• 제목/요약/키워드: Galvannealed steel

검색결과 62건 처리시간 0.037초

합금화용융아연코팅강판의 코팅층 접합강도 평가를 위한 단일 겹치기이음 시험의 적용 (Application of Single Lap-Shear Test for Extracting Adhesive Bonding Strength of Coating Layer on Galvannealed sheet)

  • 이정민;이찬주;이상곤;고대철;김병민
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2007년도 춘계학술대회A
    • /
    • pp.238-243
    • /
    • 2007
  • This paper is designed to estimate the adhesion strength of coating layer on galvannealed steel sheet using lap shear test. The single lap shear test is the most commonly used standard test for determining the strength of medium-strength and high strength bonds. The bond strength of bonded single lap joints on subjecting the substrates to loads is determined by lap shear forces in the direction of the bonded joint. In this study, specimen for adhesion strength test was made to attach coated sheet to cold rolled sheet and were heated in temperature of 180 for 20minutes. After test, detached parts of coatings on coated sheet were observed using SEM and EDX to identify substrate and complete detachment. The tested results showed that adhesive strength of coating is unrelated to anisotropy of sheet and is difficult to be extracted using conventional theory because of fine cracks of coating layers which were created during annealing process.

  • PDF

고강도 용융아연 도금강판의 파우더링 특성에 미치는 실리콘 및 합금화 열처리의 영향 (Effect of Silicon in Steels and Galvannealing Heat Cycles on Powdering Behavior of High Strength Galvannealed Steels)

  • 이호종;오용택;김종상
    • 한국표면공학회지
    • /
    • 제33권2호
    • /
    • pp.135-144
    • /
    • 2000
  • Hot-dip galvannealed sheet (GA) with high strength of $45kg/mm^2$ in tensile strength, has developed for automotive applications. However, for a successful application, the powdering behaviour of GA must be minimized. The powdering of galvannealed coatings was reduced as the silicon content in the steel increased. Rapid heating and rapid cooling rate during the galvannealing process improved the powdering resistance due to the suppression of not only the ξ phase, but also the $ \Gamma _1$, phase. An analysis of the Fe-Zn alloy phases and its relation to the powdering behaviour are discussed with SEM micrographs.

  • PDF

강판 합금화 용융아연도금용 2000kW-50kHz 유도가열 장치 개발 (Development of 2000kW-50kHz induction heating equipment for galvannealed sheet steel)

  • 유효열;심은용;강재봉;박형진;윤형진;윤형민;임진섭;이찬교
    • 전력전자학회:학술대회논문집
    • /
    • 전력전자학회 2008년도 하계학술대회 논문집
    • /
    • pp.338-341
    • /
    • 2008
  • Galvannealed Sheet Steel, which is being widely used in the automotive industry, is made by reheat after dip zinc galvanizing process. By this, A Fe-Zn alloy is created which enhance anticorrosive property and weldability. This paper describes basic design for 2000kW induction heating inverter system for galvannealling process and test result of 250kW inverter module which is used in parallel to form 2000kW inverter system.

  • PDF

합금화 용융 아연 도금강판의 온간 디프드로잉 성형성에 관한 연구 (A Study on the Warm Beep Drawabilities of Galvannealed Steel Sheet)

  • 장성호;최치수;최이천;서대교
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2000년도 추계학술대회 논문집
    • /
    • pp.168-173
    • /
    • 2000
  • The limiting drawing ratio (LDR) under uniform heating of blanks was measured at the various temperature ranges between 25 and $250^{\circ}C$ by using two different blank shapes, square and circular blanks, and six different blank sizes with the drawing ratios(DR) of 2.4 to 2.9. The galvannealed steel sheet (SCP3CM 60/60) of 0.7mm thickness was used. The LDR at warm forming condition reached 1.2 times of that at room temperature, and the maximum drawing depth reached 1.9 times. The higher temperature was adopted, the more stable and uniform thickness strain distribution was observed.

  • PDF

합금화 용융 아연 도금강판의 온간 딥드로잉 성형성에 관한 연구 (A Study on the Warm Deep Drawabilities of Galvannealed Steel Sheet)

  • 장성호;서대교
    • 소성∙가공
    • /
    • 제11권5호
    • /
    • pp.423-429
    • /
    • 2002
  • The limiting drawing ratio (LDR) under uniform heating of blanks was measured at the various temperature ranges between 25 and 25$0^{\circ}C$ by using two different blank shapes, square and circular blanks, and six different blank sizes with the drawing ratios(DR) of 2.4 to 2.9. The galvannealed steel sheet (SCP3CM 60/60) of 0.7mm thickness were used. The LDR at warm forming condition reached 1.2 times of that at room temperature, and the maximum drawing depth reached 1.9 times. The higher temperature was adopted, the more stable and uniform thickness strain distribution was observed. Some cases of the experimental results were compared with the analitical results using the commercial finite element method (FEM) code.