles. Their bond strengths were measured using the wire loop method (n = 10). Results: Except for BR, the surface pre-treatments failed to expose the zirconia substructure. A significant difference in bond strengths was found between AA-Z ($4.60{\pm}1.08MPa$) and all other groups ($13.38{\pm}2.57-15.78{\pm}2.39MPa$, p < 0.05). For AA-Z, most of the adhesive remained on the bracket. Conclusions: For bracket bonding to glazed zirconia, a simple application of silane to the cleaned surface is recommended. A zirconia primer should be used only when the zirconia substructure is definitely exposed.

Glazing 횟수가 전장지르코니아에 미치는 굴곡강도와 표면 미세구조의 변화 (A study of the changes in the strength and microstructure of the zirconia crown surface by the glazing number)

  • 오선미
    • 대한치과기공학회지
    • /
    • 제43권2호
    • /
    • pp.35-41
    • /
    • 2021
  • Purpose: This study aimed to investigate the flexural strength and surface microstructure of the zirconia crown according to the number of glazing zirconia prostheses. Methods: The specimens were made as follows. A specimen without glazing: 1ea, first glazed specimens (group B): 10ea, second glazed specimens (group C): 10ea, third glazed specimens (group D): 10ea. Three-point measuring strength equipment and electron microscopes were used for strength measurement and microstructure observation. As for statistical analysis, one-way ANOVA and t-test (level of significance level=5%) were used to determine the difference in the change in flexural strength according to the number of glazing zirconia prostheses. Results: ANOVA analysis of groups B (1st glazing), C (2nd glazing), and D (3rd glazing) revealed that the change in strength between the groups is statistically significant (p=0.023). The Mann-Whitney test for each group revealed that the difference in flexural strength between groups B and C was not statistically significant (z=-0.302, p=0.762) while that between groups C and D was statistically significant (z=-0.257, p=0.01). Microstructure observation revealed 3 changes in the microstructure of the surface of the glaze powder were observed. Conclusion: According to the number of glazing zirconia prostheses, it was found that the difference in strength between groups was statistically significant, and changes in the microstructure were observed.

Simulated occlusal adjustments and their effects on zirconia and antagonist artificial enamel

  • Alfrisany, Najm Mohsen;Shokati, Babak;Tam, Laura Eva;De Souza, Grace Mendonca
    • The Journal of Advanced Prosthodontics
    • /
    • 제11권3호
    • /
    • pp.162-168
    • /
    • 2019
  • PURPOSE. The aim of this study was to evaluate the effect of occlusal adjustments on the surface roughness of yttria-tetragonal zirconia polycrystal (Y-TZP) and wear of opposing artificial enamel. MATERIALS AND METHODS. Twenty-five Y-TZP slabs from each brand (Lava, 3M and Bruxzir, Glidewell Laboratories) with different surface conditions (Control polished - CPZ; Polished/ground - GRZ; Polished/ground/repolished - RPZ; Glazed - GZ; Porcelain-veneered - PVZ; n=5) were abraded (500,000 cycles, 80 N) against artificial enamel (6 mm diameter steatite). Y-TZP roughness (in ${\mu}m$) before and after chewing simulation (CS) and antagonist steatite volume loss (in $mm^3$) were evaluated using a contact surface profilometer. Y-TZP roughness was analyzed by three-way analysis of variance (ANOVA) and steatite wear by two-way ANOVA and Tukey Honest Difference (HSD) (P=.05). RESULTS. There was no effect of Y-TZP brand on surface roughness (P=.216) and steatite loss (P=.064). A significant interaction effect (P<.001) between surface condition and CS on Y-TZP roughness was observed. GZ specimens showed higher roughness after CS (before CS - $3.7{\pm}1.8{\mu}m$; after CS - $13.54{\pm}3.11{\mu}m$), with partial removal of the glaze layer. Indenters abraded against CPZ ($0.09{\pm}0.03mm^3$) were worn more than those abraded against PVZ ($0.02{\pm}0.01mm^3$) and GZ ($0.02{\pm}0.01mm^3$). Higher wear caused by direct abrasion against zirconia was confirmed by SEM. CONCLUSION. Polishing with an intraoral polishing system did not reduce the roughness of zirconia. Wear of the opposing artificial enamel was affected by the material on the surface rather than the finishing technique applied, indicating that polished zirconia is more deleterious to artificial enamel than are glazed and porcelain-veneered restorations.

