검색결과 122건 처리시간 0.021초

Dislocation densities of CMP processed sapphire wafers for GaN epitaxy

  • 황성원;남정환;신귀수;김근주;서남섭
    • 한국반도체및디스플레이장비학회:학술대회논문집
    • /
    • 한국반도체및디스플레이장비학회 2003년도 춘계학술대회 발표 논문집
    • /
    • pp.18-22
    • /
    • 2003
  • The sapphire wafers for blue light emitting devices were manufactured by the implementation of the surface machining technology based on micro-tribology. This process has been performed by grinding, lapping and polishing. The surfaces of sapphire wafers were mechanically affected by residual stress and surface default. This mechanical stress and strain can be cured by thermal anneal ing process. The sapphire crystalline wafers were annealed at $1100~1400^{\circ}C$ and then characterized by double crystal X-ray diffraction. The sample showed good quality of crystalline wafer surface wi th full width at hal f maximum of 16 arcsec for the 4-hour heat-treatment at $1300^{\circ}C$.

  • PDF

고전압 β-산화갈륨(β-Ga2O3) 전력 MOSFETs (High Voltage β-Ga2O3 Power Metal-Oxide-Semiconductor Field-Effect Transistors)

  • 문재경;조규준;장우진;이형석;배성범;김정진;성호근
    • 한국전기전자재료학회논문지
    • /
    • 제32권3호
    • /
    • pp.201-206
    • /
    • 2019
  • This report constitutes the first demonstration in Korea of single-crystal lateral gallium oxide ($Ga_2O_3$) as a metal-oxide-semiconductor field-effect-transistor (MOSFET), with a breakdown voltage in excess of 480 V. A Si-doped channel layer was grown on a Fe-doped semi-insulating ${\beta}-Ga_2O_3$ (010) substrate by molecular beam epitaxy. The single-crystal substrate was grown by the edge-defined film-fed growth method and wafered to a size of $10{\times}15mm^2$. Although we fabricated several types of power devices using the same process, we only report the characterization of a finger-type MOSFET with a gate length ($L_g$) of $2{\mu}m$ and a gate-drain spacing ($L_{gd}$) of $5{\mu}m$. The MOSFET showed a favorable drain current modulation according to the gate voltage swing. A complete drain current pinch-off feature was also obtained for $V_{gs}<-6V$, and the three-terminal off-state breakdown voltage was over 482 V in a $L_{gd}=5{\mu}m$ device measured in Fluorinert ambient at $V_{gs}=-10V$. A low drain leakage current of 4.7 nA at the off-state led to a high on/off drain current ratio of approximately $5.3{\times}10^5$. These device characteristics indicate the promising potential of $Ga_2O_3$-based electrical devices for next-generation high-power device applications, such as electrical autonomous vehicles, railroads, photovoltaics, renewable energy, and industry.