• 제목/요약/키워드: Gas Pressure Sintering

검색결과 88건 처리시간 0.025초

비정형 기둥 형상을 가진 나노구조에서의 가스 투과성 실험 연구 (Permeability of the Lateral Air Flow through Unstructured Pillar-like Nanostructures)

  • 김혜원;임혜원;박정우;이상민;김형모
    • Tribology and Lubricants
    • /
    • 제39권5호
    • /
    • pp.197-202
    • /
    • 2023
  • Recently, research on experimental and analytical techniques utilizing microfluidic devices has been pursued. For example, lab-on-a-chip devices that integrate micro-devices onto a single chip for processing small sample quantities have gained significant attention. However, during sample preparation, unnecessary gases can be introduced into the internal channels, thus, impeding device flow and compromising specific function efficiency, including that of analysis and separation. Several methods have been proposed to mitigate this issue, however, many involve cumbersome procedures or suffer from complexities owing to intricate structures. Recently, some approaches have been introduced that utilize hydrophobic device structures to remove gases within channels. In such cases, the permeability of gases passing through the structure becomes a crucial performance factor. In this study, a method involving the deposition and sintering of diluted Ag-ink onto a silicon wafer surface is presented. This is followed by unstructured nano-pattern creation using a Metal Assisted Chemical Etching (MACE) process, which yields a nanostructured surface with unstructured pillar shapes. Subsequently, gas permeability in the spaces formed by these surface structures is investigated. This is achieved by experiments conducted to incorporate a pressure chamber and measure gas permeability. Trends are subsequently analyzed by comparing the results with existing theories. Finally, it can be confirmed that the significance of this study primarily lies in its capability to effectively evaluate gas permeability through unstructured pillar-like nanostructures, thus, providing quantitative values for the appropriate driving pressure and expected gas removal time in practical device operation.

Effect of Sinter/HIP Technology on Properties of TiC-NiMo Cermets

  • Kollo, Lauri;Pirso, Juri;Juhani, Kristjan
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.627-628
    • /
    • 2006
  • The present work is a study on the argon gas pressure effects of Sinter/HIP sintering on microstructure and strength of different grades of TiC-NiMo cermets. Titanium carbide in the composition of different grades of TiC-NiMo cermets was ranged from 40 to 80 wt.% and the ratio of nickel to molybdenum in the initial powder composition was 1:1, 2:1 and 4:1 respectively. On the sintered alloys, the main strength characteristic, transverse rupture strength (TRS) was measured. Furthermore, the microstructure parameters of some alloys were measured and the pressure effect on pore elimination was evaluated. All the results were compared with common, vacuum sintered alloys. The TRS values of TiC-NiMo cermets could be considerably improved by using Sinter/HIP technique, for high-carbide fraction alloys and for alloys sintered at elevated temperatures.

  • PDF

Recent advances in natural gas hydrate carriers for gas transportation - A review and conceptual design

  • Kim, Kipyoung;Kim, Youtaek;Kang, Hokeun
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제38권5호
    • /
    • pp.589-601
    • /
    • 2014
  • Natural gas hydrate (NGH) is emerging as a new eco-friendly source of energy to replace fossil fuels in the 21st century. It is well known that the Natural Gas Hydrate contains large amount of natural gas about 170 times as much as its volume and it is easy to be stored and transported safely at about $-20^{\circ}C$ under atmospheric pressure due to so called "self-preservation effect". The option of gas transport by gas hydrate pellets carrier has been investigated and developed in various industry and academy. The natural gas hydrate pellet carrier is on major link in a potential gas hydrate process chain, starting with the extraction of natural gas from the reservoir, followed by the production of hydrate pellets and the transportation to an onshore terminal for further processing or marketing. In recent years, Korean project team supported by Korean Government has been working on the development of NGH total systems including novel NGH carrier since 2011. In order to increase the knowledge on the NGH pellet carrier developed and to understand the major hazards that could have significant impact on the safety of the vessel, this paper presents and evaluates the pros and cons of cargo holds, loading and unloading systems through the analysis of current patent technology. Based on the proven and well-known technologies as well as potential measures to mitigate sintering and minimize mechanical stress on the hydrate pellet in the self-preservation state, this study presents the conceptual and basic design for NGH carrier.

자기펄스성형이 적용된 Ti-Mn-Cu 합금의 미세구조 및 기계적 특성 (Microstructure and Mechanical Property of Ti-Mn-Cu Alloys with Magnetic Pulsed Compaction)

  • 윤예준;박천웅;최원준;변종민
    • 한국분말재료학회지
    • /
    • 제28권1호
    • /
    • pp.20-24
    • /
    • 2021
  • Ti-based alloys are widely used in biomaterials owing to their excellent biocompatibility. In this study, Ti-Mn-Cu alloys are prepared by high-energy ball milling, magnetic pulsed compaction, and pressureless sintering. The microstructure and microhardness of the Ti-Mn-Cu alloys with variation of the Cu addition and compaction pressure are analyzed. The correlation between the composition, compaction pressure, and density is investigated by measuring the green density and sintered density for samples with different compositions, subjected to various compaction pressures. For all compositions, it is confirmed that the green density increases proportionally as the compaction pressure increases, but the sintered density decreases owing to gas formation from the pyrolysis of TiH2 powders and reduction of oxides on the surface of the starting powders during the sintering process. In addition, an increase in the amount of Cu addition changes the volume fractions of the α-Ti and β-Ti phases, and the microstructure of the alloys with different compositions also changes. It is demonstrated that these changes in the phase volume fraction and microstructure are closely related to the mechanical properties of the Ti-Mn-Cu alloys.