Comparison of the translucency of shaded zirconia all-ceramic systems

  • Kurtulmus-Yilmaz, Sevcan;Ulusoy, Mutahhar
    • The Journal of Advanced Prosthodontics
    • /
    • 제6권5호
    • /
    • pp.415-422
    • /
    • 2014
  • PURPOSE. The purpose of this study was to evaluate and compare the translucency of shaded zirconia allceramic systems. MATERIALS AND METHODS. Translucency of 3 different zirconia all-ceramic systems colored by different techniques was compared with a lithium disilicate glass-ceramic (IPS e.max Press). Square-shaped specimens with 0.5 mm thickness were fabricated from In-Ceram YZ, ICE Zirkon and Katana systems in A1, A2 and A3.5 shades according to Vitapan Classical shade tab (n=11). Specimens were then veneered and glazed with corresponding veneer ceramic recommended by each zirconia system manufacturer and the total thickness was set to 1.5 mm. Translucency measurements were performed with VITA Easyshade Compact spectrophotometer after each stage and translucency parameter was calculated. Data were statistically analyzed with repeated measures ANOVA and Tukey multiple comparison test. RESULTS. The control group was significantly more translucent than the zirconia systems (P<.05). ICE Zirkon cores showed the least translucency; neither In-Ceram YZ nor Katana systems were superior to each other in terms of translucency. Translucency of all specimens was decreased after veneering, and the translucency rankings were changed. CONCLUSION. Coloring technique did not have a significant effect on translucency of zirconia cores. Although zirconia systems were less translucent than lithium disilicate glass ceramic, they had partial translucency and there were translucency differences among the zirconia systems. Chroma affected the translucency of precolored zirconia cores.

Surface treatment, liquid, and aging effects on color and surface properties of monolithic ceramics

  • Sertac Sariyer;Meryem Gulce Subasi
    • The Journal of Advanced Prosthodontics
    • /
    • 제16권3호
    • /
    • pp.174-188
    • /
    • 2024
  • PURPOSE. The purpose of this study was to investigate the effects of surface treatments, liquids, and aging on color, translucency, and surface properties of monolithic ceramics. MATERIALS AND METHODS. Lithium disilicate (LDS) and zirconia-reinforced lithium silicate (ZLS) ceramics (n = 135 each) were cut and divided into three groups [crystallization+glaze (single stage), crystallization-glaze (two stages), and crystallization-polish (two stages)]. One sample from each group was examined using scanning electron microscopy (SEM). Remaining samples were divided into four subgroups (distilled water, coffee, grape juice, and smoothie) (n = 11 each), stored for 12 d in the respective liquids, and thermally aged. One sample from each subgroup was analyzed using SEM. The color, gloss, and roughness values of the samples were analyzed after surface treatment (initial) and storage under different liquids+aging conditions. The initial data and both the aged data and data change values were analyzed using robust two- and three-way analyses of variance. RESULTS. The glazed groups exhibited smoother surfaces. Ceramic type and ceramic-surface treatment interactions affected the initial translucency parameter (TP) (P < .001) and the initial and aged roughness values (P ≤ .001). Surface treatment type affected the color change (P < .001), and ceramic type affected the aged TP values (P < .001). Type of ceramic, surface treatment, and their interactions affected both the initial and aged gloss (P ≤ .001) and TP change values (P ≤ .015). Surface treatment type and ceramic-surface treatment interactions affected the gloss change values (P ≤ .001). CONCLUSION. Although both ceramics and all surface treatments are clinically applicable, crystallization-glaze is recommended. When gloss and smoothness are important or when translucency is important, ZLS or LDS may be preferred, respectively.