• 제목/요약/키워드: Fracture Pressure

검색결과 889건 처리시간 0.034초

정수압이 탄소섬유/에폭시 복합재의 탄성일인자에 미치는 영향 (Effect of Hydrostatic Pressure on the Elastic Work Factor of Graphite/Epoxy Composites)

  • 이지훈;김만태;신명근;한운용;이경엽
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2003년도 춘계학술대회 논문집
    • /
    • pp.1390-1393
    • /
    • 2003
  • Work factor approach is conveniently used in metal fracture mechanics to determine fracture toughness from a single fracture test. In this work, we investigated the applicability of the work factor approach in order to determine fracture toughness of thick graphite/epoxy composites in the hydrostatic pressure environment from a single fracture test. The effect of hydrostatic pressure on the elastic work factor was studied, The stacking sequence used was multi-directional, [0$^{\circ}$/${\pm}$45$^{\circ}$/90$^{\circ}$]. The hydrostatic pressures applied were 0.1 MPa, 100 MPa, 200 MPa, and 300 MPa. The results showed that the elastic work factor was not affected by the hydrostatic pressure, The elastic work factor decreased in a linear fashion with crack length.

  • PDF

확률론적 파괴역학 기법을 이용한 압력관의 파손확률 평가 (Failure Probability Evaluation of Pressure Tube using the Probabilistic Fracture Mechanics)

  • 손종동;오동준
    • 한국안전학회지
    • /
    • 제22권4호
    • /
    • pp.7-12
    • /
    • 2007
  • In order to evaluate the integrity of Zr-2.5Nb pressure tubes, probabilistic fracture mechanics(PFM) approach was employed. Failure assessment diagram(FAD), plastic collapses, and critical crack lengths(CCL) were used for evaluating the failure probability as failure criteria. The Kr-FAD as failure assessment diagram was used because fracture of pressure tubes occurred in brittle manner due to hydrogen embrittlement of material by deuterium fluence. The probabilistic integrity evaluation observed AECL procedures and used fracture toughness parameters of EPRI and recently announced theory. In conclusion, the probabilistic approach using the Kr-FAD made it possible to determine major failure criterion in the pressure tube integrity evaluation.

Constraint-corrected fracture mechanics analysis of nozzle crotch corners in pressurized water reactors

  • Kim, Jong-Sung;Seo, Jun-Min;Kang, Ju-Yeon;Jang, Youn-Young;Lee, Yun-Joo;Kim, Kyu-Wan
    • Nuclear Engineering and Technology
    • /
    • 제54권5호
    • /
    • pp.1726-1746
    • /
    • 2022
  • This paper presents fracture mechanics analysis results for various cracks located at pressurized water reactor pressure vessel nozzle crotch corners taking into consideration constraint effect. Technical documents such as the ASME B&PV Code, Sec.XI were reviewed and then a fracture mechanics analysis procedure was proposed for structural integrity assessment of various nozzle crotch corner cracks under normal operation conditions considering the constraint effect. Linear elastic fracture mechanics analysis was performed by conducting finite element analysis with the proposed analysis procedure. Based on the evaluation results, elastic-plastic fracture mechanics analysis taking into account the constraint effect was performed only for the axial surface crack of the reactor pressure vessel outlet nozzle with cladding. The fracture mechanics analysis result shows that only the axial surface crack in the reactor pressure vessel outlet nozzle has the stress intensity factor exceeding the low bound of upper-shelf fracture toughness irrespectively of considering the constraint effect. It is confirmed that the J-integral for the axial crack of the outlet nozzle does not exceed the ductile crack initiation toughness. Hence, it can be ensured that the structural integrity of all the cracks is maintained during the normal operation.