Al-Si-SiC 복합분말과 Al-Zn-Mg계 합금분말이 혼합된 분말의 소결 거동 및 기계적 특성연구 (Investigation on the Sintering Behavior and Mechanical Properties of Al-Zn-Mg Alloy Powders Mixed with Al-Si-SiC Composite Powders)

  • 장광주;김경태;양상선;김용진;박용호
    • 한국분말재료학회지
    • /
    • 제21권6호
    • /
    • pp.460-466
    • /
    • 2014
  • Al-Si-SiC composite powders with intra-granular SiC particles were prepared by a gas atomization process. The composite powders were mixed with Al-Zn-Mg alloy powders as a function of weight percent. Those mixture powders were compacted with the pressure of 700 MPa and then sintered at the temperature of $565-585^{\circ}C$. T6 heat treatment was conducted to increase their mechanical properties by solid-solution precipitates. Each relative density according to the optimized sintering temperature of those powders were determined as 96% at $580^{\circ}C$ for Al-Zn-Mg powders (composition A), 97.9% at $575^{\circ}C$ for Al-Zn-Mg powders with 5 wt.% of Al-Si-SiC powders (composition B), and 98.2% at $570^{\circ}C$ for Al-Zn-Mg powders with 10 wt.% of Al-Si-SiC powders (composition C), respectively. Each hardness, tensile strength, and wear resistance test of those sintered samples was conducted. As the content of Al-Si-SiC powders increased, both hardness and tensile strength were decreased. However, wear resistance was increased by the increase of Al-Si-SiC powders. From these results, it was confirmed that Al-Si-SiC/Al-Zn-Mg composite could be highly densified by the sintering process, and thus the composite could have high wear resistance and tensile strength when the content of Al-Si-SiC composite powders were optimized.

Si$_3$N$_4$ Whisker의 첨가량과 배열방향이 Si$_3$N$_4$ 복합 소결체의 기계적 특성에 미치는 영향 (Effect of the Whisker Amount and Orientation on Mechanical Properties of the Si$_3$N$_4$ based Composites)

  • 김창원;박동수;박찬
    • 한국세라믹학회지
    • /
    • 제36권1호
    • /
    • pp.43-49
    • /
    • 1999
  • 0~5 wt%의 $\beta$-Si3N4 whisker를 첨가한 질화규소 가스압 소결체를 제작하였다. 첨가된 whisker들은 tape casting을 응용하여 tape 내에서 일방향으로 배열하였으며, 제작된 tape로부터 절취된 sheet들의 적층 과정을 변화하여 다양한 미세구조를 갖는 성형체를 제작하였다. 가스압 소결을 통하여 치밀화된 소결체의 조대결정립은 성형체의 whisker와 같은 방향성을 가졌으며, 소결수축률과 기계적 특성 등도 이러한 다양한 미세구조상의 특징과 일관된 결과를 나타내었다. Whisker를 일방향으로 배열하였을 경우, 소결수축률은 whisker 배열 방향과 평행한 방향보다 수직한 방향으로 크게 일어났을 때, whisker 함량이 증가함에 따라 수축률의 차이가 증가하였다. Indentationi crack length는 whisker 함량이 증가함에 따라 whisker 배열 방향과 수직한 방향의 균열 길이는 더 짧아졌고, 그와 평행한 방향의 균열 길이는 길어졌다. Whisker 첨가에 의해 결정립이 더 크게 성장하였으나 강도는 whisker를 첨가하지 않을을때보다 낮지 않았다. Whisker 배열 방향을 90$^{\circ}$ 및 45$^{\circ}$ 간격으로 엇갈리게 적층하였을 경우에는 특성의 이방성이 나타나지 않았다.

