• 제목/요약/키워드: GTAW

검색결과 147건 처리시간 0.024초

Nd:YAG LB 와 GTA 를 of용한 핵연료봉의 Zircaloy-4 봉단용접특성에 관한 연구 (A Study on the Characteristics of Zircaloy-4 End Cap Welding of Nuclear Fuel Pin Using Nd:YAG LB and GTA)

  • 김수성;이정원;양명승;이영호
    • Journal of Welding and Joining
    • /
    • 제14권6호
    • /
    • pp.81-92
    • /
    • 1996
  • This study is to compare the weldability of Zircaloy-4 end cap of nuclear fuel pin using by GTA and Nd :YAG LB. The welding parameters which affect bead width and penetration depth have been investigated. The effect of joint geometry of end cap for GTAW and LBW has been studied and optimum conditions of Zircaloy-4 endcap welding have been found. Microstructures and microhardness of GTA and LB welded zones have been also compared.

  • PDF

Varestraint Test법에 의한 Al-Li합금의 용접성 평가 (An Evaluation on the Weldability of Al-Li Alloys by Varestraint Testing Method)

  • 김형태;이창배;신현식;서창제
    • Journal of Welding and Joining
    • /
    • 제14권6호
    • /
    • pp.48-57
    • /
    • 1996
  • The weldability of high purity aluminum-lithium binary alloys has been investigated using the Varestraint test. Autogenous GTAW (gas-tungsten-arc-welds) were run along specimens of different lithium concentration using three sets of welding parameters. Welding voltage was held constant at 10 volts. Welding current (70∼100 amps) and travel speed (23∼33 cm/min) were the parameter varied. Hot-tearing susceptibility varied with lithium content and exhibited a steep peak at 2.6 weight percent lithium. Depth of penetration increased with increasing heat input and lithium concentration. The susceptibility is influenced by the wettability of dendrites by the interdendritic eutectic liquid as well as the time available for back-Siting by eutectic liquid. The welding condition of welding current 70A and travel speed 23 cm/min was showed good resistance to cracking in aluminum-lithium alloys. Suggestions for improving weld cracking resistance are also provided.

  • PDF

STS 강의 $O_2$ 및 Al함량이 용접용입량에 미치는 영향 (Effect of $O_2$ and Al Coantent on the Weld Penetration)

  • 김희봉;김정호;이창희
    • Journal of Welding and Joining
    • /
    • 제15권3호
    • /
    • pp.65-78
    • /
    • 1997
  • The effect of $O_2$and Al contents and the variation of welding parameters such as arc currents, welding speed on the weld penetration was investigated. Examination of weld penetration using GTAW was accomplished in the ferritic STS410L and austenitic STS304. Good penetration could be controlled by the variation of $O_2$ and Al contents in STS304. However, influences of $O_2$ and Al contents on the ferritic STS410L are far less than those on the austenitic STS304. Welding parameters should be considered first before controlling $O_2$ and Al contents for a good penetration in ferritic STS410L. In the simulation study under the stationary heat sources, the results of simulation and experiment have a similar tendency.

  • PDF

조사연료봉 봉단마개의 레이저용접기술 (Technology of the End Cap Laser Welding for Irradiation Fuel Rods)

  • 김수성;이정원;고진현;이영호
    • Journal of Welding and Joining
    • /
    • 제21권6호
    • /
    • pp.20-25
    • /
    • 2003
  • Various welding methods such as Gas Tungsten Arc Welding(GTAW), magnetic force electrical resistance welding and Laser Beam Welding(LBW) are now available for end cap closure of nuclear fuel rods. Even though the resistance and GTA welding processes are widely used in manufacturing commercial fuel rods, they can not be recommended for the remote seal welding of fuel rods in the hot cell Facility due to the complexity of the electrode alignment, the difficulty in replacing parts in a remote manner and the large heat input for the thin sheath. Therefore, the Nd:YAG laser system using optical fiber transmission was selected for the end cap welding of irradiation fuel rods in the hot cell. The remote laser welding apparatus in the hot cell Facility was developed using a pulsed Nd:YAG laser of 500 watt average power with an optical fiber transmission. The weldment quality such as microstructure and mechanical strength was satisfactory. The optimum conditions of laser welding for encapsulating irradiation fuel rods in the hot cell were obtained.

