마찰교반용접의 현황 및 알루미늄 철도차량에의 적용 (Introduction of Friction Stir Welding and Its Application to Aluminum Rolling Stock)

  • 서승일
    • 한국철도학회:학술대회논문집
    • /
    • 한국철도학회 2003년도 춘계학술대회 논문집
    • /
    • pp.616-621
    • /
    • 2003
  • MIG or TIG welding has been the most popular welding process for joining aluminum alloy structures. However, porosity, hot crack and distortion were serious problems in inert gas fusion welding. Since FSW(Friction Stir Welding) was invented by TWI in 1991, it has been the powerful candidate for solving the problems of inert gas welding. In this paper, the principle and characteristics of FSW is introduced and its application to rolling stocks is presented to make basis for future development in production technology of aluminum rolling Stocks.

  • PDF

이종 알루미늄 합금 용접의 용융부 특성 연구 (Fusion Zone Characteristics of Dissimilar Aluminum Alloys Joining)

  • 박선홍;박병철;김영기;백웅률
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2007년 추계학술발표대회 개요집
    • /
    • pp.141-143
    • /
    • 2007
  • Increasing demand of using low weight materials in recent automotive trends has been the challenge to develop a sound welding of aluminum alloys. A heat treatable AA6082-T6 and a non-heat treatable AA5083-0 aluminum alloys were joined in this study. Investigations revealed that about 60 UTS will be reduced due to welding process. Fracture happened in the interface between fusion zone and base metal of top specimen where penetration is shallow. Therefore, lower welding torch angle produced the better strength which allows deeper penetration to the top specimen. PWHT at $560^{\circ}C$ for 2 hours can be used to return the original UTS of the specimens.

  • PDF

Effects of Defect Size on Crush Test Load of Butt Fusion Welded MDPE Pipes

  • Tun, Nwe Ni;Lai, Huan Sheng;Jeon, Gyu Min;Yoon, Kee Bong;Kil, Seong Hee
    • 에너지공학
    • /
    • 제24권4호
    • /
    • pp.55-62
    • /
    • 2015
  • It is expected that the size of welding defect affects the mechanical performance of welded medium density polyethylene (MDPE) pipe joints. In this study, butt fusion welded MDPE pipe joints with a single spherical or planar defect of various sizes were studied using experimental crush testing and also by finite element method. The crush test showed that the mechanical performance of crush was not affected by the size and geometry of a single welding defect when the defect size was increased to 45% of the pipe's wall thickness. The simulation results indicated that the effect of the single welding defect on the Von Mises stress distribution near the defect explained the reason of the test results.

The Effect of Weld Metal Copper Content on HAZ Cracking in Austenitic Stainless Steel welded with Al-brass

  • Lee, H.W.;Lee, J.S.;Choe, W.H.
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2005년도 춘계학술발표대회 개요집
    • /
    • pp.152-154
    • /
    • 2005
  • Austenitic stainless steel has good weldability but is sensitive to hot cracking such as solidification crack and liquation crack. In this study, the specimens of dissimilar metals made between austenitic stainless steel and Al-brass were welded by GTAW process using four different filler metals. Cracks were detected in the heat-affected zone of the stainless steel when welded with CuAl, CuSn and NiCu filler metals, but no cracks were detected a Ni filler metal was used. The cracks propagated along the grain boundary in the heat affected zone near the fusion line to base metal of 316L stainless steel. The cracks were located inside the weld bead with very fine hairline crack. All cracks initiated at the fusion line and moved forward in the base metal. From energy dispersion spectroscopy (EDS), Cu peak was detected only in the crack-opening area.

  • PDF

600MPa급 TRIP강의 $CO_2$ 및 Nd:YAG 레이저 용접부의 특성 (Characteristics of $CO_2$ or Nd:YAG Laser Welded 600MPa Grade TRIP Steel)

  • 한태교;김성준;이봉근;김대업;강정윤
    • Journal of Welding and Joining
    • /
    • 제24권1호
    • /
    • pp.56-63
    • /
    • 2006
  • The characteristics of $CO_2$ or Nd:YAG laser welded 600MPa ade TRIP steel was investigated. He or Ar gas was used as a shield gas in case of $CO_2$ laser welding, but the shield gas was not used in case of Nd:YAG laser welding. Bead on plate welding was performed with various welding conditions. Defects in the joints of both welding type occurred at 1.8m/min but were not observed over the welding speed of 2.1m/min in case of Nd:YAG laser welding. However, porosity occurred in $CO_2$ laser welding and the tendency of decreasing with the increase of welding speed. The hardness was the highest at heat affected zone near fusion zone as well as at the fusion zone and decreased on approaching the base metal. In a perpendicular tensile test to the weld line, all specimens that have been welded at optimum conditions were fractured at the base metal, and the tensile properties showed the rather higher than those of raw material. In a parallel tensile test, the strength of the joints was higher than that of the base metal. Elongation was found to be lower than that of the raw material. Forming height by Erichsen test and elongation were deeply related with the ratio of base metal/weld metal and the maximum hardness of the weld metal. Also porosity induced to decrease the strength and the elongation. The maximum formability was recorded at approximately 80% as compared with that of the raw material with the optimum condition.

