사상 이론을 이용한 파이프 원주 용접의 온도 분포 예측에 관한 연구 (A Study on Prediction of Temperature Distribution in Pipe Girth Welding by Mapping Theory)

  • 조영태;나석주
    • 대한기계학회논문집A
    • /
    • 제24권12호
    • /
    • pp.2935-2944
    • /
    • 2000
  • Gas tungsten arc(GTA) welding is used to rrpiar the seat ring in swing type check valve in power plant because of its high weld quality. In order to automate the welding process, it is needed to analyze the process of inside pipe girth welding. In this study, the shapes of weld bead on pipe inside and outside were predicted and its validity was investigated. On the assumption that the welding arc had a bivariate gaussian distribution, analytical solution was derived to predict the temperature distribution in pipe weld using mapping under consideration of physical relationships. The size of weld bean could be predicted from this equation and its accuracy was verified by experiments.

가스배관에서 원주 및 심 용접부의 부식손상 부위에 대한 파열압력 평가 (The Evaluation of Burst Pressure for Corroded Weld in Gas Pipeline)

  • 김영표;김우식;오규환
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2004년도 추계학술발표대회 개요집
    • /
    • pp.165-167
    • /
    • 2004
  • The failure pressure for corroded pipeline was measured by burst testing and classified with respect to corrosion sizes and corroded regions - the body, the girth weld and the seam weld of pipe. A series of finite element analyses were performed to obtain a limit load solution for corrosion defects on the basis of burst test. As a result, the criteria for failure assessment of corrosion defect within the body, the girth weld and the seam weld of API 5L X65 gas pipeline were proposed.

  • PDF

가스배관 용접부위 부식에 대한 파열압력 평가 (The Evaluation of Burst Pressure for Corroded Weld in Gas Pipeline)

  • 김영표;김우식;이영광;오규환
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2004년도 춘계학술대회
    • /
    • pp.222-227
    • /
    • 2004
  • The failure assessment for corroded pipeline has been considered with the full scale burst test and the finite element analysis. The burst tests were conducted on 762 mm diameter, 17.5 mm wall thickness and API 5L X65 pipe that contained specially manufactured rectangular corrosion defect. The failure pressure for corroded pipeline was measured by burst testing and classified with respect to corrosion sizes and corroded regions - the body, the girth weld and the seam weld of pipe. Finite element analysis was carried out to derive failure criteria of corrosion defect on the pipe. A series of finite element analyses were performed to obtain a limit load solution for corrosion defects on the basis of burst test. As a result, the criteria for failure assessment of corrosion defect within the body, the girth weld and the seam weld of API 5L X65 gas pipeline were proposed.

  • PDF

입열량이 고변형률 강관 원주 용접부 특성에 미치는 영향 (Effect of Heat Input on Girth welds properties of High strain steel pipe)

  • 이진우;송우현;서동한;이종섭
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2010년도 춘계학술발표대회 초록집
    • /
    • pp.71-71
    • /
    • 2010
  • SBD (Strain-based design) of pipe lines have gained world-wide attention in recent years. The present research aims to evaluate the fracture characteristics of API (America Petroleum Institute) SBD X100 girth weldment that typically applied for cold climate and deep water offshore, with the focus on the influence of heat input changing with 6kJ/cm and 10kJ/cm from GMAW (Gas Metal Arc Welding). At a low heat input at 6kJ/cm, the weld metal had Multi-phase matrix (Acicular ferrite + Banite + Martensite) that could fill up both fracture toughness and strength as reported previously. Also, the weld metal exhibited 859MPa YS (Yield strength), 108J impact toughness at $-40^{\circ}C$ and 0.52mm CTOD (Crack Tip Open Displacement) at $-10^{\circ}C$. These results can be satisfied with the requirement of API SBD X100 girth weldment and Alaska pipe line project.

  • PDF

입열량이 고변형률 강관 원주 용접부 특성에 미치는 영향 (Effect of Heat Input on Girth Welds Properties of High Strain Steel Pipe)

  • 이진우;송우현;서동한;이종섭
    • Journal of Welding and Joining
    • /
    • 제27권6호
    • /
    • pp.25-30
    • /
    • 2009
  • SBD (Strain-based design) of pipe lines have gained world-wide attention in recent years. The present research aims to evaluate the fracture characteristics of API (America Petroleum Institute) SBD X100 girth weldment that typically applied for cold climate and deep water offshore, with the focus on the influence of heat input changing with 6kJ/cm and 10kJ/cm from GMAW (Gas Metal Arc Welding). At a low heat input at 6kJ/cm, the weld metal had Multi-phase matrix (Acicular ferrite + Banite + Martensite) that could fill up both fracture toughness and strength as reported previously. Also, the weld metal exhibited 859MPa YS (Yield strength), 108J impact toughness at $-40^{\circ}C$ and 0.52mm CTOD (Crack Tip Open Displacement) at $-10^{\circ}C$. These results can be satisfied with the requirement of API SBD X100 girth weldment and Alaska pipe line project.