반응표면법을 이용한 안전밸브의 최적화 (Optimal Design of the Safety Valve by Response Surface Method)

  • 이상우;신대영;변철웅
    • 한국전산구조공학회논문집
    • /
    • 제20권5호
    • /
    • pp.551-556
    • /
    • 2007
  • 소화시스템에 사용되는 고압의 소화가스 저장용기에는 저장용기의 파손을 막아주는 안전밸브가 있다. 이러한 안전밸브의 내부에는 원형 박판의 파열 판이 들어 있는데, 저장용기의 내압이 위험수준에 도달하면 파열 판이 파손하여 내압을 배출하는 역할을 한다. 안전밸브의 설계인자는 파열 판의 두께, 안전밸브의 유로 직경, 플라스틱 패킹 링의 내부 직경 그리고 파열 판을 고정하는 볼트 안쪽의 필렛 반경이 있다. 이중에서 파열 판의 두께는 0.2mm로 고정을 하였다. 요인배치법을 사용하여 주효과를 결정하였고 회귀방정식을 유도하였다. 이러한 회귀방정식은 추후 안전밸브의 설계에 있어서 기초 설계 자료로서 활용할 수 있도록 실험 결과와 비교하여 검증하였다. 검증실험 및 회귀방정식에 의한 결과의 오차는 약 $2{\sim}5%$ 정도인 것을 확인하였다. 그리고 반응표면법을 사용하여 기밀테스트 압력인 25MPa에서 파열할 수 있는 안전밸브의 최적 모델을 결정하였다.

정수압 조건에서 변형률 변화가 섬유강화 복합재의 층간분리인성에 미치는 영향에 대한 연구 (An investigation of the strain rate effect on the delamination toughness of fiber-reinforced composites in the hydrostatic pressure condition)

  • 하성록;이경엽;김현주;정동호
    • 한국정밀공학회지
    • /
    • 제22권11호
    • /
    • pp.99-103
    • /
    • 2005
  • It is generally accepted that fracture toughness of fiber-reinforced polymer composites is affected by strain rate in an atmospheric pressure condition. For a present study, the strain rate effect on the fracture toughness of fiber-reinforced laminated composites in the hydrostatic pressure condition was investigated. For this purpose, fracture tests have been conducted using graphite/epoxy laminated composites applying three steps of the strain rate at 270 MPa hydrostatic pressure condition. The strain rates applied were $0.05\%/sec,\;0.25\%/sec$, and $0.55\%/sec$. Fracture toughness was determined from the work factor approach as a function of applied strain rate. The result showed that fracture toughness decreased as the strain rate increased. Specifically, the fracture toughness decreased $12\%$ as the strain rate increased from $0.05\%/sec$ to $0.55\%/sec$.

압력용기용강의 고온파괴인성에 관한 연구 (A Study on HIGH TEMPERATURE FRACTURE TOUGHNESS of Pressure Vessel Steel SA516 at High Temperature.)

  • 박경동;김정호
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2001년도 춘계학술발표대회 개요집
    • /
    • pp.228-231
    • /
    • 2001
  • Elastic-plastic fracture toughness $J_{1c}$ can be used as an effective design criterion in elastic plastic fracture mechanics. Most of these systems are operated at high temperature and $J_{1c}$ values are affected by temperature. therefore, the $J_{1c}$ valuse at high temperature must be determined for use of integrity evaluation and designing of such systems. Elastic-plastic fracture toughness $J_{1c}$ tests were performed on SA516 carbon steel plate and test results were analyzed according to ASTM E 813-8, ASTM 1813-89. Safety and integrity are required for reactor pressure vessels vecause pthey are operated in high temperature. there are single specimen method, which used as evaluation of safety and integrity for reactor pressure vessels. In this study, elastic-plastic fracture toughness$(J_{1c})$ and $J-\Delta{a}$ of SA 516/70 steel used as reactor pressure vessel steel are measured and evaluated at room Temperature, $150^{\circ}C$, $250^{\circ}C$ and $370^{\circ}C$ according to unloading compliance method.

  • PDF

압력용기용 SA516/70강의 고온파괴인성평가 (Evaluation on High Temperature Fracture toughness of Pressure Vessel SA516/70 Steel)

  • 박경동;김정호;윤한기;박원조
    • 한국해양공학회지
    • /
    • 제15권2호
    • /
    • pp.99-104
    • /
    • 2001
  • Elastic-plastic fracture toughness $J_{lc}$ can be used as an effective design criterion in elastic plastic fracture mechanics. Most of these systems are$J_{lc}$ $J_{lc}$ value at high temperature must be determined for use of integrity evaluation and designing of such systems. Elastic-plastic fracture toughness $J_{lc}$ tests were performed on SA516/70 carbon steel plate and test results were analyzed according to ASTM E 813-87, ASTM E 813-89 and ASTM E 1152-87.safety and integrity are required for reactor pressure vessels because, they are operated in high temperature. There are single specimen method, which used as evaluation of safety and integrity for reactor pressure vessels. In this study, elastic-plastic fracture toughness($J_{lc}$) and J-$\Delta$a of SA 516/70 steel used as reactor pressure vessel steel are measured and evaluated at room temperature, 150$^{\circ}C $, 250$^{\circ}C $ and 370$^{\circ}C $ according to unloading compliance method.