  • PDF

사출성형용 Stellite미분말의 소결 치밀화에 관한 연구 (A Study on the Densifcation of Stellite Fine Powder for Iniection Molding)

  • 임태환
    • 한국분말재료학회지
    • /
    • 제4권2호
    • /
    • pp.113-121
    • /
    • 1997
  • The densification of the compacts of Co+32%Cr+20%W+l.5%C, Co+32%Cr+20%W+3.0%C and Co+32%Cr+20%W+4.5%C sintered under $H_2$ gas or vacuum was investigated. The effect of V and B addition on the densification was also investigated. The densification of these compacts were always incomplete regardless of sintering atmosphere, temperature and time. The amounts of oxygen and carbon in compacts sintered in $H_2$ for 3.6ks at 1523K were 0.105~0.160 mass% and 0.33~0.89 mass%, respectively. And those in vacuum were 0.028~0.032% and 0.957~4.08%, respectively. Relative density(Ds) of Co+29%Cr+17%W+3.0%C compact containing 6%V and Co+32%Cr+20%W+2.97%C compact containing 0.03%B were 99 and 100%, respectively, indicating complete densification by solid phase sintering. Victors hardness of sintered compacts containing 6%V or 0.03%B were 632 and 568, showing 50~60% increase in comparison to those without V or B. These results can be explained in terms of oxidation/reduction of oxides and equilibrium pressure of CO in isolated pore, instead of presence of liquid formation and grain boundary separation from pores due to large grain growth.

  • PDF

절삭 공구용 세라믹의 소결조직에 따른 파괴인성과 경도의 평가 (Effect of Microstructure on Evaluation of Fracture Toughness and Hardness of Cutting Tool Ceramics)

  • 안동길;윤명진
    • 한국생산제조학회지
    • /
    • 제9권6호
    • /
    • pp.170-177
    • /
    • 2000
  • Dense $Al_2$O$_3$-30%TiC and Si$_3$N$_4$ ceramic tool materials with various grain size were produced by sintering-HIP treatment and by gas-pressure sintering. The fracture toughness was measured by indentation fracture and indentation strength method for both ceramics with various grain size. The effect of the grain size on the fracture toughness was evaluated, and the correlation between fracture toughness and mechanical properties such as hardness, Young\`s modulus and flexural strength of these ceramic were also investigated. The highest fracture toughness of around 6.7 MPa.m(sup)1/2 was obtained in Si$_3$N$_4$ ceramics with grain size of 1.58${\mu}{\textrm}{m}$. With a larger grain size of $Al_2$O$_3$-30%TiC and Si$_3$N$_4$ ceramics, the fracture toughness was generally increased. The increased fracture toughness of these ceramic also improved the flexural strength although the hardness decreased considerably. Similar results were obtained in grain size and mechanical properties on both $Al_2$O$_3$-30%TiC and Si$_3$N$_4$ ceramic tool materials.

  • PDF

티타늄 스크랩 재활용에 의한 고순도 분말 소결 기술 (Technology of High Purity Powder Sintering by Ti Scrap Recycling)

  • 최정철;장세훈;차용훈;오익현
    • 한국재료학회지
    • /
    • 제19권7호
    • /
    • pp.397-402
    • /
    • 2009
  • In this study, Ti powder was fabricated from Ti scrap by the Hydrogenation-Dehydrogenation (HDH) method. Hydrogenation reactions of Ti scrap occurred at near 450 $^{\circ}C$ with a sudden increase in the reaction temperature and the decreasing pressure of hydrogen gas during the hydrogenation process in the furnace. The dehydrogenation process was also carried out at 750 $^{\circ}C$ for 2hrs in a vacuum of $10^{-4}$ torr. After the HDH process, a deoxidation treatment was carried out with the Ca(purity: 99.5) at 700 $^{\circ}C$ for 2hrs in the vacuum system. It was found that the oxidation content of Ti powder that was deoxidized with Ca showed noticeably lower values, compared to the content obtained by HDH process. In order to fabricate Ti compacts, Ti powder was sintered at $1100\sim1400^{\circ}C$ for 2hrs under a vacuum of $10^{-4}$ torr. The relative density of compact was 94.9% at 1300 $^{\circ}C$. After sintering, all of the Ti compacts showed brittle fracture behavior, which occurred in an elastic range with short plastic yielding up to a peak stress.

자체반응열 고온합성법에 의한 질화티타늄 합성에 관한 연구 (A Study on the Synthesis of Titanium Nitride by SHS(Self-propagating High-temperature Synthesis) Method)

  • 하호;김광래;이희철
    • 한국세라믹학회지
    • /
    • 제30권12호
    • /
    • pp.1096-1102
    • /
    • 1993
  • Titanium nitride was synthesized by reacting Ti powder with nitrogen gas using SHS method. In this process, the effects of nitrogen pressure, dilution with TiN, or additiion of titanium hydride(TiH1.924) on the conversion of Ti to TiN were investigated. In particular, much effects were given to solve the problem of the conversion drop due to partial melting and subsequent sintering of Ti parciels, by controlling combustion temperature and combustion wave velocity via mixing Ti powder with TiN or/and TiH1.924. For the diluted titanium powders with TiN, the conversion close to 100% was resulted when the nitrogen pressure was over 8atm and with diluent content of 60wt%, and the self-propagating reaction was not sustained when the diluent content was higher than 60wt%. For samples mixed to be 55wt% in Ti component in the mixture of Ti, TiH1.924, and 45% TiN, the conversion was closed to 100% when the amount of titanium hydride added was over 7wt% and the nitrogen pressure was higher than 5atm. The combustion reaction, however, was not sustained when titanium hydride added was more than 10wt%.

  • PDF