하이브리드 용접과 레이저 용접에 의한 세립강 용접부의 미세조직변화에 관한 연구 (Microstructure Evolution of UFG Steel Weld by Hybrid and Laser Welding)

  • 동현우;이목영;안용식
    • 동력기계공학회지
    • /
    • 제14권3호
    • /
    • pp.58-63
    • /
    • 2010
  • A laser beam welding and an electric arc welding were combined, and the positive points of each welding method are drawn such as high speed, low thermal load, deep penetration, and high productivity. The fiber laser-MIG conjugated welding. namely the hybrid welding has been studied mainly for the automation industry of a pipeline welding. In this study, the MIG welding was combined with a fiber laser welding to make up the hybrid welding. The weld shapes, microstructures and mechanical properties for weld zones after the hybrid welding or only fiber laser welding were investigated on the 700 MPa grade Ultra Fine Grained(UFG) high strength steel. The amount of acicular ferrite in weld metals and HAZ(heat affected zone) was observed larger after hybrid welding compared with after only laser welding. The Vickers hardness of the top area of the fusion zone after fiber laser welding was higher compared with after hybrid welding.

싱글모드 파이버 레이저를 이용한 SUS304와 Cu의 고속 겹치기 용접에서 접합부 및 인장시험 파단부의 특성에 관한 연구 (A Study on the Characteristic of Weld Joint and Tensile Fracture of SUS304 and Cu High-Speed Dissimilar Lap Welds by Single Mode Fiber Laser)

  • 이수진;김종도;카타야마 세이지
    • Journal of Welding and Joining
    • /
    • 제32권6호
    • /
    • pp.56-63
    • /
    • 2014
  • To develop and understand dissimilar metals joining of Stainless steel and Copper, ultra-high speed laser lap welding was studied using single mode fiber laser in this study. SUS304 and Cu have large differences in materials properties, and Cu and Fe have no intermetallic compounds by typical binary phase of Cu and Fe system. In this study, ultra-high speed lap welds of SUS304 and Cu dissimilar metals using single-mode fiber laser was generated, and weldability of the weld fusion zone was evaluated using a tensile shear test. To understand the phenomenon of tensile shear load, weld fusion zone of interface weld area and fracture parts after tensile shear test were observed using scanning electron microscopy (SEM) and energy dispersive X-ray spectroscopy (EDX) analysis system. And it was confirmed that Cu was easily melting and penetrating in the grain boundaries of SUS304 because of low melting temperature. And high thermal conductivity of copper occurred dissipate heat energy rapidly. These properties cause the solidification cracking in weld zone.

소결체와 저탄소강의 레이저용접 특성에 미치는 입열량 및 용접부 성분변화의 영향 (Influence of Heat Input and Weld Bead Composition on Welding Property in the Laser Welding between Sintered Segment and Mild Steel Shank)

  • 정우광;조남준;김성욱;이창희;김승대;이주형;박화수
    • 한국재료학회지
    • /
    • 제14권6호
    • /
    • pp.425-431
    • /
    • 2004
  • A laser welding was applied between sintered tip of Fe-Co-W and low carbon steel shank for the diamond saw blade. The welding characteristics and formation of defects were investigated carefully for the weld fusion zone in different welding condition. Dendrite arm spacing in weld bead decreased with decrease of heat input. Co and W increased and Fe decreased in the weld fusion zone with increase of the heat input. The corresponding change of composition was observed with the change of beam position. The maximum and total length of crack decreased with increase of the heat input. The crack in weld bead was propagated along the dendrite boundary and was caused mainly by the segregation of constituent during the solidification.

Nd:YAG 레이저빔을 이용한 아연도금강판(SECC)과 쾌삭강봉(SUM24L)의 용접에 관한 연구 (Welding behavior between Zn-coated steel plate and free cutting carbon steel rod by Nd:YAG laser beam)

  • 노영태;김병철;김도훈;윤갑식
    • 한국레이저가공학회지
    • /
    • 제4권3호
    • /
    • pp.30-39
    • /
    • 2001
  • This work was tamed out to apply a laser welding technique in joining between a Zn coated low carbon steel plate(SECC) and a free cutting carbon steel shaft(SUM24L) with or without W coating. Experiments were carried out and analysed by applying the FD(factorial design)method to obtain the optimum Laser welding condition. Optical microscopy, SEM, TEM and XRD analyses were performed in order to observe the microstructures in the fusion zone and the HAZ. Mechanical properties of the welded specimens were examined by microhardness test, tensile test and twist test. There was no flawed Zn in the fusion zone by EDS analysis. This means that during the welding process, Zn gas could be eliminated by appropriate shielding gas flow rate and butt welding gap. Ni coating itself did not influence on the tensile strength and hardness. However, twist bending strength and the weld depth of the Ni-coated free cutting carbon steel were lower as compared with those of the uncoated free cutting carbon steel. It was attributed to a lower absorbance of laser beam to the shin Ni surface. According to the results of the factorial design tests, the twist bending strength of welded specimens was primarily affected by pulse width, laser power, frequency and speed.

  • PDF