  • PDF

정수압 환경에서 해수흡수된 Carbon-Epoxy 복합재의 기계적 특성 (Material Characteristics of Seawater-abrobed Carbon-Epoxy Composite under Hydrostatic Pressure Environment)

  • 이지훈;이경엽;박훈재;이상목
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2004년도 춘계학술대회
    • /
    • pp.406-409
    • /
    • 2004
  • In this study, we investigated compressive characteristics of seawater-absorbed carbon-epoxy composite under hydrostatic pressure environment. The hydrostatic pressures applied were 0.1 MPa, 100 MPa, 200 MPa, and 270 MPa. The results showed that the compressive elastic modulus increased about 10 % as the hydrostatic pressure increased from 0.1 MPa to 200 MPa. The modulus increased 2.3 % more as the pressure increased to 270 MPa. Fracture strength and fracture strain increased with pressure in a linear fashion. Fracture strength increased 28 % and fracture strain increased 8.5 % as the hydrostatic pressure increased from 0.1 MPa to 270 MPa.

  • PDF

인공슬롯을 고려한 수압파쇄 균열의 발전양상에 관한 연구 (The Analysis of Fracture Propagation in Hydraulic Fracturing using Artificial Slot Model)

  • 최성웅;이희근
    • 터널과지하공간
    • /
    • 제5권3호
    • /
    • pp.251-265
    • /
    • 1995
  • One of the most important matters in stress measurement by hydraulic fracturing technique is the determination of the breakdown pressure, reopening pressure, and shut-in pressure, since these values are the basic input data for the calculation of the in-situ stress. The control of the fracture propagation is also important when the hydraulic fracturing technique is applied to the development of groundwater system, geothermal energy, oil, and natural gas. In this study, a laboratory scale hydraulic fracturing device was built and a series of model tests were conducted with cube blocks of Machon gabbro. A new method called 'flatjack method' was adopted to determine shut-in pressure. The initial stress calculated from the shut-in pressure measured by flatjack method showed much higher accuracy than the stress determined by the conventional method. The dependency of the direction of fracture propagation on the state of the initial stresses was measured by introducin g artificial slots in the borehole made by water jet system. Numerical modeling by BEM was also performed to simulate the fracture propagation process. Both results form numerical and laboratory tests showed good agreement. From this study which provides the extensive results on the determination of shut-in pressure and the control of fracture propagation which are the critical issue in the recent hydraulic fracturing, it is conclued that in-situ stress measurement and the control of fracture propagation could be achived more accurately.

  • PDF

하중속도가 탄소섬유/에폭시 적층복합재의 층간분리인성에 미치는 영향 (Loading rate effect on the delamination toughness of carbon/epoxy composites)

  • 하성록;이경엽;김현주;정동호
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2005년도 춘계학술대회 논문집
    • /
    • pp.593-597
    • /
    • 2005
  • It is generally accepted that fracture toughness of fiber-reinforced polymer composites is affected by loading rate in an atmospheric presure condition. For a present study, the loading rate effect on the fracture toughness of fiber-reinforced laminated composites in the hydrostatic pressure condition was investigated. For this purpose, fracture tests have been conducted using carbon/epoxy composites applying three steps of the strain rate at 270 MPa hydrostatic pressure condition. The loading rates applied were 0.05%/sec, 0.25%/sec, and 0.55%/sec. Fracture toughness was determined from the work factor approach as a function of applied loading rate. The result showed that fracture toughness decreased as the loading rate increased. Specifically, the fracture toughness decreased 12% as the loading rate increased from 0.05%/sec to 0.55%/sec.

  • PDF