소구경 분기배관 용접부의 피로강도에 미치는 용접부 형상 및 용접공정의 영향 (Influence of Welding Shapes and Welding Procedures on Fatigue Strength of Small Diameter Branch Welded Pipe Joint)

  • 백종현;김철만;김우식
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2003년도 추계학술대회
    • /
    • pp.1092-1097
    • /
    • 2003
  • S-N fatigue tests were conducted to investigate the fatigue strength of small diameter socket and butt welded joints made of carbon steels. Experimental parameters were pipe diameter, throat depth, shape of socket welds and welding procedure. Filler metals used in SMAW and GTAW procedure were E9016-G with diameter of 4.0 mm and ER70S-G with diameter of 2.4 mm. API 5L Gr.B pipes were adopted as a small diameter branch pipes. All socket fittings were machined from ASTM A105 carbon steel. Tensile strength was not affected by the welding procedure. Fatigue strength in socket weld joints increased with increasing pipe diameter, area of weld metal and weld leg length of pipe side.

  • PDF

가열주형 수평식연속주조법에 의한 Al-Si 합금 용접봉 제조 (The preparation of Al-Si alloy welding rod by the horizontal continuous casting process with the heating mold)

  • 김원태;김명한;이보영
    • Journal of Welding and Joining
    • /
    • 제12권3호
    • /
    • pp.101-108
    • /
    • 1994
  • The horizontal continuous casting process with the heating mold was adopted for fabricating defect-free 4043 Al alloy rods of 3.2m dia. with mirror surfaces. These rods were drawn into 2.4mm dia. rods for GTAW welding. The GTAW welding tests were carried out by use of these welding rods with 6061 Al alloy as a base metal. After welding, the X-ray tests, tensile strength tests, bending tests, and microstructural analysis of welded zone and HAZ were carried out. The results represented that the welding rods with good surfaces and welding properties could be made by the horizontal continuous casting, and followed by the drawing process.

  • PDF

가속기 저장링 삽입장치 진공 챔버의 용접 (The welding Characteristics of the Insertion Device Vacuum Chamber of PLS Storage Ring)

  • 최만호;한영진;김창균;정진화;권영각
    • Journal of Welding and Joining
    • /
    • 제17권4호
    • /
    • pp.32-38
    • /
    • 1999
  • PAL(Pohang Accelerator Laboratory) designed and manufactured a 5m-long straight vacuum chamber to adopt U7 undulator that is the first insertion device. Top and bottom plates of the vacuum chamber were made of Al alloy A5083-H321, and welded together by the GTAW welding. The leak rate is less than 1×{TEX}$10^{-10}${/TEX} torr·ℓ/s with negligible welding deformation. The pressure has been maintained below {TEX}$10^{-10}${/TEX} torr after installation. This paper reports the welding process and the method applied to achieve ultimate vacuum performance and t satisfy integrity of welds.

  • PDF

Inconel 617 GTA 용접조건에 따른 미세조직 특성 및 기계적성질 (The Microstructures and Mechanical Properties on the GTA Welding conditions of Inconel 617)

  • 최성부;이봉근;강정윤
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2005년도 추계학술발표대회 개요집
    • /
    • pp.171-173
    • /
    • 2005
  • Inconel 617 is a solid solution, nickel-chromium-cobalt-molybdenum alloy with an exceptional combination of high temperature strength and oxidation resistance. The combination of high strenth and oxidation resistance at temperatures over $1800^{\circ}F$ makes Inconel 617 an attractive material for such components as ducting, transition liners in both aircraft and gas turbine. In this study, the weldability and weldment characteristics of Inconel 617 are considered in GTAW associated with the two welding current and with back shielding gas using or not. After GTAW with 120A and 150A current, microstructures and hardness test, bending test, tensile test on room and elevated temperature for the determination of optical welding condition.

  • PDF