원주 용접된 압력 매설강관의 거동 분석 (Behavior of girth-welded buried steel pipes under external pressure)

  • Jeon, Juntai;Lee, Chinhyung;Chang, Kyongho
    • 한국재난정보학회 논문집
    • /
    • 제11권1호
    • /
    • pp.1-8
    • /
    • 2015
  • 본 연구에서는 토압 등의 외압이 원주 용접된 매설 강관의 잔류응력에 미치는 영향을 유한요소 해석을 통하여 명확히 하였다. 먼저 3차원 열탄소성 해석을 통하여 원주 용접된 강관의 잔류응력을 구하였으며, 이를 초기조건으로 설정하여 3차원 탄소성 해석을 수행함으로써 외압이 작용하는 경우 잔류응력 거동을 조사하였다. 해석결과 외압에 의해 원주 용접부에 발생하는 원주방향 압축응력 때문에 원주방향 잔류응력이 압축 측으로 상당히 많이 이동함을 알 수 있었고, 축방향 잔류응력은 작용하는 외압에 의해 거의 영향을 받지 않음을 알 수 있었다.

가중함수법을 적용한 파이프라인 구조건전성평가에 관한 연구 (A Study on Structural Integrity Assessment of Pipeline using Weight Function Solution)

  • 노기섭;오동진;김명현
    • Journal of Welding and Joining
    • /
    • 제35권1호
    • /
    • pp.55-60
    • /
    • 2017
  • There are many Industry Code and Standard (ICS) for Structural Integrity Assessment (SIA) on welded structure with defect. The general ICSs, such as R6, BS 7910 and API 579-1/ASME FFS-1, provide equations to determine the upper bound residual stress profiles based on collections from many literatures. However, these residual stress profiles used in the SIA cause the conservative design for welded structures. In this study, the structural integrity assessment for girth weld in pipeline has been conducted based on fracture mechanics. In addition, thermo-elastic plastic FE analysis was performed for evaluating the residual stress of girth weld in pipeline. The weight function solution is used to determine the stress intensity factor using the residual stress profile obtained by the FE analysis. This approach can account for redistribution and relaxation of residual stress as the defects grow. In order to the evaluate quantitative comparison between BS 7910 and weight function solution, structural integrity assessment determining allowable crack size on cracked pipe was performed with failure assessment diagram.

Influence of ultrasonic impact treatment on microstructure and mechanical properties of nickel-based alloy overlayer on austenitic stainless steel pipe butt girth joint

  • Xilong Zhao;Kangming Ren;Xinhong Lu;Feng He;Yuekai Jiang
    • Nuclear Engineering and Technology
    • /
    • 제54권11호
    • /
    • pp.4072-4083
    • /
    • 2022
  • Ultrasonic impact treatment (UIT) is carried out on the Ni-based alloy stainless steel pipe gas tungsten arc welding (GTAW) girth weld, the differences of microstructure, microhardness and shear strength distribution of the joint before and after ultrasonic shock are studied by microhardness test and shear punch test. The results show that after UIT, the plastic deformation layer is formed on the outside surface of the Ni-based alloy overlayer, single-phase austenite and γ type precipitates are formed in the overlayer, and a large number of columnar crystals are formed on the bottom side of the overlayer. The average microhardness of the overlayer increased from 221 H V to 254 H V by 14.9%, the shear strength increased from 696 MPa to 882 MPa with an increase of 26.7% and the transverse average residual stress decreased from 102.71 MPa (tensile stress) to -18.33 MPa (compressive stress), the longitudinal average residual stress decreased from 114.87 MPa (tensile stress) to -84.64 MPa (compressive stress). The fracture surface has been appeared obvious shear lip marks and a few dimples. The element migrates at the fusion boundary between the Ni-based alloy overlayer and the austenitic stainless steel joint, which is leaded to form a local martensite zone and appear hot cracks. The welded joint is cooled by FA solidification mode, which is forming a large number of late and skeleton ferrite phase with an average microhardness of 190 H V and no obvious change in shear strength. The base metal is all austenitic phase with an average microhardness of 206 H V and shear strength of 696 MPa.

원자력 발전 주기기 제작에 적용되는 용접공정 (Welding process for manufacturing of Nuclear power main components)

  • 정인철;김용재;심덕남
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2010년도 춘계학술발표대회 초록집
    • /
    • pp.43-46
    • /
    • 2010
  • As the nuclear power plant has been constructed continuously for several decades in Korea, the welding technology for components manufacturing and installation has been improved largely. Standardization for weld test and qualification was also established systematically according to the concerned code. The welding for the main components requires the high reliability to keep the constant quality level, which means the repeatability of weld quality. Therefore the weld process qualified by thorough test and evaluation is able to be applied for manufacturing. Narrow gap SAW and GTAW process are usually applied for girth seam welding of pressure vessel like Reactor vessel, steam generator, and etc. For the surface cladding with stainless steel and Inconel material, strip welding process is mainly used. Inside cladding of nozzles is additionally applied with Hot wire GTAW and semi-auto welding process. Especially the weld joint having elliptical weld line on curved surface needs a specialized weld system which is automatically rotating with adjusting position of the head torch. The small sized pipe, tube, and internal parts of reactor vessel requests precise weld processes like an automatic GTAW and electron beam welding. Welding of dissimilar materials including Inconel690 material has high possibility of weld defects like a lack of fusion, various types of crack. To avoid these kinds of problem, optimum weld parameters and sequence should be set up through the many tests. As the life extension of nuclear power plant is general trend, weld technologies having higher reliability is required gradually. More development of specialized welding systems, weld part analysis and evaluation, and life prediction for main components should be taken into a consideration extensively.

  • PDF