Influence of Deposition Conditions on the Adhesion of Sputter-deposited MoS$_2$-Ti Films

  • Kim, Sun-Kyu;Yongliang Li
    • Journal of the Korean institute of surface engineering
    • /
    • v.37 no.1
    • /
    • pp.1-4
    • /
    • 2004
  • MoS$_2$-Ti films were deposited on SKD-11 tool steel substrate by a D.C. magnetron sputtering system. The influence of deposition parameters on the adhesion of the films was investigated by the scratch test. Crosssection morphology was evaluated using FE-SEM. The plasma etching played an important role on the adhesion of the films. The appropriate etching conditions roughened the surface, resulting In the improved adhesion of the film. The adhesion of the film increased with the interlayer thickness up to 110 nm and then decreased slightly with further increasing of interlayer thickness. The adhesion was highest at a bias voltage of -50 V. Further increase of the bias voltage decreased the film adhesion.

Effects of Intermediate Layer in DLC Thin Film on Al2O3 for Improvement of High Temperature Strength

  • Ok, Chul-Ho
    • Transactions on Electrical and Electronic Materials
    • /
    • v.8 no.3
    • /
    • pp.125-130
    • /
    • 2007
  • DLC coating on ceramics is very useful for manufacturing the materials with hardness and low friction. Adhesion of DLC thin film on ceramics, on the other hand, is usually very weak. Adhesion of DLC film depends on many parameters such as contamination and chemical bonding between thin film and substrate. In this study, adhesion of DLC film on ceramics was improved by the intermediate layer when the plasma immersion ion deposition (PIID) technique was applied. It is found that the chemical composition and the thickness of intermediate layer have significantly an effect on the adhesion of DLC thin film on $Al_2O_3$.

The effects of Cu thin films sputter deposited at 5 and 100 mtorr on the adhesion between Cu/Cr film and polyimide (5, 100 mtorr의 증착압력에서 스퍼터 증착한 구리박막층이 Cu/Cr 박막과 폴리이미드 사이의 접착력에 미치는 영향)

  • 조철호;김영호
    • Journal of the Korean institute of surface engineering
    • /
    • v.29 no.3
    • /
    • pp.157-162
    • /
    • 1996
  • The effects of microstructural change on the adhesion strength between Cu/Cr film and polyimide have been studied. Cr films (50 nm thick) and Cu films (500 or 1000 nm thick) were deposited on polyimide by DC magnetron sputtering. During Cu deposition the Ar pressure was 5 or 100 mtorr. The microstructure was observed by SEM and the adhesion was measured by T-peel test. Plastic deformation of peeled metal strips was characterized quantitatively by using XRD technique. The film in which Cu is deposited at 100 mtorr has higher adhesion strength than the film in which Cu is deposited at 5 mtorr. And in the film with same deposition pressure of 100 mtorr, the adhesion strength is increased as the deposited thickness increases from 500 to 1000 nm. The adhesion change of Cu/Cr can be interpreted as the difference in plastic deformation.

  • PDF

Adhesion of Plasma Spray Coated Hydroxyapatite Film on the Two-Step Anodized Dental Implant

  • Choe, Han-Cheol
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2012.05a
    • /
    • pp.126-126
    • /
    • 2012
  • In this study, adhesion of plasma spray coated hydroxyapatite film on the two-step anodized dental implant was investigated. The plasma spray was carried out on the dental implant after two step anodization. The adhesion of coated HA film was investigated by FE-SEM after fatigue test. In the case of two-step anodized implant showed a good adhesion between implant and coated film.

  • PDF

Improvement of Adhesion Strength of DLC Films on Nitrided Layer Prepared by Linear Ion Source

  • Shin, Chang-Seouk;Kim, Wang-Ryeol;Park, Min-Seok;Jung, Uoo-Chang;Chung, Won-Sub
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2011.08a
    • /
    • pp.177-179
    • /
    • 2011
  • The purpose of this study is to enhance an adhesion between substrate and Diamond-like Carbon (DLC) film. DLC has many outstanding properties such as low friction, high wear resistance and corrosion resistance. However, it is difficult to achieve enough adhesion because of weak bonding between DLC film and the substrate. For improvement adhesion, a layer between DLC film and the substrate was prepared by dual post plasma. DLC film was deposited on nitrided layer by linear ion source. The composed compound layer between substrate and DLC film was investigated by Glow Discharge Spectrometer (GDS) and Scanning Electron Microscope (SEM). The synthesized bonding structure of DLC film was analyzed using a micro raman spectrometer. Mechanical properties were measured by nano-indentation. In order to clarify the mechanism for improvement in adhesive strength, it was observed by scratch test.

  • PDF

Study on the Adhesion of Diamond Like Carbon Films Using the Linear Ion Source with Nitriding Layers (Linear Ion Source에 의해 증착된 Diamond-Like Carbon(DLC) 박막의 질화층 형성에 따른 밀착력 특성 연구)

  • Shin, Chang-Seouk;Park, Min-Seok;Kwon, Ah-Ram;Kim, Seung-Jin;Chung, Won-Sub
    • Journal of the Korean institute of surface engineering
    • /
    • v.44 no.5
    • /
    • pp.190-195
    • /
    • 2011
  • Diamond-like carbon (DLC) has many outstanding properties such as low friction, high wear resistance and corrosion resistance. However, it is difficult to achieve enough adhesion on the metal substrates because of weak bonding between DLC film and the metal substrate. The purpose of this study is to enhance an adhesion of DLC film. For improving adhesion, the substrate was treated by active screen plasma nitriding before DLC film deposing. Nitrided substrates were investigated by Glow Discharge Spectrometer (GDS), Micro-Vickers Hardness. DLC films were deposited on several metals by linear ion source, and characteristics of the films were investigated using nano-indentation, Field Emission Scanning Electron Microscope (FESEM). The adhesion was measured by scratch tester. The adhesion of DLC films was increased when nitriding layer was formed before DLC deposition. Therefore, the adhesion of DLC film can be enhanced as increasing the hardness of materials.

Characteristics and Assessment of Printer Toner Adhesion (프린터 토너의 점착력 특성 및 평가 기법)

  • Lee, Jung-Eun;Kim, Kwang-Il;Kim, Hyun-Joon;Kim, Dae-Eun
    • Transactions of the Society of Information Storage Systems
    • /
    • v.5 no.2
    • /
    • pp.82-88
    • /
    • 2009
  • Understanding the adhesion behavior and characteristics of toner film is required to achieve image and text printing with high quality resolution. Toner can be considered as a thin film coating on a media such as paper or polymer film. Quantitative measurement of adhesion characteristics of the thin film is important to assess the reliability of the system. In this work the main objective was to investigate the adhesion characteristic between the toner and the media by ramp loading scratch test method. The scratch test may be used to obtain quantitative information about the adhesion of the film to the substrate. In the scratch test a diamond tip was used to scratch the surface of the toner film under an increasing normal load until the toner detached or fractured. The critical load (LC) was obtained from the experimental results. Also, the relationship between the critical load and the adhesive strength of the interface between the substrate and the toner was obtained by measuring the normal and tangential forces during the scratch test. Finally, theoretical analysis of the toner scratch characteristics was performed based on Benjamin and Weaver theory, Plowing model, and Laugier model.

  • PDF

Adhesion Characteristics between Stamp and Polymer Materials Used in Thermal Nanoimprint Lithography (열 나노임프린트 리소그래피에서 사용되는 스탬프와 폴리머 재료 사이의 점착 특성)

  • Kim Kwang-Seop;Kang Ji-Hoon;Kim Kyung-Woong
    • Tribology and Lubricants
    • /
    • v.22 no.4
    • /
    • pp.182-189
    • /
    • 2006
  • In this paper, the adhesion characteristics between a fused silica without or with an anti-sticking layer and a thermoplastic polymer film used in thermal NIL were investigated experimentally in order to identify the release performance of the anti-sticking layer. The anti-sticking layers were derived from fluoroalkylsilanes, (1H, 1 H, 2H, 2H-perfluorooctyl)trichlorosilane ($F_{13}-OTS$) and (3, 3, 3-trifluoropropyl)trichlorosilane (FPTS), and coated on the silica surface in vapor phase. The commercial polymers, mr-I 7020 and 8020 (micro resist technology, GmbH), for thermal NIL were spin-coated on Si substrate with a rectangular island which was fabricated by conventional microfabrication process to achieve small contact area and easy alignment of flat contact sur- faces. Experimental conditions were similar to the process conditions of thermal NIL. When the polymer film on the island was separated from the silica surface after imprint process, the adhesion force between the silica surface and the polymer film was measured and the surfaces of the silica and the polymer film after the separation were observed. As a result, the anti-sticking layers remarkably reduced the adhesion force and the surface damage of polymer film and the chain length of silane affects the adhesion characteristics. The anti-sticking layers derived from FPTS and $F_{13}-OTS$ reduced the adhesion force per unit area to 38% and 16% of the silica sur-faces without an anti-sticking layer, respectively. The anti-sticking layer derived from $F_{13}-OTS$ was more effective to reduce the adhesion, while both of the anti-sticking layers prevented the surface damages of the polymer film. Finally, it is also found that the adhesion characteristics of mr-I 7020 and mr-I 8020 polymer films were similar with each other.

A Molecular Simulation on the Adhesion Control of Metal Thin Film-Carbon Nanotube Interface based on Thermal Wetting (Thermal wetting 현상이 탄소나노튜브-금속박막 계면의 응착력에 미치는 영향에 관한 분자 시뮬레이션 연구)

  • Sang-Hoon Lee;Hyun-Joon Kim
    • Tribology and Lubricants
    • /
    • v.39 no.1
    • /
    • pp.8-12
    • /
    • 2023
  • This study presents a molecular simulation of adhesion control between carbon nanotube (CNT) and Ag thin film deposited on silicon substrate. Rough and flat Ag thin film models were prepared to investigate the effect of surface roughness on adhesion force. Heat treatment was applied to the models to modify the adhesion characteristics of the Ag/CNT interface based on thermal wetting. Simulation results showed that the heat treatment altered the Ag thin film morphology by thermal wetting, causing an increase in contact area of Ag/CNT interface and the adhesion force for both the flat and rough models changed. Despite the increase in contact area, the adhesion force of flat Ag/CNT interface decreased after the heat treatment because of plastic deformation of the Ag thin film. The result suggests that internal stress of the CNT induced by the substrate deformation contributes in reduction of adhesion. Contrarily, heat treatment to the rough model increases adhesion force because of the expanded contact area. The contact area is speculated to be more influential to the adhesion force rather than the internal stress of the CNT on the rough Ag thin film, because the CNT on the rough model contains internal stress regardless of the heat treatment. Therefore, as demonstrated by simulation results, the heat treatment can prevent delamination or wear of CNT coating on a rough metallic substrate by thermal wetting phenomena.

A Study on the Adhesion Property of Al-Cr Alloy Films by Evaporation (진공증착법으로 제조된 Al-Cr 박막의 밀착성에 관한 연구)

  • 주봉환;이규환;권식칠;백운승;임수근
    • Journal of the Korean institute of surface engineering
    • /
    • v.27 no.1
    • /
    • pp.19-28
    • /
    • 1994
  • A study on adhesion property of evaporated Al-Cr films was conducted on steel sheet by using two-source evaporator. Adhesion of Al-Cr coated steel was evaluated by tape test after $180^{\circ}$bending. Adhesion was decreased with increasing the Cr content in Al-Cr films. It was thought that the decrease in adhesion with increasing Cr content be related to insufficient wetting and diffusion of Cr atoms in the film. Best adhesion was achieved in the case of pure aluminum film..

  • PDF